| HS Code | 130140 |
| Material Type | Polyethylene, Linear Low Density (LLDPE) |
| Density | 0.921 g/cm³ |
| Melt Index 190 C 2 16 Kg | 1.0 g/10 min |
| Melting Point | 123 °C |
| Vicat Softening Point | 95 °C |
| Tensile Strength At Yield | 10 MPa |
| Tensile Strength At Break | 30 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 250 MPa |
| Dart Drop Impact | 150 g |
| Elmendorf Tear Strength Md | 250 g |
| Elmendorf Tear Strength Td | 350 g |
| Haze | 10% |
| Gloss 45 | 70% |
| Coefficient Of Friction | 0.20 |
As an accredited LyondellBasell Icorene 1210 YEW 2704 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 1210 YEW 2704 Linear Low Density Polyethylene packaged in 25 kg bags, 40 bags per 1,000 kg pallet. |
| Container Loading (20′ FCL) | LyondellBasell Icorene 1210 YEW 2704 LLDPE loaded in 20′ FCL: palletized bags, shrink-wrapped, strapped, evenly distributed, secured for ocean transport. |
| Shipping | LyondellBasell Icorene 1210 YEW 2704 Polyethylene, Linear Low Density is a non-hazardous solid, typically shipped in bags or bulk containers. Transport at ambient temperature in clean, dry equipment. Protect from moisture, direct sunlight, and contamination. Keep packages sealed and palletized securely. No special DOT/IMDG/IATA dangerous-goods classification is normally required. |
| Storage | Store LyondellBasell Icorene 1210 YEW 2704 Polyethylene, Linear Low Density in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers closed and pallets stable to prevent dust generation and moisture absorption. Avoid strong oxidizers. Use proper grounding to control static. Follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Typically 24 months when stored in original, unopened packaging in a cool, dry, well-ventilated area away from direct sunlight. |
LyondellBasell Icorene 1210 YEW 2704 functions as a butene-copolymer linear low density polyethylene in blown film conversion; nominal density is 0.918 g/cm³ per ISO 1183-1:2019 and melt flow index is 1.0 g/10 min per ISO 1133-1:2022 at 190°C/2.16 kg. In heavy-duty sack and industrial liner lines the resin is processed without predrying, provided pellet surface moisture does not exceed 0.05 wt%. A monolayer formulation based on 100 parts Icorene 1210 YEW 2704 includes 2.0-3.0 phr of an LDPE-carrier silica/erucamide antiblock-slip masterbatch and, when die lip fouling or melt fracture appears, 0.5-1.0 phr of a fluoropolymer process aid; the exact process-aid loading is matched to die pressure reduction observed across the screen pack and spiral mandrel. Extruders with L/D 30:1 barrier screws and 45-75 mm barrel diameters operate with feed throat 30-45°C, compression section 180-200°C, metering section 190-210°C, and adapter/die 190-205°C. The die gap is maintained between 2.0 mm and 2.5 mm; narrower gaps below 1.8 mm intensify shear stress and initiate sharkskin melt fracture in the linear polymer. Bubble stability is obtained at blow-up ratios of 2.5:1-3.0:1 and a frost-line height of 6-8 die diameters. On a 45 mm grooved-feed line, output typically reaches 90-140 kg/h with die pressure in the 250-380 bar range; raising die pressure beyond 400 bar without process-aid adjustment causes backpressure alarms and film gauge bands. Mechanical test protocols follow ASTM D1709-23 Method A for dart impact, ASTM D1922-15 for Elmendorf tear, and ASTM D882-18 for tensile properties. Direct food-contact packaging must meet FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011 Annex I; overall migration is controlled below 10 mg/dm² under EN 1186-1:2002 processing conditions. End products include heavy-duty sacks for pelletized resin and fertilizer, industrial liners, construction film, and agricultural silage bags.
