Lyondellbasell Icorene 1210 Bwn 8443 Polyethylene Linear Low Density

LyondellBasell Icorene 1210 BWN 8443 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 1210 BWN 8443 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 236894
    Density 0.921 g/cm3
    Meltindex 1.0 g/10 min
    Tensilestrengthatyield 9 MPa
    Tensilestrengthatbreak 26 MPa
    Elongationatbreak 800%
    Flexuralmodulus 250 MPa
    Dartdropimpact 150 g
    Elmendorftearstrengthmd 200 g
    Elmendorftearstrengthtd 300 g
    Haze 12%
    Gloss 75%
    Vicatsofteningpoint 100 C
    Meltingpoint 123 C
    Crystallizationtemperature 100 C

    As an accredited LyondellBasell Icorene 1210 BWN 8443 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg moisture-resistant bags, typically 55 bags per pallet (1,375 kg net weight).
    Container Loading (20′ FCL) 20′ FCL loaded with palletized 25 kg bags of LyondellBasell Icorene 1210 BWN 8443 LLDPE, securely braced for ocean shipment.
    Shipping Icorene 1210 BWN 8443 is a non-hazardous LLDPE resin. Ship in original sealed bags, boxes, or octabins on pallets. Protect from moisture, heat, sunlight, and contamination. No special dangerous-goods regulations apply. Store cool, dry, ventilated. Handle with clean equipment; secure loads for road, sea, or air transit. Use appropriate PPE.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers or packages closed and palletized to prevent moisture, contamination, and dust. Avoid prolonged UV exposure and excessive temperatures. Segregate from strong oxidizers. Use proper grounding to prevent static discharge. Follow supplier SDS and local regulations.
    Shelf Life Shelf life is 12 months from date of manufacture when stored in original unopened packaging under cool, dry, well-ventilated conditions.
    Application of LyondellBasell Icorene 1210 BWN 8443 Polyethylene, Linear Low Density

    Where a 3,000–5,000 L vertical water storage tank is rotomoulded from the black UV-stabilised powder, the powder is first conditioned at 20–25 °C and 40–60 % RH for a minimum of 8 h to stabilise bulk density before mould charging. The mould is charged with 4.8–5.4 kg/m² of internal surface area per 1.0 mm of nominal wall thickness, producing a final wall of 5.0–6.0 mm for non-pressurised agricultural water service. Oven air temperature is held at 275–290 °C with a peak internal air temperature of 190–205 °C. The rotational speed ratio is maintained at 4.0:1 with a primary axis speed of 6–8 rev/min. The cooling phase uses forced air for 15–20 min followed by water mist at 0.5–1.0 L/min until the mould surface temperature reaches 80 °C. Demoulding at a higher surface temperature produces sidewall warp in flat tank bottoms, while demoulding below 60 °C increases cycle time without measurable crystallinity gain. For potable water service, the natural lot of the resin is normally used because the carbon black version may remain outside a specific NSF/ANSI/CAN 61 certification unless the fabricated article is approved as a complete tank. For agricultural chemical storage, the moulded wall is checked for a maximum mass change of 2.5 % after 7-day immersion in 10 % ammonium nitrate solution and 5 % glyphosate solution according to ASTM D543-21. The nominal density of 0.936 g/cm³ and melt index of 4.0 g/10 min place the grade in the medium-density class where environmental stress crack resistance, not short-term modulus, controls tank life.

    Production-scale failure modes in this sector are concentrated at the lower knuckle radius and around moulded-in threaded bosses. If the tank is under-sintered, the fracture surface shows white, unmelted powder particles and pinholes appear at the intersection of the sidewall and bottom radius after 0.2 MPa hydrostatic test. If the tank is over-sintered, the inner wall shifts from a matte finish to a glossy amber surface and the notched impact value can fall from 60–65 kJ/m² to 35–40 kJ/m² at −20 °C. Batch-to-batch melt index drift of ±0.2 g/10 min moves the required peak internal air temperature by approximately 3–5 °C; converters compensate by adjusting oven dwell time by 45–60 s per 1 °C rather than altering oven set point. When a colour change is required, 3–5 wt% of a PE-based colour concentrate with a melt index of 8–12 g/10 min is added in a low-shear paddle mixer for 5 min at 20 rpm. Longer mixing at higher speed reduces bulk density by up to 6 % and causes the shot weight to fall if the mould is charged by volume rather than by mass.

