| HS Code | 934936 |
| Density | 0.921 g/cm³ |
| Melt Flow Rate | 12 g/10 min |
| Tensile Strength At Yield | 9.65 MPa |
| Tensile Strength At Break | 10.3 MPa |
| Elongation At Break | 800% |
| Flexural Modulus | 276 MPa |
| Vicat Softening Point | 93 °C |
| Brittleness Temperature | < -70 °C |
| Hardness Shore D | 50 |
| Environmental Stress Crack Resistance | > 1000 hr |
| Melting Point | 120 °C |
| Thermal Conductivity | 0.33 W/m·K |
| Specific Heat Capacity | 2.3 J/g·°C |
| Dielectric Constant | 2.3 |
| Dissipation Factor | 0.0002 |
| Volume Resistivity | 1e16 ohm·cm |
| Dielectric Strength | 20 kV/mm |
As an accredited LyondellBasell Icorene 1210 YEW 2228 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 1210 YEW 2228 LLDPE supplied in 25 kg moisture-resistant paper bags, palletized and shrink-wrapped for secure industrial transport. |
| Container Loading (20′ FCL) | 20′ FCL loading: LyondellBasell Icorene 1210 YEW 2228 LLDPE, palletized 25 kg bags, shrink-wrapped, evenly distributed, securely braced for shipment. |
| Shipping | LyondellBasell Icorene 1210 YEW 2228 Polyethylene, Linear Low Density is shipped as a non-hazardous solid resin in 25 kg bags, octabins, or bulk bags on pallets, in dry containers. Not regulated as dangerous goods. Keep dry and avoid excessive heat, sunlight, and moisture. Follow SDS guidance. |
| Storage | Store LyondellBasell Icorene 1210 YEW 2228 Polyethylene, Linear Low Density in a cool, dry, well-ventilated warehouse. Keep original bags closed and palletized, away from direct sunlight, heat, flames, and strong oxidizers. Prevent moisture, dust, and contamination. Avoid excessive stacking and prolonged high temperatures. Maintain clean, dry conditions, inspect containers regularly, and use first-in, first-out stock rotation. |
| Shelf Life | Two years from manufacture when stored unopened in original packaging, dry, below 50°C, and protected from direct sunlight. |
Icorene 1210 YEW 2228 is a linear low-density polyethylene powder supplied for rotational moulding operations where the nominal melt flow rate of 3.5 g/10 min under ASTM D1238 conditions (190°C, 2.16 kg) and nominal density of 0.935 g/cm³ under ASTM D1505 define a processing window that balances powder coalescence against melt sag. The powder is dry-blended with pigment masterbatch or UV stabiliser concentrates at the moulding plant; typical rotomoulding machines operate with a primary arm speed of 6–12 rpm and secondary speed of 1.5–3 rpm, producing a biaxial rotation ratio between 3:1 and 5:1 on carousel or shuttle equipment. Because the grade is a powder, sieve retention is typically controlled on a 35 mesh screen, and excessive fines generated during regrind can alter bulk density and bridging behaviour inside the mould cavity.
Rotational moulding of vertical chemical storage tanks from the same powder begins with tooling designed to limit the occurrence of pinholing at the upper corners when the cavity rotates through a heated oven. A 1,000 L cylindrical tank mould typically enters a forced-air convection oven at 280–300°C, and the internal air temperature is held at 190–205°C until the melt film has coalesced at a wall thickness of 5–7 mm. Peak internal air temperature is the controlling variable rather than oven setpoint because tool mass and powder bed depth shift the thermal lag by 10–15 minutes between light and heavy sections. If the cycle is terminated before the internal air temperature reaches the melting onset range, the inner wall retains a dry, powdery layer that fails hydrostatic pressure testing under ASTM D1998-21. For tanks holding caustic or acidic process fluids, the lower crystallinity associated with 0.935 g/cm³ density provides improved environmental stress crack resistance relative to homopolymer HDPE rotomoulding grades, as measured by ASTM D1693-15e1 Condition B. Formulation-specific chemical compatibility with the stored fluid must still be confirmed by immersion testing at 60°C for 30 days because ESCR data alone do not predict oxidation or plasticiser extraction. Wall-thickness verification follows an ultrasonic grid pattern on the cooled part, and welds at spin-welded or hot-plate-welded bung fittings are sectioned for porosity inspection. The operational boundary is moisture-driven: powder stored below dew point or exposed to relative humidity above 70% without pre-drying can generate steam pinholes during the coalescence stage, so a 60–70°C desiccant-air preconditioning cycle is commonly applied before charging.
