Lyondellbasell Icorene 1761 Blk 9005 Polyethylene Linear Low Density Metallocene

LyondellBasell Icorene 1761 BLK 9005 Polyethylene, Linear Low Density, Metallocene

    • Product Name: LyondellBasell Icorene 1761 BLK 9005 Polyethylene, Linear Low Density, Metallocene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 515995
    Polymer Type Polyethylene, Linear Low Density, Metallocene
    Color Black
    Form Powder
    Processing Method Rotational Molding
    Density 0.935 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 3.5 g/10 min
    Tensile Strength At Yield 14 MPa
    Tensile Strength At Break 20 MPa
    Elongation At Break 700%
    Flexural Modulus 700 MPa
    Shore D Hardness 50
    Vicat Softening Temperature 110 °C
    Melting Temperature 124 °C
    Crystallization Temperature 106 °C
    Brittleness Temperature < -70 °C
    Environmental Stress Crack Resistance >1000 h
    Thermal Conductivity 0.35 W/m·K
    Specific Heat 1.9 J/g·°C
    Dielectric Constant 2.3
    Dielectric Strength 20 kV/mm
    Volume Resistivity >1e15 ohm·cm
    Water Absorption <0.01%
    Uv Stabilization Yes
    Ul 94 Flammability Rating HB
    Linear Mold Shrinkage 0.020 cm/cm
    Thermal Expansion Coefficient 1.5e-4 /°C

    As an accredited LyondellBasell Icorene 1761 BLK 9005 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged as pellets in sealed 25 kg polyethylene bags, 40 bags per pallet, totaling 1,000 kg net weight.
    Container Loading (20′ FCL) 20′ FCL container loading: LyondellBasell Icorene 1761 BLK 9005 metallocene linear low-density polyethylene, typically in 25 kg bags.
    Shipping LyondellBasell Icorene 1761 BLK 9005 is typically shipped as black metallocene LLDPE pellets in moisture-resistant 25 kg bags or bulk containers. It is non-hazardous, requiring no special placards. Keep dry, cool, and out of direct sunlight during transport; avoid contamination. Handle with standard PPE, prevent bag damage, and palletize securely for truck or container shipment.
    Storage Store LyondellBasell Icorene 1761 BLK 9005 in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizing agents. Keep original containers or bags closed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking. Use grounded handling equipment to control static. Maintain moderate ambient temperatures and follow local regulations and supplier guidance.
    Shelf Life Shelf life approximately 24 months when stored in original unopened packaging under cool, dry, well-ventilated conditions away from direct sunlight.
    Application of LyondellBasell Icorene 1761 BLK 9005 Polyethylene, Linear Low Density, Metallocene

    In rotational moulding of black potable water and utility tanks, LyondellBasell Icorene 1761 BLK 9005 linear low-density metallocene polyethylene is charged as a high-bulk-density powder that has been ambient-ground to a particle size distribution passing 35 mesh (500 µm), with less than 10% retained on 60 mesh (250 µm). The metallocene architecture permits sintering at a peak internal air temperature of 190 °C to 205 °C; below 185 °C inter-particle cohesion at mould parting lines is inadequate, while above 210 °C oxidative degradation and surface bubble formation occur in thick-walled sections. If the powder is stored in bulk bags at relative humidity above 60%, pre-drying at 60 °C to 70 °C for 1 h to 2 h reduces the risk of steam porosity in the sintered wall. No external colour masterbatch is required because the black 9005 formulation incorporates dispersed carbon black at a final wall content above 0.5% by mass, eliminating an additional let-down step and reducing contaminant load for water-contact parts. The formulation addition ratio for certified first-quality vessels is 100% virgin grade as supplied; internally generated regrind may be blended at 10% to 20% by mass when the regrind is segregated by lot, screened through 35 mesh, and validated for low-temperature tensile impact retention at -40 °C according to ASTM D1822. External release agents are avoided because they can raise extractables and interfere with certification compliance. Finished potable water tanks are qualified under NSF/ANSI/CAN 61 for ambient and hot-water extraction, while the base olefin polymer must satisfy FDA 21 CFR 177.1520(c) for repeated-use resin and, for EU-supplied vessels, Regulation (EU) No 10/2011 overall migration limits. Moulding is performed on biaxial carousel machines using cast-aluminium or fabricated steel moulds with inward-facing venting; heating in a forced-air recirculation oven at 280 °C to 320 °C is followed by forced-air cooling at 6 °C/min to 8 °C/min until demoulding at wall temperatures below 70 °C. Terminal components include vertical cylindrical storage tanks up to 50,000 L, conical-bottom process tanks for dosing and mixing, horizontal water transport tanks for skid mounting, and insulated buffer vessels for municipal well systems.

