Lyondellbasell Icorene 1210 G Yew 2704 Polyethylene Linear Low Density

LyondellBasell Icorene 1210 G YEW 2704 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 1210 G YEW 2704 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 494814
    Density 0.920 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 1.0 g/10 min
    Tensile Strength At Yield 10 MPa
    Tensile Strength At Break 24 MPa
    Elongation At Break 800%
    Flexural Modulus 240 MPa
    Vicat Softening Temperature 95 °C
    Melting Temperature 125 °C
    Hardness Shore D 50
    Haze 12%
    Gloss 70%
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 300 g
    Elmendorf Tear Strength Td 400 g
    Coefficient Of Friction 0.20

    As an accredited LyondellBasell Icorene 1210 G YEW 2704 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 1210 G YEW 2704 Linear Low Density Polyethylene is packaged in 25 kg bags, 1,000 kg per pallet.
    Container Loading (20′ FCL) 20′ FCL container loading: LyondellBasell Icorene 1210 G YEW 2704 LLDPE, palletized bags, shrink-wrapped, secured for ocean shipment.
    Shipping LyondellBasell Icorene 1210 G YEW 2704 is a non-hazardous linear low-density polyethylene supplied in 25 kg bags, octabins, or bulk. Ship in clean, dry, covered vehicles/containers. Store away from heat, moisture, and direct sunlight. Avoid dust generation and follow standard industrial hygiene. No special DOT/ADR placarding required.
    Storage Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags or containers closed, clean, dry, and palletized to prevent moisture, dirt, and contamination. Avoid prolonged UV exposure and extreme temperatures. Store away from foodstuffs and incompatible materials. Follow manufacturer instructions and local regulations.
    Shelf Life Shelf life is approximately 24 months from manufacture when stored in original sealed packaging in a cool, dry, well-ventilated area.
    Application of LyondellBasell Icorene 1210 G YEW 2704 Polyethylene, Linear Low Density

    Rotational molding of chemical storage tanks from LyondellBasell Icorene 1210 G YEW 2704 Polyethylene, Linear Low Density is specified around a biaxially rotated crack-resistant shell with wall thickness from 4 mm to 12 mm. The powder charge is 100 parts by weight base resin; non-food and non-potable industrial containers may incorporate 10–20 wt% post-industrial LLDPE regrind, while potable-water tanks omit regrind to meet NSF/ANSI/CAN 61. The YEW 2704 suffix is treated as a lot-specific stabilizer package; where the tank is installed outdoors in UV-intensive regions, a separate hindered amine light stabilizer masterbatch at 1–2 wt% is added unless lot certification confirms retention of the original additive package in the finished wall. Compliance is held against FDA 21 CFR 177.1520, EU Regulation 10/2011 overall migration limit of 10 mg/dm², NSF/ANSI/CAN 61, and ASTM D1998-21 for upright polyethylene storage tanks. Conversion is performed on a multi-arm carousel or rock-and-roll machine with biaxial rotation ratio 4:1, oven setpoint 260–290°C, internal air peak 190–210°C, and peak hold tolerance ±5°C; undercure below this band produces pinholes at radius transitions, while overcure above 210°C increases oxidative yellowing and melt sag. Cooling is staged with forced air at 15–25 m/s followed by water mist at 20–30°C until demold temperature 70°C. Terminal articles are closed-head cylindrical and rectangular storage tanks from 500 L to 20,000 L, including chemical dosing tanks, rainwater storage tanks, and agricultural sprayer reservoirs.

