| HS Code | 481217 |
| Density | 0.917 g/cm³ |
| Meltindex | 1.0 g/10 min (190°C/2.16 kg) |
| Filmtensilestrengthatyieldmd | 8.96 MPa |
| Filmtensilestrengthatyieldtd | 8.27 MPa |
| Filmtensilestrengthatbreakmd | 33.1 MPa |
| Filmtensilestrengthatbreaktd | 27.6 MPa |
| Filmelongationatbreakmd | 500 % |
| Filmelongationatbreaktd | 700 % |
| Filmtearstrengthmd | 80 g |
| Filmtearstrengthtd | 200 g |
| Dartdrop | 150 g |
| Haze | 6 % |
| Gloss | 80 % |
As an accredited LyondellBasell Icorene 1761 BEI 2109 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Icorene 1761 BEI 2109 polyethylene is supplied in 25 kg polyethylene-lined paper bags, palletized; bulk options include 1,000 kg FIBCs. |
| Container Loading (20′ FCL) | 20′ FCL: approx. 20–22 MT LyondellBasell Icorene 1761 BEI 2109 mLLDPE in 25 kg bags, palletized, shrink-wrapped, securely stowed. |
| Shipping | LyondellBasell Icorene 1761 BEI 2109 is shipped as non-hazardous, free-flowing polyethylene pellets in 25 kg bags, bulk bags, octabins, or bulk trucks/railcars. Store dry and clean, away from heat, sunlight, and moisture. Standard freight applies; no DOT/IMDG placarding required. Follow supplier handling guidance. |
| Storage | Store LyondellBasell Icorene 1761 BEI 2109 Polyethylene, Linear Low Density, Metallocene in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep containers tightly closed to prevent moisture and contamination. Avoid dust generation and contact with strong oxidizers. Follow the manufacturer’s SDS and local regulations for safe handling, storage, and incompatible materials. Protect from physical damage. |
| Shelf Life | Shelf life is typically 24 months when stored unopened in original packaging, dry, below 50°C, and protected from sunlight. |
Blown-film coextrusion lines producing sealant and abuse layers for frozen-food pouches operate with LyondellBasell Icorene 1761 BEI 2109 incorporated at 30–60 wt% in the skin plies; the core ply remains an LDPE or conventional Ziegler-Natta LLDPE blend to maintain bubble formation and gauge uniformity. At these addition levels, seal initiation temperature measured under ASTM F88/F88M can be reduced by 8–15°C relative to an LDPE-only sealant layer, while hot-tack strength under ASTM F1921 remains above 2 N/25 mm across a 90–130°C sealing range. The film must comply with EU Regulation 10/2011, including the 10 mg/dm² overall migration limit in Annex I and specific migration limits for slip or antiblock additives, and with 21 CFR 177.1520 for polyolefin food-contact articles, with end-use testing under 21 CFR 176.170(c)(3) when the package contacts aqueous, acidic, or fatty foods. On production lines, the skin-layer extruders are typically 45–65 mm barrier screws with L/D ratios between 24:1 and 28:1; the coextrusion die is 250–400 mm in diameter with a die gap of 1.6–2.4 mm. Blow-up ratio is held at 2.0–2.8, melt temperature at 185–215°C, and frost-line height at 4–8 die diameters. If the metallocene content exceeds 60 wt% in the skin layer, low melt strength can cause bubble wander and film thickness variation beyond ±8%, particularly at BUR values above 2.5; internal bubble cooling and a dual-lip air ring are then required to stabilize the bubble. Terminal product types include stand-up pouches for frozen fruits and vegetables, lidding films for dairy cups, horizontal form-fill-seal pillow packs for snack foods, and side-gusset bags for fresh-cut produce.
