| HS Code | 399454 |
| Density | 0.921 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 1.0 g/10 min |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 15.2 MPa |
| Tensile Elongation At Break | 800 % |
| Flexural Modulus | 241 MPa |
| Hardness Shore D | 50 |
| Vicat Softening Temperature | 93 °C |
| Melting Temperature | 123 °C |
| Crystallization Temperature | 104 °C |
| Coefficient Of Linear Thermal Expansion | 1.5E-4 cm/cm/°C |
| Mold Shrinkage | 1.5 % |
| Water Absorption | 0.01 % |
As an accredited LyondellBasell Icorene 1210 GRY 7853 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Typically supplied in 25 kg multi-wall bags with polyethylene liners, palletized for secure transport and storage. |
| Container Loading (20′ FCL) | 20′ FCL loading of LyondellBasell Icorene 1210 GRY 7853 Polyethylene, Linear Low Density, palletized and shrink-wrapped for secure ocean transport. |
| Shipping | LyondellBasell Icorene 1210 GRY 7853 Polyethylene, Linear Low Density is shipped as non-hazardous plastic pellets in sealed 25 kg bags, octabins, or bulk trucks/railcars. Store in a cool, dry, ventilated area away from ignition sources, sunlight, and moisture. Not regulated for DOT/ADR/IMDG transport; follow local rules. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep original containers closed and palletized to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking. Maintain ambient temperature and good housekeeping. Use first-in, first-out inventory. Protect bags from punctures and tearing. Keep away from strong oxidizers. |
| Shelf Life | Typical shelf life is 24 months from date of shipment when stored unopened in original packaging, cool and dry. |
LyondellBasell Icorene 1210 GRY 7853 is a grey, pulverized linear low density polyethylene supplied for rotational moulding and dry-blending operations. Where independent published data for the specific 7853 grey variant is limited, the processing windows that follow are aligned with industrial practice for LLDPE rotational moulding powders characterised by a melt flow index of 10 g/10 min to 12 g/10 min under ASTM D1238-20 Condition 190 °C/2.16 kg and density near 0.910 g/cm³ under ASTM D1505.
In single-arm shuttle rotational moulding of vertical chemical storage tanks with nominal capacities from 5,000 L to 20,000 L, the powder is dry-charged into steel or cast aluminium tools after a sacrificial release agent is applied to the cavity. For non-buried thermoplastic storage vessels, the design standard is EN 13575:2012; for cyclic hydraulic loading, hydrostatic pressure tests follow ASTM D1998-21. When the tank is intended for transport of liquid chemicals in an intermediate bulk container, UN certification requires the packaging type to pass bottom lift, drop, stack, and hydraulic pressure sequences specified in the applicable UN protocol. The powder is used at 100 wt% for monolayer walls; if exterior weathering is specified for outdoor installations, a UV masterbatch is dry-blended at 0.2 wt% to 0.5 wt% before charging. On a four-arm carousel machine with a 3,000 mm swing diameter and an arm ratio of 4:1, the oven set point is held at 270 °C to 300 °C, while the internal air temperature at the vent is brought to 180 °C to 220 °C and maintained for 8 min to 15 min depending on wall thickness. Demoulding occurs only after internal air has cooled below 70 °C to prevent sidewall warpage. Finished components include vertical cylindrical tanks, secondary containment bunds, acid and caustic dosing stations, and floor-level process sumps.
Dry-blend coloration of the grey LLDPE powder for outdoor traffic furniture depends on particle-size distribution and liquid pigment compatibility. Roadside components are exposed in ISO 4892-2 Xenon-arc conditions with a target exposure of 3,400 kJ/m²; the moulding material designation is assigned under ISO 17855-1. The addition ratio for liquid pigments is 0.5 wt% to 2.0 wt%, with a phosphite antioxidant co-dispersed at 0.1 wt% to 0.3 wt% to limit oxidative degradation during short high-speed mixing. Mixing is performed in a vertical high-intensity mixer at 800 rpm to 1,200 rpm for 30 s to 60 s; when the powder contains a top-size fraction above 500 µm, pigment wetting becomes uneven and the resultant moulding shows dark and light surface bands. The dry blend is charged at 20 kg to 25 kg per arm in shuttle machines with oven set points from 280 °C to 300 °C and internal air temperature from 190 °C to 210 °C. Storage at relative humidity above 60% without sealed containers can introduce surface moisture that produces pinholes in the outer skin. Terminal products include road bollards, folding sign bases, removable traffic island bodies, and utility marker posts.