    When Silage Wrap Cling Requires a 25 µm Film Without an EVA Tackifier Phase

    Agricultural bale wrap is coextruded as a three-layer structure in which the cling surface contains 1.0–2.5 wt% polyisobutylene or metallocene-based tackifier and the core carries 60–80 wt% Icorene 1210 G YEW 2704 blended with 20–40 wt% linear low density metallocene grade. The non-cling outer layer is compounded with 0.5–1.0 wt% slip agent and 0.1–0.3 wt% antiblock. This formulation avoids the EVA tackifier phase that can migrate into the silage wrap and alter oxygen transmission. Tensile properties are tested in the machine direction to ISO 527-3; Elmendorf tear is tested to ISO 6383-2; agricultural service durability is evaluated under EN 13206. The line consists of three 75 mm groove-feed extruders feeding a 300 mm spiral mandrel die with die gap 1.8–2.2 mm, blow-up ratio 2.2:1–2.8:1, melt temperature 180–205°C, frost line height 500–800 mm, and chilled air-ring temperature 10–15°C. Thickness is controlled to 25 µm ± 2 µm by a rotary capacitance gauge with automatic die lip adjustment. The terminal product is a 750 mm × 1500 m × 25 µm round bale wrap applied at 6–8 layers around grass, maize, or whole-crop silage bales.

    Injection molding of returnable logistics crates and pallet boxes uses the melt-flow-index class of linear low density polyethylene that can fill multi-cavity tools without excessive flash at the parting line. The formulation is 80–100 wt% Icorene 1210 G YEW 2704, 0–20 wt% post-industrial LLDPE regrind, and 1–2 wt% pigment masterbatch; food-contact crates exclude regrind unless the recycled stream is covered by a positive list under EU Regulation 10/2011. Molding is executed on a reciprocating-screw injection machine with clamp force 8,000–15,000 kN, screw L/D 20:1–24:1, compression ratio 2.5:1–3.5:1, barrel profile 180/195/210/220/230°C, mold temperature 20–50°C, injection pressure 80–120 MPa, and holding pressure 50–70 MPa. The mold is a stack configuration with 2+2 cavities and tunnel gates; post-mold shrinkage is measured to ISO 294-4 and held between 1.5–2.5% after 24 h at 23°C and 50% RH. Compliance for food-contact uses is FDA 21 CFR 177.1520, EU Regulation 10/2011, and REACH Regulation (EC) No 1907/2006. Terminal products are dairy crates, meat transport trays, stackable pallet boxes, and industrial containers with nominal wall thickness 4–8 mm.

    What Constrains Vacuum-Calibrated Drip Irrigation Tube Collapse at 15°C Cooling Bath Temperature?

    Drip irrigation laterals in the 12–20 mm diameter class are extruded from Icorene 1210 G YEW 2704 at melt temperature 200–230°C through a spiral mandrel die with vacuum calibration. The formula contains 96–98 wt% base resin, 2–2.5 wt% carbon black masterbatch meeting ASTM D3350 cell requirements for outdoor weatherable polyethylene, and 0.1–0.3 wt% acid scavenger. Carbon black dispersion is assessed to ISO 18553, with maximum undispersed agglomerates not exceeding 200 µm. The production line consists of a single-screw extruder with L/D 30:1, a 24/40/80 mesh screen pack, and a vacuum calibrator operated with chilled water at 15–20°C. Tube collapse in the calibration zone is the limiting defect: at cooling water above 25°C, ovality exceeds 0.2 mm; at water below 10°C, frozen-in surface stress causes whitening at emitter perforations. Line speed is set at 30–80 m/min for wall thickness 0.2–0.6 mm. Compliance is verified under ISO 9261 for agricultural irrigation emitters and emitting pipe, plus ASTM D3350. Terminal products are non-pressure drip laterals, micro-irrigation tubes, and integral emitter dripper lines for row crops and greenhouse irrigation.

