Lyondellbasell Icorene 1210 Whi 1616 Polyethylene Linear Low Density

LyondellBasell Icorene 1210 WHI 1616 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 1210 WHI 1616 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 653853
    Density 0.918 g/cm³
    Melt Index 190 C 2 16 Kg 1.0 g/10 min
    Melting Point 120 °C
    Vicat Softening Point 95 °C
    Tensile Strength At Yield 9.0 MPa
    Tensile Strength At Break 25.0 MPa
    Elongation At Break 600 %
    Tensile Modulus 1 Secant 200 MPa
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 300 g
    Elmendorf Tear Strength Td 400 g
    Haze 12 %
    Gloss 45 60 %
    Coefficient Of Friction 0.20
    Brittleness Temperature -70 °C

    As an accredited LyondellBasell Icorene 1210 WHI 1616 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 1210 WHI 1616 LLDPE is supplied in 25 kg polyethylene-lined paper bags, palletized for industrial handling.
    Container Loading (20′ FCL) 20′ FCL loaded with LyondellBasell Icorene 1210 WHI 1616 LLDPE in 25 kg bags, palletized, stretch-wrapped, and secured for shipment.
    Shipping Typically shipped as free-flowing white pellets in 25 kg polyethylene bags or bulk containers, palletized and stretch-wrapped. Nonhazardous, not DOT/IMDG/IATA regulated. Transport by truck or rail; store dry, cool, away from direct sunlight and ignition sources. Handle to prevent bag damage and moisture contamination.
    Storage Store LyondellBasell Icorene 1210 WHI 1616 Polyethylene, Linear Low Density resin in a cool, dry, well-ventilated warehouse, preferably below 50°C. Keep original packaging closed and palletized, away from direct sunlight, heat, ignition sources, and strong oxidizers. Prevent moisture, dust, and static buildup; ground equipment. Do not store near foodstuffs or incompatible materials. Ensure containers are clearly labeled and follow local regulations.
    Shelf Life Typically 24 months from manufacture when stored in original, unopened packaging in a dry, cool, well-ventilated area away from sunlight.
    Application of LyondellBasell Icorene 1210 WHI 1616 Polyethylene, Linear Low Density
    A 1210 WHI 1616 Polyethylene, Linear Low Density powder is charged as the sole thermoplastic matrix at 100 wt% in the shell layer. No drying is required when the powder has been stored at relative humidity below 60%; otherwise, conditioning at 23–25 °C for 24–48 h is applied to prevent surface pinholes caused by moisture desorption. Where a colour or functional masterbatch is required, the addition is limited to 0.5–2.0 wt% to avoid altering the sintering window and powder flow characteristics. During production, the powder is charged into a preheated cast aluminium or CNC-machined steel mould and processed on a multi-axis carousel or shuttle machine with a biaxial rotation ratio between 1:4 and 1:5. Oven air temperature is typically maintained at 280–320 °C, while peak internal air temperature is held in the 190–215 °C range for 25–45 s to complete particle coalescence and bubble elimination. Termination of heating before the internal air temperature reaches this window produces under-sintered walls with reduced tensile elongation; excess dwell creates oxidative degradation, visible yellowing, and a loss of impact strength. Cooling is conducted with forced air followed by water mist or spray, with demolding initiated between 85–95 °C to limit warpage on large flat tank walls. Finished product types include 500 L to 16,000 L vertical water storage tanks, underground cisterns, rainwater harvesting tanks, and mobile potable water transport tanks. Tank wall thickness is generally maintained between 4.5 mm and 12 mm, depending on design load and sidewall stiffening.Chemical containment vessels fabricated from linear low-density polyethylene powder impose a different set of design and processing constraints. The material’s short-chain branching distribution and narrow powder particle size range support consistent wall fusion in double-wall structures where the inner contact layer must resist aggressive liquid media and the outer layer must withstand external UV and mechanical abuse. Compliance in this application is anchored to EN 13575:2012 for above-ground thermoplastic storage tanks, DVS 2205-1 for lifetime prediction of welded and rotomolded polyolefin tanks, ISO 175:2010 for chemical resistance evaluation under applied strain, and ASTM D1693-15 for environmental stress-crack resistance. The resin is charged at 100 wt% in the chemical contact layer; in dual-layer systems, an external black UV-stabilised polyethylene skin may incorporate carbon black masterbatch at 2.0–2.5 wt%. Post-consumer regrind is excluded from the contact layer when the stored medium contains surfactants or oxidising agents because even small reductions in stress-crack resistance can initiate microcracks at weld lines, threaded insert bosses, and internal rib junctions. In production, a drop-box or multi-shot rotational moulding cycle is used on a carousel machine with independent arm temperature control. The powder charge is sintered at a peak internal air temperature of 200–215 °C, and the mould surface temperature is kept above 180 °C for a period sufficient to fuse the inner and outer shells at intermediate ribs. Pinholing, gel formation, and plate-out on the mould surface are the main process failure modes; these are controlled by maintaining mould release application below 0.3 g/m² and avoiding contamination with fines smaller than 75 µm. Demolding is sequenced after the part reaches an average wall temperature of 90 °C or lower. Finished product types include double-wall chemical dosing tanks from 1,000 L to 10,000 L, secondary containment sumps, wastewater treatment tanks, and intermediate bulk containers for non-potable liquid storage. The most severe operational boundary occurs with surfactant-heavy media at elevated temperatures: sustained service above 40 °C should be validated by full-scale ESCR testing because laboratory coupon data may understate the effect of internal ribs and planar fusion lines.

