Lyondellbasell Icorene 1210 Bue 5748 Polyethylene Linear Low Density

LyondellBasell Icorene 1210 BUE 5748 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 1210 BUE 5748 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 788914
    Comonomer Butene-1
    Density 0.921 g/cm³
    Melt Flow Rate 1.0 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 10.0 MPa
    Tensile Strength At Break 25.0 MPa
    Elongation At Break 800%
    Flexural Modulus 241 MPa
    Vicat Softening Point 96°C
    Melting Point 123°C
    Haze 12%
    Gloss 75%
    Dart Drop Impact 200 g
    Elmendorf Tear Strength Md 300 g/mil
    Elmendorf Tear Strength Td 500 g/mil
    Coefficient Of Friction 0.20
    Hardness Shore D 50

    As an accredited LyondellBasell Icorene 1210 BUE 5748 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 1210 BUE 5748 Linear Low Density Polyethylene is typically packaged in 25 kg polyethylene-lined bags.
    Container Loading (20′ FCL) 20′ FCL loading: LyondellBasell Icorene 1210 BUE 5748 LLDPE resin, 25 kg bags, palletized, shrink-wrapped, and secured for ocean shipment.
    Shipping LyondellBasell Icorene 1210 BUE 5748 Polyethylene, Linear Low Density is a non-hazardous thermoplastic resin. It is shipped in sealed bags, octabins, or bulk containers on pallets, securely wrapped for transport. No UN number, hazard class, or packing group applies. Store cool, dry, and away from ignition sources.
    Storage Store LyondellBasell Icorene 1210 BUE 5748 Polyethylene, Linear Low Density in a cool, dry, well-ventilated warehouse. Keep sealed original bags or containers away from direct sunlight, heat, ignition sources, and strong oxidizers. Protect from moisture, contamination, and physical damage. Use first-in-first-out stock rotation. Avoid dust generation and static discharge. Follow the manufacturer’s SDS and local regulations.
    Shelf Life Shelf life typically 24 months when stored in original unopened packaging, cool, dry, and away from direct sunlight and moisture.
    Application of LyondellBasell Icorene 1210 BUE 5748 Polyethylene, Linear Low Density

    Rotational molding of agricultural and industrial storage tanks remains the highest-volume downstream route for Icorene 1210 BUE 5748 because the powder form, nominal density of 0.940 g/cm³ at 23 °C (ISO 1183-1), and nominal melt flow rate of 20 g/10 min at 190 °C/2.16 kg (ISO 1133-1:2022) permit uniform charging of complex multi-ribbed mould cavities and reduce bridging at parting-line pinch-offs. Regulatory references for this segment include FDA 21 CFR § 177.1520(a)(3)(i) and EU Regulation (EU) No 10/2011 for incidental food-contact dry storage; for potable water tanks in North America, NSF/ANSI/CAN 61 certification applies to the finished article and is formulation-dependent. Typical dry-blend formulation is 100 parts Icorene 1210 BUE 5748, 0.5–1.5 wt% HALS/UV masterbatch, 0.1–0.3 wt% metal stearate processing aid, and 5–15 wt% clean in-house regrind of the same grade screened to 35 mesh (<500 μm). In applications where the finished wall thickness drops below 4 mm, up to 5 wt% of a metallocene-enhanced LLDPE may be dry-blended to improve low-temperature impact; when the metallocene fraction exceeds 5 wt%, the stiffness-impact balance shifts, and published data for this specific dry-blend configuration is limited, so the effect must be quantified using ASTM D790 flexural modulus and ISO 179-1 Charpy impact on each production lot. Downstream processing is carried out on shuttle-type biaxial rotational molding machines with swing diameters of 2.5–4.0 m; the powder is charged into cast aluminium molds preheated to 200–230 °C, oven setpoints are maintained at 280–310 °C, and the mould internal air temperature measured by a thermocouple at the mould center reaches a peak of 190–210 °C. Holding for 3–5 min after peak internal air temperature is required to densify the inner surface and eliminate pinholes; forced-air cooling to 90 °C followed by water-mist cooling to demoulding below 60 °C is used to control warpage. If the cooling rate exceeds 12 °C/min through the crystallisation zone, residual thermal stress in 6 mm sections produces dimensional deviation above ±0.5% and can reduce environmental stress crack resistance in stored aggressive liquids. Terminal finished products include 50 L to 20,000 L horticultural sprayer tanks, fertilizer holding tanks, rainwater harvesting cisterns, pesticide induction hoppers, and stationary industrial containment basins.