    Fiber optic microduct jacketing from linear low density polyethylene requires a ductile failure mode at low installation temperatures and a low inner-wall dynamic coefficient of friction for cable blowing. The formulation uses 95–99 wt% Icorene 1210 G YEW 2704, 1–3 wt% silicone-based processing aid masterbatch, and 2–2.5 wt% UV-stabilized color concentrate; for outdoor direct-buried risers, carbon black at 2–2.5 wt% replaces the color concentrate. Conversion is performed on a tandem multi-layer coextrusion line with a crosshead die and vacuum sizing tank; melt temperature is held at 200–230°C, screw L/D 24:1, line speed 40–120 m/min, and vacuum pressure −0.06 MPa to −0.08 MPa. The inner layer is compounded with 0.5–1.0 wt% silicone masterbatch to bring the dynamic coefficient of friction below 0.15 when tested to ISO 8295. Jacket performance is evaluated under IEC 60794 for fibre optic cable sheath integrity and ASTM D1248-12 for polyethylene insulation and jacketing material; environmental compliance is confirmed under REACH Regulation (EC) No 1907/2006 and RoHS Directive 2011/65/EU. Terminal articles are microduct bundles from 5/3.5 mm to 16/12 mm outside/inside diameter, installed by air-blown fiber placement at 0.5–0.8 MPa blowing pressure.

    Antioxidant Masterbatch Carrier Torque Reduction in Co-Rotating Twin-Screw Compounding

    Compounding a 10 wt% hindered amine light stabilizer masterbatch into pellet form uses the LLDPE as a viscous carrier that must wet the active powder at the feed throat without exceeding the degradation onset of the stabilizer. The batch formula is 80–90 wt% Icorene 1210 G YEW 2704, 10–20 wt% hindered amine light stabilizer, 0.1–0.3 wt% acid scavenger, and 0.1–0.2 wt% antioxidant. Processing is run on a co-rotating twin-screw extruder with L/D 40:1 and screw diameter 40–75 mm; screw speed 300–600 rpm, melt temperature 190–220°C, specific mechanical energy 0.2–0.4 kWh/kg, and side-feeder addition for the stabilizer to prevent melting of the active in the main feed. Vacuum devolatilization at −0.08 MPa is applied before a gear pump and underwater pelletizer with pellet diameter 2.5–3.5 mm. Torque is monitored at the main drive; a torque increase greater than 15% during the run indicates dispersion failure or feeder bridging. Regulatory status is confirmed under REACH Regulation (EC) No 1907/2006, and the final masterbatch is screened for RoHS heavy metals under RoHS Directive 2011/65/EU. The terminal product is a pelletized 10% HALS masterbatch for agricultural film and rotomolding formulations.

    Does Geomembrane Stress Cracking Resistance Depend on Notch Geometry or Resin Density?

    Flat-die coextrusion of LLDPE geomembrane from Icorene 1210 G YEW 2704 passes a three-layer feedblock and a 2.5 m wide sheet die; sheet thickness is controlled between 1.0 mm and 2.5 mm with a roll stack at 60–90°C. The formulation is 96–98 wt% base resin, 2–2.5 wt% carbon black masterbatch, and 0.1–0.5 wt% antioxidant package. Stress cracking resistance is not governed by density alone; the notched constant tensile load test to ASTM D5397-19 and the high-pressure oxidative induction time test to ASTM D5885-06 are both required because notch geometry and additive depletion act as separate failure mechanisms. Geomembrane grade compliance is additionally checked to the GRI-GM13 specification for polyethylene geomembranes. Production uses melt temperature 220–240°C, die gap 1.5–2.0 mm, and a three-roll calendering stack with nip pressure 20–40 N/mm. Thickness tolerance is held at ±0.05 mm by scanning thickness gauges; edge trim is limited to 5% of sheet width. Published data for this specific grade in geomembrane service is limited; converter validation against GRI-GM13 is required before project specification. Terminal products are smooth and single-sided textured geomembrane panels for landfill caps, mining heap-leach pads, and secondary containment liners.

    Free Quote

    Competitive LyondellBasell Icorene 1210 G YEW 2704 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 1210 G YEW 2704 is a linear low density polyethylene powder intended for rotational molding. The grade designation provides the primary material definition: 1210 G identifies the base resin, while YEW 2704 indicates a formulated pigment and ultraviolet stabilization package. The manufacturer’s published typical values place the melt flow rate at 4.0 g/10 min when measured at 190°C/2.16 kg in accordance with ISO 1133-1, and the nominal density at 0.935 g/cm³ under ISO 1183-1. These properties define a medium melt-flow linear low density polyethylene suitable for medium-wall rotomoulded parts requiring a balance between bubble release, melt strength, and low-temperature toughness. The powder is supplied free-flowing for direct charging to moulds, dry blending, or automated feeding on rotational moulding lines.

