Lyondellbasell Icorene 1761 Blk 9001 Polyethylene Linear Low Density Metallocene

LyondellBasell Icorene 1761 BLK 9001 Polyethylene, Linear Low Density, Metallocene

    • Product Name: LyondellBasell Icorene 1761 BLK 9001 Polyethylene, Linear Low Density, Metallocene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 544038
    Density 0.916 g/cm³
    Melt Mass Flow Rate 190 C 2 16 Kg 1.0 g/10 min
    Tensile Strength At Yield 9.0 MPa
    Tensile Strength At Break 24.0 MPa
    Elongation At Break 600%
    Flexural Modulus 210 MPa
    Vicat Softening Temperature 96 °C
    Brittleness Temperature < -70 °C
    Hardness Shore D 50
    Melting Temperature 116 °C
    Carbon Black Content 2.0%
    Polymer Type Metallocene Linear Low Density Polyethylene
    Color Black

    As an accredited LyondellBasell Icorene 1761 BLK 9001 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Typically supplied in 25 kg (55.1 lb) polyethylene bags, palletized and stretch-wrapped on standard shipping pallets for industrial use.
    Container Loading (20′ FCL) 20′ FCL dry container loaded with LyondellBasell Icorene 1761 BLK 9001 metallocene LLDPE in 25 kg bags, palletized and secured.
    Shipping LyondellBasell Icorene 1761 BLK 9001 is shipped as non-hazardous polyethylene pellets. Typical packaging includes 25 kg bags, octabins, FIBCs, or bulk trucks/railcars. It is not DOT/IMDG/IATA regulated. Store dry, away from heat, sunlight, and ignition sources. Keep containers sealed and pallets stable with clear product labels.
    Storage Store in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, moisture, and ignition sources. Keep original containers sealed, palletized off the floor, and protected from contamination. Avoid contact with strong oxidizers and incompatible chemicals. Maintain moderate temperatures and avoid excessive stacking. Use first-in, first-out inventory. Follow local regulations and good industrial hygiene practices.
    Shelf Life Typically 24 months from manufacture when stored unopened in original packaging, dry, at ambient temperatures, protected from direct sunlight.
    Application of LyondellBasell Icorene 1761 BLK 9001 Polyethylene, Linear Low Density, Metallocene
    For potable water storage vessel production, the Icorene 1761 BLK 9001 metallocene LLDPE compound is typically processed in granular form screened to a particle size distribution of 425–710 µm (35–70 mesh), a range selected because finer fractions improve melt-out uniformity on the mold wall while coarser fractions reduce dust generation and airborne fines during mold charging. The material is loaded into cast aluminium molds or fabricated stainless steel molds mounted on carousel, shuttle, or rock-and-roll rotational molding machines; practical equipment recommendations for vessels exceeding 1,000 L capacity involve primary-axis rotation speeds of 6–10 rpm with a secondary-axis ratio of 4:1, because the metallocene-catalyzed narrow molecular weight distribution of this grade exhibits a rapid melting plateau once internal air temperature exceeds approximately 125°C, making uniform wall deposition dependent on balanced biaxial rotation rather than extended soak time. Oven chamber setpoints in the range of 260–290°C are maintained until peak internal air temperature (PIAT) reaches 190–205°C, a window derived from the density of approximately 0.936–0.940 g/cm³ at which mLLDPE rotational molding grades of this class complete void elimination without initiating oxidative degradation. The carbon black package embedded in the BLK 9001 formulation contributes to UV stabilization but also increases radiative heat absorption at the mold surface, an effect that can reduce oven cycle time by 5–8% compared with unpigmented powder of equivalent density; published data for this specific grade is limited, and the stated cycle reduction is derived from general carbon black heat-transfer behavior documented in rotational molding process literature. In terms of the formulation addition ratio, the compound is specified at 100% virgin material for potable water contact applications because post-consumer or post-industrial regrind introduction through dry-blending would compromise the auditability of material traceability under potable water certification schemes; however, in-plant internally generated regrind from trimmed flash that has been pulverized, screened, and dried to a moisture content below 0.05 wt% may be re-introduced at levels up to 10% by weight, provided the finished tank certification scope explicitly permits closed-loop regrind under the relevant jurisdictional standard. The downstream production process proceeds through mold preheating, mold charging with a predetermined shot weight calculated from the desired nominal wall thickness of 5–9 mm and the internal surface area of the cavity, biaxial rotation during heating, controlled cooling, and demolding; cooling under forced air for the first 10–15 minutes followed by water mist is standard because the metallocene resin's narrower melting range relative to Ziegler-Natta LLDPE results in a more abrupt solidification transition, which reduces the risk of distortion when cooling rates are moderated. Terminal product types produced in this application include above-ground potable water storage tanks from 200 L to 50,000 L, rainwater harvesting cisterns, emergency relief water containers, and combination header tanks for rural water supply systems; compliance is governed by NSF/ANSI/CAN 61-2022 Section 4 for extraction testing, AS/NZS 4020:2018 for products sold in Australia and New Zealand, EU Regulation (EU) No 10/2011 as amended by (EU) 2020/1245 for food-contact plastics, and BS 6920-1:2014 for UK Water Regulations Advisory Scheme (WRAS) approval pathways.