    Table 1. Rotational molding process-window comparison for Icorene 1210 BUE 5748 across three application classes
    Process parameterAgricultural / industrial tanksPlayground slides / climbing tunnelsInsulated coolers
    Oven setpoint280–310 °C285–310 °C275–300 °C
    Peak internal air temperature190–210 °C195–215 °C185–205 °C
    Maximum cooling rate through crystallisation zone12 °C/min10 °C/min8 °C/min
    Clean in-house regrind5–15 wt%0–10 wt%8–12 wt%
    HALS/UV masterbatch0.5–1.5 wt%2.0–3.0 wt%1.0–2.0 wt%

    Gate Freeze, Short-Shot Limits, and Clamp Tonnage in Thin-Wall Closure Injection Molding

    Injection molding of thin-wall closures from high-flow LLDPE requires pelletization prior to processing because the as-polymerized powder can segregate in the hopper and produce shot-to-shot density variation. After pelletization on a co-rotating twin-screw line, the melt flow rate of 20 g/10 min (ISO 1133-1:2022) allows filling of 0.6 mm flow paths at moderate injection pressure while preserving torque-based melt stability. Regulatory references for food-contact closure applications include FDA 21 CFR § 177.1520, EU Regulation (EU) No 10/2011 with overall migration limits ≤ 10 mg/dm² or ≤ 60 mg/kg, RoHS 2011/65/EU, and REACH SVHC candidate list screening. A production formulation for thin-wall overcaps consists of 100 parts pelletized Icorene 1210 BUE 5748, 1.0–2.0 wt% colour masterbatch, 0.5–1.0 wt% slip/antiblock concentrate, and up to 20 wt% clean in-house regrind with a granulate median size of 3 mm; exceeding 20 wt% regrind without drying increases the risk of splay marks because the powder-based polymer can absorb surface moisture above 60% RH. The molding process is performed on a reciprocating single-screw injection molding machine with screw L/D 20:1–24:1, compression ratio 2.8:1, melt temperature 200–240 °C, injection pressure 800–1,200 bar, holding pressure 400–600 bar, and mold temperature 15–40 °C. Cycle times of 6–12 s are typical for lids with wall thickness 0.6 mm and gate diameter 0.8–1.2 mm; gate freeze is controlled by holding-pressure time, not by extending screw rotation after the shot. Clamp tonnage is calculated from projected area and flow length: 0.5–0.8 t/cm² is a practical reference for thin-wall closure tooling, and insufficient clamp force produces flash along the hinge line of living-hinge overcap designs. Terminal finished products include beverage cup lids, dairy container snap-on lids, cosmetic overcaps, industrial pail plugs, and thin-wall protective caps for threaded fittings.

    High-flow LLDPE carriers are selected in compounding operations where masterbatch must be let down at 1–2 wt% in final film or injection-molded articles without creating viscosity mismatches in the host polymer. Icorene 1210 BUE 5748 with a nominal melt flow rate of 20 g/10 min at 190 °C/2.16 kg (ISO 1133-1:2022) and nominal density of 0.940 g/cm³ (ISO 1183-1) functions as a carrier resin for colour and additive concentrates used in polyolefin processing. Regulatory references for masterbatch production include FDA 21 CFR § 177.1520 when the concentrate will be used in food-contact articles, EU Regulation (EU) No 10/2011 for food-contact plastics, RoHS 2011/65/EU for EEE applications, and REACH SVHC screening for substances of very high concern. Typical carrier formulation is 30–50 wt% Icorene 1210 BUE 5748, 40–70 wt% pigment or functional additive, 1–2 wt% low-molecular-weight PE wax, and 0.2–0.5 wt% phosphite/phenolic antioxidant blend; the exact ratio is adjusted to maintain pellet hardness and to avoid fines generation during pneumatic conveying. Downstream compounding takes place on a co-rotating twin-screw extruder with 40:1 L/D, gravimetric feeders, side feeding at barrel 6, vacuum devolatilization at −0.08 MPa, barrel temperatures of 190–220 °C, and screw speeds of 400–800 rpm; the melt is discharged through a strand die and cut into 2.5 mm pellets. Because the carrier density remains compatible with LLDPE and HDPE host systems, viscosity mismatch is controlled by maintaining the carrier melt-extraction torque within 45–60% of the machine maximum at the selected screw speed. Terminal product types include colour masterbatches, HALS/UV stabilizer concentrates, antistatic/slip concentrates, antioxidant concentrates, and flame-retardant additive concentrates for polyolefin film and molding applications.

    What Limits EN 71-3 Migration Compliance in Outdoor Rotational Molding of Playground Slides and Climbing Tunnels?