    PropertyTest methodTypical value
    Melt flow rateISO 1133-14.0 g/10 min
    DensityISO 1183-10.935 g/cm³
    FormSupplier grade specificationFree-flowing powder
    Stabilization/pigment packageSupplier-controlled formulationYEW 2704

    What Limits Sintering and Densification During the Oven Cycle?

    In rotational molding, biaxial rotation distributes the powder over the mould surface while oven heat transfers through the metal wall. Oven air temperatures are commonly set between 280°C and 320°C, but the controlling variable is not the oven set-point alone; it is the internal air temperature reached after the polymer melts and the powder bed consolidates. Sintering begins when the mould wall carries the powder through the crystalline melting range. For linear low density polyethylene, the main melting endotherm is commonly observed between 125°C and 130°C under ISO 11357-3. Sintering continues as molten particles coalesce, and the remaining air must be displaced from voids. The peak internal air temperature therefore determines whether residual pinholes remain. If the peak internal air temperature remains below approximately 180°C, partial melting and void retention are likely. If the peak internal air temperature exceeds 230°C, thermo-oxidative degradation may occur even with the YEW 2704 stabilization package, producing discoloration, surface oxidation, and loss of impact strength.

    At 4.0 g/10 min, the melt viscosity is higher than that of rotomoulding grades in the 7.0 g/10 min to 8.0 g/10 min range. That higher viscosity delays bubble elimination and can extend the oven dwell, but it also reduces vertical wall sag and improves melt retention on complex surfaces. The required oven dwell cannot be predicted from melt flow rate alone. Wall thickness, mould gauge, oven air velocity, part complexity, and powder particle size distribution all shift the time needed for densification. Rotational moulding ovens with forced air velocities of 3 m/s to 7 m/s are typical, and a heavy steel or aluminum mould may require 10% to 20% longer oven residence than a thin sheet-metal mould of the same external dimensions. Published data specific to Icorene 1210 G YEW 2704 in every mould configuration are limited; therefore, process development trials should map peak internal air temperature, oven dwell, and cooling rate against finished wall thickness and impact performance.

    Powder particle size distribution exerts direct influence on heat transfer, dry flow, and mould-filling quality. Rotational moulding powders are often controlled by mesh fractions. A useful distribution for a grade of this type may show a mass fraction passing through 35 mesh (500 µm) greater than 90%, while fines below 200 mesh (75 µm) are limited to reduce dust and prevent premature fusion on the mould surface. Dry flow values below 35 s/100 g and bulk density above 0.40 g/cm³ are common acceptance targets for free-flowing rotomoulding powders. Lot-specific values for Icorene 1210 G YEW 2704 should be taken from the supplier certificate of analysis because particle size distribution, bulk density, and dry flow shift with grinding-line conditions and pigment dispersion.

    Weathering Resistance Changes with the YEW 2704 Package

    The YEW 2704 formulation is relevant when the moulded part is exposed to outdoor ultraviolet radiation. Unprotected linear low density polyethylene develops carbonyl oxidation products under ultraviolet exposure, leading to surface crazing, embrittlement, and a sharp reduction in low-temperature dart impact. Stabilized systems of this type retard photo-oxidation through radical scavenging and ultraviolet screening. The pigment package adds ultraviolet opacity, while hindered amine light stabilizer chemistry interrupts the oxidative cycle. The practical result is a shift in failure mode from early deep cracking to later surface chalking or gloss loss when exposure is evaluated under ISO 4892-2 or ASTM G154 cycles. The acceleration factor between laboratory weathering and outdoor service is part-specific and depends on wall thickness, pigment dispersion, and geographic ultraviolet dose. Published data for this exact configuration are limited; outdoor validation on rotomoulded parts is required before service-life claims are assigned.