In marine buoyancy bodies, slow crack growth rather than short-term impact is the dominant failure mode when a float is clamped to a dock structure and subjected to cyclic wave flexure at the attachment point. The grade’s density of 0.935 g/cm³ positions it in the medium-density range for linear low-density polyethylene, where lower crystallinity contributes to a longer stable crack initiation phase under stress than typical 0.940–0.945 g/cm³ rotomoulding grades. Floats are ordinarily moulded as hollow double-wall shells with wall thickness from 4 mm to 6 mm; closed-cell expanded polystyrene at 32–40 kg/m³ is injected after demoulding, or the cavity is filled with two-component polyurethane foam for structural rigidity. The foam-filling step can reheat the shell above the polymer softening point if the exotherm is not controlled, causing sink marks on flat deck faces. Service validation for a seawater-filled float requires crack resistance testing under ISO 18489 or ASTM D1693 after ageing in synthetic seawater at 60°C for at least 1,000 h. Ultraviolet stabilisation is not provided by the base resin; unpigmented natural powder requires a hindered-amine light stabiliser and UV absorber package to reach weathering thresholds measured by ISO 4892-3 accelerated exposure. Impact testing after cold conditioning is specified at −20°C for 24 h, using ISO 6603-2 instrumented puncture testing at 4.4 m/s. The processing bottleneck occurs during demoulding of long rectangular floats: uneven forced-air cooling on one side produces a bow along the length, and the part must be restrained in a cooling fixture until its surface temperature falls below 60°C.
Agricultural chemical tank production places intermittent chemical exposure on the inner surface rather than continuous hydrostatic load, so the critical property is resistance to stress cracking induced by surfactants, aromatic solvents, and oxidising agents in pesticide formulations. Rotationally moulded tanks of 800 L to 5,000 L are used for liquid urea ammonium nitrate, glyphosate isopropylamine salt, and diluted systemic fungicides. The grade is dry-blended with an LLDPE-compatible pigment concentrate; a non-compatible carrier can create low-melt-index regions that persist as visible gels or pinholes on the inner wall. Moulded-in drain fittings are the most common failure location because the transition from 6 mm sidewall to thick insert boss distorts the local cooling profile. Insert retention is improved by designing a raised boss of at least 1.5 times the insert outer diameter and post-mould reaming to remove resin-rich shrinkage around the thread. Chemical compatibility is not adequately predicted by ESCR data alone; a tank sample exposed to the actual formulation at 40°C and 60°C for 30 days under constant strain is used to detect cracking before production approval. The use of oxidising sterilants such as sodium hypochlorite at concentrations above 5% can accelerate surface embrittlement, and annual replacement of rubber gaskets at the lid flange is necessary when the tank alternates between wet and dry service.
In a diesel fuel tank programme, the relationship between wall thickness and hydrocarbon permeation is treated as a design control rather than an afterthought because linear low-density polyethylene is not a barrier resin. Single-layer rotationally moulded LLDPE tanks can reduce water ingress and impact-related fracture, but aromatic and aliphatic fuel constituents permeate through the polymer network at rates that rise with service temperature and ethanol or biodiesel blend content. Tank wall thickness is therefore fixed only after permeation measurement according to SAE J2659 or SAE J1737, using test fuel compositions matched to the intended market. For applications with evaporative emission limits, surface fluorination or sulfonation post-treatment is applied to the inner wall to create a polar barrier layer; untreated LLDPE alone is generally unsuitable for gasoline and may fail diesel emission thresholds in stacked-tank valley applications where heat accumulates. The moulding cycle requires a lower peak internal air temperature of 185–195°C when metallic closure plates are inserted, because excessive local heat at the insert interface causes oxidation and loss of impact strength around the fuel sender opening. Insert plates are clamped with torque values specified by the tank manufacturer, and hydrostatic leak testing after insert welding is performed at 25 kPa internal pressure with ultrasonic leak detection. Published data for this specific grade in fuel tank service remain limited; qualification batches should always include cold-impact testing at −20°C per ISO 6603-2 and chemical immersion of welded assemblies in reference diesel fuel for 500 h at 60°C.