    Playground Impact Requirements and UV Aging in Outdoor Components

    Rotational moulding of playground components from white UV-stabilised LLDPE requires a narrow processing window because outdoor impact strength and UV retention are both sensitive to thermal history. The material is charged at 100 wt% as the structural resin; where colour variation is specified, masterbatch addition is held between 0.5 wt% and 2.0 wt% to avoid excessive pigment particle loading that reduces crack arrest capacity. The relevant compliance frame includes EN 71-3:2019+A1:2021 for migration of elements, EN 1176-1:2017 for playground equipment safety, and ASTM F963-17 for toy-like components. Processing is carried out on shuttle-type rotational moulding machines using a biaxial rotation ratio of 1:3.5 to 1:4.5; wall thickness is typically controlled from 5 mm to 8 mm to meet impact attenuation and durability requirements. The main production bottleneck is achieving uniform wall thickness around deep-drawn geometries such as slides and climb-through tunnels, where the powder pool may dwell too long in concave pockets and create thickened sections that cool unevenly. Mould surface texturing and post-mould trimming are used to manage aesthetic defects without reducing protective wall thickness. Continuous exposure to UV radiation is acceptable in white grades because the stabilisation package is formulated into the resin; however, thin sections below 4 mm should be avoided in exterior applications where long-term embrittlement is a functional concern. Terminals include rotomolded slides, tunnel elements, activity panels, outdoor seating, and protective housings for play equipment.

    Agricultural sprayer tanks and dry fertiliser hoppers are rotomolded from linear low-density polyethylene powder where chemical resistance, low-temperature ductility, and light weight are required on field equipment. In this segment, the resin is charged at 100 wt% for the tank body; no fillers or plasticisers are introduced because field impact at cold temperatures and resistance to agrochemical concentrates demand an unfilled LLDPE matrix. Functional masterbatches for colour or antistatic property are limited to 1.0–3.0 wt% and must be pre-dispersed in the same polyethylene carrier to prevent delamination and surface voids. Compliance is defined by ISO 16119-2:2013 for crop protection equipment, EN 13575:2012 for thermoplastic tank integrity, and REACH Annex XVII for restricted substances. Production uses rock-and-roll or clamshell rotational moulding machines; the mould is charged with powder and rotated at a ratio between 1:4 and 1:5 while oven air is held at 270–310 °C. Peak internal air temperature is brought to 195–210 °C for 20–40 s to ensure complete fusion at tank ribs and threaded nozzle mounts. The main process failure mode encountered on production lines is deformation at the flat front wall during air cooling; this is controlled by lowering the cooling rate to 1.0–2.0 K/min between 150 °C and 90 °C and by using internal air pressure or water mist cooling in a controlled sequence. Finished product types include 300 L to 3,000 L pesticide spray tanks, fertiliser hoppers, foamer tanks, and secondary chemical mixing vessels mounted on agricultural equipment.