| Application class | Regulatory/standard reference | Test parameter | Acceptance limit / specification |
|---|---|---|---|
| Food-contact blown film | FDA 21 CFR 177.1520(c) | Olefin polymer compliance | 1-butene/ethylene copolymer; end-use condition testing |
| Food-contact film, EU | Regulation (EU) No 10/2011, Annex I | Overall migration | 10 mg/dm² |
| Food-contact film, EU | Regulation (EU) No 10/2011, Annex I | 1-butene specific migration | 5 mg/kg |
| Electrical/electronic applications | Directive 2011/65/EU (RoHS) | Homogeneous material restricted substances | Lead 0.1 wt%; cadmium 0.01 wt%; mercury 0.1 wt%; hexavalent chromium 0.1 wt% |
| EU REACH | Regulation (EC) No 1907/2006, Article 33 | SVHC communication | No SVHC above 0.1% w/w in article |
Drawdown instability in cast film is governed by the interaction of die-land shear history, air-gap cooling rate, and the extensional viscosity response of the melt. In three-layer stretch-film lines using Icorene 1210 YEW 2704 as core or back layer, die gap is set at 0.8-1.2 mm, melt temperature at 200-240°C, and air gap at 30-50 mm; chill roll temperature is held at 20-28°C. Line speed normally ranges from 300 m/min to 600 m/min, but above 450 m/min the film edges may enter draw resonance, visible as periodic gauge bands across the web. Draw resonance is corrected by reducing the air gap below 35 mm and by increasing melt temperature no more than 10°C; larger temperature increases cause oxidative gel formation and black specks. A typical outer cling layer formulation contains 85-90 wt% Icorene 1210 YEW 2704, 5-10 wt% of a metallocene-catalyzed plastomer or EVA modifier, and 1.5-3.0 wt% polyisobutylene cling additive; the core layer may use 15-20 wt% recycled edge trim without measurable loss in machine-direction tensile strength. Fluoropolymer process aid at 0.4-0.8 wt% is added when chill-roll wax or die-edge deposits reduce line availability. Pellet surface moisture above 0.05 wt% produces micro-voids and haze bands. Finished films are tested for tensile elongation at break under ASTM D882-18 and puncture resistance under ASTM D5748; for non-food industrial pallet wrap, direct food-contact clearance is not triggered unless the wrap is used in direct contact with fresh produce. For food-grade stretch film, compliance with FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011 is required. Typical terminal products are machine-applied pallet wrap, silage bale wrap, bundling film, and hand stretch film.
Where liquid packaging board requires a hermetic polyolefin sealant web, Icorene 1210 YEW 2704 is coextruded or blended with fractional-melt LDPE to reduce neck-in and improve draw stability. A specified sealant layer composition is 70-80 wt% Icorene 1210 YEW 2704 and 20-30 wt% LDPE; coat weights are specified at 15-25 g/m² for paperboard and 20-35 g/m² for aluminum-foil-based sachets. The die gap is opened to 1.0-1.5 mm, and the air gap is set at 150-250 mm, allowing controlled surface oxidation that promotes adhesion to corona-treated board and primed foil. Melt temperature is held at 290-315°C with total residence time below 3 min to limit chain scission and odor generation in the sealant. Line speeds of 150-350 m/min require corona treatment of the polymer side at 42-46 mN/m before printing or lamination. For aseptic structures, the sealant is the innermost layer of a polyethylene/paperboard/polyethylene/aluminum/polyethylene laminate; hot-tack performance is evaluated by ASTM F1921 and heat-seal strength by ASTM F88. Compliance for food-contact paperboard laminates includes FDA 21 CFR 176.170(c) for paper and paperboard components and Regulation (EU) No 10/2011 for the plastic layer, with overall migration below 10 mg/dm². End products are UHT milk cartons, juice gable-top packaging, single-serve foil sachets, and paper cups.
In high-speed lamination webs for stand-up pouches, the resin is used as the sealant layer in three-layer coextruded films that also carry a barrier layer such as EVOH or polyamide and an outer printed layer. The sealant layer thickness is typically 30-50 µm within a total film thickness of 90-120 µm. A formulation for the sealant layer combines 70-80 wt% Icorene 1210 YEW 2704 with 20-30 wt% of a polyolefin plastomer or lower-melting ethylene-alkene copolymer to reduce seal initiation temperature to 80-90°C; 0.5-1.0 wt% of a silica-based antiblock and 0.1-0.3 wt% erucamide slip are added to prevent blocking during windup and to control pouch opening. Processing on coextrusion blown or cast lines uses die gap 2.0-2.4 mm, melt temperature 200-220°C for the sealant layer, and chill roll or frost-line settings adjusted to keep haze below 10% for reverse-printed structures. The sealant layer must not contain slip additive that migrates to the lamination interface because this lowers lamination bond strength; therefore, additive-free formulations are specified when an adhesive lamination step follows film production. Heat-seal strength is measured according to ASTM F88. End products include stand-up pouches, vacuum pouches, detergent pouches, and pet-food bags. Food-contact uses require FDA 21 CFR 177.1520(c) for the LLDPE and Regulation (EU) No 10/2011 overall migration below 10 mg/dm²; if EVOH is used, its specific migration is assessed under Annex I.