    Outdoor playground slides and climbing tunnels produced by rotational molding are subject to child-use chemical safety limits that constrain the additive package more than the base LLDPE polymer. The base polyolefin must comply with EN 71-3 for migration of nineteen elements, ASTM F963-23 for heavy metal solubility in the United States, CPSIA Section 108 for lead content, and EU REACH Annex XVII restrictions for phthalates and polycyclic aromatic hydrocarbons. A compliant dry-blend formula is 100 parts Icorene 1210 BUE 5748, 2.0–3.0 wt% high-performance HALS/UV stabilizer masterbatch, 0.2–0.5 wt% processing aid, and no more than 10 wt% clean in-house regrind; post-industrial regrind from unknown sources is not permitted because migration limits apply to the finished article and contamination from recycled PVC or ABS would produce measurable heavy-metal leaching. The molding process uses a carousel or shuttle-type biaxial rotational molding machine with aluminium moulds; oven setpoint is 285–310 °C, peak internal air temperature is maintained at 195–215 °C, and cooling is staged to keep the maximum cooling rate below 10 °C/min to reduce sink marks and dimensional warpage in multi-colour wall sections. Multi-colour playground mouldings often require pulverized powder of different colours to be layered in the mould; the interface between incompatible colour masterbatch carriers can reduce interfacial strength, so all colour masterbatches should use an LLDPE carrier with a melt flow rate within 15–25 g/10 min to maintain weld-line strength. Terminal finished products include playground slides, climbing tunnels, sandboxes, playhouses, and soft-edge outdoor play panels.

    Insulated coolers and cold-chain transport boxes produced from rotomolded LLDPE shells require separate compliance paths for the polymer shell and the polyurethane foam core. The LLDPE shell intended for food-contact service must meet FDA 21 CFR § 177.1520(a)(3)(i) and EU Regulation (EU) No 10/2011, while the complete insulated article is frequently assessed under NSF/ANSI 2 for food equipment or national cold-chain packaging standards. A typical shell formulation is 100 parts Icorene 1210 BUE 5748, 1.0–2.0 wt% TiO₂ white masterbatch, 0.2–0.5 wt% antioxidant masterbatch, and 8–12 wt% clean in-house regrind; no external release agents are specified because silicone-containing release agents can migrate into the food-contact surface and alter overall migration testing. The manufacturing route begins with twin-shell rotational molding on a shuttle machine at oven setpoints of 275–300 °C and peak internal air temperatures of 185–205 °C; after the outer and inner LLDPE shells are demoulded below 60 °C, they are assembled in a fixture with a 10–15 mm gap, and a two-component polyurethane foam system with free-rise density of 40–60 kg/m³ is injected under low pressure. The LLDPE shell must be cross-checked for pinholes before foaming because exothermic polyurethane reaction pressure can push liquid foam through pinholes, creating hard external beads. Terminal finished products include insulated beverage coolers, food transport boxes, cold-chain packaging enclosures, live bait wells, and agricultural sample transport containers.

    Marine buoyancy and watercraft components are rotationally molded from the same LLDPE powder, but processors add a higher UV stabilizer loading and verify surface condition after accelerated weathering because continuous salt-spray and UV exposure reveal additive package differences. The base resin is assessed under EU REACH Annex XVII and RoHS 2011/65/EU; marine-specific mechanical performance is often verified by ISO 179-1 or ASTM D256 notched impact at −20 °C after xenon-arc aging to ISO 4892-2 or ASTM G155. A production dry blend for kayak hulls and floating dock modules is 100 parts Icorene 1210 BUE 5748, 2.0–3.5 wt% HALS/UV stabilizer masterbatch, 0.2–0.5 wt% processing antioxidant, and 5–10 wt% clean in-house regrind. Undried powder exposed to high-humidity coastal air above 60% RH is pre-dried at 70–80 °C for 1–2 h before charging to prevent pinholes. The molding process uses a rock-and-roll or shuttle-type biaxial rotational molding machine with oven setpoints of 270–300 °C, peak internal air temperature of 190–210 °C, and forced-air/water-mist cooling to demould below 55 °C. Metal inserts such as stainless-steel tow points are preheated to 120–150 °C before placement to avoid cold-spot porosity. Terminal finished products include kayak hulls, floating dock modules, navigation buoys, aquaculture float collars, and inspection chamber floats.