    When Low-Temperature Impact Retention Governs Diesel Tank Wall Design

    The use of white LLDPE powder in off-highway diesel tanks requires careful evaluation of impact retention at sub-zero temperatures and the balance between wall thickness, fuel permeation, and mould cycle time. The resin is charged at 100 wt% for the structural wall; where a pigmented outer layer is specified, carbon black masterbatch is added at 2.0–2.5 wt% in the outer skin only to avoid altering the weld-line integrity of the inner fuel-contact surface. In single-layer diesel tanks, post-moulding fluorination is applied at fluorine concentrations of 0.5–1.5 vol% in nitrogen for 10–30 min at 20–60 °C to reduce fuel permeation. Compliance for such components is anchored to UN ECE R34.01 for fire resistance of plastic fuel tanks, SAE J1681 for impact testing, and ISO 16859-1:2014 for low-temperature mechanical behaviour of polyethylene. In production, a carousel machine with a drop-box or multi-layer charging system is used; the moulder must reach a peak internal air temperature of 205–220 °C to fuse the internal baffle inserts and filler neck boss. The critical processing threshold is the cooling step: rapid water quench from 170 °C to 80 °C can generate residual thermal stresses that reduce low-temperature impact strength at the tank seam. Controlled air cooling at 1.0–1.5 K/min is therefore preferred, even though it increases cycle time by 12–20%. Typical wall sections range from 6 mm to 14 mm, with thicker walls used on lower side panels exposed to stone strike. Field-scale failure data indicate that under-sintering around metal inserts is the dominant cause of diesel weepage after vibration testing; insert bosses must be designed with a minimum wall thickness of 8 mm and preheated to within 10 °C of the mould surface before charging. Terminals include agricultural tractor diesel tanks, generator fuel tanks, off-road vehicle reservoirs, and auxiliary hydraulic oil tanks where resistance to low-temperature impact and outdoor weathering is required.

    In cold-chain material handling, insulated fish boxes and seafood totes utilise rotomolded LLDPE powder as the inner and outer skins because the material resists repeated high-humidity washdown, common cleaning agents, and mechanical abuse at temperatures down to -40 °C. For this segment, the skins are charged at 100 wt%; the core cavity is filled after rotomolding with closed-cell polyurethane foam occupying 60–80 vol% of the internal void to provide thermal insulation. Colour masterbatch, if used in the outer skin, is limited to 1.0–2.0 wt% to prevent a reduction in low-temperature ductility. Compliance is referenced to 21 CFR 177.1520 for food-contact polyolefins, EU Regulation No 10/2011 for plastic materials intended for food contact, and EN 1122:2001 or REACH Annex XVII for trace metal and restricted substance verification. Processing is performed on shuttle or carousel machines with a biaxial rotation ratio of 1:4 to 1:5; the mould is heated to an oven air temperature of 280–310 °C and held to an internal air temperature of 190–210 °C until the powder has coalesced into a void-free skin. The two skins are demolded separately and adhesively bonded or fusion-welded to the foam core, or a single-wall shell is foamed in situ using a two-component polyurethane system with a cream time below 25 s. The principal process limitation is foam exotherm: polyurethane core temperatures above 120 °C can soften the LLDPE skin and cause localised deformation; therefore, the foam must be dispensed in lifts not exceeding 150 mm. Terminal products include 20 kg to 100 kg insulated fish tubs, seafood transport boxes, and cold-chain bins for processed food handling.

    Free Quote

    Competitive LyondellBasell Icorene 1210 WHI 1616 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 1210 WHI 1616 is a linear low-density polyethylene (LLDPE) supplied as a white-pigmented rotational molding powder. The grade designation separates the melt flow/density class, the white color package identified by WHI, and the manufacturer’s additive/package identifier 1616. The product is intended for biaxial rotational molding of parts requiring low-temperature ductility, moderate stiffness, and outdoor surface durability. Published data for this specific configuration are limited; nominal values in this document are drawn from supplier technical literature and standard LLDPE rotomolding practice, and batch-specific conformance must be verified against the certificate of analysis. The material is differentiated from injection molding and blown film LLDPE by its powder morphology, higher melt flow rate for the density class, and the absence of migratory slip/antiblock amides that could compromise paint adhesion or mold release.

    Which Standard Methods Are Used for Density and Melt Flow Rate Confirmation?

