Lyondellbasell Icorene 1210 Whi 1101 Polyethylene Linear Low Density

LyondellBasell Icorene 1210 WHI 1101 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 1210 WHI 1101 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 353753
    Density 0.939 g/cm³
    Melt Flow Rate 5.0 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 16.0 MPa
    Tensile Strength At Break 20.0 MPa
    Elongation At Break 700%
    Flexural Modulus 758 MPa
    Vicat Softening Point 118 °C
    Brittleness Temperature -70 °C
    Hardness Shore D 55
    Deflection Temperature At 0 46 Mpa 70 °C
    Thermal Conductivity 0.33 W/m·K
    Specific Heat 2.3 J/g·°C
    Thermal Expansion Coefficient 1.5e-4 1/°C
    Water Absorption <0.01%
    Moisture Absorption <0.01%
    Uv Stabilization Yes
    Color White
    Form Pellets

    As an accredited LyondellBasell Icorene 1210 WHI 1101 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 1210 WHI 1101 is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped; 1,000 kg bulk octabins are available.
    Container Loading (20′ FCL) Container Loading (20′ FCL): LyondellBasell Icorene 1210 WHI 1101 Linear Low Density Polyethylene, securely palletized in bags for export.
    Shipping LyondellBasell Icorene 1210 WHI 1101 LLDPE is shipped as non-hazardous resin pellets in 25 kg bags, bulk bags, or octabins on pallets. It is not regulated for DOT, IMDG, or IATA transport. Store in a cool, dry, ventilated area with containers closed; protect from moisture and direct sunlight.
    Storage Store LyondellBasell Icorene 1210 WHI 1101 Polyethylene, Linear Low Density in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and open flames. Keep original containers or bags tightly closed to prevent moisture, dust, and contamination. Follow first-in, first-out stock rotation, avoid prolonged UV exposure, and maintain good housekeeping.
    Shelf Life Typically 12 months when stored in original, unopened packaging under dry, cool conditions, away from sunlight and contamination.
    Application of LyondellBasell Icorene 1210 WHI 1101 Polyethylene, Linear Low Density

    Potable water cisterns are rotomoulded from Icorene 1210 WHI 1101 as a dry-flowing white powder. The mould charge weight is calculated from part surface area, specified wall thickness, and a melt density of 0.935 g/cm³, with an additional 2–4% for parting-line bead trimming. On three-station carousel machines, the oven air temperature is set between 280°C and 300°C. The peak internal air temperature measured through the vent port is controlled at 195–205°C. Lower values leave unmelted powder on the inner wall. Prolonged values above 210°C increase oxidative yellowing. The biaxial rotation ratio for cylindrical cistern bodies is maintained at 4:1. Transition cones use 2:1 to avoid thin sidewall bands. Cooling is staged with forced air to 110°C and atomized water to 60°C before demoulding. The incoming powder lot is verified by ISO 1133-1:2022 at 190°C under 2.16 kg. Significant drift from the supplier’s target alters wall thickness distribution. The resulting shell is tested for hydrostatic integrity and environmental stress crack resistance. ESCR specimens are cut from the moulded wall and tested under ASTM D1693-15e1 Condition B with 10% Igepal CO-630 at 50°C. A minimum failure time of 500 h is a typical acceptance requirement for water tank procurement. Published data for this specific powder grade in potable water service may be limited; the finished tank certification under NSF/ANSI/CAN 61 remains the controlling regulatory document. Terminal articles include 500 L to 10,000 L vertical cisterns, horizontal hauling tanks, and septic safety chambers. The inner wall is not post-painted because coating adhesion on the nonpolar surface requires flame or corona treatment that is not standard in rotomoulding shops.