| Application | Standard / test method | Critical parameter |
|---|---|---|
| Rotomoulded chemical tanks | EN 13575:2012 / ASTM D1998-21 | Hydrostatic test at 23 °C |
| Outdoor traffic furniture | ISO 4892-2 | Xenon-arc exposure 3,400 kJ/m² |
| Waste containers from recyclate | EN 840-1:2020 | Drop test at -18 °C and 20 °C |
| Masterbatch carrier | FDA 21 CFR 177.1520 | Extraction per 21 CFR migration protocols |
| Playground components | EN 1176-1:2017 | Headform impact criteria |
In reclaim lines processing post-consumer HDPE regrind for 240 L wheeled waste containers, the grey LLDPE powder is metered into the feed throat at 10 wt% to 30 wt% to restore notched impact strength and environmental stress crack resistance lost during multiple heat histories. The governing product standard is EN 840-1:2020 for mobile waste and recycling containers; recyclate traceability follows ISO 15270 and the EU REACH framework for recovered substances. Compounding is run on a single-screw extruder with L/D 30:1, barrel zones from 190 °C to 220 °C, and a slide-plate screen changer with 120 µm mesh to remove tramp contamination. The compound is then injection moulded on a press with clamping force of 8,000 kN to 16,000 kN and a melt temperature of 210 °C to 230 °C. The LLDPE powder addition reduces flexural modulus relative to 100% HDPE regrind; therefore load-bearing internal ribs retain HDPE-rich material and the modification ratio is kept below 30 wt% for stacking stiffness. Published data for the specific 7853 grey grade in mixed recyclate is limited. Finished parts include wheeled refuse container bodies, lifting trunnion reinforcements, and industrial collection bins.
When Icorene 1210 GRY 7853 is used as a carrier for grey and black polyethylene masterbatch, the powder is supplied via loss-in-weight feeder into a co-rotating twin-screw extruder with 44:1 L/D and D/d ratio 1.55. The carrier loading is 40 wt% to 60 wt% of the masterbatch, with carbon black or inorganic pigments at 30 wt% to 45 wt% and the balance a polyethylene wax. The compounding melt temperature is maintained between 180 °C and 220 °C, with screw speed 300 rpm to 500 rpm and a side-feeder discharge temperature below 200 °C to limit wax volatilisation. Underwater pelletizing produces 2.5 mm to 3.5 mm cylindrical pellets. The finished masterbatch is let down at 2 wt% to 5 wt% in natural polyethylene. Compliance for olefin carrier resin in food-contact applications is FDA 21 CFR 177.1520; non-food industrial masterbatch is managed under ISO 9001 batch traceability and EU REACH registration for the pigment and additive package. Terminal products include grey masterbatch granules for rotomoulded traffic components, injection-moulded crates, and film edge-trim recycling compounds.
For outdoor recreational components such as slide hoods, climbing panels, and activity boards, the part is moulded in a clamshell tool with 5 mm nominal wall thickness. The playground safety standard is EN 1176-1:2017 for general safety, while U.S. production follows ASTM F1487-21 for impact attenuation zones. The powder is used at 100 wt%; where colour is not supplied in the grey base, external colour matching is achieved by dry-blending 1 wt% to 2 wt% of a PE-based masterbatch. The primary rotational axis runs at 8 rpm to 12 rpm, the secondary axis at 1 rpm to 2 rpm, and oven temperature is held at 280 °C to 300 °C until internal air reaches 190 °C to 210 °C. Forced-air cooling then reduces internal air to 70 °C before ejection; demoulding above this threshold causes panel warpage and brittle failure in drop tests. The moulded wall thickness is verified by ultrasonic gauge at 5 points per panel. Terminal products include slide canopies, activity panels, and tunnel sections installed in public playgrounds.
Competitive LyondellBasell Icorene 1210 GRY 7853 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 1210 GRY 7853 Polyethylene, Linear Low Density is a pre-pigmented rotomoulding powder produced from a linear low-density polyethylene base resin. The suffix GRY 7853 designates a gray colorant system; the base Icorene 1210 grade is an ethylene/alpha-olefin copolymer intended for low-shear, biaxial rotational moulding of hollow parts. Published data for this exact gray-pigmented variant are limited relative to the natural base grade; therefore, compliance statements for a particular production batch should be derived from the supplier’s certificate of analysis and retained sample data rather than from generic class values. The powder is supplied as a free-flowing, high-bulk-density material with a particle-size distribution suitable for 35 mesh (500 µm) processing. Apparent density values for this class of rotomoulding LLDPE typically fall in the range 0.36–0.42 g/cm³ under ASTM D1895, and dry-flow consistency is assessed by the same standard using a 2.54 cm orifice. Particle-size distribution is characterized by ASTM D1921, and the product is designed to minimize fines below 75 µm, which can cause powder bridging in narrow mold passages.
