| HS Code | 162625 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Density | 0.920 g/cm3 |
| Melt Index | 12 g/10 min (190°C/2.16 kg) |
| Tensile Strength At Yield | 9.00 MPa |
| Tensile Strength At Break | 12.0 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 250 MPa |
| Vicat Softening Point | 85.0 °C |
| Melting Point | 123 °C |
| Shore D Hardness | 48 |
| Uv Stabilization | Yes |
| Color | Red |
| Additive | UV Stabilizer |
| Processing Method | Injection Molding |
| Water Absorption | <0.01% |
| Dielectric Constant | 2.3 |
As an accredited LyondellBasell Icorene 1210 UV+ RED 4733 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 1210 UV+ RED 4733 is supplied in 25 kg bags, palletized and stretch-wrapped for bulk shipment. |
| Container Loading (20′ FCL) | 20′ FCL loaded with LyondellBasell Icorene 1210 UV+ RED 4733 Linear Low Density Polyethylene bags, palletized and secured for shipment. |
| Shipping | LyondellBasell Icorene 1210 UV+ RED 4733 is a non-hazardous, UV-stabilized linear low-density polyethylene supplied as red pellets. It is typically shipped in 25 kg bags, octabins, or bulk trucks/containers. Not regulated for transport. Store dry, below 50°C, away from direct sunlight, moisture, and ignition sources; handle per SDS. |
| Storage | Store LyondellBasell Icorene 1210 UV+ RED 4733 Polyethylene, Linear Low Density in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, flames, and strong oxidizing agents. Keep original packaging sealed to prevent moisture, dust, and contamination. Avoid excessive stacking and prolonged high temperatures. Follow first-in, first-out stock rotation. Protect bags from punctures and UV degradation. |
| Shelf Life | Shelf life is 24 months from production when stored in original unopened packaging, protected from direct sunlight, heat, and moisture. |
For rotational moulding of agricultural chemical storage tanks, LyondellBasell Icorene 1210 UV+ RED 4733 is charged directly as a pre-compounded powder. Biaxial rotation ratios of 4:1 are common on shuttle and carousel machines; oven air temperature is set at 270–300 °C, and the peak internal air temperature is held between 190 °C and 210 °C. Wall thickness in this application ranges from 6 mm to 12 mm. Cooling is performed under forced air at 8–12 °C/min until the mould temperature falls below 60 °C. A faster cooling rate reduces warpage on flat sidewalls but can introduce internal stresses at bosses and threaded inserts. Production-scale rotomoulders report that red-pigmented LLDPE of this type may show surface temperature variation of 5–10 °C across the mould during heating when the tool has deep pockets or narrow rib sections. That variation must be managed by adjusting oven residence time rather than by increasing oven air temperature. Chemical exposure tests are specified per ASTM D543-20; tensile property retention after immersion is evaluated with moulded plaques taken from the same lot. The material is suitable for aqueous fertiliser solutions, dilute acids, and dilute alkalies at ambient temperature. It is not suitable for concentrated nitric acid, free chlorine above municipal dosing levels, or aromatic solvents. Tank design and hydrostatic integrity follow ASTM D1998-21. ESCR is monitored by ASTM D1693-15, Condition C; the pass/fail threshold is set by the tank specification. Published data for this specific configuration is limited, so fabricators qualify each lot against the end-tank test programme. For outdoor installation, the UV+ stabiliser system is the controlling additive for maintaining mechanical integrity. The Red 4733 pigment gives a dark surface that heats above ambient in direct solar exposure. Service life estimates are therefore based on accelerated weathering under ISO 4892-3:2016 with a minimum exposure of 2,000 h for agricultural tank pre-qualification. Elongation at break after weathering is tested per ASTM D638-14; retention criteria are negotiated between the moulder and the agricultural equipment manufacturer. The grade should not be dry-blended with unpigmented natural powder when UV performance is part of the tank warranty.