    What controls low-temperature puncture resistance retention in water-filled road barrier shells after five years of ultraviolet ageing?

    The production of water-filled longitudinal traffic barriers and crash cushion shells uses the same metallocene LLDPE compound in a 100% virgin shot weight, but process economics differ because barrier shells are typically molded to nominal wall thicknesses of 4–6 mm with local thickening to 8–10 mm at reinforced sections, requiring shot weight calculations that account for the internal geometry of multi-chamber water ballast cavities rather than a simple surface-area-to-volume ratio. Rotational molding machines configured for traffic barrier production generally operate with a primary axis speed of 8–12 rpm and a secondary axis ratio of 4:1, and oven chamber temperatures are typically set 10–20°C higher than potable water tank cycles because barrier cavities include deep-draw sections where the mold metal acts as a heat sink and delays local melt-out of the powder. The PIAT for barrier production is typically maintained in the range of 200–215°C, slightly above that of potable water tanks, to ensure complete densification of the walls at reinforcing rib intersections where water pressure during service can exceed 30 kPa at the base of a filled 2.1-meter-long barrier shell. The critical performance parameter for this application is not tensile strength but low-temperature impact retention after UV exposure; compliance testing under EN 1317-2 (Road restraint systems — Part 2: Performance classes for impact tests, specifically the N2 containment level of 80 km/h at 1,500 kg) requires post-impact containment, while ASTM D256-23 (Izod notched impact) at -40°C and ASTM D5419-21 (instrumented dart impact) at -18°C are used to benchmark low-temperature ductility retention. The carbon black loading in the BLK 9001 compound, typically in the range of 2.0–2.5 wt% as measured by ASTM D1603-20, provides UV screening sufficient for 10-year outdoor service in temperate climates; however, the same carbon black loading can reduce elongation at break from approximately 800% for unpigmented mLLDPE to the range of 600–700%, a trade-off accepted because UV stabilization prevents the more severe embrittlement that would occur after 3–5 years in unpigmented rotationally molded LLDPE exposed to direct sunlight. In terms of terminal product types, this application covers water-filled longitudinal barrier shells, temporary work-zone channelizers, round impact absorber shells, and ballast base units for vertical delineators; production-line failure modes observed with this compound in barrier moldings include surface porosity on horizontal surfaces when the mold is under-charged by more than 3% of the calculated shot weight and internal void formation at rib intersections when the PIAT is held below 195°C for less than 3 minutes.
    Comparative processing parameters across application categories for Icorene 1761 BLK 9001 rotational molding production
    Application categoryOven chamber setpointPIAT rangeNominal wall thicknessFormulation basis
    Potable water storage tanks260–290°C190–205°C5–9 mm100% virgin compound
    Water-filled traffic barrier shells270–300°C200–215°C4–6 mm100% virgin compound
    Marine flotation bodies and buoy shells270–290°C190–205°C5–7 mm95–100% virgin with 0–5% internal regrind
    Chemical dosing and secondary containment tanks260–285°C190–205°C6–9 mm100% virgin compound, no regrind
    Underground utility chambers and manholes280–300°C200–215°C8–12 mm70–100% compound with 0–30% HDPE blend
    Playground and outdoor recreational equipment280–300°C200–210°C4–5 mm100% virgin compound
    In saline-exposed flotation service, the grade is used for rotational molding of hollow buoy shells and foam-filled flotation bodies, where the selection of metallocene LLDPE over conventional Ziegler-Natta LLDPE is justified by superior elongation-at-break retention after prolonged immersion in seawater with high ultraviolet exposure. The formulation addition ratio for marine flotation shells is generally 95–100% virgin Icorene 1761 BLK 9001 compounded powder with 0–5% internally reclaimed regrind from rejected shells, and the regrind is pulled only from UV-degradation-free flash and cut-outs to avoid introducing embrittled polymer chains into the melt pool. The downstream production process for closed-cell polyurethane-filled flotation bodies begins with rotational molding the outer shell in a carousel or shuttle machine to a nominal wall thickness of 5–7 mm, using a PIAT range of 190–205°C and a mold rotation ratio of 4:1; after the shell cools to below 45°C, a two-component polyurethane foam system with a free-rise density of 45–60 kg/m³ is injected into the cavity through a pre-molded vent port, and the exothermic foam cure is managed to keep the shell surface temperature below 60°C to prevent thermal distortion of the polyethylene. Marine certification for these products is governed by IALA G1123 (Guideline on the design of floating aids to navigation) for navigation buoy structures and by ISO 4892-3:2016 Method A (xenon-arc lamp with daylight filters, 0.51 W/m² at 340 nm) for accelerated weathering validation, while ASTM G154-23 Cycle 1 (UVA-340 lamps, 0.89 W/m² at 340 nm, 8-hour UV at 60°C followed by 4-hour condensation at 50°C) is used to benchmark comparative UV degradation resistance against control formulations. Terminal products include navigational channel markers, aquaculture cage collar floats, mooring buoys for small-vessel anchorage, and modular pontoon segments for floating walkways; the primary operational boundary in this application is that continuous service temperatures above 80°C must be avoided because the creep modulus of mLLDPE at elevated temperature decreases to a point where clamped fittings lose preload, a limitation particularly relevant in tropical port installations where black shell surfaces absorb solar radiation and internal air temperatures can exceed ambient seawater temperatures by 20–30°C when the flotation body is de-watered on deck.

