Lyondellbasell Icorene 1210 Gry 7264 Polyethylene Linear Low Density

LyondellBasell Icorene 1210 GRY 7264 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 1210 GRY 7264 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 970691
    Density 0.939 g/cm³
    Meltmassflowrate 190c 2 16kg 3.5 g/10 min
    Tensilestrength At Yield 17.2 MPa
    Tensilestrength At Break 15.2 MPa
    Elongation At Break 700 %
    Flexuralmodulus 758 MPa
    Vicatsofteningtemperature 111 °C
    Meltingpoint 124 °C
    Hardness Shored 55
    Notchedizodimpact 0.534 J/cm
    Deflectiontemperature At 0 46mpa 60 °C
    Coefficientoflinearthermalexpansion 1.5E-4 cm/cm/°C

    As an accredited LyondellBasell Icorene 1210 GRY 7264 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 1210 GRY 7264 Polyethylene, Linear Low Density is supplied in 25 kg bags, palletized and stretch-wrapped.
    Container Loading (20′ FCL) LyondellBasell Icorene 1210 GRY 7264 Polyethylene, Linear Low Density loaded in 20-foot FCL container; palletized bags, dry, secure, ambient stowage.
    Shipping LyondellBasell Icorene 1210 GRY 7264 Polyethylene, Linear Low Density is shipped as non-hazardous resin pellets in 25 kg bags or 1,000 kg bulk bags, palletized and stretch-wrapped. It is not DOT/IMDG/ADR regulated. Store cool, dry, away from heat, sunlight, and ignition sources. Handle carefully to avoid package damage.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers or bags tightly closed to prevent moisture, dust, and contamination. Avoid contact with strong oxidizers, acids, or bases. Maintain stable, labeled packaging, protect from physical damage, and follow the SDS and local regulations. Prevent pellet release into drains or the environment.
    Shelf Life Shelf life is 24 months from production when stored in original unopened packaging, dry, below 30°C, away from sunlight.
    Application of LyondellBasell Icorene 1210 GRY 7264 Polyethylene, Linear Low Density

    Rotomoulded Chemical Storage Vessels Depend on a Controlled Cooling Window

    The LyondellBasell Icorene 1210 GRY 7264 linear low density polyethylene grade is charged as a 35-mesh powder into cast aluminium or fabricated steel moulds on carousel-type rotational moulding machines with biaxial rotation ratios between 3.6:1 and 4.2:1. The polymer is distributed under gravity and centrifugal force as the mould rotates through an oven air setpoint of 270–305°C; internal air temperature is held at 185–225°C until full particle coalescence is confirmed by sacrificial trial parts or process temperature logging. Type K thermocouples inserted through vent ports record internal air temperature every 5 seconds to initiate cooling automatically. Cooling then proceeds through forced ambient air followed by light water mist only after the mould surface temperature drops below 70°C. Early water quench on wall sections thicker than 8 mm creates non-uniform crystallinity gradients and can lock in warpage of 1–3% of the nominal tank diameter, while excessively slow air cooling may extend cycle time without improving impact strength. Formulation for this application is 100 parts by weight of Icorene 1210 GRY 7264; if tropical UV service is specified, a HALS/UV masterbatch is dry-blended at 0.5–1.5 phr in a high-speed blender operating at 1,200–1,800 rpm for 3–5 minutes. Handling must avoid surface condensation above 0.3 wt% because steam pinholing occurs at the mould wall interface. Compliance for industrial chemical storage tanks is anchored to ASTM D1998-15 for upright storage tanks, ASTM D4976-12a for polyethylene moulding and extrusion materials, and FDA 21 CFR 177.1520 for olefin polymers where incidental food-contact sections are required. Terminal finished product types include vertical chemical storage tanks up to 10,000 L, secondary containment basins, and rotationally moulded outer shells for intermediate bulk containers, with wall thickness typically 3–10 mm depending on diameter and hydrostatic head. Published data for this specific grey-pigmented configuration is limited, so tank wall thickness calculations should be verified against hoop stress from ASTM D1998 and supplier-certified tensile yield data.