    When Polyethylene Tank Certification Collides with Fertilizer Compatibility Requirements

    Agricultural chemical storage and sprayer tanks made from Icorene 1761 BLK 9005 are designed around simultaneous resistance to environmental stress cracking and permeation of aqueous fertilizer salts, plant-protection products, and acidic or alkaline cleaning suspensions. The metallocene narrow short-chain branching distribution reduces the frequency of low-molecular-weight extractable species, but chemical compatibility is not inferred from resin type alone; coupon immersion tests under ASTM D543-21 for 30 days at 40 °C in the intended chemical formulation establish service limits for each product mix. The standard tank fabrication specification is ASTM D1998 for upright polyethylene storage tanks; where the vessel is installed as part of a pesticide application system, hydraulic proof testing and tank integrity verification are commonly aligned with ISO 16119 sprayer safety requirements. The addition ratio for the primary containment wall is maintained at 100% virgin Icorene 1761 BLK 9005 to preserve a minimum tensile elongation at break above 800% measured per ASTM D638-14 at 23 °C; regrind may be introduced only in secondary containment shells and non-load-bearing lids at up to 25% by mass, provided that the regrind is from the same base grade and the finished part passes a 300 h environmental stress crack resistance screen under ASTM D1693-21 Condition C. Downstream processing involves a closed-mould rotational moulding cycle with oven air temperature set between 290 °C and 310 °C, a mould rotation ratio of 4:1 primary-to-secondary axis speed, and a slow cooling ramp of 4 °C/min to 6 °C/min through the polyethylene crystallisation region to minimise internal stress. Fittings are spin-welded or hot-plate welded to the moulded shell, and each tank is pressure decay tested at 30 kPa to 50 kPa for leak detection before shipment. End products include broadacre sprayer tanks with capacities from 600 L to 8,000 L, fertigation batch tanks, chemical induction hoppers, nurse-trailer transports, and secondary containment basins with integrated sump detail.

    For off-highway diesel fuel reservoirs and hydraulic oil sumps, Icorene 1761 BLK 9005 is rotationally moulded at wall thicknesses between 5 mm and 10 mm where service temperatures may reach -30 °C. For non-metallic aboveground diesel storage tanks, the finished-component compliance path is UL 2258 for aboveground nonmetallic fuel tanks, with evaporative emission control governed in the United States by 40 CFR Part 1060 for nonroad fuel-system components; generator-set fuel tanks additionally require compatibility with diesel fuel containing up to 20% biodiesel by volume, with post-soak mass gain measured under ASTM D543-21 using fuel simulants. Where the tank is sold into California, permeation data are established under CARB TP-501-4 rather than inferred from base-resin density. The regrind addition ratio in fuel-contact walls is limited to 10% by mass because post-consumer or mixed-source regrind can carry incompatible fuel residues and increase permeation variability. The grade is supplied with carbon black but without an antistatic package; when diesel tanks are specified for hazardous-area use, static dissipative liners or external grounding points are installed instead of modifying the polyethylene formulation with conductive filler. Moulding is carried out with multi-part aluminium tooling and internal baffle inserts at a peak internal air temperature of 195 °C to 205 °C; after demoulding, bung openings are machined and fittings are spin-welded under axial load. Each tank is pressure decay tested at 20 kPa to 40 kPa and subjected to a 24 h diesel soak at 40 °C before release. Terminal products include day tanks for generator sets from 100 L to 5,000 L, hydraulic reservoirs for compact construction equipment, diesel transfer tanks for service vehicles, and remote fuel storage cubes. Published comparative permeation data for this specific metallocene LLDPE at variable regrind levels is limited; tank qualification therefore relies on formulation-specific fuel immersion and pressure decay testing.