Flat-bottom kayak hulls exhibit the largest internal stress differential when one side of the mould is water-cooled or fan-cooled more rapidly than the deck line, producing longitudinal twist that cannot be corrected after demoulding. Rotomoulding of a single-wall hull with a target shell thickness of 4–6 mm uses the same 190–200°C internal air temperature range, but the mould is removed from the oven earlier than a chemical tank shell to limit inner-surface oxidation. The grade’s linear low-density structure gives a higher elongation at break and multiaxial impact resistance than a high-density rotomoulding grade of equivalent melt flow, but flexural modulus is correspondingly lower; hull stiffening is achieved through chine contours, internal bulkheads, or aluminium stringers rather than resin selection alone. Impact acceptance is typically measured after conditioning at −20°C for 24 h, using ASTM D3763-23 or ISO 6603-2 at an impact velocity of 4.4 m/s. The warpage control procedure involves a post-mould cooling jig that holds the keel line straight while both sides cool below 70°C; free cooling of a flat-bottom hull on a rack can produce more than 8 mm of bow over a 1 m length. Ultraviolet protection for coloured hulls is delivered by pigment concentration and HALS loading; white hulls are especially sensitive to chalking if only titanium dioxide is used without an adequate UV package tested to ISO 4892-3 for at least 1,000 h.
For rotationally moulded forklift bins, insulated fish boxes, and dry bulk intermediate containers, the same powder is processed at a 4:1 rotation ratio and demoulded at 70–80°C; impact resistance is verified by ISO 6603-2 after −20°C conditioning for 24 h, and no additional surface treatment is required for dry cargoes.
Competitive LyondellBasell Icorene 1210 YEW 2228 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 1210 YEW 2228 Polyethylene, Linear Low Density is identified by the base-grade designation Icorene 1210 and the suffix YEW 2228, which in LyondellBasell lot-and-packaging coding commonly denotes colour, additive package, or physical form rather than a change in the base polymer. The product belongs to the LLDPE class, comprising ethylene copolymerised with an α-olefin comonomer to produce a linear backbone with short-chain branches. This architecture provides a different melt rheology and solid-state property balance from long-chain branched LDPE and from higher-density HDPE. Converters evaluating this product typically target blown film, cast film, injection moulding, or rotational moulding, depending on the melt flow rate and additive package stated in the current producer data sheet. Because the YEW 2228 suffix is not sufficient to establish grade-specific property release limits, specification should be carried out using the LyondellBasell certificate of analysis and the standard test methods noted below.
Conventional LDPE is synthesised in high-pressure free-radical polymerisation and contains long-chain branching. That long-chain branching imparts high melt strength and bubble stability in blown film but limits tensile strength and creep resistance relative to LLDPE. HDPE, with density above 0.940 g/cm³, has a highly linear backbone and minimal short-chain branching, giving higher flexural modulus and chemical resistance but reduced dart impact and clarity. LLDPE grades such as the 1210 base resin are normally polymerised at low pressure using Ziegler-Natta or metallocene catalysts and incorporate butene, hexene, or octene as comonomer. The short-chain branch length and distribution control the balance between tear strength, dart impact, and modulus. A converter cannot determine comonomer type from the YEW 2228 suffix alone; the producer technical data sheet must be consulted.
Relative to metallocene LLDPE, conventional LLDPE often has a broader molecular weight distribution and higher processing torque at equivalent melt index, while metallocene grades can yield improved puncture resistance and lower haze. Relative to LDPE, LLDPE exhibits higher tensile strength and lower melt strength, so stable blown film operation often requires die-gap adjustment or LDPE blending. The absence of long-chain branching also modifies strain-hardening behaviour in extrusion coating and film blowing.
Specification of LLDPE starts with melt flow rate under 190 °C and 2.16 kg, determined by ASTM D1238 or ISO 1133-1:2022. Density is tested by ASTM D1505 or ISO 1183-1:2019; the LLDPE class typically spans 0.915–0.940 g/cm³, but the nominal value for this grade must be taken from the lot certificate. Mechanical characterisation for film and moulded parts uses ASTM D638 or ISO 527-2 for tensile properties, ISO 178 or ASTM D790 for flexural modulus, ASTM D1525 or ISO 306 for Vicat softening, and ASTM D1709 or ISO 7765-1 for dart impact. Published numerical property data for this specific configuration is limited; therefore, the matrix below lists only the release-test designations and conditions that a converter should request for a given production lot.