    StandardScopeCondition
    FDA 21 CFR 177.1520Olefin polymer base for food-contact articlesEnd-use migration limits apply to the moulded article
    Regulation (EU) No 10/2011Plastic materials intended for food contactOverall migration < 10 mg/dm²; specific migration limits for additives
    NSF/ANSI/CAN 61Drinking water system componentsFinished tank certification; contaminant extraction testing
    ASTM D1998-21Polyethylene tanks for above-ground or underground serviceDesign, hydrostatic test, dimensional stability
    RoHS 2011/65/EULead, cadmium, mercury restrictions in homogeneous materialsPb < 1000 ppm; Cd < 100 ppm
    REACH SVHC candidate listEU market accessLot-level confirmation of no listed substances above reporting thresholds

    What Internal Air Temperature Profiles Prevent Pinholing in Chemical Tanks?

    Agricultural sprayer tanks and fertiliser reservoirs are rotomoulded from the same white powder. The critical variable is not the oven set point alone but the peak internal air temperature and the dwell above the crystalline melting region. A peak internal air temperature of 195–210°C held for 3–5 min is used for dense walls without pinholing. The moulding is cooled slowly through the crystalline solidification range. Forced air at 6–10 K/min is applied until internal air reaches 110°C. Atomized water then brings the part to 60°C. This sequence reduces thermal gradients that create inner-wall micro-voids. The rotomoulded tank is inspected for pinholing by light-box and by static pressure test at 1.2 times the rated head. Chemical compatibility is evaluated by ASTM D543-21 immersion at 23°C and 60°C in the actual fertilizer or pesticide formulation, not only in surrogate media. A change in tensile properties greater than 15% after 90 days or visible crazing requires redesign. The terminal articles are boom sprayer tanks, nurse tanks, induction hoppers, fertigation reservoirs, and acid-dosing secondary containment shells. Metallic inserts are avoided at the chemical-contact surface. The moulder should specify plastic bosses welded by heated-tool welding rather than through-bolted metal brackets, because the stress concentration around drilled holes becomes the dominant ESCR failure site under pesticide exposure.

    Marine buoyancy shells produced from Icorene 1210 WHI 1101 demand a different processing envelope than chemical tanks. The low density of 0.935 g/cm³ provides a theoretical buoyancy of approximately 90 kg/m³ relative to seawater. Wall thickness is 6–10 mm for flotation pontoons. The mould charge is calculated for a finished part mass. No chemical blowing agent is used unless a closed-cell foam fill is specified. The rotation ratio for spherical buoys is 6:1. Cylindrical fender shells use 3:1. Peak internal air temperature is controlled at 190–200°C with 4 min dwell. Water absorption is assessed by ASTM D570-22; a 0.01% maximum 24-h gain is typical for unfoamed polyethylene. Low-temperature impact is tested by ASTM D5628-18 or ISO 6603-2. The moulder should test at -20°C and -40°C because sea surface temperatures do not capture Arctic service. The white pigmentation package slows surface gloss loss under UV. Mooring lines and shackle bosses create localized stress and must be reinforced with thick boss walls of at least 1.5 times the shell wall. Terminal articles are harbour marker buoys, aquaculture float collars, floating dock pontoons, dredge pipeline collars, and offshore cable floats. The material is not intended for permanent exposure to aliphatic hydrocarbon sheens unless an external coating or sacrificial layer is specified.

    When the Same Powder Is Dry-Blended with 2.5 wt% Carbon Black for UV-Stabilised Fenders

    For black external fenders, the powder is dry-blended with 2.5 wt% carbon black masterbatch or micronized black in a vertical high-speed mixer at 90–120 rpm for 6–8 min. The mixer is not heated. Dry blending is used instead of melt compounding because the powder form is required for rotational moulding; twin-screw compounding would densify the powder and destroy the 35-mesh particle distribution. Higher loadings above 3.0 wt% increase low-temperature stiffness and reduce melt flow, which may require a 5°C higher oven set point. Lower loadings below 1.5 wt% give insufficient UV shielding for prolonged outdoor use. The dry blend is transferred to the mould by vacuum loader. Segregation across the hopper is checked by filler content per ASTM D5630. Fenders with ribbed back surfaces and metal mounting brackets are rotomoulded in CNC-machined aluminium moulds. Oven air temperature is 285–305°C. The primary and secondary arm speeds are set to achieve a 4:1 rotation ratio. The mould is indexed at the 45° position to densify rib intersections. Peak internal air temperature is held at 200–210°C for 5 min. After demoulding, mounting holes are drilled and stress relief annealing is not required if cooling was uniform. Automotive exterior parts are evaluated under FMVSS 302 flammability and ISO 188 heat ageing at 100°C for 168 h. Dimensional stability is checked after 24 h at 80°C per ASTM D1204-14. Black parts can exceed 70°C surface temperature under direct solar load. If the fender is used as a safety barrier, the moulder must validate impact at the lowest service temperature, not at 23°C only. Terminal articles are truck mudguards, trailer fender extensions, dock edge fenders, and industrial bumper blocks.