    Marine Flotation Cell Wall Thickness and Buoyancy Retention

    Closed-cell hollow floats and aquaculture collar floats are rotationally moulded from Icorene 1761 BLK 9005 at wall thicknesses of 3 mm to 8 mm, with the black 9005 UV package specified for long-term sunlight exposure in salt-water service. The resin is processed without blowing agent; buoyancy derives from the sealed air cavity, and the moulded wall density is held below 0.942 g/cm³ to prevent the carbon black and stabiliser package from reducing net buoyancy margin. Industry compliance for solid-state marine flotation is referenced to ASTM F1755-22 where applicable, and cold-water mechanical requirements are verified through tensile elongation at break per ASTM D638-14 after 7-day immersion in 3.5% sodium chloride solution at 5 °C. The formulation addition ratio for marine floats is 100% virgin powder as supplied when the float must survive repeated impact against vessel hulls or concrete docks; regrind is limited to 10% by mass for non-structural buoyancy blocks, provided that low-temperature impact after 1,000 h xenon arc weathering per ISO 4892-2:2021 does not fall below 50% of the unweathered value. The downstream process includes rotational moulding with metal through-rod inserts for hinge or rope attachments, followed by optional post-mould injection of polyurethane foam into the hollow cavity through a transient vent hole; foam filling adds crush resistance but changes thermal expansion behaviour, so the polyethylene shell is moulded with a minimum wall thickness of 4 mm to resist foam exotherm pressure. Terminal products include cylindrical aquaculture pen collars, dredge pipe floats, fender floats for marinas and bridge pilings, and subsea cable buoyancy modules. Published industrial fatigue data for this specific marine float configuration is limited; project qualification therefore relies on front-loaded field trials or service-simulation testing rather than extrapolated laboratory values.

    What Limits Low-Temperature Ductility in Underground Utility Vaults?

    In underground utility pull boxes and splice vaults, the key service load is vertical AASHTO H-20 wheel loading combined with lateral soil pressure and sub-zero temperature exposure; once buried, the enclosure operates without continuous inspection. Icorene 1761 BLK 9005 parts are therefore designed against brittle crack initiation at wall transitions and load-bearing ribs when impacted at temperatures below -20 °C. The formulation addition ratio is set at 80% minimum virgin Icorene 1761 BLK 9005 by mass for northern-climate enclosures ordered with impact verification at -29 °C; processors permitted to use post-industrial regrind at 20% to 30% by mass for temperate regions must screen the blended powder and verify melt flow rate per ISO 1133-1:2022 to avoid a melt-flow shift that alters wall thinning at rib corners. The finished enclosure is evaluated under ANSI/SCTE 77-2017 for underground enclosure integrity, with proof load testing performed using a steel plate loaded to 22.7 kN or higher over a 305 mm × 305 mm footprint to simulate H-20 traffic. Moulding uses fabricated steel or cast-aluminium tooling with internal rib cavities and threaded brass inserts for racking; the critical process variable is the cooling step through the crystallisation region, which is controlled at ≤5 °C/min from the mould surface until the wall centre reaches 85 °C to prevent differential shrinkage at rib intersections. Demoulding at a wall temperature below 60 °C avoids residual stress cracking around inserts. Terminal products include pull boxes for telecom and power distribution, splice vaults with load-rated lids, valve and meter boxes for gas and water utilities, and equipment pads with internal conduit stubs. Published data on long-term creep behaviour of this specific metallocene LLDPE under continuous H-20 cyclic loading is limited; accelerated load testing at ambient temperature does not fully substitute for soil-burial creep validation.

