    Specifications
    HS Code 332434
    Manufacturer LyondellBasell
    Brand Icorene
    Grade 1210 GRN 6800
    Polymer Type Polyethylene, Linear Low Density (LLDPE)
    Density 0.935 g/cm³
    Melt Flow Rate 3.0 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 17.0 MPa
    Tensile Strength At Break 25.0 MPa
    Elongation At Break 700%
    Flexural Modulus 700 MPa
    Vicat Softening Point 110°C
    Melting Point 125°C
    Hardness Shore D 55
    Notched Izod Impact Strength 300 J/m
    Thermal Conductivity 0.33 W/mK
    Specific Heat 2.0 J/g°C
    Coefficient Of Thermal Expansion 1.3E-4 1/°C
    Dielectric Constant 2.3
    Volume Resistivity 1E15 ohm-cm
    Color Green
    Form Powder
    Uv Stabilizer Yes

    As an accredited LyondellBasell Icorene 1210 GRN 6800 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 1210 GRN 6800 LLDPE is packaged in 25 kg polyethylene bags, 40 bags per pallet (1,000 kg).
    Container Loading (20′ FCL) 20′ FCL container loaded with 25 kg bags of LyondellBasell Icorene 1210 GRN 6800 linear low-density polyethylene, palletized, shrink-wrapped, secured.
    Shipping LyondellBasell Icorene 1210 GRN 6800 Polyethylene, Linear Low Density is a non-hazardous thermoplastic resin, not classified as dangerous goods (DOT/IMDG/IATA/ADR). Ship in original bags, octabins, or bulk hopper trucks/railcars. Keep dry, clean, and protected from heat, sunlight, moisture, and contamination. Follow applicable local, national, and international shipping regulations.
    Storage Store LyondellBasell Icorene 1210 GRN 6800 Polyethylene, Linear Low Density in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and oxidizing agents. Keep containers tightly closed to prevent moisture and contamination. Avoid dust generation and static discharge. Use appropriate grounding and personal protective equipment. Follow local regulations and manufacturer’s safety data sheet recommendations.
    Shelf Life Shelf life is typically 24 months when stored in unopened original packaging, dry, cool, and away from direct sunlight.
    Application of LyondellBasell Icorene 1210 GRN 6800 Polyethylene, Linear Low Density

    On a three-layer blown film line equipped with an internal bubble cooling system and a 2.0–2.5 mm die gap, LyondellBasell Icorene 1210 GRN 6800 linear low density polyethylene is typically extruded in an LLDPE-rich skin layer with an LDPE blending ratio of 20–30 wt% to suppress draw resonance without removing the tear anisotropy that LLDPE contributes. The melt temperature at the die is maintained between 195 °C and 225 °C, the blow-up ratio is held at 2.2:1–2.8:1, and frost line height is adjusted to 500–800 mm depending on tower geometry. Polymeric processing aid is added at 0.02–0.05 wt% when surface roughness or die-lip buildup becomes measurable; slip and antiblock masterbatches are dosed at 1–3 wt% only after methyl oleamide migration is verified against seal performance. Direct food-contact compliance is governed by 21 CFR 177.1520(c) and European Commission Regulation EU No 10/2011, with overall migration not exceeding 10 mg/dm². Mechanical acceptance is measured on 25 µm monolayer samples using ASTM D882 for tensile, ASTM D1922 for Elmendorf tear, and ASTM D1709 for dart drop. Terminal applications include green-tinted agricultural silage covers, heavy-duty industrial liners, and overwrap where UV stabilization is not required.

    Direct-food-contact compliance matrix for Icorene 1210 GRN 6800 film
    Standard or regulationCondition / simulantAcceptance criterion
    FDA 21 CFR 177.1520(c)Food types I–IX, microwave reheatingNo migration of polymer components exceeding regulation limits
    EU No 10/20113% acetic acid, 20% ethanol, 50% ethanol, olive oilOverall migration ≤ 10 mg/dm²
    ASTM F124938 °C, 90% RH water vapor transmissionApplication-specific; not a compliance limit

    What limits seal initiation temperature consistency in cast film from Icorene 1210 GRN 6800?