    What Changes in a Hydraulic Reservoir When the Peak Internal Air Temperature Falls Below 185 °C?

    The switch from atmospheric water tanks to hydraulic reservoirs introduces a wall-thickness reduction from 5.5–6.0 mm to 3.2–4.0 mm around metal insert bosses, which concentrates residual stress at the insert interface. For a compact construction-equipment reservoir of 40–80 L capacity, the mould is charged to produce a nominal wall of 3.5–4.5 mm and is run at an oven set point of 275–285 °C. The peak internal air temperature is held at 195–210 °C, and the internal air probe is placed 25 mm above the lowest insert flange. If the peak internal air temperature falls below 185 °C, the resin particles around the moulded-in steel hydraulic fittings do not fully coalesce because the local heat sink of the insert delays fusion. The failure appears during service as oil migration from the insert boss at pressures as low as 0.15–0.25 MPa, accompanied by white spots on the fracture surface when the part is sectioned. The acceptance protocol therefore rejects any reservoir lot with a notched Charpy impact below 45 kJ/m² at −20 °C measured according to ISO 179-1/1eA.

    Chemical resistance of the moulded reservoir is screened using ASTM D543-21 with 7-day immersion in ISO VG 46 hydraulic oil at 60 °C. The maximum acceptable mass change is 2.5 % and maximum volume swell is 3.0 %; values above these limits indicate that the inner surface has not densified sufficiently or that the grade has been contaminated with an incompatible lower-density polyethylene. Environmental stress crack resistance remains the major long-term control. The black UV-stabilised powder form of this grade is expected to exceed 1000 h in ASTM D1693-21 using 100 % Igepal at 50 °C. However, the test is not a substitute for full article validation because the moulded-in inserts create tensile stress concentrations that do not exist in the standard compression-moulded plaque. Moulders running hydraulic reservoirs often add 2 wt% of carbon black masterbatch only when using the natural form; the black version requires no additional carbon black. Over-addition of carbon black above 3 wt% in thin insert bosses is avoided because it accelerates local heat absorption and can cause incipient degradation in the 3.0 mm wall sections adjacent to the boss.

    Twin-sheet rotomoulded floating dock sections use the same base powder but require a two-stage charging sequence to fill the lower and upper shell cavities without rib bridging. The lower mould half is charged first with 60 % of the shot weight, rotated for 4 min, and then the upper half is closed and charged with the remaining 40 % through a removable vent port. This prevents the powder from packing into narrow rib cores before the mould reaches full fusion temperature. For a dock section with a projected area of 2.5 m², the nominal wall is 8.0–12.0 mm, and the oven set point is 280–295 °C. Peak internal air temperature is held at 195–210 °C for 18–22 min. The part is demoulded at 70 °C to limit sink marks at the rib intersections. After demoulding, a water-blown two-component polyurethane foam of 40–50 kg/m³ density is injected through pre-moulded holes to approximately 80 % of the cavity volume. This provides reserve buoyancy and reduces drumming sound on wave impact.

    The weathering requirement separates marine dock moulding from general tank work. The black UV-stabilised system is expected to retain at least 75 % of initial tensile elongation after 2000 h accelerated weathering according to ASTM G154-16 Cycle 1. Tensile properties are measured according to ASTM D638-14 at 23 °C. Marine components are also screened for environmental stress crack resistance using ASTM D1693-21 because constant flexure of the float under wave loading creates low-level strain that can initiate slow crack growth. In field service, the primary moulding defect is hollow rib formation caused by powder bridging. When the powder is not conditioned to 20–25 °C or when bulk density varies by more than 0.03 g/cm³ between lots, rib cores can remain partially unfilled even though the outer walls appear fully sintered. Sectioning of one test piece per 50 shots is the usual control method for this failure mode.