    In agricultural crop-protection sprayer tank rotomoulding, the process sequence from the storage-tank scenario is modified by double-wall construction or a vented mould design to compensate thermal expansion of internal air during demoulding. The base polymer charge remains 100 wt% Icorene 1210 GRY 7264, but a high-density polyethylene outer skin may be charged first at 15–25 wt% of total shot weight where additional environmental stress crack resistance against dilute pesticide formulations is required. The mould is indexed through a first oven pass at 255–285°C to fuse the skin, followed by a second pass after the LLDPE charge at 270–300°C; the internal air temperature is kept below 220°C during the second pass to avoid interfacial discolouration. For tanks intended as IBC or portable agricultural packaging, type approval may require a drop test at −18°C under the relevant UN packaging code, and material traceability requires batch-level melt flow rate records under ASTM D1238-20 at 190°C and 2.16 kg. The finished component is marked according to ISO 11469:2016 with the polymer code and colour or filler designation. Terminal finished product types include tractor-mounted sprayer tanks, fertilizer distribution tanks, and drift-control water tanks, with volumes commonly between 150 L and 3,000 L.

    What Limits Thin-Wall Injection Moulding of Heavy-Duty Logistics Bins and Hopper Liners?

    Thin-wall injection moulding of Icorene 1210 GRY 7264 is limited less by melt flow than by differential shrinkage across flow and transverse directions. The grade is processed on a reciprocating-screw injection moulding machine with a screw L/D ratio between 20:1 and 24:1, a compression ratio of 2.5:1–3.0:1, and a reverse-taper nozzle to prevent drool. Melt temperature is maintained at 200–230°C, and the mould is held at 15–40°C with turbulent water channels. Injection pressure of 70–100 MPa is common for wall sections of 1.8–3.0 mm; below 1.8 mm, flow length should be calculated against a spiral flow test rather than assumed from HDPE data. Shot-to-shot variation in cushion should not exceed 2–3 mm, otherwise gate freeze-off becomes inconsistent and causes sink marks near bosses. Valve-gated hot runners are preferred over edge gates for thin-wall LLDPE because extended flow paths cause premature freeze-off at gate thickness below 60% of the wall. Formulation addition is 100 wt% Icorene 1210 GRY 7264, with up to 20 wt% of post-industrial regrind permissible where logistics containers are not food-contact. The regrind fraction should be sieved through a 40-mesh screen and dried to surface moisture below 0.2 wt% if stored outdoors. Compliance testing for this sector uses ASTM D4976-12a for material classification, ASTM D638-14 for tensile yield at 50 mm/min, ASTM D256-10 for Izod impact, and ASTM D790-17 for flexural modulus. Terminal finished product types include collapsible bulk bins, freezer-grade distribution totes, hopper liners for bulk solids handling, and food-contact reusable trays only when supported by FDA 21 CFR 177.1520 or EU No 10/2011 migration testing. A process limitation is continuous service above 50°C; LLDPE’s lower flexural modulus compared with HDPE makes unsupported sidewalls prone to creep under sustained load.

    Incoming-lot testMethodCondition
    Melt mass-flow rateASTM D1238-20190°C, 2.16 kg
    DensityASTM D150523°C, gradient column
    Tensile yield stressASTM D638-14Type IV, 50 mm/min
    Flexural modulusASTM D790-172%/min
    Izod impact, notchedASTM D256-1023°C
    Environmental stress-cracking resistanceASTM D1693-15Condition B, 10% Igepal

    When grey-pigmented LLDPE powder is specified for marine fuel tanks and automotive fluid reservoirs, the moulding cycle differs from industrial tank production primarily in cooling control, insert integration, and fuel permeation validation. Brass or stainless-steel threaded inserts are placed in the mould before charging to avoid post-machining stress concentrators; the powder charge remains 100 parts by weight Icorene 1210 GRY 7264. Where additional UV stabilization is required for open-cockpit marine service, a HALS/UV masterbatch is dry-blended at 0.5–1.0 phr, but excessive masterbatch above 1.5 phr can lower weld-line strength at insert bosses. Oven air temperature is reduced to 255–290°C for aluminium moulds with wall thickness below 6 mm to prevent over-heating at thin sections. Internal air temperature is held at 180–210°C and the cooling phase uses a slow ambient-air ramp to below 60°C before demoulding; this reduces insert pull-out from differential shrinkage between metal and LLDPE. For marine petrol tanks, final component testing is aligned with ISO 21487:2012 and any applicable EPA evaporative emission requirements, while automotive fluid reservoirs are validated for burst pressure and coolant ageing according to OEM specifications. Terminal finished product types include outboard fuel tanks, auxiliary diesel day tanks, windshield washer reservoirs, and coolant overflow bottles, with nominal wall thickness of 3–8 mm. The operational boundary is petrol containing high aromatic fractions; long-term fuel swelling should be measured under CE10 or CE85 test fuels because LLDPE gains mass in hydrocarbon service, and published data for this specific grey-pigmented configuration is limited.