For liquid packaging board, extrusion coating with Icorene 1761 BEI 2109 as the sealing ply operates at coating weights of 15–30 g/m²; the resin is either run at 100% or blended with 10–30 wt% LDPE to reduce neck-in and improve oxidative stability in the air gap. The process is validated under EU Regulation 10/2011, Annex I, with overall migration ≤ 10 mg/dm² and Annex II restrictions on catalyst residues and additives, and under 21 CFR 176.170(c)(3) for coated paperboard. For aseptic and hygienic packaging, seal integrity tests follow ISO 11607-1, and peel strength follows ASTM F88/F88M. The coating line uses a 90–120 mm single-screw extruder with an L/D ratio of 30:1 and a barrier screw; barrel temperatures are set from 205°C at the feed section to 280–300°C at the adapter and die. The T-slot die is internally deckled, with an air gap of 150–250 mm, line speed of 300–600 m/min, chill roll temperature of 10–20°C, and vacuum box pressure of 0.02–0.05 MPa. Neck-in of the metallocene LLDPE is typically 30–60 mm per edge; the main processing conflict is that the grade’s narrower molecular weight distribution and limited long-chain branching reduce draw resonance resistance. Too long an air gap or too low a melt temperature produces surging and edge tear, while too short an air gap or too high a chill-roll temperature reduces adhesion to the board and creates pinning bubbles or orange-peel surface defects. Addition of 10–20 wt% LDPE widens the draw window and lowers neck-in but increases seal initiation temperature by 5–10°C. Terminal product types include gable-top milk cartons, aseptic juice bricks, paperboard trays with peelable film, medical device pouch lidding, and single-dose cosmetic sachets.
When form-fill-seal packaging for pelletized resins, petrochemical powders, and construction materials demands high puncture resistance, Icorene 1761 BEI 2109 is used at 60–100 wt% in the inner or outer plies of a three-layer heavy-duty sack, typically with 10–20 wt% LDPE in the same layer when melt strength is limiting. Compliance for dangerous goods packaging may require UN Model Regulations testing, including drop test at -18°C for materials classified as dangerous goods, while food-contact liners are evaluated under EU Regulation 10/2011 and 21 CFR 177.1520. Film properties are characterized by dart impact per ASTM D1709, Elmendorf tear per ASTM D1922, and puncture propagation per ASTM D2582. A 75 μm three-layer film with 60 wt% metallocene LLDPE in the outer layers commonly exhibits dart impact values 30–50% higher than a conventional LLDPE/LDPE film at equivalent gauge, while elongation at break under ASTM D882 exceeds 600% in both machine and transverse directions. Production uses a 65 mm barrier screw extruder for skin layers and an 80 mm extruder for the core, L/D ratios of 25:1–30:1, die diameter of 200–450 mm, die gap of 1.8–2.8 mm, blow-up ratio of 1.8–2.5, and melt temperature of 190–220°C. Internal bubble cooling and a dual-lip air ring improve gauge uniformity to within ±7%; without IBC, high metallocene content can cause low-frequency bubble oscillation and short-wavelength thickness bands. Terminal product types include FIBC inner liners, box liners, heavy-duty shipping sacks for polymer pellets, salt and fertilizer bags, and construction materials packaging.
In multi-season greenhouse and silage-bale operations where ultraviolet stabilizer masterbatch is dosed at 5–12 wt% into the outer layer, Icorene 1761 BEI 2109 is used at 40–80 wt% in three-layer agricultural film formulations to raise dart impact and low-temperature flexibility while retaining bubble stability through a 20–30 wt% LDPE addition. The film must comply with EN 13206 for thermoplastics films for agricultural and horticultural use, including tensile properties tested under EN ISO 527-3 and tear resistance under ASTM D1922; UV stabilisation is assessed by accelerated weathering under EN ISO 4892-2 or ASTM G154, with retained elongation above 50% after exposure periods specified by the converter. Production takes place on three-layer blown-film lines with die diameter of 250–500 mm, die gap of 1.8–2.8 mm, blow-up ratio of 2.5–3.5, melt temperature of 190–215°C, and twin-lip air ring. The collapsible frame is set to avoid film blocking because metallocene LLDPE surface tack increases at high wind-up tension; slip additive masterbatches are incorporated at 0.5–1.5 wt% to control coefficient of friction. In silage covers, puncture resistance per ASTM D5748 at 100 μm thickness is a critical criterion because bale wrapping machines impose high shear and tensile loads during pre-stretching. Terminal product types include greenhouse covering film, low tunnel film, silage bunker covers, bale wrap film, and soil fumigation film.