    Playground Equipment and Outdoor Furniture: EN 71-3 Migration Limits and Mould Texturing

    When the black UV-stabilised powder is coloured for playground use, the carrier resin must be selected with a melt index no more than 6 g/10 min above the base resin to avoid localised early fusion in thin sections. Colour concentrate addition is normally 4–6 wt%, and the concentrate is dry-blended in a low-shear mixer for 4–6 min at 20–25 rpm. For a slide canopy or climbing panel with a nominal wall of 3.5–4.5 mm, the oven set point is 285–295 °C and the peak internal air temperature is 190–200 °C. The mould surface is textured to 25–50 µm average roughness to hide sink marks and reduce visible scratch formation. Release-agent application is limited to the parting line and critical undercut surfaces; overspray onto the cavity face prevents full replication of the texture and produces low-gloss patches that are rejected by playground equipment buyers according to visual inspection criteria.

    Compliance for this sector is based on the fabricated article, not the resin alone. The moulded components are tested to EN 71-3 for migration of heavy metals and to ASTM F963-17 for the full child-use article when applicable. Colourant packages are screened against the REACH candidate list for SVHC content, and the converter is responsible for confirming that the final colour concentrate does not push the component out of the grade’s food-contact status if the furniture is also marketed for childcare use. Lightfastness of pigmented parts is assessed by ISO 4892-2 with a xenon-arc source. The acceptance limit for severe outdoor exposure is a maximum colour change of 3 CIELAB units after 1000 h and retention of at least 70 % of tensile elongation. The black UV-stabilised grade generally meets this requirement without an additional UV masterbatch; colour versions may require a light-stable pigment concentrate and 1–2 wt% of a hindered amine stabiliser masterbatch depending on the pigment class.

    Failure modes in playground moulding are usually related to demoulding temperature and cooling rate. Because the wall thickness is thin, cooling with forced air at 4–6 °C/min from PIAT to 80 °C is preferred. Water mist is avoided on large flat panels because rapid differential cooling causes edge curl. The part is held in the mould until the surface temperature falls below 75 °C; then it is transferred to a flat cooling fixture for 30 min. Moulders observe short-shot areas at the top of tall ribbed features if the powder is overdried to below 0.05 % moisture or if the charge is increased without adjusting the vent size. The correction is to increase vent diameter by 15–20 % and to reduce shot weight by 2–3 % rather than to raise oven set point.

    When the Powder Is Blended with 15–25 wt% In-House Regrind for Insulated Material Handling Bins

    The first process variable affected by regrind addition is not viscosity but bulk density; a 20 wt% regrind blend can reduce bulk density from 0.36 g/cm³ to 0.33 g/cm³, leading to undercharge if the shot volume is not adjusted. For an insulated bin with a nominal wall of 6.0–8.0 mm, the shot weight is corrected by a factor of 1.06–1.09 when regrind fraction exceeds 15 wt%. The regrind must be stone-ground or granulated to 35–60 mesh; coarse particles above 500 µm create surface blemishes on the inner cavity, while fines below 100 µm reduce bulk density further and increase static cling. In-house regrind from the same grade is added at 15–25 wt% for non-food insulated logistics boxes. For food-contact insulated containers, regrind is permitted only if the scrap comes from the same compliant material, free of contamination, and the final article meets the end-use extraction limits of FDA 21 CFR 177.1520(c) 3.1a or 3.2a as applicable to the density and additive package.

    Because regrind particles have already undergone one thermal history, they fuse 10–20 s earlier than virgin powder. The oven set point is therefore reduced by 5–8 °C when regrind exceeds 15 wt%, yielding a typical set point of 270–280 °C and a peak internal air temperature of 190–200 °C. This prevents over-sintering of the inner surface and reduces the formation of volatiles from residual oil or paper labels carried into the regrind stream. The cooling ramp for flat-panel insulated bins is controlled at 3–4 °C/min to 80 °C, followed by fixture cooling for 60 min. Faster cooling on thin sidewalls combined with thicker corner radii causes differential shrinkage; the resulting bow can exceed 4 mm across a 600 mm panel and makes the lid fit unacceptable. The final bin must pass a 0.2 MPa hydrostatic test for liquid-tight liners and a 2.0 m drop test at −20 °C for frozen logistics service. The type of end product includes insulated fish tubs, pharmaceutical gel-pack carriers, and controlled-temperature material handling totes.