    When the same metallocene LLDPE powder is selected for rotationally moulded pallet bins, bulk material hoppers and abrasion-resistant trays, the relevant performance variable shifts from chemical exposure to high-cycle fork-tine impact, point-load deflection and surface wear on concrete. Pallets and heavy-duty bins made from Icorene 1761 BLK 9005 are typically moulded at wall thicknesses of 6 mm to 12 mm, with top decks reinforced by kiss-off ribs to reduce flexural deflection under load. Industry compliance for pallet performance is evaluated according to ISO 8611-1:2021 for bending and corner-drop load classes; distribution simulation may also follow ASTM D4169-22 conditioning profiles. The addition ratio for indoor material handling bins is 100% as-supplied black grade; no external slip, antistatic or nucleating masterbatch is required. For outdoor or high-UV service where regrind content above 30% is introduced to lower moulding cost, a stabiliser refresh masterbatch at 0.5% to 1.0% by mass may be added only after the blended melt-flow rate is confirmed within ±15% of virgin material by ISO 1133-1:2022. Downstream processing uses biaxial rotational moulding with textured cavity surfaces for slip resistance and fork-entry pockets formed by mould-in steel cores; after cooling, flash around the fork pockets is routed and high-load surfaces may receive secondary machining. Terminal products include bulk feed and seed transport bins from 300 L to 3,000 L, stackable industrial hopper trays, pallet boxes for controlled-temperature logistics, and mineral aggregate or concrete batching bins that are replaced on an abrasion-wear interval rather than by chemical degradation.

    Free Quote

    Competitive LyondellBasell Icorene 1761 BLK 9005 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 1761 BLK 9005 is classified as a linear low density polyethylene produced via metallocene catalysis and supplied as a black rotational molding powder. The grade designation “BLK 9005” corresponds to an integrally compounded jet black color package rather than a separate carbon black masterbatch addition, which reduces dry-blend weighing error and pigment dispersion variation on the shop floor. The nominal melt flow rate is 4.5 g/10 min when measured at 190 °C under a 2.16 kg load according to ISO 1133-1:2022 or ASTM D1238-23a. The nominal density is 0.938 g/cm³ when determined to ISO 1183-1:2019 or ASTM D1505-18. Typical downstream uses include rotationally molded agricultural tanks, marine buoys, insulated transport boxes, recreational parts, and machinery covers where low-temperature ductility, moderate stiffness, and stress crack resistance are required. Compared with a conventional Ziegler-Natta LLDPE rotomolding resin of similar density and melt flow rate, the metallocene architecture creates a narrower molecular weight distribution and a more homogeneous comonomer sequence distribution. That molecular structure reduces the incidence of warpage and pinhole formation in thick sections, but it also narrows the processing window for peak internal air temperature because the temperature interval between complete densification and oxidation-induced embrittlement is compressed.

    How Does the Metallocene Catalysis Route Alter the Low-Temperature Impact and Warpage Behavior of Icorene 1761 BLK 9005?

    In conventional Ziegler-Natta LLDPE, the distribution of comonomer branches is biased toward the low-molecular-weight chains; the high-molecular-weight tail remains relatively homopolymer-like and crystallizes into stiff spherulites. In Icorene 1761 BLK 9005, the single-site catalyst places the comonomer more uniformly across the molar mass distribution. The resulting short-chain branch distribution increases the concentration of tie molecules between lamellae and suppresses the formation of large spherulites. The practical consequence is that a 6.0 mm rotationally molded wall can sustain higher strain before stress whitening at sub-zero temperature. Low-temperature impact is commonly screened by the Association of Rotational Molders International low-temperature impact method at -40 °C using a conditioned plaque; reported values for this product class are typically above 130 J, but the exact result depends on tool surface, cooling rate, and plaque thickness. Tensile yield stress is tabulated at 18 MPa to ISO 527-2:2012; elongation at break exceeds 800 % when specimens are extracted from a fully coalesced wall. The more uniform comonomer distribution also narrows the differential shrinkage between the outer and inner surfaces, which reduces corner-lift warpage in flat-sided parts compared with Ziegler-Natta grades of equivalent density. This is not a stiffness-dominated selection; flexural modulus is approximately 720 MPa to ISO 178:2019, placing the grade between a soft plastomer and a rigid high-density polyethylene rotomolding resin.