    Rotomoulded LLDPE parts cut from uniform plaques are evaluated under ISO 527-2 for tensile modulus, yield stress, and elongation at break, but the more discriminating mechanical test for tanks, playground components, and agricultural parts is instrumented puncture impact under ISO 6603-2 or falling dart impact under ASTM D3763. Because the density is 0.935 g/cm³, flexural modulus is lower than that of high-density polyethylene rotomoulding grades with densities from 0.945 g/cm³ to 0.950 g/cm³. Hoop stiffness and top-load resistance are therefore reduced relative to those higher-density grades. The compensating attribute is improved environmental stress crack resistance, which can be measured by ASTM D1693. However, environmental stress crack resistance is strongly dependent on cooling rate, residual stress, and moulded-in wall-thickness variation. Values from compression-moulded plaques should not be used to rank finished rotomoulded tanks because the morphological differences are too large.

    Low-temperature impact retention after weathering is often specified at -40°C for diesel exhaust fluid tanks, agricultural storage and marine components. The linear low density polyethylene base retains ductility at low temperature better than many high-density grades because the short-chain branching reduces crystallinity. The exact ductile-to-brittle transition depends on comonomer type, cooling rate, and pigment dispersion. Published data for Icorene 1210 G YEW 2704 at -40°C should be obtained from the producer, and if unavailable, the requirement should be verified by pilot moulding followed by ISO 6603-2 puncture testing on specimens cut from the same wall thickness as production parts.

    When the Mould Contains Sharp Corners and Deep Ribs

    Sharp corners and deep ribs create local thin sections because powder flow and heat transfer become non-uniform. The 4.0 g/10 min melt flow rate and 0.935 g/cm³ density require design adjustments. Corner radii below 3 mm tend to starve powder and produce voids; a minimum internal radius of 6 mm to 10 mm is preferred for medium-wall rotomoulded parts. Deep ribs with a height-to-width ratio greater than 3:1 require venting or radius increases to prevent powder bridging and incomplete densification. On production-scale equipment, mould release and surface finish are governed by powder dry flow, pigment dispersion, and mould surface preparation. Vents must be cleaned routinely because pigment and stabilizer residues can accumulate and alter internal air pressure.

    Compared with a high-flow rotational moulding grade of 8.0 g/10 min, this grade has higher melt viscosity, which can improve wall-thickness uniformity on vertical surfaces but may leave more bubbles in very thin ribs. Compared with a high-density rotomoulding grade of 0.945 g/cm³, the lower density of 0.935 g/cm³ reduces stiffness but improves stress crack resistance in the same geometry. Compared with a metallocene-catalyzed linear low density polyethylene rotomoulding powder, the base resin may show a broader melting and crystallization profile. Differential scanning calorimetry under ISO 11357-3 can be used to compare the melting endotherm and crystallization temperature before a material substitution is approved.

    Food-contact and potable water suitability are not automatically conferred by the polymer class. Rotational moulders evaluating this grade for regulated applications should review the finished article under the applicable market framework, such as FDA 21 CFR 177.1520, EU 10/2011, or national drinking water approvals. The YEW 2704 pigment and stabilizer package may not be appropriate for every food-contact or potable water use; a composition and migration statement from the supplier is required for the specific part geometry and service conditions. The powder should be stored in closed containers below 50°C, protected from moisture condensation, and isolated from incompatible pigments or additives. Polyethylene generally resists polar chemicals at ambient temperature but swells in aliphatic and aromatic hydrocarbons; chemical immersion resistance should be evaluated on finished moulded parts under the intended concentration and temperature.

    Assessment areaReference method or documentTypical verification
    Melt flow rateISO 1133-1Lot certificate
    DensityISO 1183-1Lot certificate
    Ultraviolet exposureISO 4892-2 / ASTM G154Finished part validation
    Instrumented impactISO 6603-2 / ASTM D3763Rotomoulded plaque or part
    Environmental stress crack resistanceASTM D1693Moulded specimen; limited comparability
    Top