    Insulated Food-Processing Bin Wall Formation and Foam-Interface Cooling

    Insulated fish crates, dairy transport boxes, and laboratory sample boxes are produced as double-wall shells. The outer shell is rotomoulded from the powder to a minimum wall thickness of 6–8 mm. The process uses a peak internal air temperature of 190–200°C and a rotation ratio of 4:1. After cooling, a rigid polyurethane foam system with a density of 40–60 kg/m³ is injected into the cavity. The foam exotherm is limited to 80°C against the LLDPE wall because higher interface temperatures cause localized softening and foam-side wall deformation. The foam cream time is specified above 30 s to allow complete filling. Gel time is kept below 120 s to prevent excessive exotherm concentration. Tensile properties of the moulded wall are measured per ASTM D638-14 Type IV specimens cut from flat sections. Flexural modulus is measured per ASTM D790-17. Migration kinetics of the pigment package are governed by Fickian diffusion through the semi-crystalline LLDPE matrix. The moulder must not assume food-contact compliance from the raw material alone. The base polyethylene is assessed under FDA 21 CFR 177.1520. The moulded article must be tested for overall migration under Regulation (EU) No 10/2011 with the intended food simulant. The white pigment package must meet RoHS Pb and Cd limits. Silicone-containing mould release agents are not used on the food-contact surface because they can complicate migration testing. The material is not suitable for hot-fill above 60°C continuous service because the wall may deform under load. Steam sterilization at 121°C is outside the continuous-use envelope. Terminal articles are insulated fish tubs, dairy transport boxes, iced seafood crates, and institutional meal delivery bins.

    Playground slide segments and outdoor furniture panels use the powder in aluminium moulds with deep concave features and grained surfaces. The oven air temperature is reduced to 260–275°C for thin-walled decorative panels below 5 mm. The rotation ratio is held at 5:1 to fill deep slide channels without overbuilding the adjoining flat areas. The mould is cooled with forced air until 100°C, then with water mist to 55°C. Parts are inspected for sink marks around brass boss inserts. Any wall thickness below 3.5 mm at a boss is rejected because impact performance drops below playground safety requirements. The terminal components are slide beds, tunnel sections, climbing rock forms, planter liners, and outdoor seating shells. Compliance is governed by the finished equipment standard, not the polymer alone. ASTM F1487-21 and CSA Z614-20 set the impact and entrapment requirements for public playgrounds. The polymer surface is tested for accelerated weathering under ASTM D2565-23. A crack or a loss of elongation beyond 50% of the original value after 4000 h xenon-arc exposure triggers a formulation review. The processing boundary is corner radius. Radii below 12 mm in moulds increase internal stress concentration and should be avoided unless the moulder has validated the specific geometry by drop-impact testing at -20°C.

    Across Septic and Inspection Chambers, Wall Thickness Is Driven by ESCR Not Impact