    On production-scale single-arm shuttle machines, the grade is processed with an oven air temperature range of 260 °C to 315 °C. The internal air temperature plateau is the primary control variable because the polymer surface temperature follows the tool metal temperature with a lag. A 4:1 biaxial rotation ratio and primary arm rotation near 8 min⁻¹ with secondary rotation near 2 min⁻¹ are typical starting points for a 1.2 m³ cubic steel tool producing a 6 mm nominal wall. Heating time is adjusted to hold the peak internal air temperature (PIAT) between 190 °C and 205 °C. At the lower boundary, densification is complete and the inner surface is smooth; below 185 °C, unfused powder may remain on the inner surface and tensile elongation can fall below 400 %. At the upper boundary, oxidative chain scission begins to compete with molecular weight growth. The cooling cycle should use forced air first, followed by mist or staged water spray, to keep the cooling rate below 10 °C/min through the crystallization range. Direct water quenching of thick sections increases residual stress and post-mold shrinkage. Powder stored at relative humidity above 60 % should be conditioned at 60 °C for 2 h before charging to reduce steam-induced pinholes.

    When Peak Internal Air Temperature Deviates Beyond the 190 °C to 205 °C Plateau

    Rotational molding grades made with metallocene catalysts exhibit a sharper melting transition, which is advantageous for short cycle time and inner-surface smoothness but disadvantageous for overheating tolerance. If the PIAT exceeds 210 °C, the inner surface can show gloss loss and micro-bubbles caused by volatile products from chain scission and degraded carbon black carrier resin. The oxidation induction time, measured to ASTM D3895-19 at 200 °C, is a more sensitive indicator than color in black compounds because carbon black masks yellowing. A drop in retained OIT below 10 min after one pass through the rotomolding oven indicates that the antioxidant package has been consumed and the part should not be regrind-blended at high levels. Conversely, a PIAT below 185 °C leaves the inner surface under-fused; instrumented impact testing then shows a wide scatter in peak force because the inner layer remains porous. In production practice, a two-stage internal air profile is sometimes used for thick-walled parts: a first plateau at 150 °C for 8 min to purge moisture and low-molecular-weight volatiles, followed by a second plateau at 195 °C until the bubble-elimination endpoint is reached. Mold release selection requires verification; silicone-based external releases are generally compatible, but amine-containing release agents should be avoided because amine residues can accelerate oxidative degradation at the polymer-air interface. The use of this grade in dry blends with high-density polyethylene rotational molding powder is possible, but blend ratios above 20 wt% HDPE tend to create visible flow lines on the inner surface because the metallocene matrix and the Ziegler-Natta HDPE have different zero-shear viscosities.

    The grade belongs to the olefin polymer class covered by FDA 21 CFR 177.1520(c) for food-contact use; however, the specific migration of carbon black and low-molecular-weight oligomers into food simulants must be confirmed against European Commission Regulation (EU) No 10/2011 for the intended food matrix and temperature. The supplier’s product data sheet and safety data sheet should be reviewed for lot-specific compliance. The material is not intended for continuous service above 60 °C in contact with strong oxidizing acids or for medical implant applications. Under normal handling, the carbon black in the 9005 color package provides ultraviolet protection, but weathering performance in outdoor service is also a function of part wall thickness, exposure geometry, and cleaning chemicals. For applications requiring a formal weatherability statement, a 10-year outdoor exposure claim cannot be made without data from ISO 4892-2 accelerated weathering or ISO 877-1 natural exposure testing on the finished part.

    Thermo-Mechanical Reference Data and Test Standard Matrix

    The values in the following matrix are typical values from the manufacturer’s technical bulletin, not specification limits. They are provided for material selection only and should be confirmed against the certificate of analysis for the specific lot because rotational molding powder properties can shift with storage and grinding history.

    PropertyTest MethodTypical Value
    Melt flow rate (190 °C, 2.16 kg)ISO 1133-1:2022 / ASTM D1238-23a4.5 g/10 min
    DensityISO 1183-1:2019 / ASTM D1505-180.938 g/cm³
    Tensile yield stressISO 527-2:2012 / ASTM D638-2218 MPa
    Elongation at breakISO 527-2:2012 / ASTM D638-22>800 %
    Flexural modulusISO 178:2019 / ASTM D790-17720 MPa
    Environmental stress crack resistance, 10% Igepal, condition BASTM D1693-15e1>1000 h
    Vicat softening temperature, A50ISO 306:2022 / ASTM D1525-17e1121 °C
    Peak melting temperatureISO 11357-3:2018 / ASTM D3418-21126 °C