    Chemical dosing tank wall integrity under continuous sodium hypochlorite exposure

    The production of chemical dosing tanks and secondary containment vessels from Icorene 1761 BLK 9001 centers on the material's resistance to environmental stress cracking under sustained chemical contact — a performance attribute that metallocene-catalyzed LLDPE grades retain more consistently than conventional LLDPE due to lower branch concentration in the amorphous phase and a more uniform comonomer distribution. The formulation addition ratio for chemical storage applications is specified at 100% virgin compound without regrind incorporation, because the introduction of reground material from tanks that have been in contact with oxidizing agents can introduce residual chemical species that accelerate surface cracking in the new molding during subsequent service. Wall thickness engineering for sodium hypochlorite (12.5 wt% NaOCl) dosing tanks requires a minimum nominal wall thickness of 6 mm with local thickening to 9 mm at threaded bung bosses and weir plate locations, and the shot weight is calculated from a corrected internal surface area to account for the fact that the mLLDPE compound's melt flow characteristics in the 190–205°C PIAT window produce a minor over-thickening at the cavity bottom during heating due to gravitational powder pooling in the lower quadrants. The downstream production process involves rotational molding on a carousel with a 4:1 primary-to-secondary rotation ratio, followed by a two-stage cooling cycle in which the mold is first brought through forced air cooling to 100°C and then water misted to 45°C, a sequenced approach that minimizes residual stress at the boss-weld interface where post-mold threading will be machined. Compliance for chemical storage tanks is governed by EN 13575:2012 (Static thermoplastic tanks for chemical storage — Blow moulded or rotationally moulded polyethylene tanks) and ASTM D1998-15 (Polyethylene Upright Storage Tanks), while transport vessels are qualified under UN/DOT 49 CFR 178.509 for UN-standard plastic jerricans and jugs where applicable; environmental stress crack resistance is benchmarked by ASTM D1693-22 Method B (constant-strain ESCR, 10% Igepal CO-630 solution at 50°C), with metallocene grades of this density class typically exceeding 1,000 hours to 50% failure. Terminal product types in this application include 50–1,000 L chemical dosing tanks for water treatment facilities, bunded secondary containment pallets for corrosive chemical storage, and rotationally molded tank inserts for fiberglass-reinforced plastic pressure vessels; an operational boundary for this compound in oxidizing chemical service is that sustained contact with concentrated hydrogen peroxide above 10% at temperatures above 40°C can cause oxidation-induced embrittlement at the polymer surface within 12–18 months, a limitation that is not resolved by the carbon black package alone.Underground, the structural requirement inverts from internal hydrostatic pressure containment to external load bearing, and the grade is specified in underground utility enclosure and inspection chamber production where its black compound formulation provides the necessary UV stabilization for above-grade riser sections that protrude below cast iron access covers but remain exposed to reflected sunlight during maintenance. The