    Film Extrusion Parameters for Heavy-Duty Industrial Liners and Flexible Intermediate Bulk Containers

    Blown film extrusion of Icorene 1210 GRY 7264 requires a blend with low density polyethylene to stabilize the bubble. A formulation of 70–85 wt% Icorene 1210 GRY 7264 and 15–30 wt% LDPE is processed on a single-screw extruder with an L/D ratio of 25:1–30:1, a barrier screw with Maddock mixing section, and an annular die gap of 1.2–2.2 mm. Melt temperature is kept between 190°C and 220°C; the blow-up ratio is set at 2.0:1–2.8:1 and frost-line height is controlled between 1.5 and 2.5 die diameters. The LLDPE fraction reduces melt tension compared with HDPE, so screw speeds above 100 rpm on a 30:1 L/D extruder can introduce interfacial bubble instability and gauge variation exceeding ±15%. Where the film is converted into flexible intermediate bulk container baffle panels or liners, compliance testing uses ASTM D882-18 for tensile properties, ASTM D1709-16a for dart impact, and ASTM D6693 for geomembrane tensile and tear where applicable. Terminal finished product types include industrial heavy-duty liners, FIBC side panels, and temporary containment films, in thicknesses from 80 µm to 300 µm. The processing boundary is low melt strength; blends with LDPE below 15 wt% may not maintain bubble stability on high-output lines, while LDPE above 30 wt% lowers puncture resistance in the finished liner.

    If Outdoor Electrical Enclosures Require Impact Resistance at Sub-Zero Temperatures

    Outdoor electrical and telecommunications enclosures are rotomoulded from Icorene 1210 GRY 7264 using fabricated steel or cast aluminium moulds with large flat panels. The powder charge is 100 parts by weight of the grey-pigmented grade; where long-term exposure above 10 years is specified, a HALS/UV stabilizer masterbatch is dry-blended at 0.5–1.0 phr. The mould is heated at 260–290°C and internal air temperature is limited to 185–215°C; large flat walls require slower rotation and longer coalescence time to avoid crawling defects at corners. Cooling is performed in still ambient air between 15°C and 25°C, and the part is left on the mould until surface temperature falls below 55°C to minimize panel warpage. The final enclosure is tested for flammability according to UL 94 HB and horizontal burn rate under ASTM D635, and the material meets RoHS Directive 2011/65/EU and REACH Regulation EC 1907/2006 raw material obligations. Terminal finished product types include padmount transformer covers, traffic control cabinets, telecom vaults, and signal junction enclosures, with wall thickness between 5 mm and 12 mm. A key limitation is that polyethylene does not provide inherent flame retardancy; enclosures requiring UL 94 V-0 are outside the operating range of this grade unless an intumescent coating or approved flame-retardant masterbatch is applied and validated for the full assembly.

    Free Quote

    Competitive LyondellBasell Icorene 1210 GRY 7264 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 1210 GRY 7264 Polyethylene, Linear Low Density is supplied as a precompounded gray linear low density polyethylene, with the suffix GRY 7264 identifying the gray pigment formulation rather than a natural resin or a post-process dry color addition. The product designation places the material in the LLDPE family, which distinguishes it from high-pressure LDPE and from higher-density ethylene copolymers through comonomer-controlled short-chain branching. Published independent data for this exact gray-compounded configuration is limited; converter qualification therefore depends on the supplier certificate of analysis, which reports melt mass-flow rate according to ASTM D1238 or ISO 1133-1:2022 at 190 °C under 2.16 kg load, density according to ASTM D792 or ISO 1183, and often additional thermal or mechanical values specific to the manufacturing lot. Typical LLDPE resins in the same class occupy a melt mass-flow rate band of 3–5 g/10 min and a density band of 0.915–0.925 g/cm³; these class boundaries are not a substitute for the purchase specification. The gray compounding step introduces operational controls not present in natural resin: pigment dispersion, carrier-resin viscosity match, letdown ratio, and the effect of gray colorants on rheology must be controlled. On production-scale compounding equipment such as a 75 mm twin-screw extruder with an L/D of 44:1 and underwater pelletising, poor gray uniformity is more often caused by feeder segregation of the pigment masterbatch than by screw speed. A first-article evaluation on a laboratory-scale line is therefore required before large-lot commitments.

    What Separates Icorene 1210 GRY 7264 From High-Pressure LDPE and HDPE?