    For underground valve boxes and meter pit covers, the critical specification is resistance to slow crack growth under constant load rather than short-term tensile yield. Moulded walls are typically 9.0–12.0 mm thick to provide structural stiffness without steel reinforcement. The oven set point is 280–290 °C and the peak internal air temperature is 200–210 °C. The thick wall requires a long soak time of 22–28 min to ensure complete particle coalescence at the centre of the wall. Cooling is performed with forced air only until the surface temperature reaches 60 °C; water mist is avoided because severe thermal shock can create microcracks at the edges of access openings. The part is loaded into a flat fixture for 90 min after demoulding. Municipal load rating is determined on the finished cover, typically to EN 124-5 class B125 or C250 depending on installation location. The resin itself is not certified to the load class; the geometry, wall thickness, and rib pattern determine the final load capacity.

    The acceptance protocol uses ASTM D1693-21 environmental stress crack resistance above 1000 h as a screening test, with ASTM D638-14 tensile yield at 17 MPa as a secondary check for lot-to-lot consistency. In service, the primary failure mode is not sudden fracture but slow crack propagation at the corners of the moulded access slot. Published multi-year crack-growth data for this exact black LLDPE powder in underground vault service is limited; therefore the acceptance protocol normally uses ESCR as the screening test and a 12-month field validation on a sample lot before full release. If additional creep resistance is required, 10–20 wt% of a high-density PE powder can be dry-blended, but this raises density, increases oven set point by 5–8 °C, and reduces low-temperature impact unless the part thickness is increased.

    Application sectorNominal wall thicknessOven set pointPeak internal air temperatureDemoulding surface temperatureKey acceptance standard
    Agricultural water tanks5.0–6.0 mm275–290 °C190–205 °C80 °CASTM D543-21
    Hydraulic reservoirs3.2–4.0 mm275–285 °C195–210 °C75 °CISO 179-1/1eA
    Floating dock sections8.0–12.0 mm280–295 °C195–210 °C70 °CASTM G154-16
    Playground components3.5–4.5 mm285–295 °C190–200 °C75 °CEN 71-3
    Insulated bins6.0–8.0 mm270–280 °C190–200 °C80 °CFDA 21 CFR 177.1520(c)
    Underground vault covers9.0–12.0 mm280–290 °C200–210 °C60 °CEN 124-5
    Downstream sectorRegulatory or standard referenceTest methodAcceptance value or condition
    Potable water contactNSF/ANSI/CAN 61Fabricated article extractionCertification required on final tank
    Food contactFDA 21 CFR 177.1520(c) 3.1a/3.2aEnd-use extractionGrade-specific confirmation required
    Children’s articlesEN 71-3Heavy metal migrationLimit per element class
    Children’s articlesASTM F963-17Full article testArticle-level compliance
    Hydraulic oil immersionASTM D543-217-day immersion at 60 °CMass change <2.5 %, volume swell <3.0 %
    WeatheringASTM G154-16QUV cycle 1, 2000 hElongation retention >75 %
    Stress crack resistanceASTM D1693-21100 % Igepal, 50 °C>1000 h
    Municipal load ratingEN 124-5Load class on finished coverB125 or C250 by design
    Free Quote

    Competitive LyondellBasell Icorene 1210 BWN 8443 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 1210 BWN 8443 is a linear low-density polyethylene grade supplied for thin-gauge film conversion. The base polymer is produced from ethylene and a butene comonomer, which introduces short-chain branching along the polyethylene backbone. These short-chain branches reduce lamellar thickness and overall crystallinity compared with high-pressure LDPE and high-density polyethylene, giving the resin a distinctive balance of melt drawdown, seal initiation, and solid-state toughness. In commercial documentation, the grade is listed under the Icorene polyethylene range and is ordered through LyondellBasell distribution channels with the full alphanumeric suffix BWN 8443, which identifies the stabilizer/color configuration and lot-related additive package. The material is not marketed as a single-property performance resin; rather, it occupies a converter-relevant position in blown-film and cast-film operations where film property testing under ASTM D882, ASTM D1922, and ASTM D1709 determines fitness for packaging or industrial film.