Marine buoy shells are rotationally moulded as hollow single-wall bodies with wall thickness 5–8 mm. The oven set point is reduced relative to agricultural tanks because thin walls reach peak internal air temperature quickly. Peak internal air temperature is limited to 195–205 °C; excursions beyond 210 °C cause pigment darkening and surface pinholes at the mould parting line. Shot weight is controlled to ±1% because small deviations in thin-wall buoy shells create non-uniform wall thickness and weak spots at the mooring eye. After demoulding, shells are filled with closed-cell polyurethane foam of density 35–50 kg/m³. Foam exotherm must not exceed 80 °C at the shell interface; otherwise, local softening and deformation occur. The low surface energy of polyethylene requires flame or plasma treatment before antifouling paint application. Wettability is raised from below 32 mN/m to above 38 mN/m. Adhesion is checked by cross-cut tape test using ISO 2409:2020. Red-pigmented shells show visible chalking earlier than unpigmented white shells when UV stabiliser is partially consumed; therefore, coating application must be completed before significant weathering of stored shells. In coastal service, the stabiliser package protects against salt spray and sunlight; the red colour satisfies navigation visibility requirements. Low-velocity impact from small vessel contact is evaluated by instrumented falling-weight impact per ISO 6603-2:2023 on panels cut from moulded buoy walls. Published data for this specific configuration is limited; pre-production trials should include foam adhesion and seawater immersion on the finished shell assembly.
When road safety barrier shells are moulded as single-piece hollow structures, the cooling step determines crashworthiness and final dimensions. The tool is rotated biaxially at 4:1 and heated in a forced-air oven at 280–300 °C. Wall thickness is 8–12 mm; large flat surfaces require internal air pressure monitoring to prevent ballooning. Mould release is delayed until the average metal surface temperature falls below 70 °C. Premature release causes warpage on the long vertical faces, which later leads to interlocking misalignment and excessive gap between adjacent units. Production-scale fabricators observe that shot-to-shot variation increases when recycled powder fines exceed 10 wt% of the charge; hopper bridging occurs with fines above 15 wt%. The red pigment does not eliminate the need for retroreflective sheeting, but it does provide a high-contrast background under low-light conditions. Barrier shells are filled with water or sand ballast. Moulded-in fill ports and anchor points are formed by inserts; the insert boss radius must not be smaller than 3 mm to avoid stress cracking. The material resists de-icing salts and road runoff but is not intended for continuous exposure to diesel or petrol spills. Low-temperature performance is evaluated by instrumented falling-weight impact per ISO 6603-2:2023 at -10 °C and -20 °C depending on the regional specification. Accelerated weathering per ISO 4892-3:2016 is used to verify that impact retention remains above the agreed threshold after 3,000 h. Published data for this specific configuration is limited; qualification trials are performed on the complete barrier assembly.
Septic tanks, pump chambers, and risers are rotationally moulded with wall thickness 10–25 mm. Fabricators use steel or cast aluminium moulds; internal air pressure control prevents pinholes at the intersection between the wall and bottom corner. A single-layer charge is preferred because sequential charging of multiple layers can produce interlayer fusion defects if the first layer is over-cured. Underground components are subjected to soil pressure, ground-water buoyancy, and occasional vehicle surcharge. Structural design follows ASTM D1998-21 and local load standards. Creep modulus under sustained load is measured by ISO 899-1:2018 on samples cut from moulded walls; the data are used for long-term deflection calculations. Wastewater contains sulfides, volatile fatty acids, and detergent residues. The LLDPE matrix resists these at ambient temperature. Stress cracking resistance is verified under ASTM D1693-15, Condition C, using 100% Igepal CO-630 as the wetting agent. The red pigment has no functional effect in buried service but does not reduce ESCR when the powder is processed within the specified thermal window. Above-grade risers and lids benefit from the UV+ stabiliser package. Continuous service above 60 °C is not recommended because creep resistance falls and stress cracking sensitivity increases. Connections to inlet and outlet pipes are made through rotationally moulded stubs or moulded-in gaskets; the gasket groove must be smooth to avoid leakage paths.
Dry-blending the red UV-stabilised powder with recycled or natural LLDPE is used to reduce cost or to create a bulk core layer. The practice dilutes both the Red 4733 pigment and the UV+ additive package. If 20 wt% natural LLDPE is added, the original stabiliser concentration falls to 80% of the pre-compounded level, assuming perfect distribution. In production, distribution is not perfect because the powder fractions segregate during mould rotation and the recycled fraction may have a different bulk density. The resulting wall can contain local regions of reduced UV resistance and visible colour streaking. Notched impact and ESCR do not decline linearly with dilution; the decline is often faster in the diluted zones. The table below summarises expected trends for equivalent LLDPE rotomoulding powders. Published data for this specific configuration is limited; lot-specific qualification is required.