    The structural difference is not a minor shift in density; it is a change in molecular architecture. LLDPE is polymerised with an α-olefin comonomer such as 1-butene, 1-hexene, or 1-octene, producing a linear backbone with short-chain branches of controlled length and spacing. High-pressure LDPE receives long-chain branches from free-radical propagation. That architectural distinction gives LLDPE class materials a combination of improved tensile elongation, dart impact, and environmental stress crack resistance relative to general-purpose LDPE at the same melt index. However, the linear backbone also reduces melt strength, increases shear viscosity at high extrusion rates, and lowers extrudate swell. Replacement of LDPE with LLDPE in an existing tool or profile die is not a drop-in substitution; die swell differences change wall-thickness distribution in blow moulding, and melt-temperature readings may shift because of higher viscous dissipation. Compared with HDPE, the LLDPE base under consideration sits in a lower-density range, providing higher low-temperature impact and ESCR but lower flexural modulus and heat deflection temperature. The following class-level comparison is drawn from general polyolefin grade data, not from the exact gray lot, and is intended to position the material rather than serve as a specification.

    Resin classDensity by ASTM D792 (g/cm³)MFR by ASTM D1238 (g/10 min, 190 °C/2.16 kg)Processing / property trade-off
    High-pressure LDPE0.910–0.9250.2–70Higher melt strength; lower ESCR and tensile strength
    LLDPE class under discussion0.915–0.9253–5Higher ESCR; lower melt strength and higher extrusion torque
    MDPE0.926–0.9400.7–4Higher stiffness; lower low-temperature impact
    HDPE0.941–0.9650.2–20Higher heat deflection temperature; reduced ESCR

    For Icorene 1210 GRY 7264, the gray color package can shift the comparative position slightly: if the pigment carrier resin is a high-flow LLDPE or an LDPE, the melt mass-flow rate of the final compound may be higher than the base powder, while density may increase by a small but measurable amount. Because published data for this specific configuration is limited, the direction and magnitude of these shifts require a lot-specific measurement rather than class-average prediction. Compared with metallocene-catalysed LLDPE, a conventional Ziegler-Natta LLDPE of the same density and melt index can have a broader composition distribution and slightly lower dart impact, but easier processability in thick parts. The distinction matters for rotomoulded parts with high wall thickness, where fast sintering and low shear are more important than film-grade clarity.

    Short-chain branching density and comonomer type control environmental stress crack resistance in ethylene copolymers. When a gray LLDPE grade is specified for industrial containers or outdoor housings, the first technical issue is not color, but whether the comonomer distribution and molecular weight are sufficient to resist slow crack growth in the presence of a stress-cracking medium such as a surfactant solution. The accepted comparative test is ASTM D1693, usually reported under condition B or C; higher failure times generally correspond to higher molar mass and more uniform comonomer incorporation. A production-scale failure mode observed on compression-moulded plaques is not cracking through the wall, but surface microvoiding caused by pigment agglomerates acting as stress concentrators. For this reason, the gray pigment dispersion is not an aesthetic variable; it is a mechanical variable that can reduce ESCR if the pigment package is not fully dispersed. In injection moulding or rotomoulding, fountain-flow effects can push poorly dispersed pigment to the inner surface, creating a weak boundary layer. Processors who test only tensile yield and ignore dispersion quality may miss a batch-to-batch ESCR shift. Quality control for such a grade should therefore include both a melt-flow curve and an optical inspection of microtomed sections against a reference standard.

    Melt Flow, Density, and the Cost of Pigmentation

    The melt mass-flow rate is the primary process-control variable for LLDPE conversion. For class-typical materials near 3–5 g/10 min at 190 °C/2.16 kg, rotational moulding and injection moulding operate close to the lower and middle portions of the shear range; extrusion coating and high-shear compounding require separate rheological data, preferably a flow curve obtained by capillary rheometry according to ISO 11443. Density affects crystallinity, shrinkage, and stiffness. A lower density within the LLDPE band reduces modulus but improves low-temperature impact and ESCR; a higher density moves performance toward HDPE-like stiffness but sacrifices the properties that justify the LLDPE selection. Gray pigmentation at the supplier level commonly raises density by 0.001–0.003 g/cm³, although the exact shift depends on the pigment type and concentration. The melt flow may remain within the same specification band if the pigment carrier resin is matched to the host resin; a mismatched high-flow carrier can raise the final compound MFR by 0.2–0.5 g/10 min. This is why the certificate of analysis matters more than the base-grade datasheet. The following test methods are applicable to incoming inspection of such a compound:

    Incoming inspection should never assume that a gray compound retains the exact MFR, density, and ESCR of the natural precursor. A documented first-article procedure involving melt-flow checks every 25 packaging units, density checks every 50 units, and retention of a physical reference sample is common on industrial lines where lot-to-lot consistency below ±5% of nominal MFR is required. If injection moulding is selected, a general-purpose polyolefin screw with a compression ratio of 2.5:1 to 3.5:1 and an L/D of at least 20:1 is appropriate. Clamp force requirements follow the projected area and cavity pressure; for LLDPE, a cavity pressure estimate of 25–40 MPa is used for preliminary sizing, but mold-filling simulation with actual melt viscosity is necessary for multicavity tools.