    Material Identity and Nomenclature Read-Out

    The suffix BWN 8443 is a batch and additive identifier rather than a direct descriptor of polymer architecture. The numeric block 1210 reflects the manufacturer’s internal grade family and should not be interpreted as a literal melt-index/density conversion. Distributor-published typical values for the grade include a density of 0.918 g/cm³ and a melt mass-flow rate of 1.0 g/10 min at 190 °C under 2.16 kg, measured according to ISO 1183-1 and ISO 1133-1/ASTM D1238. The butene comonomer weight fraction is not usually disclosed on standard technical data sheets, but its effect is expressed through a lower melting range than HDPE and a broader composition distribution than many metallocene LLDPE grades. Certificates of analysis control lot-specific acceptance because melt-flow rate and density vary within manufacturing tolerance. Converters should treat the technical data sheet as a starting specification and qualify each production lot against the target film gauge, line speed, and end-use requirement.

    What Processing Boundaries Arise from Butene-LLDPE Rheology?

    The viscosity profile of a butene-copolymer LLDPE is more Newtonian than LDPE at low shear rates and displays a lower shear-thinning exponent across the shear range encountered in blown-film dies, approximately 100 s⁻¹ to 1000 s⁻¹. On single-screw extruders with screw lengths of 24:1 to 30:1 L/D, the resin is preferably processed with barrier screws or high-work Maddock sections because the comonomer distribution influences melt homogeneity and gel fraction. Die gaps for LLDPE are normally set between 1.5 mm and 2.0 mm, wider than the 0.8 mm gaps used for LDPE, to reduce melt fracture and prevent excessive die-head pressure. Barrel temperatures are typically profiled from 160 °C in the feed zone to 220 °C at the metering zone; die-head melt temperature is typically held between 200 °C and 230 °C. At temperatures exceeding 250 °C, oxidative chain scission begins to produce low-molecular-weight carbonyl products, which can be detected by FTIR and appear as unstable bubble movement or streak defects. Blow-up ratios between 2.0:1 and 2.5:1 are common; lower ratios increase machine-direction orientation, while higher ratios improve transverse-direction tear but reduce bubble stability on low-melt-strength formulations.

    In blown-film lines equipped with internal bubble cooling and dual-lip air rings, the frost line height is maintained at 3 to 5 die diameters for films in the 20 µm to 80 µm range. A rising frost line is an early signal that cooling air volume is insufficient or that the extruder output has exceeded the die quench capacity, leading to higher transverse-direction orientation and reduced dart impact. On production-scale lines with die diameters above 200 mm, die-head pressure fluctuations above 35 MPa frequently correlate with feed-throat bridging or gel build-up at the screen pack. Screen packs with mesh combinations from 40/60/80 are used to protect the die lip, but frequent screen changes can shift residence time and change film tear balance. The resin is not hygroscopic and does not require pre-drying; however, cold-pellet condensation at ambient relative humidity above 60% should be avoided because surface moisture enters the screw and creates bubble defects.

    When the Grade Is Substituted for LDPE in Thin-Gauge Blown Film

    Replacement of a high-pressure LDPE with LLDPE in a thin-gauge packaging structure changes the melt-strength and solid-state balance. High-pressure LDPE retains a long-chain branched architecture that grants higher melt tension and wider bubble-stability windows; the Icorene grade has lower melt tension and must be processed with a wider die gap or a more aggressive cooling setup. In exchange, the LLDPE delivers higher tensile break stress and greater dart impact at reduced gauge. Converters commonly introduce the resin at 20 wt% to 40 wt% in LDPE-rich blends to retain processability while lowering thickness. The seal initiation temperature is lower than LDPE in similar-density films, but the final seal window must be measured according to ASTM F88 after corona treatment and printed lamination. When used without slip or antiblock additives, the coefficient of friction remains surface-controlled; converter-added masterbatch is the accepted route for COF control.

    For cast-film lines with chilled-roll quenching, the grade is extruded through flat dies with die gaps of 0.5 mm to 0.8 mm. Vacuum box assist and air-knife sealing are required above 150 m/min line speed to maintain film flatness and contact with the chill roll. Chill-roll temperatures below 25 °C are used to suppress secondary crystallization and limit haze development. Because cast film is quenched rapidly, the butene branch distribution yields lower modulus than oriented LDPE, but elongation and tear resistance are retained at higher line speeds. Extrusion coating onto paperboard or foil is possible only if the melt curtain remains stable; published data for this specific configuration is limited, and neck-in must be characterized on the target substrate with the actual die width and air gap.