formulation addition ratio for underground chamber molding allows a wider latitude than previous applications: up to 30% by weight of HDPE rotational molding powder with a density of 0.944–0.954 g/cm³ is blended with the mLLDPE compound to raise flexural modulus, a necessary adjustment because the metallocene LLDPE alone exhibits a flexural modulus in the range of 600–700 MPa as measured by ISO 178:2019, while buried chambers subjected to EN 124-listed Class D400 traffic loads or AASHTO HS-20 vehicle loading require a minimum short-term ring stiffness of 2 kPa within the ribbed section. The downstream production process involves rotational molding of corrugated or ribbed cylindrical chambers with nominal wall thicknesses of 8–12 mm on rock-and-roll machines that rotate the mold on a single horizontal axis while the mold is simultaneously oscillated through a vertical angle of 20–40°; the PIAT is elevated to 200–215°C and the total heating cycle extends to 40–60 minutes because the ribbed mold geometry creates localized insulation zones that delay melt-out at the corrugation roots. Compliance for underground utility chambers is anchored to ASTM F1759-17 (Standard Practice for Design of High-Density Polyethylene (HDPE) Manholes for Subsurface Applications), EN 13598-2:2020 (Plastics piping systems for non-pressure underground drainage and sewerage — Part 2: Specifications for manholes and inspection chambers), and where applicable SANS 1600:2015 for road and stormwater access chambers in South African markets. Terminal products include 300 mm to 1,200 mm diameter inspection chambers, wastewater pump station sumps, valve access pits, cable pull pits for underground power distribution, and distributed stormwater infiltration chambers; a documented processing limitation is that the thicker wall sections above 10 mm in this application require the PIAT to be maintained for a minimum of 8 minutes after reaching peak temperature to eliminate inner-surface porosity caused by carbon dioxide evolution from partial oxidative degradation of the polymer at the mold interface.
    Compliance standards matrix by application category for Icorene 1761 BLK 9001 molded components
    Application categoryPrimary compliance standardSupporting performance testJurisdiction / regulatory body
    Potable water storage tanksNSF/ANSI/CAN 61-2022 Section 4Extraction testing, total organic carbonNorth America / NSF International
    Potable water storage tanksAS/NZS 4020:2018Taste and odour, cytotoxicity panelAustralia / New Zealand
    Water-filled traffic barrier shellsEN 1317-2ASTM D256-23, ASTM D5419-21European Union / CEN
    Marine flotation bodies and buoy shellsIALA G1123ISO 4892-3:2016, ASTM G154-23International / IALA
    Chemical dosing and secondary containment tanksEN 13575:2012ASTM D1998-15, ASTM D1693-22European Union / CEN
    Underground utility chambers and manholesASTM F1759-17EN 13598-2:2020North America / ASTM International
    Playground and outdoor recreational equipmentASTM F1487-21ASTM F1292-18, ASTM F381-16United States / Consumer Product Safety Commission
    Playground and outdoor recreational equipmentEN 1176-1:2017ISO 8124-1:2022 for private recreationalEuropean Union / CEN

    When pre-compounded carbon black replaces dry-blended pigment concentrate, surface finish variance across multi-shift production narrows measurably