    Buried septic tanks, sewage treatment chambers, and inspection risers are rotomoulded as large one-piece shells. For a 2,000 L vertical chamber with a specified wall of 8–10 mm, the oven residence time typically exceeds 40 min because the steel-framed aluminium mould has large thermal mass and ribbed base intersections. The peak internal air temperature is held at 200–210°C for 8–12 min to remove internal micro-voids at the base radius. The cooling phase uses forced air to 100°C then atomized water to 55°C. Demoulding before this temperature range leads to warpage at the lid flange. The governing specification for buried polyethylene tanks is ASTM D1998-21 in North America. EN 12566-1 applies to small wastewater treatment systems in Europe. Environmental stress crack resistance is measured on specimens cut from the moulded wall according to ASTM D1693-15e1 Condition B with 10% Igepal CO-630 at 50°C. Weld lines from moulded-in inserts and the base-to-sidewall junction are tested separately. A minimum failure time of 500 h is common in procurement documents for this sector. LLDPE rotational moulding powders typically exceed 1000 h, but the moulder must confirm the result on the actual wall because cooling history affects crystallinity and ESCR. The terminal articles are septic tank risers, inspection chambers, pump vaults, drainage manifolds, and underground rainwater harvesting shells. Backfill around the buried tank must use a material with a maximum particle size of 25 mm and be compacted to at least 90% of standard Proctor density to avoid point loading on the shell. The material is not intended for contact with gasoline, neat aromatic solvents, or compressed gases without specific permeation testing.

    Free Quote

    Competitive LyondellBasell Icorene 1210 WHI 1101 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 1210 WHI 1101 Polyethylene, Linear Low Density is supplied as a pelletised linear low density polyethylene grade in the Icorene series. The base polymer is a copolymer of ethylene and an α-olefin, produced in a low-pressure process that yields a predominantly linear backbone with controlled short-chain branches. The grade identifier 1210 places the resin within the manufacturer’s melt-flow and density grid, while the suffix WHI 1101 identifies a supplier-specific presentation, typically associated with white pigmentation and an additive package. Public compositional data for the exact WHI 1101 suffix are limited; therefore lot certificates of analysis are required before the material is released into food-contact or cosmetic packaging. The polyethylene base is assigned CAS number 9002-88-4.

    Model Designation and Certification Data Needs

    Incoming inspection should verify that the delivery documents state the full commercial name, LyondellBasell Icorene 1210 WHI 1101 Polyethylene, Linear Low Density, rather than a generic linear low density polyethylene grade. The minimum release parameters stated in standard trade documentation include melt mass-flow rate under ISO 1133-1:2022 at 190 °C and 2.16 kg, density under ISO 1183-1:2019, and tensile properties under ISO 527-2:2012. Thermal softening may be reported under ISO 306:2013. Because the WHI suffix often corresponds to a white-pigmented or additivated stock, the certificate of analysis should also state ash content, pigment concentration, or filler content if applicable. A melt-flow certificate alone is insufficient for lot release when opacity or colour is critical, because pigment dispersion and additive concentration can vary without altering melt-flow rate beyond the test repeatability interval.

    For injection moulding of closures, overcaps, and thin-wall housewares, the first process check is whether the lot melt-flow rate is within the validated window for the tool. On hydraulic injection presses with clamp force from 80 t to 150 t, LLDPE grades of this class are typically started with a rear zone near 170 °C, a middle zone near 190 °C, a front zone near 210 °C, and a nozzle not exceeding 230 °C. Grade-specific processing data for the Icorene 1210 WHI 1101 suffix are limited; initial shot weight, cushion, and hold pressure should therefore be transferred from a validated linear low density polyethylene of matched melt-flow rate and density. Gate-seal studies are required because the shrinkage behaviour of a linear low density polyethylene differs from high-pressure LDPE and can increase sink-mark depth in thick bosses or ribs. Melt residence time above 240 °C should be minimised to avoid gel formation and black specks. If the white suffix is pigmented, moulders should also check the melt cushion during a colour-change or lot-change trial; a shift in cushion stability can reflect pigment agglomeration or feed-bridge formation in the hopper.

    White-pigmented LLDPE batches may show colour streak defects in fast-cycle injection moulding when the pigment masterbatch has been diluted below the carrier-resin compatibility limit. A melt soaking test on a small laboratory extruder can expose agglomerates within 15 min of start-up. If the specific WHI 1101 lot is intended for moulded articles with uniform opacity, the incoming material should be checked by optical microscopy at 100× magnification after compression moulding a thin disc under 190 °C. Published data for the specific WHI 1101 formulation are limited; this test is a general dispersibility screening method used for white polyolefin compounds.