Medium-flow rotomoulding LLDPE formulations of this type are commonly associated with a melt flow rate of 3–5 g/10 min at 190 °C under 2.16 kg load according to ISO 1133-1:2022 or ASTM D1238-23a, and with a density near 0.925–0.940 g/cm³ according to ISO 1183-1:2019 or ASTM D792-20. The lower density and reduced crystallinity relative to high-density polyethylene produce lower flexural modulus but substantially higher environmental stress crack resistance as measured by ASTM D1693-15 and improved low-temperature impact resistance as measured by ASTM D746-20. The actual property set of the gray variant may differ from natural Icorene 1210 because the pigment phase can nucleate crystallization and alter the amorphous tie-molecule population.
| Property | Test Method | Typical Range |
|---|---|---|
| Density | ISO 1183-1:2019, ASTM D792-20 | 0.925–0.940 g/cm³ |
| Melt flow rate | ISO 1133-1:2022, ASTM D1238-23a (190 °C, 2.16 kg) | 3–5 g/10 min |
| Tensile strength at yield | ISO 527-2:2021, ASTM D638-22 | 10–20 MPa |
| Tensile elongation at break | ISO 527-2:2021, ASTM D638-22 | 600–1000% |
| Flexural modulus | ISO 178:2019, ASTM D790-17 | 400–800 MPa |
| ESCR, 100% Igepal | ASTM D1693-15 | >300 h |
| Brittleness temperature | ASTM D746-20 | < -60 °C |
| Vicat softening temperature | ISO 306:2022 | 90–120 °C |
The linear low-density classification indicates that the polymer backbone contains short-chain branches introduced by copolymerization with butene, hexene, or octene. The comonomer type and distribution influence slow crack growth resistance and melt elasticity. Rotomoulding LLDPE formulations often favor butene or hexene comonomer for balanced impact and processability, while octene-based resins may provide higher toughness at similar density. The exact comonomer for Icorene 1210 GRY 7853 is not always disclosed; the supplier may provide infrared or high-temperature gel permeation chromatography data for root cause analysis of batch-to-batch variation when downstream quality issues occur.
Unlike LLDPE film resins that are often melt-flow-indexed near 1.0 g/10 min and processed in blown-film dies at melt temperatures above 200 °C, the Icorene 1210 class is supplied as a powder with a controlled particle-size distribution for rotomoulding. The rotomoulding process does not use high-shear plastication; instead, the powder is placed in a cold or hot mold and exposed to convection and radiant heat in an oven, followed by cooling. A medium melt flow in the 3–5 g/10 min range is selected to promote powder coalescence and bubble collapse without excessive sag or pinhole formation. Injection moulding LLDPE grades are often formulated with lower molecular weight or higher melt flow to fill thin-wall molds under 70–140 MPa injection pressure, whereas rotomoulding powder must exhibit sufficient low-shear melt strength to remain on the mold wall during rotation and to form a uniform wall thickness without internal voiding.
Compared with HDPE rotomoulding grades having a density of 0.940–0.957 g/cm³, the LLDPE backbone of Icorene 1210 GRY 7853 has lower stiffness and lower heat deflection temperature, but typically offers higher environmental stress crack resistance and better low-temperature ductility. This positions the material for applications where frequent thermal expansion, chemical exposure, or impact loading occurs. The gray precompound differs from natural powder dry-blended with color concentrate because the pigment is dispersed into the polymer at the resin supplier level, reducing color streaks, pigment agglomerates, and variability associated with operator dosing. The trade-off is that the moulder cannot adjust color loading on-site and must verify that the precompounded pigment affects the rotomoulding thermal profile.
Processing trials on instrumented rotomoulding machines indicate that gray-pigmented LLDPE powders may absorb radiant heat differently from natural or white powders. A gray or black pigment can increase the rate of surface temperature rise in the mold, potentially shortening the time to reach a given peak internal air temperature by several minutes relative to an unpigmented powder at the same oven setpoint. This effect is dependent on mold material, mold wall thickness, oven emissivity, and pigment concentration. Therefore, cycle settings validated for natural Icorene 1210 should not be transferred directly to Icorene 1210 GRY 7853 without instrumented verification. On carousel or shuttle machines with propane-fired ovens, rotomoulding LLDPE parts with a nominal wall thickness of 6 mm are commonly processed with oven setpoints of 260–320 °C, peak internal air temperature targets of 190–205 °C, primary-axis rotation speeds of 4–8 rpm, and secondary-axis speeds of 0.8–2.0 rpm. Mold release agents and venting configurations must be selected to avoid surface defects caused by pigment plate-out or off-gassing.