    The base resin is characterized in accordance with ASTM D1238 and ISO 1133-1:2022 at 190 °C under a 2.16 kg load. The published nominal melt flow rate for the grade is approximately 12 g/10 min, a value that supports flow into thin ribs and textured mold surfaces under biaxial rotation. Density is measured by ASTM D1505 or ISO 1183-1; the nominal density is near 0.912 g/cm³. Density at this level indicates a higher comonomer fraction than conventional 0.918–0.926 g/cm³ LLDPE film grades, lowering crystalline content and increasing chain flexibility. The powder particle size distribution is usually assessed by ASTM D1921 or standard sieving; a median particle size between 250 μm and 400 μm is typical for rotomolding feedstocks, though the certificate of analysis should be consulted for the specific sieve fraction.

    Property Test method Nominal value Unit
    Density ASTM D1505 / ISO 1183-1 0.912 g/cm³
    Melt flow rate ISO 1133-1:2022 12 g/10 min
    Melting peak temperature ASTM D3418 / ISO 11357-3 122 °C
    Tensile yield strength ASTM D638 / ISO 527-2 10–12 MPa
    Ultimate elongation ASTM D638 / ISO 527-2 >700 %
    Flexural modulus ASTM D790 / ISO 178 230–270 MPa

    The tabulated values are nominal and are not specification limits. Thermal analysis by differential scanning calorimetry frequently identifies a crystallization temperature near 106 °C for this density class. The degree of crystallinity can be estimated by dividing the observed melting enthalpy by 293 J/g for fully crystalline polyethylene; a density of 0.912 g/cm³ corresponds to approximately 30–35 % crystallinity. Oxidative induction time by ASTM D3895 should be evaluated if the powder is stored in heated silos; values below 20 min at 200 °C may indicate stabilizer depletion. Melt flow rate alone does not quantify coalescence or sagging; for mold-filling simulation, oscillatory shear rheometry by ISO 6721-10 across 0.01–100 rad/s at 190 °C provides the necessary viscosity function.

    On production-scale carousel and shuttle rotational molding machines, the grade is processed as a dry blend or directly charged into the mold cavity. Oven air temperature is commonly set between 260 °C and 320 °C, but the control parameter is peak internal air temperature. The densification mechanism requires the mold surface to exceed the crystalline melting band and the adjacent powder layer to sinter. Peak internal air temperature should reach 200–220 °C before cooling; below 190 °C, incomplete coalescence creates subsurface porosity at sharp corners and deep offset ribs, while above 230 °C, oxidative chain scission can yellow the white surface and reduce low-temperature impact. Production audits on carousel machines with mold cavities larger than 0.2 m³ frequently trace low-temperature drop failures to excessive peak internal air temperature rather than to the base resin. For wall thicknesses from 3 mm to 8 mm, rotation ratios of 4:1 are common for symmetric parts; asymmetric parts may require 10:1 or higher tooling-specific ratios. Cooling is staged: forced air at 10–15 °C/min, followed by water mist at 15–25 °C/min, then final forced air. Quenching too rapidly sets residual stresses; a slow cool below 5 °C/min prolongs cycle time and can increase warpage. Residence time at peak internal air temperature should not exceed 20–30 min for sections thicker than 8 mm.

    Powder morphology influences mold fill. The product is supplied as a powder with bulk density typically between 0.45 g/cm³ and 0.55 g/cm³ by ASTM D1895 Method A. Dry flow, measured by ASTM D1895 Method B, should be verified because fines below 100 μm can bridge in hoppers, while particles above 600 μm can produce orange-peel surfaces. If relative humidity exceeds 60 %, pre-drying at 70–80 °C for 2–4 h in a dehumidified hopper reduces moisture defects; thicker sections and cold weather storage increase the need for drying. Silo storage should avoid localized heating above 35 °C, because low-molecular-weight stabilizer components can cause agglomeration and rat-holing. Pneumatic conveying should use short radii and moderate air velocity to prevent fines segregation that alters bulk density and produces inconsistent shot weight.

    Linear low-density polyethylene exhibits anisotropic shrinkage in rotational molding; typical tool shrinkage allowance is 2–3 % for unfilled parts, depending on mold surface temperature and cooling rate. White pigmentation can increase shrinkage slightly by nucleating faster crystallization, but the difference is usually below 0.5 % absolute. Mold surfaces should be vented to allow gas escape during sintering; vent tubes with diameters of 1–3 mm are common. The low melt strength means thick sections can slump on vertical walls if rotation stops before cooling begins.