Machine stretch film for pallet unitization uses Icorene 1761 BEI 2109 as a major component in the core and skin layers, with addition rates of 40–80 wt% depending on the layer, while cling layers are formulated with very-low-density polyethylene or polyisobutylene to maintain cling force. In high-performance machine film, the metallocene LLDPE provides tensile stress retention after pre-stretch; tensile properties are measured under ASTM D882, stretchability and load retention under ASTM D4649, cling peel force under ASTM D5458, puncture resistance under ASTM D5748, and tear under ASTM D1922. Compliance for pallet wrap is generally covered by REACH and RoHS; if used for direct food contact, EU Regulation 10/2011 and 21 CFR 177.1520 apply. The cast-film line uses 65–150 mm barrier screw extruders, L/D ratios of 26:1–30:1, melt temperatures of 240–270°C, a slot die with gap of 0.5–1.0 mm, and a polished chill roll at 15–30°C. A vacuum box and electrostatic pinning wire are used to maintain contact; edge tension and die bolt adjustments control gauge variation to within ±5%. Pre-stretch ratios on machine wrapping systems commonly range from 200–300%; at high metallocene content, low-speed unwind noise and film blocking are controlled by anti-block masterbatch at 0.3–1.0 wt%. Terminal product types include machine stretch film, hand pallet wrap, pre-stretched pallet wrap, and agricultural bale wrap.
On collation shrink lines handling beverage multipacks, Icorene 1761 BEI 2109 is added at 30–70 wt% in blends with high-pressure LDPE to shift seal initiation downwards and improve elongation and puncture without eliminating the shrink force needed for bundle tightening. Thermal shrinkage is tested under ASTM D2732, typically 55–80% in machine direction and 0–20% in transverse direction at 120°C; shrink force and shrink stress are measured under ISO 14616. Compliance with EU Directive 94/62/EC applies where the film is used as secondary packaging, and food-contact status is not required unless the film is converted into primary packaging. Production uses a high-stalk blown-film configuration, die gap of 1.4–2.0 mm, blow-up ratio of 2.0–3.0, melt temperature of 190–215°C, and an elevated frost-line height to set machine-direction orientation. The main defect modes are burn-through and seal contamination from high-speed shrink tunnels; the metallocene LLDPE lowers seal initiation but can increase blocking at take-off temperatures above 40°C, requiring anti-block additive masterbatch at 0.5–1.5 wt%. Published data for this specific grade in collation shrink formulations is limited; converter trials are required to confirm final addition ratios. Terminal product types include collation shrink film for bottled water, carbonated soft drink multipacks, canned goods, pet food multipacks, and dairy logistics bundles.
Competitive LyondellBasell Icorene 1761 BEI 2109 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 1761 BEI 2109 is a metallocene-catalyzed linear low density polyethylene supplied as a pelletized film resin. The grade belongs to the Icorene mLLDPE portfolio, in which single-site catalyst chemistry is used to control molar mass distribution and comonomer placement. Publicly available data for the BEI 2109 suffix are limited; the supplier certificate of analysis therefore governs lot-specific values for melt mass-flow rate, density, additive loading, and regulatory status. The product is not a conventional Ziegler-Natta LLDPE or a high-pressure LDPE. The metallocene architecture produces a more uniform short-chain branching distribution and a different melt viscosity response.
Because the 1761 designation in olefin film-grade nomenclature is commonly associated with a density near 0.917 g/cm³ and a melt mass-flow rate near 1.0 g/10 min at 190°C/2.16 kg, the technical envelope in Table 1 is provided as a reference for that class of metallocene LLDPE. The table is not a product specification.
| Property | Method | Reference window | Status |
|---|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022, 190°C/2.16 kg | 0.8–1.2 g/10 min | Lot certificate |
| Density | ISO 1183-1:2019 | 0.916–0.920 g/cm³ | Lot certificate |
| Tensile modulus, machine direction, 25 µm blown film | ISO 527-3:2018 | 180–230 MPa | Process-dependent |
| Dart impact energy, 25 µm | ISO 7765-1:2004, method A | 400–1000 g | Process-dependent |
| Elmendorf tear, transverse direction | ISO 6383-2:1983 | 3–8 N | Process-dependent |
| Haze, 25 µm | ISO 14782:2021 | 5–12% | Additive-dependent |
The spread in Table 1 is process-dependent and additive-dependent; acceptance limits for the finished article must be established by the producer on the target line.