    Cast film conversion of Icorene 1210 GRN 6800 is dominated by the air gap and chill roll quenching path, because the absence of a frost line reduces melt orientation and produces a narrower crystallite size distribution than blown film. Published data for this specific colored grade is limited; a converter should establish the seal initiation temperature by ASTM F1921 rather than assume the blown-film value. The resin is fed neat or in an 80–90 wt% blend with a metallocene plastomer for puncture improvement; the plastomer should not exceed 20 wt% because sealing force under ASTM F88/F88M may decline in high-speed packaging due to interfacial dilution. Melt temperature at the flat die is held at 220–240 °C, the air gap between die lip and chill roll is kept below 20 mm, and chill roll temperature is maintained at 15–25 °C to minimize post-extrusion crystal growth. Roller wrap and edge trim reuse should be limited to 15 wt% unless an online melt filter with 100–150 µm screen mesh is installed because trim streams carry oxidized gel particles that reduce hot tack. Compliance requires EU No 10/2011 overall migration testing and FDA 21 CFR 177.1520(c) for food packaging, specifically fatty food simulants if the film contacts meat or cheese. Terminal products include machine hand-stretch pallet wrap, collation film, and agricultural bale wrap where uniaxial pre-stretch is applied at 150–250%.

    Rotomolding surface finish, bubble dissolution and cooling rate mismatch in green-tinted LLDPE grinds

    For rotational molding grades, dry-sieve validation of the powder grind, not pellet melt index, determines whether Icorene 1210 GRN 6800 will densify without surface porosity. The target grind distribution is verified by sieve analysis per ASTM D1921 or an equivalent method; typical rotomolding LLDPE powder retains less than 5 wt% on 35 mesh and allows no more than 35 wt% fines below 200 mesh, though published data for this specific grade is limited. The mold surface is coated with a semi-permanent release system; mold release levels above 0.5 g/m² can produce surface porosity if residual solvent is not burned off. Oven heat is supplied by forced-air convection, with box temperature set between 290 °C and 315 °C, and a peak internal air temperature of 190–200 °C is targeted for full densification. Rotational speed ratio is maintained at 4:1 major to minor axis; deviations above 4.5:1 create thicker upper-wall sections in asymmetric tanks. Cooling must be staged: ambient fan cooling at 8–12 °C/min until the part reaches 80 °C, followed by water mist cooling no faster than 15 °C/min to control shrinkage and corner pull-in. The green pigment package may increase infrared absorption in the mold skin, so infrared thermocouple readings are used instead of oven air temperature alone. Food-contact water tanks require 21 CFR 177.1520(c) and, where potable water is stored, NSF/ANSI 61 extraction data that is specific to the compounded colorant. Terminal products include green agricultural storage tanks, chemical dosing tanks with secondary containment, and material-handling bins where no UV stabilizer is required.

    Thin-wall injection molding tools running this LLDPE are set with barrel zones from 180 °C at the feed throat to 230 °C at the nozzle, and the screw is a general-purpose metering profile with a compression ratio of 2.5:1–3.0:1; when surface splay appears, the first corrective action is to lower back pressure from 10 bar to 5 bar and check hopper moisture because the precolored resin can retain surface moisture above 60% RH. The material is processed at shot sizes between 30% and 70% of barrel capacity to avoid residence time above 5 min; longer residence degrades the LLDPE and raises yellowness index measured by ASTM E313. Injection velocity is profiled to fill a 1.0–1.5 mm wall section in 0.8–1.5 s; pack pressure is set at 400–600 bar and held for 3–6 s, then released before the gate freezes to lower molded-in stress. Mold temperature is held at 15–30 °C using turbulent-flow water circuits. Part ejection can cause cutting or tearing at undercuts; draft angles of 1–2° and polished stripper plates reduce this failure mode. Compliance for food-contact closures is assessed under 21 CFR 177.1520(c) and EU No 10/2011, with total migration limits of 10 mg/dm². Terminal products include flexible over-caps, tamper-evident dust covers, and thin-wall pail lids where the low modulus of LLDPE provides snap-on retention without stress whitening.