    Comparative Thermal and Rheological Position Against Film and Injection Molding Grades

    The grade occupies a rheological position between blown film and injection molding LLDPE. Its melt flow rate is higher than film extrusion grades, allowing the powder to densify into narrow ribs and textured surfaces under low shear. The higher comonomer content indicated by the 0.912 g/cm³ density lowers crystalline content and stiffness. The following comparative data are typical industrial ranges; exact values for film and injection molding grades depend on the specific supplier and grade.

    Parameter Icorene 1210 WHI 1616 LLDPE blown film grade LLDPE injection molding grade
    Nominal melt flow rate 12 g/10 min 1–3 g/10 min 20–50 g/10 min
    Nominal density 0.912 g/cm³ 0.918–0.926 g/cm³ 0.924–0.940 g/cm³
    Primary conversion process Rotational molding Blown film extrusion Injection molding
    Typical additive package White pigment plus UV stabilizer Slip and antiblock Nucleating/clarifier
    Melt processing window Oven air 260–320 °C, peak internal air 200–220 °C Die melt 190–240 °C Barrel 200–250 °C

    Compared with higher-density LLDPE film grades, the product exhibits lower flexural modulus and longer environmental stress crack resistance. Falling-weight impact testing of rotomolded parts generally shows ductile deformation at -20 °C for 0.912 g/cm³ grades, while thicker sections of 0.926 g/cm³ film-grade LLDPE can fall below their ductile-to-brittle transition near 0 °C. The higher melt flow rate reduces melt strength, but in rotational molding the melt is not drawn under elongation as in film blowing; the loss of melt strength is therefore less critical. Compared with HDPE rotomolding grades, the LLDPE powder has lower chemical resistance to aromatic and halogenated hydrocarbons and higher oxygen and water vapor permeability. It is better suited to water storage tanks, playground components, marine buoys, and general containers than to fuel or solvent tanks unless permeation testing demonstrates fitness. The finished part can be painted after flame or plasma treatment; pigment and processing additives do not necessarily improve paint adhesion. Grade-specific environmental stress crack resistance should be compared by ASTM D1693; published data for this exact white-pigmented configuration are limited.

    If the White-Pigmented Formulation Is Used Outdoors, What Testing and Additive Interactions Apply?

    The WHI 1616 package indicates white pigmentation and, in standard configurations, an ultraviolet stabilization package. The white pigment is ordinarily rutile titanium dioxide. Rotomolded white parts commonly use titanium dioxide loadings between 1 wt% and 3 wt%, but the exact loading is proprietary. Titanium dioxide can increase low-temperature modulus slightly and can increase melt viscosity at high loadings; dispersive mixing is accomplished before grinding or during extrusion of the compound. Ultraviolet stability should be evaluated by ASTM G154 or ISO 4892-3, not inferred from pigment presence alone. Titanium dioxide plus hindered amine stabilizers can interact with oxygen at the upper end of the oven window; therefore, peak internal air temperature should be held near the lower bound 200–210 °C for white parts unless accelerated weathering data justify a higher peak. Residual peroxides from mold release or cleaning agents can deplete the stabilizer package and should be avoided.

    For food-contact use, base olefin polymer compliance is commonly assessed under FDA 21 CFR 177.1520, and the titanium dioxide colorant may be covered under 21 CFR 73.575 or the appropriate national regulation. European food-contact compliance is evaluated under Regulation (EU) No 10/2011 using migration simulants selected for the intended food type. The white pigment and stabilizer package are not automatically included in base resin certifications; end-use migration testing remains necessary. REACH and RoHS status must be confirmed from the supplier’s batch declaration. The powder should not be blended with plasticized vinyl or acetal scrap during recycling, because acid byproducts from these resins can accelerate degradation of the LLDPE.

    Operational boundaries: the material should not be held at melt temperatures above 240 °C for extended hold-up during compounding or pelletizing because the high comonomer content and stabilizer package can undergo chain scission. Transfer lines and silos should be purged with nitrogen if storage exceeds 48 h at ambient temperatures above 30 °C. When changing from natural to white lots, hopper and grinder cleanup is required to prevent color streaks in subsequent rotomolded parts. Baked-on silicone mold release layers at 10–20 μm thickness are common for complex molds; excessive release agent can transfer to the part surface and reduce paint adhesion. The resin is not recommended for extrusion blow molding or blown film processes without prior compounding into pellet form and re-stabilization, because the powder-grade stabilization and rheology are designed for low-shear biaxial molding.