In melt rheology, a 1.0 g/10 min metallocene LLDPE generally shows less shear thinning than a Ziegler-Natta LLDPE of identical melt index, with a power-law index closer to 1 in capillary rheometry according to ISO 11443:2021. This produces higher die pressure and increases the sensitivity of the process to die-gap and melt-temperature changes. The die pressure should be trended lot-to-lot; a shift greater than 5% at constant screw speed and melt temperature may indicate a molar mass distribution shift or contamination.
The primary structural difference is the distribution of comonomer across the molar mass distribution. In Ziegler-Natta LLDPE, the catalyst contains multiple active-site populations; low molar mass chains can be highly branched while high molar mass chains remain more linear. In metallocene LLDPE, comonomer insertion is more uniform. High-temperature gel permeation chromatography according to ISO 16014-4:2019 typically reports Mw/Mn of 2.0–3.0 for mLLDPE and 3.5–5.0 for Ziegler-Natta LLDPE. The narrower distribution reduces low molecular mass extractables and improves impact toughness at a given density.
Differential scanning calorimetry according to ISO 11357-3:2018 for a 0.917 g/cm³ metallocene LLDPE generally records a melting peak between 118°C and 126°C, with crystallinity of 30–40% normalized to a perfect polyethylene crystal enthalpy of 293 J/g. The narrower melting endotherm relative to a Ziegler-Natta resin reflects more uniform lamellar thickness. This thermal uniformity lowers seal initiation temperature and supports faster hot-tack development on packaging machines.
In film form, the uniform branching distribution raises dart impact energy at equal density and melt index because the polymer network contains a higher concentration of effective tie molecules. The same feature can reduce machine-direction tear strength relative to a butene-based Ziegler-Natta LLDPE, especially at high blow-up ratios. The exact tear balance depends on die gap, blow-up ratio, frost line height, and film gauge; it should be measured according to ISO 6383-2 on production film rather than inferred from resin type alone.
Analytical fractionation by temperature rising elution fractionation or crystallization analysis fractionation is often used to quantify comonomer distribution; a metallocene LLDPE shows a narrower elution band than a Ziegler-Natta LLDPE of the same density. The reduction of the comonomer-rich low-molar-mass fraction and the highly linear high-molar-mass fraction is consistent with the lower seal initiation temperature and higher dart impact strength. These differences should be confirmed by standard physical tests rather than inferred from catalyst type alone.
Compared with LDPE, metallocene LLDPE has fewer long-chain branches, so extensional strain hardening is lower and melt strength under bubble formation is reduced. In sealant films, mLLDPE of this density class often shows a seal initiation temperature 5–15°C lower than an equivalent Ziegler-Natta butene LLDPE when measured by ASTM F2029 at a sealing pressure of 0.275 N/mm². That advantage must be confirmed on the specific sealing jaw geometry and dwell time used in the packaging operation.
On a 30:1 L/D, 75 mm grooved-barrel extruder running at constant screw speed, a transition from Ziegler-Natta LLDPE to a metallocene LLDPE may increase die pressure by 10–25%. The narrower molecular weight distribution reduces shear thinning, so the melt retains viscosity more strongly under die-lip shear. The blown-film die gap is usually opened to 1.8–2.5 mm to reduce shear stress and delay shark-skin melt fracture. Melt temperature should be maintained below 240°C; higher temperatures increase the risk of gel formation and organoleptic defects, particularly in stagnant regions of the adapter and die. A low-MFR LDPE purge is recommended before and after shutdown to displace high-viscosity mLLDPE and reduce residence time.
Moisture drying is not normally required. If condensation has formed during storage at relative humidity above 60%, pellet surface water can produce splay or bubble defects; drying at 60–70°C for 2–4 h in a desiccant dryer is sufficient. The resin should not be held at melt temperature for more than 10 min during line stoppages; if a stoppage exceeds this limit, the barrel should be purged with LDPE or the temperature reduced to 160–180°C.