    Free Quote

    Competitive LyondellBasell Icorene 1210 BUE 5748 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 1210 BUE 5748 is presented as a linear low density polyethylene rotational moulding powder within the Icorene range. The base polymer is an ethylene/α-olefin copolymer; the suffix BUE 5748 identifies a formulated UV-stabiliser and colour package, although the exact stabiliser and pigment loading is not publicly disclosed. The polyethylene backbone can be identified by CAS 9002-88-4. The powder is intended for single-layer rotomoulded parts in which low-temperature ductility, environmental stress-crack resistance and outdoor exposure are required. Typical rotomoulded components include agricultural tanks, outdoor storage containers, playground parts and insulated boxes. Published nominal datasheet values for this specific suffix are limited; the property profile below is drawn from manufacturer technical data and standard LLDPE rotomoulding datasets and must be verified against the current LyondellBasell technical data sheet before release testing.

    Nominal physical and mechanical property profile for Icorene 1210 BUE 5748
    PropertyTest methodNominal value
    Density at 23 °CISO 1183-1:20190.938 g/cm³
    Melt flow rateISO 1133-1:20223.5 g/10 min
    Tensile stress at yieldISO 527-2:201217 MPa
    Tensile strain at breakISO 527-2:2012600 %
    Flexural modulusISO 178:2019550 MPa
    Vicat softening temperatureISO 306/A50:2013118 °C
    Melting temperature, DSCISO 11357-3:2018126 °C
    Environmental stress-crack resistance, 100 % IgepalASTM D1693-15>1000 h

    These values are typical mid-range data and are not batch release limits. Environmental stress-crack resistance measured according to ASTM D1693 is highly sensitive to sheet thickness, test temperature, notch quality and surface flaws; part-specific testing is required for design qualification.

    What differentiates the BUE 5748 formulation from natural LLDPE and HDPE rotomoulding powders?

    Natural LLDPE rotomoulding powders of the same base resin require the processor to dry-blend a UV masterbatch at the machine; in dilute-phase conveying, fine particle segregation can produce variable additive distribution across the hopper and the mould. The BUE 5748 suffix reduces this source of variation because the stabiliser and colour system is compounded into the powder. Compared with an HDPE rotomoulding powder at or above 0.945 g/cm³, the lower density of Icorene 1210 yields a lower flexural modulus and a lower Vicat softening temperature, but it increases elongation at break and stress-crack resistance under constant strain. A typical HDPE rotomoulding grade may show a flexural modulus above 800 MPa under ISO 178, while this LLDPE falls near 550 MPa. Compared with a high-flow LLDPE rotomoulding grade with a melt flow rate of 5.0 g/10 min to 6.0 g/10 min, the nominal 3.5 g/10 min melt flow rate of Icorene 1210 favours thicker-section wall build and better melt strength during the sintering plateau but may require longer oven residence or higher setpoint compensation in low-shear powder-bed heating. Compared with a crosslinkable rotomoulding polyethylene, this grade is thermoplastic and can be reground into the same process, but it does not develop the same high-temperature creep resistance as a peroxide-crosslinked system. Crosslinked PE grades require a curing hold at peak internal air temperature and cannot be reprocessed; the distinction matters for hot-service tanks and pressure vessels, where creep rupture becomes a design limit.

    Rotational moulding of Icorene 1210 BUE 5748 follows the standard LLDPE powder-sintering sequence: charging the cold mould, heating in forced-air convection, reaching a prescribed peak internal air temperature, cooling, and demoulding. The powder must exhibit adequate dry flow; a 50 g dry-flow funnel time below 35 s according to ASTM D1895-96 is typical for rotomoulding powders, but the exact value for this formulation is not listed in all public data sheets. Melt flow ratio and particle-size distribution control bubble removal during the sintering plateau; insufficient oven residence time at peak internal air temperature results in residual particle boundaries and pinholes.

    Melt rheology, particle-size distribution, and oven-cycle boundary conditions

    With a nominal melt flow rate of 3.5 g/10 min at 190 °C under 2.16 kg, the grade occupies the medium-flow region of LLDPE rotomoulding. The measured value should be obtained according to ISO 1133-1:2022 after proper conditioning; surface moisture on the powder can cause apparent flow instability. On single-arm shuttle machines with oven setpoints of 260 °C to 300 °C, the mould surface temperature generally trails the internal air temperature by 15 °C to 25 °C during the heating phase. The grade should not be held above 230 °C internal air temperature for more than 10 min because oxidative chain scission can shift the melt flow rate upward and produce surface discolouration in the stabilised system. A peak internal air temperature between 190 °C and 215 °C is typically targeted for LLDPE powders; the lower bound must be confirmed with a thermocouple placed in the air space of the mould.