    When Icorene 1210 GRN 6800 becomes a carrier resin for 40–60% additive masterbatch on a co-rotating twin-screw line

    In a co-rotating twin-screw compounding line with 36:1 L/D and segmented screw elements, this grade can serve as the carrier for carbon black, mineral filler, or pigment concentrates at additive loadings of 40–60 wt%. The screw profile typically uses two pairs of kneading blocks after the side feeder and a dispersive mixing zone before vacuum devolatilization; specific energy input is kept between 0.18 kWh/kg and 0.25 kWh/kg by adjusting screw speed from 300 rpm to 500 rpm. Melt temperature at the die plate should not exceed 230 °C for organic pigments or 250 °C for carbon black concentrates; a gear pump upstream of the screen changer holds die pressure at 80–120 bar. Screens are stacked at 100/150/100 mesh to catch agglomerates, and pressure rise beyond 0.3 bar/kg indicates poor dispersion. The carrier letdown ratio in film or pipe is typically 20–25:1, meaning 4–5 wt% masterbatch in the final product; a higher dilution ratio above 50:1 is avoided unless a distributive mixing screw is used in the converter extruder. Compliance testing for pigment-specific migration follows EU No 10/2011 and FDA 21 CFR 177.1520(c) only if the final article contacts food; for heavy-metal content, EU Directive 94/62/EC packaging limits apply. Terminal products include agricultural mulch film, geomembrane extrusion, and drip irrigation pipe where the carrier must not shift density beyond the target value.

    Low-voltage jacketing lines fed with a pellet blend of Icorene 1210 GRN 6800 and LDPE at 70/30 wt% benefit from the LLDPE fraction’s environmental stress crack resistance, provided the carbon black concentrate is limited to 2.5–3.5 wt% and the antioxidant package is dosed at 0.2–0.5 wt% to avoid excessive die buildup. The extruder is a 24:1 L/D single-screw machine with a compression ratio of 2.8:1; melt temperature at the crosshead is maintained at 200–220 °C, and head pressure is allowed to reach 150–250 bar before screen pack replacement. Water trough cooling is staged from 80 °C at the first section to 20 °C at the cable take-up to prevent shrinkage voids between the jacket and insulated core. Oxidative induction time is measured by ASTM D3895 at 200 °C; a common acceptance value is >20 min for jacketing compound. Hot set behavior is not applicable to thermoplastic LLDPE unless the formulation includes crosslinking agents; therefore, this grade is limited to non-crosslinked service temperatures below 70 °C. Compliance is evaluated against IEC 60811-401 for thermal ageing, the IEC 60811 series for ozone resistance if required, ASTM D1248 for classification, and RoHS Directive 2011/65/EU for cadmium and lead in the pigment package. Terminal products include indoor low-voltage equipment wire, outdoor lighting cable jackets, and temporary power distribution extensions where UV exposure is intermittent.

    Free Quote

    Competitive LyondellBasell Icorene 1210 GRN 6800 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 1210 GRN 6800 Polyethylene, Linear Low Density is a rotational-molding-grade linear low-density polyethylene supplied as a pigmented powder. The base resin Icorene 1210 carries a nominal density of 0.940 g/cm3 when measured according to ASTM D1505 or ISO 1183-1:2019, and a nominal melt flow rate of 4.0 g/10 min under ASTM D1238 or ISO 1133-1:2022 at 190 °C/2.16 kg. The GRN 6800 suffix identifies a green colorant package; the pigment loading and particle-size distribution are supplier-controlled and proprietary. The material is intended for biaxial rotational molding machines producing closed-mold articles such as chemical storage tanks, agricultural hoppers, electrical enclosures, and outdoor leisure components in which molded-in green color avoids secondary painting. The product is not a general-purpose injection-molding or blown-film grade; its powder form and controlled melt flow rate are matched to the low-shear, high-heat-transfer environment of rotational molding.