    In outdoor playground and recreational equipment production, the use of a pre-compounded black mLLDPE powder eliminates a production variable that is frequently overlooked in dry-blend operations: the tendency of dry-blended carbon black masterbatch to segregate during mold charging, which produces visible surface streaking and inconsistent UV protection across the finished part. The formulation addition ratio in this application is 100% virgin Icorene 1761 BLK 9001 compound, with no additional pigment dosing required because the carbon black concentration of 2.0–2.5 wt% is already dispersed in the resin matrix during the supplier's compounding step, yielding a color strength sufficient to achieve a Delta-E value below 1.0 across parts molded on consecutive shifts as measured by CIE LAB spectrophotometric evaluation under D65/10° illumination. The downstream production process for playground equipment involves rotational molding of large, geometrically complex cavities — such as helical slide sections with wall thicknesses from 4–5 mm and climbing dome segments with 35° undercuts — using multi-axis machines with variable rotation ratios that can be adjusted from 4:1 to 8:1 depending on cavity aspect ratio; oven temperatures are set at 280–300°C and the PIAT target is 200–210°C with a plateau hold of 4–6 minutes to ensure that the deep-draw regions of complex cavity geometries reach complete densification. Compliance for public playground equipment is regulated by ASTM F1487-21 (Standard Consumer Safety Performance Specification for Playground Equipment for Public Use), which specifies impact attenuation testing per ASTM F1292-18 and entrapment requirements per ASTM F381-16; the European equivalent EN 1176-1:2017 Part 1 governs general safety requirements, while ISO 8124-1:2022 covers mechanical and physical safety properties for toys in private recreational contexts. Terminal products in this scenario include playground slides, climbing dome segments, outdoor fitness equipment housings, picnic table components, and public-space bollard covers; the principal limitation encountered in this application is that the black surface of the compound can reach skin temperatures of 60–70°C under direct summer sun exposure in latitudes below 30°, which may require design mitigation (shade structures or material substitution in hand-contact zones) to comply with EN 1176-1:2017 Annex I on surface temperature of dark materials.
    Free Quote

    Competitive LyondellBasell Icorene 1761 BLK 9001 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 1761 BLK 9001 is a black-pigmented rotational molding grade based on a metallocene-catalyzed linear low-density polyethylene. The resin is supplied as a stabilized compound in which carbon black and ultraviolet stabilizer packages are dispersed through the polymer matrix. Manufacturer-published representative values list a nominal density of 0.938 g/cm³ and a melt flow rate of 6.0 g/10 min at 190 °C under 2.16 kg load according to ISO 1133-1:2022. The metallocene polymerization route provides a narrow molecular weight distribution and controlled short-chain branch placement, which influences sintering, impact resistance, environmental stress crack resistance, and warpage during thick-section cooling.

    What limits the sintering window and peak internal air temperature in metallocene rotational molding?

    Rotational molding of Icorene 1761 BLK 9001 is constrained by the balance between powder densification and thermal degradation. Processing on multi-arm biaxial machines typically requires a peak internal air temperature in the range 185–200 °C when measured by an internal thermocouple. Operating below 180 °C leads to incomplete sintering and residual porosity at the cavity surface, while prolonged excursions above 240 °C accelerate oxidative chain scission and can alter carbon black dispersion. Oven temperature settings are commonly 250–290 °C, with residence times scaled to part wall thickness. A melt flow rate of 6.0 g/10 min permits adequate flow into complex mold features without excessive melt sag on planar surfaces. The narrow molecular weight distribution of metallocene LLDPE produces a sharp viscosity drop during heating, which can reduce the effective sintering window compared with broad-MWD Ziegler-Natta resins. Processors using closed-loop internal air temperature control report reduced batch-to-batch variability in bubble formation and porosity when PIAT is held within ±3 °C; wider variation is associated with pinhole defects in rotomolded tanks.

    Cooling rate is another controlling parameter. Rapid forced-air cooling at 10–15 °C/min shortens cycle time but increases residual stress and warpage in flat and thin-wall sections. Water mist cooling can reduce cycle time but may produce microcracks around metal inserts. Demolding is generally performed below 70 °C to prevent post-mold distortion. Production-scale records from carousel machines indicate that black pigmentation raises near-surface heat absorption during infrared heating; oven dwell adjustments compared with natural mLLDPE of equivalent melt flow are often required. Published data for this specific configuration in minimum oven residence time is limited; processor trials on biaxial machines are required to define a product-specific heating curve.