    How Does the Linear Architecture Alter Melt Strength Versus High-Pressure LDPE?

    The principal structural difference is the lower concentration of long-chain branches in linear low density polyethylene. High-pressure LDPE contains long-chain branches that generate extensional strain hardening, high melt tension, and stable bubble geometry during film blowing. In the 1210 WHI 1101 grade, the predominantly linear chains contain short-chain branches from α-olefin insertion; the absence of long-chain branching reduces sag resistance and draw-resonance stability. At equivalent melt-flow rate, the linear polymer may also show lower shear thinning and therefore higher melt pressure in the adapter and die. In extrusion coating, the material is likely to exhibit greater neck-in than high-pressure LDPE unless the die gap is reduced and the draw distance is shortened. In blown film, a higher frost line height or a more aggressive air-ring setting is often required to stabilise the bubble. These architecture-dependent differences are well documented for Ziegler-Natta LLDPE and should be evaluated by torque rheometry and melt strength tests before grade substitution.

    Parallel-plate oscillatory rheometry at 190 °C and 1 % strain provides a more discriminating lot-to-lot comparison than melt-flow rate alone. A frequency sweep from 0.1 rad/s to 100 rad/s can be used to locate the storage modulus cross-over frequency, which is an indirect measure of the relaxation-time distribution. Compared with high-pressure LDPE of similar density, linear low density polyethylene typically shows a higher cross-over frequency and lower low-frequency storage modulus, consistent with reduced melt elasticity. For the WHI 1101 suffix, the base-rheology signature should not be assumed to be identical to clear LLDPE of the same nominal melt-flow rate because inorganic pigment particles can increase low-frequency viscosity and alter yield-stress behaviour. If rheological testing is unavailable, a spiral-flow mould with a fixed clamp force can provide a practical injection-moulding comparator for lot acceptance.

    When the Grade Is Run on Single-Screw Film Lines Equipped with Grooved-Feed Throats

    Single-screw extruders with a grooved-feed throat and a barrier screw of L/D ratio 24:1 to 30:1 are common for LLDPE film and coating. On this equipment class, the die melt temperature should be monitored separately from the barrel set point; sustained operation above 230 °C can accelerate oxidative degradation, die-lip deposit, and odour. The grooved-feed section increases pressure generation and may raise screw torque compared with smooth-bore machines. At constant screw speed, a change from high-pressure LDPE to Icorene 1210 WHI 1101 can increase specific energy input because the linear chains do not shear-thin as readily. Operators should trend screw amperage, melt pressure, and die temperature at fixed intervals. If melt-pressure variation at constant rpm is greater than the normal lot-to-lot envelope, pigment dispersion or feed blockage should be investigated. A screen pack with a 60/80/100 mesh configuration is a useful starting point for pigment dispersion, provided the head pressure remains below the machine limit. In cast-film or extrusion-coating operations, the draw ratio should be reduced relative to high-pressure LDPE because of lower melt tension and earlier onset of edge instability.

    In extrusion coating of paper, board, or aluminium foil, neck-in of the molten curtain is one of the most direct indicators of substitution viability. The shorter the draw length, the less time the web has to deform under extensional stress. For LLDPE, the die gap is frequently set between 0.4 mm and 0.7 mm to increase shear and reduce draw resonance; high-pressure LDPE often tolerates wider gaps. Because the WHI 1101 pigment package can affect surface roughness and adhesion, corona discharge treatment should be set after primer application and verified by wetting-tension testing under ASTM D2578. Published grade-specific adhesion data are limited; the converter should qualify the structure with the exact lot.

    Pre-drying is not normally required for linear low density polyethylene unless surface moisture is visible or the resin has been stored at a relative humidity above 60 % for more than 24 h. When drying is necessary, 70 °C for 2 h in a desiccant or hot-air dryer is a conservative preparation before extrusion. Drying above 80 °C for extended periods can cause pellet softening, bridging, and oxidative yellowing. The material should be kept away from strong oxidising agents, chlorinated solvents, and aromatic hydrocarbons during storage and purging. Avoid purging with halogenated compounds that can generate acidic residues at melt temperature.