    Polyethylene processing is bounded less by a single melt temperature than by the interaction of melt temperature, residence time, and oxygen ingress. For the LLDPE class represented by this grade, the usable melt-processing window generally extends from 180 °C to 240 °C. At melt temperatures above 250 °C, oxidative chain scission becomes measurable through an increase in MFR and a reduction in low-temperature impact. In rotomoulding, a common limitation is not melt temperature in the bulk polymer, but the mold-cavity internal air temperature; typical rotomoulding air temperatures of 280–300 °C heat the outer powder layer intensely while the inner wall remains close to the melting plateau. Degradation is therefore controlled by cycle length and part mass, not by the setpoint alone. Polyethylene does not require drying for bulk moisture, but when ambient relative humidity exceeds 60%, surface moisture on powder or pellets can create pinholes and internal bubbles. A hot-air treatment at 70–80 °C for 2–4 h is usually sufficient for surface water removal; the same operation also reduces agglomeration in stored powder. Rotomoulding grades are often milled to a particle-size distribution with a median below 500 µm. Bulk density is measured by ASTM D1895, and a shift of 10–15% in bulk density can alter wall thickness distribution in large flat panels. A production-line observation on a 65 mm single-screw extruder with a 24:1 L/D and a Maddock mixing section is that switching from natural to gray LLDPE can shift head pressure by 3–5% when the pigment carrier resin lowers the average viscosity; this is not an indication of melt fracture but does require resetting die-bolt adjustments.

    When rotomoulding cycle time conflicts with impact performance

    In rotational moulding, the major processing conflict is between complete sintering and low-temperature impact. A short cycle at high oven temperature can sinter the outer surface while leaving microporosity at the inner wall; an overlong cycle may densify the wall but degrade the LLDPE molecular weight. Production-scale rotational moulders mitigate this by monitoring internal air temperature rather than oven temperature alone; a plateau in internal air temperature indicates the endothermic melting stage has ended, but it does not confirm that the powder has fully densified. For an LLDPE-based gray compound, the pigment package can create additional nucleation sites during crystallisation, altering cooling-rate sensitivity. Parts with thick bosses and ribs cool at different rates, causing differential shrinkage. Warpage in large gray panels is often misclassified as a pigment problem when the root cause is nonuniform cooling. Compared with a rotomoulding HDPE grade, the LLDPE base provides higher ESCR and impact resistance but lower flexural modulus; parts that require structural stiffness may need thicker walls, ribbing, or a shift to an MDPE compromise. Compared with an LDPE rotomoulding grade, the LLDPE product generally gives longer ESCR failure times under ASTM D1693 but may require more careful powder handling because of its lower melt strength at the same MFR. Published data for this specific gray configuration is limited, so first-article rotomoulded parts must be sectioned and tested for wall-thickness distribution, bubble count, and low-temperature dart impact rather than relying on datasheet values.

    Regulatory compliance for a gray LLDPE compound is split between the base polymer and the color package. The base polyolefin may be evaluated under FDA 21 CFR 177.1520(c) for food-contact use, but the gray pigment package requires a separate supplier declaration covering migration limits and permitted colorants. For industrial articles placed on the EU market, the compound must meet the applicable REACH registration and any restriction entries; for electrical and electronic applications, RoHS Directive 2011/65/EU Annex II substance limits apply. The following checklist is not a product certification; it identifies the standard or regulation that the converter must verify for a specific application.

    Standard or regulationParameterVerification requirement
    FDA 21 CFR 177.1520(c)Olefin base polymerBase-resin compliance; pigment package and final compound require separate migration data
    EU 10/2011Plastic food-contact migrationOverall migration and specific migration limits for pigments must be measured on the finished article
    REACHRegistration and restrictionsSubstance-registration status and Annex XVII restrictions apply
    RoHS 2011/65/EUHeavy metals and phthalatesConditional on end-use electrical or electronic equipment category

    The practical storage limitation is not polymer hydrolysis; it is ultraviolet exposure of the gray surface if the stabilizer package is not configured for outdoor service. For outdoor industrial components, the converter must confirm UV stabiliser content and testing according to ASTM D638 after accelerated weathering or natural weathering. If the grade is supplied without a specified UV system, long-term sunlight exposure can cause chalking and loss of tensile elongation. The grade should be stored away from direct sunlight in a dry area below 40 °C and used within the supplier’s recommended shelf life to preserve pigment dispersion and antioxidant activity.