| Blend ratio (compounded red / uncoloured or recycled) | Relative UV stabiliser concentration | ESCR trend | Colour uniformity risk | Observed processing behaviour |
|---|---|---|---|---|
| 100:0 | 100% | Reference | Uniform | Stable densification; lowest pinhole risk |
| 90:10 | 90% | Slight decline | Minor streak potential | Negligible shift in cycle time |
| 80:20 | 80% | Accelerated decline | Visible streaking reported | Localised pinholes at thin corners |
| 70:30 | 70% | High failure risk in wetting-agent service | Unacceptable for visual parts | Warpage and shot weight variation increase |
Dry-blending is not recommended for tanks governed by ASTM D1998-21 because the standard assumes homogeneous wall properties. If the practice is used for non-regulated covers or counterweights, the final part must be tested for ESCR and UV retention against the original specification. The UV+ package cannot be fully compensated by a separate masterbatch unless the masterbatch is pre-mixed under high-intensity mixing; even then, the recycled fraction may contain residual detergent or oil that reduces stress crack resistance.
Rotationally moulded irrigation tanks in arid regions are exposed to prolonged UV, high daytime temperatures, and low night temperatures. The UV+ package is the controlling variable for service life beyond 10 years in heliothermal environments. The red surface reaches higher equilibrium skin temperatures than white or natural tanks; the oxidative induction time measured by ISO 11357-6:2018 is therefore a more sensitive quality-control indicator than visual colour retention. Tanks are moulded with wall thickness 6–10 mm. Weld line strength at baffles, outlet bosses, and drain fittings is a common failure location when the cooling cycle is too aggressive. Internal air release during cooling must be controlled to avoid vacuum collapse in large flat areas. Water stress cracking at internal fittings is evaluated under constant strain with wetting agents. The grade is resistant to sodium hypochlorite at typical irrigation disinfection levels; continuous exposure to high-concentration chlorine or ozone systems is not recommended. Fittings are fusion-welded or mechanically sealed; sharp threads must be radiused to avoid notch effects. UV retention is confirmed by tensile elongation at break after 2,000 h of ISO 4892-3:2016 exposure; the retention criterion is set by the irrigation equipment manufacturer. Batch-to-batch variation in powder dry flow affects shot weight reproducibility on multi-cavity tools; moisture-related surface pitting from cold storage should be managed when relative humidity exceeds 60%.
Competitive LyondellBasell Icorene 1210 UV+ RED 4733 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 1210 UV+ RED 4733 is a fully compounded rotary-moulding grade of linear low density polyethylene supplied as a dry-flowable powder with a red pigment package and an ultraviolet stabilization system. The grade occupies the Icorene 1210 series; the UV+ suffix indicates formulated outdoor weathering resistance, and RED 4733 identifies the producer-specific red colour concentrate. It is intended for single-layer rotational moulding of large, deep-draw, variable-wall parts where dry-blend colouring can produce streaks and where post-moulding painting is not acceptable.
Specifications are commonly reported by the producer as nominal density per ISO 1183-1, melt flow index per ISO 1133-1 at 190°C with 2.16 kg applied mass, tensile properties per ISO 527-2, flexural modulus per ISO 178, and environmental stress crack resistance per ASTM D1693. The RED 4733 masterbatch and UV stabilizer are melt compounded into the LLDPE powder, so the pigmented product may show small but measurable differences in melt flow and density compared with the unpigmented base. The batch-specific certificate of analysis is the controlling specification; published neutral-source data for this specific coloured configuration is limited.
| Property or characteristic | Test method | Technical role in rotomoulding |
|---|---|---|
| Melt flow index | ISO 1133-1 | Approximates molecular weight; controls melt viscosity and cycle time |
| Density | ISO 1183-1 | Influences stiffness, chemical resistance, and low-temperature ductility |
| Tensile yield stress and elongation at break | ISO 527-2 | Provides short-term mechanical design data |
| Flexural modulus | ISO 178 | Defines rigidity under bending |
| Environmental stress crack resistance | ASTM D1693 | Measures crack resistance under stress and wetting agents |
| Low-temperature brittleness | ASTM D746 or ISO 974 | Establishes cold-weather impact boundary |
| Accelerated weathering | ISO 4892-3 or ASTM G155 | Ranks UV stabilizer and pigment durability |
| Particle size distribution | ASTM D1921 | Controls powder flow, dusting, and surface finish |
| Bulk density | ASTM D1895 | Affects hopper fill, conveying, and mould fill consistency |
Reference windows for rotomoulding LLDPE as a polymer class include density from 0.915 g/cm³ to 0.940 g/cm³, melt flow index from 2 g/10 min to 8 g/10 min at 190°C/2.16 kg, tensile yield stress from 12 MPa to 18 MPa, flexural modulus from 300 MPa to 700 MPa, and elongation at break above 300%. These are material-class reference values, not grade-specific values for Icorene 1210 UV+ RED 4733.