    Storage and handling constraints are operationally relevant because the powder surface area is much larger than pellet feed. The product should be kept in sealed packaging below 40 °C and away from open flames or strong oxidizers because polyethylene dust can form a combustible dust cloud. Pre-drying at 60–70 °C for 4–6 h is recommended when the powder has been exposed to relative humidity above 60%; moisture pinholes can form when the peak internal air temperature exceeds the local boiling point of absorbed water. Internal regrind from flash and rejected parts can be added to virgin powder on a lot-controlled basis; addition above 15% by weight should be validated with melt flow testing under ASTM D1238 and dart impact testing under ASTM D5420 or ISO 6603-2 because the particle-size distribution and thermal history shift with repeated passes.

    What Distinguishes a Colored Rotomolding LLDPE from Extrusion-Grade LLDPE?

    Rotomolding LLDPE differs from extrusion-grade LLDPE in four ways: physical form, molecular flow characteristics, additive package, and final-part property requirements. The powder form of Icorene 1210 GRN 6800 is not suitable for single-screw or twin-screw melt feeding because its low bulk density and irregular particle shape create feed instability and air entrainment. Its melt flow rate of 4.0 g/10 min is higher than that of a typical blown-film grade and lower than that of many injection grades; this flow window allows the melt to re-distribute under the low-shear gravitational and rotational forces applied during rotational molding without excessive sag in large flat roofs. Colorant addition is not a simple tumbling operation; the green 6800 package is compounded to maintain dry-flow properties. In production-scale equipment, incomplete dispersion of a green concentrate may appear as streaking or color clouds in long-flow paths rather than as melt fracture, because the dominant flow is powder laydown followed by densification and sintering.

    Compared with a 0.918 g/cm3 film-grade LLDPE, the 0.940 g/cm3 density of this product raises modulus and lowers low-temperature impact. Compared with a high-density polyethylene rotomolding grade of 0.950–0.955 g/cm3, the Icorene 1210 base resin provides greater environmental stress-crack resistance and improved ductility at the expense of stiffness. This trade-off is visible in the property comparison described below. Compared with a single-site catalysed hexene LLDPE, the Icorene 1210 grade may show slightly different warpage and shrinkage behavior; direct published data for the green 6800 variant against specific metallocene grades is limited, so direct substitution should be validated by molding a 5 mm plaque and measuring thickness-dependent shrinkage. The product is a thermoplastic and should not be formulated with peroxide or other crosslinking additives because crosslinking would alter melt flow and reclaim behavior.

    Property Data Block for Incoming-Material Verification

    Incoming material should be checked against the supplier certificate of analysis. Published data for the exact green 6800 configuration is limited for tensile and flexural properties; the following table therefore reports the base-resin nominal values and does not replace the supplier certificate.

    PropertyMethodBase-resin valueVerification note
    DensityASTM D1505 / ISO 1183-1:20190.940 g/cm3Compression-molded plaque or density column
    Melt flow rateASTM D1238 / ISO 1133-1:20224.0 g/10 min190 °C/2.16 kg; useful for lot consistency
    Environmental stress-crack resistanceASTM D1693 Condition B, 10% Igepal> 1,000 hNatural base resin; pigmented parts may shift
    Nominal colorSupplier colorimeter or visual standardGRN 6800 greenDo not use natural-grade pigment acceptance
    FormSupplier internal sieve methodFree-flowing powderPublished particle-size curve is limited

    Tensile properties may be measured under ASTM D638-14 or ISO 527-2; for a 0.940 g/cm3 rotomolding LLDPE, tensile yield strength typically falls between 16 MPa and 20 MPa and elongation at break frequently exceeds 500%. The green colorant package may shift these values by a few percent, so the pigmented product should not be accepted or rejected using tensile data generated on natural material. Melt flow rate and density are the most useful routine lot-to-lot control parameters because they are rapid and correlate with processing performance.