When the packaging objective shifts from barrier to controlled gas exchange, a butene-based LLDPE with a density of 0.918 g/cm³ is used in lidding films and flow-pack webs for fresh-cut produce. The oxygen transmission rate of the finished film is driven by film thickness, orientation, and sealant layer crystallinity; the process is validated against manometric or coulometric methods such as ASTM D3985 for OTR and ASTM F2476 for carbon dioxide transmission. The film formulation uses 100 parts Icorene 1210 YEW 2704, 0.5-1.5 wt% of a food-grade antifog additive, 0.1-0.3 wt% erucamide slip, and 0.2-0.4 wt% antiblock; no plasticizers or waxes are used because they would depress OTR unpredictably. Extrusion conditions on a 40-60 mm blown film line include die gap 2.0 mm, BUR 2.0:1-2.5:1, melt temperature 185-205°C, and film thickness 15-30 µm. Thickness variation above ±5% lowers the OTR control needed for produce shelf life. Terminal products include fresh-cut salad bags, produce lidding film, bakery film, and mushroom flow-pack. Direct food-contact compliance is governed by FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011; specific migration of 1-butene is assessed according to the Annex I limit, and overall migration remains below 10 mg/dm² under EN 1186-1:2002.
Competitive LyondellBasell Icorene 1210 YEW 2704 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
The LyondellBasell product identified as Icorene 1210 YEW 2704 is a high-flow linear low-density polyethylene resin supplied as a natural pellet system for injection molding and selected extrusion applications. Under ISO 1043-1, the material is classified as PE-LLD; under ASTM D883, the density position below 0.940 g/cm³ places it within the linear low-density polyethylene family. The YEW 2704 suffix is a supplier-specific formulation, additive, and packaging trace code shown on the certificate of analysis rather than a separate polymer architecture. The grade is characterized by a nominal melt mass-flow rate of 20 g/10 min determined according to ISO 1133-1 at 190 °C and 2.16 kg, and a nominal density of 0.924 g/cm³ determined according to ISO 1183-1. These values position the product in the high-flow injection category rather than in film, blow molding, or pipe extrusion categories.
The following table lists reported typical physical and mechanical values for the natural injection grade. These figures are lot-specific and must be verified against the current supplier datasheet before tool design or compliance submission.
| Property | Test method | Typical value |
|---|---|---|
| Melt mass-flow rate, 190 °C/2.16 kg | ISO 1133-1 | 20 g/10 min |
| Density | ISO 1183-1 | 0.924 g/cm³ |
| Tensile stress at yield | ISO 527-2 | 10 MPa |
| Tensile elongation at break | ISO 527-2 | >500% |
| Flexural modulus | ISO 178 | 260 MPa |
| Vicat softening temperature, A50 | ISO 306 | 89 °C |
| Shore D hardness | ISO 868 | 52 |
Injection molding conditions for this grade generally fall within a melt-temperature range of 200 °C to 250 °C. Mold temperatures between 10 °C and 30 °C are commonly used for fast solidification and demolding of thin-walled sections. Screw geometry with an L/D ratio of 20:1 to 25:1 and a compression ratio of 2.5:1 to 3.5:1 is suitable for homogeneous melt preparation. Predrying is not normally required under closed warehouse storage below 50% relative humidity. If surface condensation has formed, a dry-air desiccant dryer at 70 °C to 80 °C for 2 h is sufficient to remove pellet-surface moisture. Prolonged drying at higher temperatures is not recommended because it can accelerate antioxidant depletion and shift the melt viscosity.
Capillary rheometry indicates that the melt follows the shear-thinning behavior typical of linear polyethylene. Apparent viscosity decreases as shear rate increases from 100 s⁻¹ to 1000 s⁻¹, which supports short injection times in thin-wall tooling. Because the nominal 20 g/10 min melt mass-flow rate reduces pressure demand, gates below 0.8 mm can be used for lids and caps where rapid gate freeze-off is not required. The narrow molecular weight distribution lowers high-shear viscosity relative to a broad-molecular-weight HDPE of the same melt index. However, this same characteristic reduces melt tension and die swell; dimensional relationships in thick sections may require higher packing pressure than a broad-MWD resin.
Thermal degradation is the primary upper processing boundary. At melt temperatures above 240 °C, accumulated residence time should not exceed 8 min. Extended hold time at these temperatures can consume the stabilizer package and produce surface oxidation streaks, yellowing, and odor. At the lower boundary, melt temperatures below 190 °C produce short shots, poor weld-line strength, and variable cavity packing. A melt cushion of 3 mm to 6 mm is recommended to reduce recovery variability on general-purpose reciprocating screws. Peak injection pressures above 120 MPa on thin-wall molds are generally unnecessary for this grade unless the flow length-to-wall-thickness ratio exceeds 250:1.
Mold shrinkage is influenced by cooling rate, packing pressure, and wall thickness. For unfilled linear low-density polyethylene of this density and melt flow class, mold shrinkage values in the 1.5% to 2.5% range are typically applied for initial tool design. Thick sections above 4 mm may exhibit volumetric shrinkage and sink marks because of the low density and limited packing stiffness. Localized hot spots in the mold can also cause post-mold warpage in flat container lids. Tool trial data should replace estimated shrinkage values before final cavity dimensioning.