The grade is classified as a polyethylene plastics moulding and extrusion material under ASTM D4976, with the exact cell classification assigned by the producer on the certificate of analysis. The base LLDPE may satisfy the olefin polymer requirements of FDA 21 CFR 177.1520 for food-contact use, but the finished red moulding requires confirmation that the RED 4733 pigment and UV stabilizer package meet the intended food-simulant, temperature, and contact-time conditions. In the European Union, the material is subject to REACH Regulation (EC) No 1907/2006; the safety data sheet sections 2, 3, and 11 provide hazard classification and exposure-control measures for the powder. For electrical or electronic enclosures, the supplier should be required to document compliance with RoHS Directive 2011/65/EU restrictions for lead, cadmium, mercury, hexavalent chromium, PBB, and PBDE in the coloured compound.
Because the product is a pigmented thermoplastic powder, it is not a thermosetting system. It can be reprocessed after demoulding, but repeated heat histories may deplete the UV stabilizer and alter the red pigment dispersion. Scrap rework is typically limited to internally generated regrind and is not recommended for food-contact articles unless supported by migration testing under the relevant national legislation.
When red-pigmented LLDPE is processed in a closed bivalve mould on a shuttle-type rotational moulding machine, the pigment modifies radiant heat absorption compared with natural powder. A red concentrate based on iron oxide or an organic red can shorten the time required to tackify the powder at the mould surface; if oven air temperature is held above 300°C, the outer wall can undergo thermo-oxidative degradation before the inner wall reaches full coalescence. The reliable control is peak internal air temperature, not oven dwell time alone. For this class of rotomoulding LLDPE, peak internal air temperature is usually maintained between 180°C and 210°C before forced-air or water-mist cooling begins. If peak internal air temperature remains below 170°C, incomplete sintering can leave pinholes and reduce tensile elongation at break.
Production-scale shuttle and carousel machines impose fixed oven residence times, so visual colour development in a red powder can mask under-cure. Mould rotation ratios in the range of 4:1 to 8:1 primary and 1:5 to 1:2 secondary are used to distribute the melt; however, rotation cannot compensate for severe wall-thickness imbalances. Thick bosses may remain below peak internal air temperature while thin webs over-cure. Mould design should limit diameter-to-thickness ratios and avoid sharp internal corners that generate stress concentrations. Published data for this specific configuration is limited; machine-specific trials with internal air-temperature probes are the standard method for establishing cycle parameters.
Pigment dispersion in rotomoulding powder is governed by masterbatch carrier compatibility, melt-mixing intensity, and grinding conditions. Poorly dispersed red pigment agglomerates larger than 10 µm can act as stress concentrators in thin-walled sections, lowering notched impact strength and producing visible specks. In fully compounded grades such as Icorene 1210 UV+ RED 4733, the pigment is incorporated into the powder particle during melt compounding and subsequent grinding, which reduces segregation relative to dry-blend masterbatch but does not eliminate the need for particle-size control.
Hindered amine light stabilizers and phenolic antioxidants used in UV+ systems can migrate within nonpolar LLDPE and can be extracted by hot water or aggressive detergents over long immersion. Outdoor failure in red rotomoulded parts generally appears first as gloss loss and micro-cracking, then as tensile embrittlement. Accelerated weathering by ISO 4892-3 or ASTM G155 provides comparative data, but published data for this specific pigment grade is limited. Long-term field exposure should be confirmed under ISO 877 or an equivalent regional outdoor weathering protocol.
Dry-flowable rotomoulding powder is characterized by sieve analysis per ASTM D1921. Ground LLDPE powders typically show a median particle size from 150 µm to 500 µm. Fines below 75 µm improve surface appearance but raise dust and reduce bulk density; coarse particles above 600 µm may not sinter in narrow ribs or engraved details. Because Icorene 1210 UV+ RED 4733 is supplied as a pre-coloured powder, the pigment is distributed inside the LLDPE particle; this reduces colour segregation in hoppers and flexible screw conveyors but makes particle-size control critical for colour uniformity.