The effective processing window for medium-flow LLDPE rotomoulding powder lies between sufficient coalescence and the onset of oxidative degradation. If the peak internal air temperature remains below approximately 180 °C, powder particles may fuse incompletely, leaving pinholes, internal bubbles, or low burst strength. If the peak internal air temperature exceeds 210–220 °C for extended periods, the antioxidant package can be consumed, and the material may display yellowing, release of volatile degradation products, and a decline in impact and tensile properties. The practical width of the acceptable window is often no more than 10–15 °C for a fixed wall thickness and oven cycle; this requires thermocouple or digital data logger control rather than simple timer-based oven residence.
Oxidative stability of stabilized rotomoulding LLDPE is frequently characterized by oxidation induction time under ISO 11357-6:2018 or ASTM D3895-19 at 200 °C. Stabilized formulations used in long-life outdoor tanks may show an initial OIT above 20 min, but repeated recycling of trimmed flash and in-mold residence at high temperature reduce the active stabilizer reservoir. The gray pigment can accelerate surface heating and may also contain transition-metal components that influence oxidation kinetics; therefore, the OIT of the final rotomoulded article should be measured on a representative wall section rather than on the raw powder alone. Differential scanning calorimetry under ISO 11357-3:2018 can detect shifts in crystallization onset temperature between natural and pigmented samples; pigment-induced nucleation of 1–3 °C has been reported in some polyolefin colorant systems. A higher crystallization onset may enable earlier demolding after cooling but can also increase crystallite population and reduce slow crack growth resistance if cooling is too rapid.
Typical application fields for gray rotomoulding LLDPE include agricultural chemical tanks, water-treatment housings, industrial storage containers, outdoor furniture shells, marine fenders and buoy shells, automotive fender liners, and equipment covers requiring low-temperature impact and environmental stress crack resistance. The gray coloration is often selected where a neutral dark appearance is desired or where the end-use environment tolerates higher surface temperatures. In outdoor service, gray parts can reach higher equilibrium skin temperatures than white or light-colored parts under solar loading; this thermal condition accelerates oxidative induction time consumption and may require additional stabilization. Weathering resistance of rotomoulded articles is assessed by ASTM D2565-16 or ISO 4892-2:2013, with property retention judged by ISO 527-2:2021 tensile elongation after exposure. If the application requires potable-water contact, the final article, not merely the base resin, must satisfy the applicable regulatory requirements such as FDA 21 CFR 177.1520 in the United States or EU Regulation (EU) No 10/2011 and relevant national migration limits in the European Union. The use of a pre-compounded pigment does not automatically confer food-contact approval; the pigment composition and final extraction behavior must be documented.
On production-scale rotomoulding lines, common failure modes observed with pigmented LLDPE include pinholes at weld lines, localized wall thinning in deeply recessed mold cores, internal bubble coalescence failure, and color streaking when the powder is improperly handled or stored. These defects are usually addressed by adjusting the mold rotation ratio, adding or relocating vents, reducing mold surface temperature, or changing the loading procedure rather than by increasing peak internal air temperature above the degradation threshold. The powder should be stored in sealed containers at low humidity; although polyethylene is not hygroscopic, surface condensation on cold powder taken into a warm molding bay can introduce moisture that forms steam pinholes during heating. If storage occurs above 60% relative humidity or the powder temperature is below the dew point, pre-drying at 40–60 °C for 2–4 h in a desiccant-bed or hot-air dryer is common practice. The material should not be mixed with polypropylene, polyvinyl chloride, acetal, or ionomer purge compounds, because incompatible phases can create delamination and surface defects in the rotomoulded part.
| Item | Method or Equipment | Parameter or Limit |
|---|---|---|
| Melt flow rate | ISO 1133-1:2022, ASTM D1238-23a | 190 °C, 2.16 kg |
| Oven setpoint | Rotomoulding shuttle or carousel, propane-fired | 260–320 °C |
| Peak internal air temperature | Digital data logger with thermocouple | 190–205 °C |
| Powder apparent density | ASTM D1895 | 0.36–0.42 g/cm³ |
| Particle size | ASTM D1921 | < 500 µm, minimize < 75 µm fines |
| Oxidative stability | ISO 11357-6:2018 | Initial OIT > 20 min at 200 °C |
| Weathering resistance | ASTM D2565-16, ISO 4892-2:2013 | Property retention per product specification |
| Pre-drying threshold | Hot-air or desiccant dryer | Only if condensation at > 60% RH; 40–60 °C for 2–4 h |
Published data for the exact GRY 7853 gray variant are limited; therefore, the values in this document are class-typical for medium-flow rotomoulding LLDPE and are not a substitute for the supplier’s certificate of analysis. The moulder should establish batch-specific process conditions through instrumented mold trials and should retain molded plaques for laboratory testing according to the methods listed. Particular attention is required when the material is used in applications with repeated chemical exposure, because environmental stress crack resistance depends on the combined effect of stress, temperature, and the specific chemical environment; material selection should be confirmed by immersion testing under representative service conditions rather than by density or melt flow rate alone.