In cast film, flat-to-reverse barrel profiles are typically used, with the die temperature set 5–10°C above the adapter to reduce frozen-in orientation. Chill-roll temperatures between 15°C and 30°C influence quench rate and therefore film stiffness, optical haze, and sealant performance. The air gap should be minimized when low film haze is required; however, too small an air gap can cause draw resonance at high line speed.
High-output blown-film lines running metallocene LLDPE at die rates above 0.5 kg/h/mm die circumference generally require internal bubble cooling and a dual-lip air ring. The blow-up ratio is commonly held at 2.0–3.0, and the frost line height is set at 4–8 die diameters. A lower frost line improves optical clarity but can increase blocking and reduce dart impact. If bubble flutter or draw resonance appears, reducing melt temperature by 5–10°C or increasing die gap by 0.2–0.5 mm may stabilize the bubble. Blending with 10–20 wt% LDPE is a standard remedy but changes tear balance and seal initiation temperature; the blend ratio must be controlled within ±2 wt% to keep seal performance inside the specification.
The critical difference between mLLDPE and Ziegler-Natta LLDPE on high-speed lines is the narrower bubble-stability window caused by lower extensional strain hardening. Conditions that are acceptable on a low-speed pilot line cannot be transferred directly to a high-output line without adjusting die gap and air-ring geometry. Published data for the exact Icorene 1761 BEI 2109 configuration on high-speed lines are limited; a structured pilot-line response surface study is required to fix frost line height, cooling air velocity, and blow-up ratio for a given film width and gauge.
Typical selections for this class of mLLDPE include stretch-hood films, heavy-duty sacks, lamination webs, and sealant layers in multilayer flexible packaging. In a three-layer coextruded film with a metallocene sealant skin, the grade is selected when seal initiation below 105°C is required and hot-tack strength measured by ASTM F1921 must be maintained across the packaging line. The Vicat softening temperature for a 0.917 g/cm³ metallocene LLDPE typically falls between 95°C and 105°C by ISO 306/A50. Compared with an equal-density Ziegler-Natta LLDPE, the metallocene resin typically improves dart impact and seal strength but may require a higher slip-agent level to achieve a coefficient of friction below 0.20 when tested according to ISO 8295.
For stretch-film applications, puncture force determined by ASTM D5748 and load retention after 200% elongation are commonly used as discriminators. Metallocene LLDPE of this density class generally improves puncture force relative to conventional butene LLDPE at equal gauge, allowing thickness reductions of 5–15% at equal puncture resistance. The down-gauging must be validated on the packaging line because load retention and tear resistance do not scale linearly with thickness. The resin is not intended for rigid articles requiring long-term creep resistance above the Vicat softening point, nor for contact with strong oxidizing acids or chlorinated solvents.
For food-contact uses, the processor should obtain a lot-specific compliance statement from LyondellBasell confirming that the grade falls within FDA 21 CFR 177.1520 and EU Regulation 10/2011. Overall migration testing may be required under EN 1186-1:2002 using the appropriate food simulant; the overall migration limit for plastic food-contact materials is 10 mg/dm² under EU Regulation 10/2011. The formulated grade may contain processing stabilizers and neutralizing agents; specific migration of antioxidants and processing aids must be checked against the positive list before the final packaging structure is placed on the market.
When the material is used in electrical and electronic equipment, the supplier should confirm that the grade does not intentionally contain substances restricted by RoHS Directive 2011/65/EU. For REACH, the safety data sheet and Commission candidate list should be reviewed at the point of use. The resin should be stored below 40°C and managed on a first-in-first-out basis to reduce lot-to-lot variation in additive migration and organoleptics. Combining the resin with amine-based antistatic additives at high levels should be avoided unless validated, because interaction with catalyst residues or stabilizers can produce color shifts. The same restriction applies to low-molecular-weight hydrocarbon oil additions above 1 wt%; migration and organoleptic testing are required before such compounds are used in food-contact film.