Melt flow index for rotomoulding LLDPE is lower than that of injection-moulding LLDPE; a typical range for this product class is 2 g/10 min to 8 g/10 min at 190°C/2.16 kg. Lower melt flow indicates higher average molecular weight and higher zero-shear viscosity, which slows bubble escape but improves environmental stress crack resistance and low-temperature impact. During the heating phase, air trapped between powder particles and gas released from mould release or moisture must dissolve or escape through the melt. Bubble removal depends on viscosity, internal air pressure, and peak temperature; if the melt is too viscous at peak temperature, voids remain at the inner wall and produce micro-porosity that reduces tensile stress at yield.
Moisture on the powder surface is a known process interference. In humid environments, LLDPE powder stored at relative humidity above 60% may carry enough surface moisture to generate steam in the mould; pre-drying in a dehumidified hopper at 60°C to 80°C for 2 h to 4 h is a standard corrective action when surface sorption is suspected. Red-pigmented grades may show surface moisture more readily as uneven colour development during early rotation, but the underlying film formation follows the same densification mechanism.
For agricultural tanks, water-storage vessels, marine buoys, traffic barriers, chemical-containment cabinets, and outdoor equipment enclosures, the product combines LLDPE toughness with a red colour that allows product identification without external painting. The UV+ package is intended for outdoor exposure, but the part design must avoid sharp internal corners, excessive wall-thickness transitions, and moulded-in metallic inserts that create stress concentrations. Compared with unpigmented LLDPE rotomoulding powder, RED 4733 provides opacity and some ultraviolet screening but may reduce notched impact if pigment dispersion is poor. Compared with HDPE rotomoulding powder, the LLDPE base offers higher environmental stress crack resistance and superior low-temperature impact, but lower flexural modulus and lower creep resistance at elevated temperature. Compared with crosslinkable PE rotomoulding powder, the thermoplastic LLDPE remains weldable and reprocessable but does not exhibit the same creep and heat-distortion performance.
| Material class | Density range | Stiffness | Low-temperature impact | ESCR | UV/color package |
|---|---|---|---|---|---|
| Icorene 1210 UV+ RED 4733 LLDPE | 0.915–0.940 g/cm³ | Low to moderate | High | High | Pre-added red 4733 and UV+ |
| Unpigmented LLDPE rotomoulding | 0.915–0.940 g/cm³ | Low to moderate | High | High | Usually none; dry-blend colour optional |
| HDPE rotomoulding | 0.940–0.970 g/cm³ | Moderate to high | Moderate | Moderate | Often unpigmented or black |
| Crosslinkable PE rotomoulding | 0.935–0.960 g/cm³ | Moderate | Moderate to high | Moderate | Often unpigmented; crosslinking required |
In twin-carriage shuttle machines with independent oven and cooling chambers, substituting a fully compounded red powder for a natural powder plus dry-blend masterbatch changes material handling and colour consistency. Dry-blend masterbatch may segregate in hoppers, flexible screw conveyors, and mould fill lines, producing colour striations in deep corrugated parts. The pre-compounded RED 4733 powder eliminates that segregation mechanism because the pigment is within each LLDPE particle. The cleaning burden between colour changes may increase, however, because red pigment deposits on hopper walls and mould surfaces require longer purge cycles. Processors also report that oven dwell time adjustments of ±5% are sometimes required when moving from natural to heavily pigmented LLDPE; the exact shift depends on mould geometry, wall thickness, and the pigment’s infrared absorption behaviour. Published data for this specific configuration is limited, so a machine trial is required to establish internal air-temperature profiles.
The product should be stored in a dry, covered area away from direct sunlight and sources of ignition. For applications involving continuous contact with oxidizing chemicals, aromatic hydrocarbons, or high-pressure hydrocarbon service, the compatibility of the red pigment and UV stabilizer package under stress must be confirmed by testing on the finished article. Accelerated weathering data should not be extrapolated beyond the tested exposure conditions; outdoor warranties for periods longer than 5 years require long-term field data or a validated service-life prediction model. The material is not intended for continuous service above 60°C under sustained load, because creep and stabilizer depletion become design-limiting before the LLDPE melt point is reached.