    Influence of Butene Branching on Melting Point and Seal Window

    Because butene branches disrupt ethylene chain folding, the melting peak of film-grade butene LLDPE is typically between 120 °C and 125 °C, lower than high-density grades and slightly lower than octene-based LLDPE at equivalent comonomer molar content. This lowering of the crystalline melting point expands the seal-initiation window but limits upper-end service temperature. Continuous service above 80 °C in stressed film applications accelerates creep and orientation relaxation; thermoforming and boil-in-bag use require suitability verification under the target sterilization conditions. Differential scanning calorimetry under ISO 11357-3 records a broad melting endotherm due to the interchain composition distribution. The crystallinity is commonly between 35% and 45% based on the enthalpy of fusion of a perfect polyethylene crystal, which is reflected in lower modulus and higher elongation than high-density polyethylene.

    Tensile, Tear, and Impact Response Benchmarks

    Film property testing follows ASTM D882 for tensile stress and strain, ASTM D1922 for Elmendorf tear, ASTM D1709 for falling-dart impact, and ASTM D1003 for haze. In 25 µm blown film, butene-LLDPE grades in this class typically show machine-direction tensile strength at break from 30 MPa to 40 MPa, transverse-direction tensile strength at break from 25 MPa to 35 MPa, and elongation at break above 500%. Elmendorf tear is anisotropic: the machine-direction tear is generally lower than the transverse-direction tear because of molecular orientation induced along the bubble axis. Dart impact for 25 µm film commonly exceeds 80 g under Method A; however, lot-specific values should be drawn from the certificate of analysis because comonomer distribution and film-fabrication history shift dart impact more than density. Compared with hexene or octene metallocene LLDPE, a butene-catalyst LLDPE of identical density and melt index typically shows lower dart impact, lower clarity, and higher haze. The difference arises from broad interchain composition distribution in conventional Ziegler-Natta butene resins, which creates a wider melting range and more light-scattering tie-chain defects.

    Normative Compliance Matrix for Olefin Film and Sheet Contact

    The table below lists standard designations commonly referenced for olefin-based food-contact and industrial film. The grade is not automatically compliant in every jurisdiction; final compliance is a function of the finished article, thickness, migration limits, and conditions of use.

    Normative reference Scope Implication for Icorene 1210 BWN 8443
    FDA 21 CFR 177.1520 Olefin polymers for food-contact articles May be used for direct food contact when the final article meets conditions of use and thickness requirements.
    EU Regulation (EU) No 10/2011 Plastic materials intended to come into contact with food Requires overall migration testing under assigned food simulants and verification of specific migration limits.
    REACH (EC) No 1907/2006 Registration, evaluation, authorisation of chemical substances Polymer substances are generally exempt from registration; monomer and additive obligations remain.
    RoHS Directive 2011/65/EU Restriction of hazardous substances in electrical and electronic equipment Applies only where the resin is incorporated into EEE; heavy-metal limits must be verified on the finished component.
    ISO 1183-1:2019 Density measurement of plastics Used to verify lot density and calculate crystallinity approximations.
    ISO 1133-1:2022 Determination of melt mass-flow rate Used for lot acceptance and incoming resin verification at 190 °C/2.16 kg.
    ASTM D1238 Melt flow rate of thermoplastics by extrusion plastometer Alternative melt-flow verification method used in North American supply chains.
    ASTM D882 Tensile properties of thin plastic sheeting Determines machine-direction and transverse-direction film strength and elongation.

    Polyethylene resins of this type are generally produced without intentionally added heavy metals and are not classified as hazardous under REACH. However, converters must evaluate specific migration of any masterbatch, printing ink, or lamination adhesive, because additives can alter organoleptic and migration performance. The grade should not be combined with amine-based additives in high-temperature processing above 230 °C unless the stabilizer interaction is tested, as premature yellowing and loss of oxidative induction time can occur. Long-term outdoor exposure requires a UV-stabilized post-added masterbatch unless the suffix-specific datasheet confirms a UV package. Sterilization by autoclaving above 121 °C should be qualified on the final film structure because dimensional distortion and seal-strength reduction are governed by total thermal history, not by resin identity alone.

    Top