    In direct comparison with high-density polyethylene rotomolding powder of density 0.950 g/cm³, Icorene 1761 BLK 9005 sacrifices approximately 25 % to 30 % of flexural modulus but extends the -40 °C ARM impact by a factor of 2 to 3 in thick sections. The environmental stress crack resistance is commonly an order of magnitude higher than an HDPE homopolymer of equivalent melt flow rate when measured to ASTM D1693-15e1. In comparison with a Ziegler-Natta LLDPE rotomolding grade, the metallocene grade produces less warpage in flat-sided tanks and a smoother inner surface at the same peak internal air temperature, but it is more sensitive to over-heating because the narrower melting range leaves less time for air release before oxidative degradation begins. The black 9005 compound has a lower net heat input requirement than a natural grade because carbon black absorbs infrared radiation; cycle time reductions should be validated with thermocouple and pressure-decay leak testing rather than by visual inspection alone.

    Powder dry flow and particle size distribution influence wall thickness uniformity. The grade is supplied as a ground powder; the apparent bulk density is typically between 0.48 g/cm³ and 0.52 g/cm³ when measured to ISO 60:2023, and the pourability through a 10 mm funnel orifice is commonly less than 35 s for 100 g. These values are not part of the specification but are monitored because a shift in dry flow alters the bed movement inside the rotating tool. A powder with excessive fines may build up in mold corners and produce thin spots; a powder with too coarse a cut may trap air and generate pinholes. The recommended ambient charging temperature is 15 °C to 35 °C. Below 10 °C, static charge increases and powder clumping can cause charge weight variation; above 40 °C, the powder may compact in the hopper and feed irregularly.

    Part design should avoid sharp inside corners with radii below 12 mm in 6 mm walls because the powder flow pattern leaves thin corners. Ribs and bosses should be designed with draft angles of 2° or more and a base radius of at least 0.8 times the nominal wall thickness to avoid stress concentration. The coefficient of thermal expansion of linear low density polyethylene, approximately 1.5 × 10⁻⁴ K⁻¹ in the solid state, must be accommodated in large flat panels; post-mold shrinkage in cooled parts ranges from 1.5 % to 2.5 % depending on mold material and cooling rate. Tool surface preparation affects the appearance of the black grade; a vapor-honed steel surface lowers gloss and conceals minor flow marks, while a chrome-plated surface raises gloss but magnifies surface defects. The black compound reaches higher surface temperatures under infrared heating than a natural grade; infrared pyrometry should therefore be used during cycle development to avoid exceeding the mold surface temperature limit of the tool material.

    Production-scale failure modes associated with this powder include inner-surface orange peel, pinholes at the bubble-release phase, and black specks caused by carbon black agglomerates. Orange peel is often traced to excessive primary arm speed or insufficient powder flow during the first rotation; reducing primary speed to 7 min⁻¹ and raising the mold surface temperature before charging can eliminate the defect. Pinholes are minimized by holding the PIAT plateau at 195 °C for at least 5 min and by using a slow initial heating ramp so that trapped air escapes before the inner surface seals. Black specks are not typical if the carbon black dispersion is above a 2.5 rating when evaluated by ISO 18553:2018 or equivalent microscopic dispersion analysis; the supplier controls dispersion to a finer level, but regrind containing foreign polymer should be screened with a 1.0 mm mesh before reuse.

    The metallocene LLDPE matrix resists dilute acids, alkalis, and polar solvents at ambient temperature. Immersion in strong oxidizing acids, chlorinated solvents, or aromatic hydrocarbons above 30 °C causes swelling and stress cracking; environmental stress crack testing to ASTM D1693-15e1 is a more discriminating selection tool than tensile strength for tanks holding detergent or agricultural chemicals. The grade should not be used for continuous storage of hydrocarbons above 40 °C without a permeation barrier, because linear low density polyethylene has higher permeation rates than high density polyethylene. For pressure-vessel service, long-term hydrostatic design data must be generated to ISO 9080:2012; published data for this specific rotational molding configuration is limited, and the supplier’s technical authority should be consulted before the material is used in a regulated pressure boundary.

    Top