| Property | Test standard | Measurement condition |
|---|---|---|
| Melt flow rate | ISO 1133-1:2022, ASTM D1238 | 190 °C, 2.16 kg |
| Density | ISO 1183-1:2019, ASTM D1505 | 23 °C, conditioned specimen |
| Tensile properties | ISO 527-2, ASTM D638 | Type 5A or Type IV specimen, 50 mm/min |
| Flexural modulus | ISO 178, ASTM D790 | 2 mm/min, three-point bending |
| Vicat softening temperature | ISO 306, ASTM D1525 | Method A50, 10 N, 50 °C/h |
| Dart impact resistance | ISO 7765-1, ASTM D1709 | Method A, F50, conditioned at 23 °C |
LLDPE processing on a single-screw extruder with 24:1 L/D requires attention to shear heating and melt temperature. Barrel zone set points commonly range from 160 °C near the hopper to 210–220 °C at the die, with the melt-temperature upper limit held below 240 °C to reduce gel formation and off-odour. Screw compression ratios between 3:1 and 4:1 with a mixing or barrier section are used to homogenise comonomer-rich regions. The higher viscosity of LLDPE at film shear rates can raise extruder torque and melt pressure relative to LDPE. Die pressure in cast film lines commonly falls between 30 MPa and 40 MPa depending on output, die gap, and melt index. If the extruder is not equipped with a melt pressure sensor, head pressure should be treated as a release variable and monitored against the drive load.
The principal processing conflict is melt fracture at low melt temperatures and oxidative degradation at high melt temperatures. Melt fracture may appear as sharkskin on the web and is mitigated by raising the die temperature, widening the die gap, or adding polymer processing aid. Oxidation is controlled by stabiliser package and by minimising residence time at full temperature. For this specific Icorene 1210 YEW 2228 configuration, published processing data for extreme shear rates is limited; a trial window of ±5 °C around the producer’s recommended die set point is advisable when start-up scrap rates exceed line-specific targets.
Blown film conversion of the 1210 base grade, where the grade is formulated for film, typically operates at blow-up ratios from 2.0:1 to 3.5:1. LLDPE bubble stability is lower than LDPE because of the absence of long-chain branching; air ring selection and die geometry therefore require closer adjustment. Die gaps of 1.6–2.4 mm are common to control melt fracture in linear resins. Frost-line height affects MD/TD tear balance: a high frost line can raise transverse-direction tear, while a low frost line can improve haze and increase machine-direction orientation. Cast film uses chill roll temperatures from 15 °C to 30 °C to control quench rate and reduce haze. Heat seal performance is measured by ASTM F2029 or ASTM F88; slip and antiblock additives, if present in the YEW 2228 package, may lower seal strength at high loadings. Dart impact, puncture, and Elmendorf tear are determined following ASTM D1709, ASTM D5748, and ASTM D1922.
Thin-gauge film below 25 µm often requires blending with LDPE to improve bubble stability and output; however, excessive LDPE addition shifts the property profile toward lower tensile strength and lower dart impact. The substitution of Icorene 1210 YEW 2228 for a conventional LDPE line should not be made without confirming melt strength compatibility through the producer’s data sheet.
If the melt flow rate of the 1210 base grade is suitable for injection moulding, melt temperatures between 190 °C and 240 °C and mould temperatures between 10 °C and 40 °C are common for LLDPE containers and closures. Peak cavity pressures in semi-crystalline polyolefins generally fall between 40 MPa and 70 MPa; clamp force is calculated from the projected part area and the maximum melt pressure at the gate. Injection speed is adjusted to avoid jetting and shear splay. Long flow paths can cause differential shrinkage; packing pressure and gate freeze-off must be set to maintain dimensional control.
Rotational moulding with LLDPE requires a powder or micropellet form with controlled particle size distribution. Oven peak internal air temperature usually reaches 180–220 °C, and the mould should be cooled to below 70 °C before demoulding to prevent warpage. In rotomoulding, the use of a pelletised film grade may produce poor wall formation; therefore, the exact physical form of YEW 2228 must be confirmed against the packaging code.
Food-contact status for polyethylene is evaluated under FDA 21 CFR §177.1520 and EU Regulation (EU) No 10/2011. Any slip, antiblock, or processing-stabiliser additives present in the formulation must meet specific migration limits appropriate to the food type and contact temperature. REACH registration obligations apply to the European Economic Area, and the product should be checked against the producer’s REACH declaration. RoHS Directive 2011/65/EU compliance for electrical and electronic applications is typically available for natural polyolefin grades when heavy-metal-containing pigments are not added. Processors should not combine this resin with pro-oxidant additives, unsaturated rubber crumb, or amine-based stabilisers outside the supplier’s recommended limits because such additions can reduce oxidation induction time and create melt-processing instability.
Moisture pickup on pellet surfaces can occur in humid storage conditions; although polyolefins are not hydrolytically sensitive, surface moisture may produce splay or surface defects. If condensation is visible, drying at 60–80 °C for 1–2 h using dry-air or desiccant equipment is sufficient. Long drying times at higher temperatures can oxidise the stabiliser package, so a maximum of 4 h at 80 °C should be observed unless the producer specifies otherwise. Published data for the YEW 2228 configuration is limited; industrial trials should be confined to validated process windows and supported by incoming lot testing.