    When Oven Temperature and Cooling Rate Fall Outside the Recommended Envelope

    Rotational molding of this product is usually performed on multi-station carousel or shuttle machines with a biaxial rotation ratio of 4:1 to 5:1. Oven air temperature is typically set between 265 °C and 315 °C. The actual control variable is peak internal air temperature. For a wall thickness of 3–10 mm, a peak internal air temperature of 180–200 °C generally produces full densification. If peak internal air temperature exceeds 210 °C, the green pigment may begin to shift toward a brown-green hue and the inner surface may develop pinholes from volatilization of low-molecular-weight fractions. If peak internal air temperature remains below 170 °C, the inner surface remains granular and weld lines remain visible. Oven residence time should be adjusted to reach the target peak internal air temperature slowly enough to avoid scorching the outer wall; this is especially critical when mold wall thickness is less than 3 mm.

    Cooling is equally critical. Forced-air cooling at 8–15 °C/min is preferred. Water-mist cooling may be used after the part has crystallized to shorten cycle time, but cooling rates above 15 °C/min can increase warpage and internal stress, particularly in parts with wall-thickness transitions greater than 2:1. Mold release should be a semi-permanent system suitable for pigmented polyethylene; silicone oil release can create surface defects and interfere with color acceptance. Rotation should continue until the mold surface temperature drops below 80 °C to reduce warpage. Early demolding creates post-shrinkage and dimensional drift. Thick sections above 10 mm require extended cooling because the internal temperature may still exceed 100 °C even when the outer surface is cool.

    The antioxidant package is designed for limited heat histories. Repeated regrind addition beyond 15% by weight can reduce oxidative stability. Oxidation induction time under ISO 11357-6 at 210 °C should be monitored if more than two recycle passes are used. The product should not be blended with large proportions of HDPE regrind without evaluation because density and modulus shifts can alter part wall thickness distribution.

    For food-contact applications, the base olefin may fall under FDA 21 CFR 177.1520; however, the pigmented grade requires specific evaluation of the green colorant. Potable-water applications may require NSF/ANSI 61 or similar certification and should not be assumed. The product is not recommended for continuous chlorinated water service above 50 °C unless stress-crack testing of the welded assembly has been performed under ASTM D1693. REACH and RoHS documentation should be requested from the supplier for the exact color code.

    Comparative Position Against HDPE and Single-Site LLDPE

    The following table contrasts the density class of Icorene 1210 GRN 6800 with common HDPE and metallocene LLDPE rotational molding alternatives. Values are class-level ranges drawn from industrial data; direct published values for the green 6800 variant may differ.

    PropertyIcorene 1210 GRN 6800 classHDPE rotomolding grademLLDPE rotomolding grade
    Density0.940 g/cm30.950–0.955 g/cm30.935–0.940 g/cm3
    Melt flow rate4.0 g/10 min3.0–5.0 g/10 min4.0–5.5 g/10 min
    Flexural modulus550–700 MPa850–1,100 MPa500–650 MPa
    Environmental stress-crack resistance> 1,000 h40–150 h> 1,000 h

    The comparison indicates that this product should be selected when low-temperature ductility and stress-crack resistance are more important than maximum modulus. For high-stiffness hoppers or valve bodies, HDPE is often preferable. For thinner-wall parts requiring high flow and exact shrinkage control, a single-site LLDPE may be preferable; however, direct substitution should be validated by molding trials because pigment and powder characteristics influence surface finish and color stability.

    On a three-arm shuttle machine with a 2.5 m swing and a 350 L mold, the main process bottleneck is often cooling uniformity across the dome and the lower knuckle radius rather than oven heat input. The green pigment can make flow lines visible if the mold surface is below 230 °C during powder laydown; this condition is typically corrected by increasing the primary-axis rotation speed from 10 min-1 to 14 min-1 rather than by raising oven temperature. In parts with metallic inserts, the inserts should be preheated to the mold surface temperature to prevent local cold spots and resin pull-back. Published data for this specific configuration is limited; the most commonly reported defect is inner-surface roughness when the cooling rate exceeds 15 °C/min.