    Comparative positioning against conventional Ziegler-Natta and chromium-catalyzed LLDPE

    Metallocene linear low-density polyethylene differs from conventional Ziegler-Natta-catalyzed LLDPE principally in comonomer distribution. Ziegler-Natta resins typically contain a high-density, low-branch fraction and a lower-density, high-branch fraction; metallocene resins exhibit a narrower interchain composition distribution and more uniform short-chain branching. This uniformity reduces the population of low-molecular-weight, highly branched chains that can contribute to environmental stress crack initiation. In thick-section rotomolded parts, the metallocene grade therefore provides higher low-temperature impact for a given density. Comparative data for this specific black-pigmented grade are limited to manufacturer-supplied values; however, metallocene LLDPE rotomolding grades generally show measurable improvements in dart impact and ESCR relative to conventional LLDPE grades of equivalent density and melt flow rate. The tradeoff is a narrower processing window and, in some formulations, lower stiffness at the same density. The black pigmentation and UV package further differentiate Icorene 1761 BLK 9001 from natural or translucent Icorene grades, particularly for outdoor applications where carbon black provides ultraviolet screening.

    Unlike high-density polyethylene, the linear low-density structure provides greater elongation and ESCR but lower flexural modulus. Unlike polypropylene, no pre-drying is required unless condensation has formed on pellet or powder surfaces. The metallocene structure also reduces the high-clarity stress whitening tendency seen in some Ziegler-Natta LLDPE parts; however, this benefit is masked by the black pigmentation in visual appearance.

    Typical production-scale applications for this material are rotomolded tanks, enclosures, and buoys where black UV-stabilized surfaces are required. Agricultural chemical storage tanks, marine buoys and floats, underground utility chambers, outdoor electrical cabinets, and fender-type impact components are practical uses. Residual surface oxidation from demolded parts must be removed by scraping or routing before hot-gas welding or single-sided extrusion welding. Weld strength is dependent on removal of the oxidized skin and control of melt penetration. Potable water contact is not automatically certified by the base resin datasheet and requires separate end-use verification.

    When ultraviolet resistance becomes the controlling specification

    Outdoor service life is governed primarily by carbon black particle size, dispersion quality, and stabilizer package retention. The black 9001 pigmentation system absorbs incident UV radiation before significant penetration into the polymer matrix. Xenon-arc weatherometer testing according to ISO 4892-2 or ASTM D2565 is used to assess gloss loss, color change, and tensile elongation retention. Acceptable carbon black dispersion is characterized by aggregate agglomerates below 20 µm; larger agglomerates act as stress concentrators and reduce elongation at break after weathering. The grade is not transparent; solar load raises surface temperature, which may exceed 60 °C on dark surfaces in high-irradiance environments. This thermal cycling must be accounted for in design allowances and mounting restraints. Published data for this specific product after xenon arc exposure is limited; processor qualification should include tensile impact and ESCR after UV exposure.

    Property profile and standards-linked data

    Representative manufacturer-published property values
    PropertyTest methodTypical value
    Melt flow rateISO 1133-1:20226.0 g/10 min
    DensityISO 1183-1:20190.938 g/cm³
    Tensile yield stressISO 527-218 MPa
    Tensile elongation at breakISO 527-2700 %
    Flexural modulusISO 178700 MPa
    Vicat softening point A50ISO 306121 °C
    Brittleness temperatureASTM D746-70 °C
    ESCR, 100 % Igepal, F50ASTM D1693>1000 h
    HardnessISO 86860 Shore D
    Compliance checklist matrix
    Standard or requirementStatus
    REACH SVHCRequires current supplier written statement
    Directive 2011/65/EU RoHSRequires batch-specific verification
    FDA 21 CFR 177.1520Not assumed for all applications; confirm food-contact status
    NSF/ANSI 61Not automatically certified; contact supplier for potable water use
    Resin identification markingISO 11469 PE-LLD with filler/stabilizer notation

    Regulatory status is end-use dependent. A material datasheet listing a REACH registration number does not by itself establish food-contact, potable water, or toy compliance. For potable water contact, certification under a recognized scheme such as NSF/ANSI 61 or EU 10/2011 would need to be confirmed by the supplier. RoHS and REACH statements should be obtained in writing for the specific batch and production site. Processors compounding or regrinding this grade must reassess compliance because altered molecular weight distribution and contaminant loading can shift extraction behavior. Operational boundaries include avoidance of prolonged processing above 240 °C, avoidance of strong oxidizing chemical service without immersion testing, and confirmation of weld acceptance criteria when the material is used in multi-part assemblies.