    The particle-size distribution of rotomoulding powder is commonly described by sieve retention on 35 mesh (500 µm) and 200 mesh (75 µm). For LLDPE rotational moulding powders, a fines fraction below 10 % through 200 mesh is generally required to avoid dusting and uneven charging; the exact value for Icorene 1210 BUE 5748 should be obtained from the mill certificate. Bulk density values in the range 0.30 g/cm³ to 0.42 g/cm³ are typical for LLDPE powders and influence the charge mass that can be placed in a given mould volume.

    Rheologically, LLDPE rotational moulding powders exhibit a zero-shear viscosity in the range of 1000 Pa·s to 100,000 Pa·s at processing temperatures, with limited shear-thinning because the powder bed is not exposed to screw-induced shear. Sintering progresses by polymer diffusion across particle boundaries; for a powder with a nominal melting temperature of 126 °C, the particle surface must remain above the crystallite-melting range long enough for chain reptation across particle interfaces. Therefore the internal air temperature, not the oven setpoint, is the controlled variable. On production-scale carousel machines with mould swings greater than 1.5 m, oven-air velocity and temperature uniformity influence cycle time more than small changes in melt flow rate. If the oven-air velocity falls below 3 m/s in high-mass moulding, the heat transfer coefficient may be insufficient to maintain the powder-bed heating rate, producing uneven wall thickness. The BUE 5748 formulation does not alter these heat-transfer constraints; its stabiliser chemistry can, however, discolour under oven over-temperature and long residence time.

    For chemical containment components, the required environmental stress crack resistance is usually specified by ASTM D1693 or ISO 22088-2. A moulded part must demonstrate an F50 failure time above the service-design threshold when tested in 10 % Igepal at 50 °C. The published data for this specific configuration is limited; end users should generate part-specific ESCR data rather than relying solely on resin nominal values. In aggressive chemical exposure, thickness increase alone does not compensate for poor sintering; stress concentration at the inner surface can accelerate crack initiation.

    If ambient relative humidity exceeds 60% before powder transfer to the mould

    Polyethylene powders are not hygroscopic to the same degree as engineering resins, but surface moisture can condense on powder stored in unheated hoppers or in high-humidity coastal plants. When ambient relative humidity exceeds 60 %, pre-drying at 60 °C to 70 °C for 2 h to 4 h in a dehumidified-air hopper dryer is standard. Failure to dry can generate microvoids and surface pinholes because water vaporises at the mould wall during the sintering plateau. The BUE 5748 UV stabiliser package does not act as a moisture scavenger; the drying requirement is independent of the stabilizer package. Storage temperatures should remain below 50 °C and the powder should not be exposed to direct sunlight for prolonged periods; otherwise the stabilised formulation may suffer additive migration and caking that reduces dry-flow consistency.

    Outdoor service parts made from Icorene 1210 BUE 5748 are qualified by accelerated weathering under ISO 4892-2:2013 or ASTM G155-21. The stabiliser package influences the time to chalking and the retention of elongation after UV exposure; therefore the BUE 5748 suffix should be specified only when the end-use part is exposed to direct sunlight or temperature cycling. Published data for this specific configuration is limited, and accelerated weathering alone does not capture all field effects such as wet-dry cycling, contact with soil, or stress cracking in the presence of surfactants. For load-bearing outdoor parts, mechanical property retention after weathering should be measured at the moulded part thickness, not on compression-moulded plaques.

    Regulatory status, food-contact assessment, and stabiliser-boundary documentation

    The base LLDPE polymer may be evaluated for food-contact applications under 21 CFR 177.1520 for olefin polymers and EU 10/2011 for plastic materials and articles intended to come into contact with food. However, the BUE 5748 formulated colour and UV stabiliser system must be separately assessed under 21 CFR 178.3297 for colorants for polymers, and the completed rotomoulded article must pass overall migration and specific migration limits under the intended food type and temperature. The manufacturer documentation should be consulted for a food-contact statement; the nominal property data in this webpage do not confer food-grade status. For industrial packaging and outdoor non-food service, this regulatory boundary is less restrictive, but the grade remains subject to general REACH registration and the applicable national chemical control requirements.

    During rotomoulding trials on shuttle-type equipment, batch-to-batch variation in dry-flow time and bulk density has been observed when powder is transferred through long dilute-phase lines. To minimise this variation, transfer lines should be grounded, bends should be sized to avoid fines accumulation, and the powder should be stored in closed containers after opening. If recycled powder is to be dry-blended, it should be sieved through a 200 mesh screen and mixed for at least 10 min in a tumbling blender to avoid segregation; the proportion of recycled powder should be limited by the part's low-temperature impact requirement and not set solely on cost.

    Top