    Property Comparisons That Influence Grade Substitution

    Substitution of Icorene 1210 WHI 1101 into an existing LDPE or metallocene LLDPE application should be based on end-use properties rather than melt-flow rate alone. Grade-specific data for the WHI 1101 suffix are limited in public literature; the following table summarises architecture-dependent tendencies under standard test protocols and does not represent release specifications for the grade.

    Architecture-dependent property tendencies for polyethylene classes
    Property or protocolHigh-pressure LDPEIcorene 1210 WHI 1101 class positionMetallocene LLDPE
    Melt tension under extensional strainHighModerateLow-moderate
    Dart impact ASTM D1709LowerIntermediateHigher
    Seal initiation temperature ASTM F1921HigherLowerLower
    Optical haze ASTM D1003LowModerateLow
    Melt fracture onset at high shearLaterEarlierEarlier

    For design calculations, tensile yield strength and elongation at break should be measured on injection-moulded specimens, not on compression-moulded sheets, because orientation and skin-core morphology affect the result. Under ISO 527-2:2012, a type 1A specimen at 50 mm/min is commonly used for polyolefin quality control; the reported values are not design allowables but are sufficient for incoming lot comparison. If the application requires environmental stress-crack resistance, the material should be tested under ASTM D1693 or a notched constant tensile load method, because the Icorene 1210 WHI 1101 grade classification does not automatically guarantee a specific ESCR rating.

    Regulatory Boundary Conditions Under Food-Contact and EU Packaging Frameworks

    Polyethylene grades intended for food contact are assessed under FDA 21 CFR 177.1520(c) in the United States and EU Regulation 10/2011 in the European Union. Compliance is formulation-specific; the WHI 1101 additive package may change overall migration or specific migration behaviour compared with clear LLDPE. Processors should obtain a manufacturer compliance statement for the exact commercial suffix and should not rely on a generic linear low density polyethylene approval. Under REACH, the polymer may fall under the existing polymer exemption if the monomer and auxiliary substances are registered; this does not automatically cover toy or cosmetic standards such as EN 71-3 or EU Regulation 1223/2009. When white pigments are present, the supplier should be asked to confirm that heavy-metal colourants are absent from the formulation.

    Recommended documentation checks for lot acceptance
    ParameterStandard or referenceVerification document
    Melt mass-flow rateISO 1133-1:2022Batch certificate of analysis
    DensityISO 1183-1:2019Batch certificate of analysis
    Tensile yield and elongationISO 527-2:2012Grade data sheet or release test
    Vicat softeningISO 306:2013Grade data sheet
    US food-contact statusFDA 21 CFR 177.1520(c)Manufacturer compliance statement
    EU food-contact statusEU Regulation 10/2011Declaration of Compliance and migration test report

    For non-food industrial applications, RoHS screening is typically limited to cadmium, lead, mercury, hexavalent chromium, and specific brominated flame retardants. Polyethylene is not expected to contain these substances, but the pigment route warrants verification.

    Why Lot-to-Lot Melt Flow Variation Is More Critical in Extrusion Coating Than in Sheet Extrusion

    Extrusion coating is more sensitive to melt-flow variation than thick sheet extrusion because the coating layer is thin and the curtain or melt web has a short draw distance. A small shift in melt-flow rate can alter curtain stability, edge neck-in, coating-weight uniformity, and adhesion to the substrate. On a coating line, melt-flow drift of 0.2 g/10 min can produce measurable changes in coating weight at constant line speed. Sheet extrusion above 1 mm thickness has greater thermal mass and gauge-control authority, so similar variation is less likely to create severe dimensional deviation. For LyondellBasell Icorene 1210 WHI 1101 Polyethylene, Linear Low Density, lots should be trended under ISO 1133-1:2022. If a lot approaches the upper or lower limit of the release window, line speed, die gap, and draw ratio should be adjusted before roll stock is converted.