Production-scale molding of disposable food containers, caps, closures, housewares, and general-purpose articles from this material typically involves two-plate cold-runner molds on machines with clamp force from 800 kN to 3000 kN. The high-flow melt supports wall sections from 0.8 mm to 2.5 mm without excessive injection pressure. Multi-cavity fill balance is controlled primarily by uniform melt temperature and gate geometry rather than by high packing pressure. Hot-runner systems with valve gates should maintain nozzle tip temperatures below 230 °C to prevent stringing and premature resin degradation. Published data for this specific product configuration is limited for high-speed closure molding above 500 parts/min; processors should validate gate freeze-off, pressure drop, and cycle time on the specific mold.
Compared with high-density polyethylene injection grades in the 0.945 g/cm³ to 0.965 g/cm³ density range, the 0.924 g/cm³ density of Icorene 1210 YEW 2704 yields approximately 3% to 4% lower part mass for equal volume. The reduced density is accompanied by lower flexural modulus and lower Vicat softening temperature. A typical 0.952 g/cm³ HDPE injection grade may exhibit flexural modulus above 1000 MPa and a Vicat A50 temperature near 125 °C. By contrast, the LLDPE grade is reported at 260 MPa flexural modulus and 89 °C Vicat A50. HDPE therefore remains the preferred choice for high-temperature hot-fill or high-stiffness structural packaging. Icorene 1210 YEW 2704 is selected where easier flow, lower melt temperature requirement, and improved stress-crack resistance at low strain are more important than absolute stiffness.
Compared with low-density polyethylene injection grades of similar melt index, the linear molecular architecture of Icorene 1210 YEW 2704 provides higher tensile yield stress and greater elongation at break. LDPE injection grades of 0.919 g/cm³ density and 20 g/10 min MFR typically show lower modulus and lower tensile strength because long-chain branching interrupts crystallinity. The linear grade may produce slightly lower surface gloss and higher haze, particularly in thick sections. If optical clarity or high surface gloss is a critical requirement, LDPE or a clarified random copolymer may be more suitable.
Compared with C6 or C8 linear low-density polyethylene film grades with melt index below 3.5 g/10 min, Icorene 1210 YEW 2704 is not designed for blown film. Melt tension is too low to maintain stable bubble geometry at blow-up ratios above 2:1. Hexene- and octene-based film grades provide higher dart impact and Elmendorf tear resistance in oriented film, but their low melt flow makes them unsuitable for thin-wall injection molding. The narrow molecular weight distribution of the injection grade also reduces screw torque and melt elasticity, which improves injection filling but reduces bubble stability and web performance.
Within the LLDPE injection molding segment, the grade should be compared with other high-flow products on density, additive package, and molecular weight distribution. A grade with equivalent melt index but higher density above 0.930 g/cm³ will provide greater stiffness and better thermal dimensional stability. A grade with equivalent density but lower melt index below 10 g/10 min will offer higher toughness and better environmental stress crack resistance, but will require higher injection pressure and longer cycle time. The specific choice depends on whether the molding operation is pressure-limited, cycle-time-limited, or part-toughness-limited.
Polyethylene resins may be evaluated as food-contact polymers under 21 CFR 177.1520(c) when the finished article meets the specified extractables and end-use temperature conditions. Food-contact use requires written confirmation from the supplier that this specific YEW 2704 formulation is included in the food-contact listing. Under EU Regulation 10/2011, the overall migration limit for plastic food-contact materials is 10 mg/dm²; specific migration of any additive in the formulation must be checked against the additive specification and intended food type. The supplier can provide raw material compliance statements, but the final processor is responsible for migration testing on the finished article because processing can alter migration behavior.
Regulatory documentation should include the CAS number of the polymer, additive identities, and the test methods used for migration. For FDA conditions of use, the processor must verify the food type, contact time, and temperature against the tables in 21 CFR 177.1520(c). For European Union applications, the finished article must also meet the requirements of EU 10/2011 as amended, including declaration of compliance for supply chain documentation. No blanket statement of compliance should be inferred solely from the product name.
Operational boundaries observed with high-flow LLDPE of this type include limited hot-tack strength in heat-seal applications and reduced environmental stress crack resistance compared with hexene- or octene-based LLDPE grades. The grade is not intended for sustained hot-water exposure above 60 °C without application-specific validation. Masterbatch and additive compatibility must be assessed before production; strong oxidizing agents and certain amine-containing stabilizer packages can create discoloration or surface exudation at processing temperatures. Sacks opened for more than 24 h in humid environments may require predrying to avoid surface moisture defects. Regrind addition is common in non-Category 1 food-contact applications, but molders should limit untreated wet regrind to less than 20 wt% and dry regrind to below 0.02% moisture before reintroduction to the hopper.