| HS Code | 618025 |
| Density | 0.935 g/cm3 |
| Melt Index | 5.0 g/10 min |
| Tensile Strength At Yield | 17.0 MPa |
| Tensile Strength At Break | 14.0 MPa |
| Elongation At Break | 800% |
| Flexural Modulus | 690 MPa |
| Hardness Shore D | 55 |
| Notched Izod Impact | 60 J/m |
| Vicat Softening Point | 115 °C |
| Brittleness Temperature | -70 °C |
| Melting Point | 125 °C |
| Environmental Stress Crack Resistance | >1000 hr |
| Coefficient Of Linear Thermal Expansion | 1.5E-4 1/°C |
| Water Absorption | 0.010% |
| Specific Gravity | 0.935 |
As an accredited LyondellBasell Icorene 1210 BLK 9001 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 1210 BLK 9001 Linear Low Density Polyethylene is supplied in 25 kg polyethylene bags, palletized for handling. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): LyondellBasell Icorene 1210 BLK 9001 LLDPE, bagged, palletized, shrink-wrapped, and secured in a 20-foot FCL container. |
| Shipping | LyondellBasell Icorene 1210 BLK 9001 Polyethylene, Linear Low Density is shipped as non-hazardous solid resin pellets in sealed bags, boxes, or bulk containers. Transport in clean, dry, covered vehicles. Store away from heat, moisture, sunlight, and contamination. No UN hazard class; consult SDS for handling. |
| Storage | Store LyondellBasell Icorene 1210 BLK 9001 polyethylene in a cool, dry, well-ventilated area using tightly closed original containers or bags. Protect from direct sunlight, heat, sparks, flames, and oxidizing agents. Keep away from moisture and contamination. Use first-in, first-out rotation. Avoid prolonged outdoor storage, and do not store near food, feed, or drinking water. Maintain good housekeeping and inspect containers regularly. |
| Shelf Life | Shelf life is 24 months when stored unopened in original packaging, in a cool, dry place, away from direct sunlight. |
Geomembrane liner welding with Icorene 1210 BLK 9001 is specified around dual-track hot-wedge fusion rather than extrusion fillet welding because the carbon black package alters surface melt rheology and slows air-gap oxidation. Sheet thickness in this application class is normally 0.75 mm to 2.00 mm, with weld overlap set to 40 mm to 60 mm and wedge temperature maintained at 340 °C to 400 °C depending on line speed. A peel test to ASTM D6392-12 must fail in the parent sheet; any separation along the weld plane is rejected as a setup failure. Carbon black content is kept between 2.0 wt% and 3.0 wt% when tested to ASTM D1603-14, and dispersion is graded to ISO 18553:2002; agglomerates above 25 µm are counted as a batch defect when present in more than three fields of view. Oxidative induction time is measured to ASTM D3895 at 200 °C on the unaged sheet and after 90 days at 85 °C. A residual OIT below 50% of the unaged value is treated as stabilizer depletion. The governing specification is GRI-GM17 for LLDPE geomembranes, not the HDPE-oriented GRI-GM13; this distinction avoids imposing stress-crack-resistance requirements that are not applicable to flexible LLDPE liners. End products include heap leach pads, secondary containment cells, anaerobic lagoon covers, and canal liners where installation at −20 °C requires the compound to retain tear resistance and weld strength.
In thin-wall emitter tubing, the principal failure location is the emitter barb root, not the tube burst surface. The compound is extruded at a melt temperature of 210 °C to 225 °C through a single-screw extruder with a 30:1 L/D barrier screw and a screen pack of 80/60/20 mesh. The die land is held 5 °C to 8 °C above the die body to prevent shark-skin on 0.20 mm wall sections. Because the material is a precompounded black LLDPE, the converter does not dose carbon black masterbatch at the feed throat; this eliminates the screw-slippage variability of 0.3% to 0.7% observed when a 50% black masterbatch is added separately. Carbon black loading remains at 2.0 wt% to 2.5 wt%, and agglomerates above 20 µm are rejected under ISO 18553:2002. Tubing is tested to ISO 9261 for emitting pipes and to ISO 1167-1:2006 for hydrostatic strength at 60 °C. For 16 mm diameter, 0.9 mm wall stock, burst pressure at 23 °C is required to exceed 0.6 MPa; the 60 °C value is permitted to fall by no more than 30%. A 10 wt% to 20 wt% addition of unpigmented LLDPE may be used to reduce die pressure, but it dilutes carbon black below the 2.0 wt% UV threshold and invalidates outdoor weatherability unless re-qualified. End products include non-pressure-compensating drip tape, integral drip line, and subsurface fertigation laterals buried at 0.25 m to 0.40 m depth.
In silage clamp sealing and silage bag manufacture, the black LLDPE is processed on a three-layer blown-film line with die diameter of 250 mm to 350 mm, die gap of 2.0 mm, and blow-up ratio of 2.2:1 to 2.8:1. The outer layers contain the black compound at 60 wt% to 70 wt% of total film mass; the core layer carries 30 wt% to 40 wt% recycled trim or unpigmented LLDPE. This structure keeps the exposed-surface carbon black concentration above 2.0 wt% while preserving dart impact resistance. Melt temperature at the die lip is limited to 195 °C to 205 °C because carbon black raises elongational viscosity; if the frost-line height drops below 1.0 m, bubble instability and thickness gauge bands develop. Film thickness is controlled at 0.150 mm to 0.250 mm for wholecrop rye and maize silage covers. Oxygen transmission measured to ASTM D3985 at 23 °C and 0% RH above 2,500 cm³/(m²·day·atm) is rejected for long-term silage because aerobic yeast and mould activity accelerates. Tear retention is tested to ASTM D1922 after 500 h xenon-arc weathering to ISO 4892-2; retention below 60% of unexposed tear strength is a UV-stabilizer failure. End products include clamp films, side-sheet films, and round-bale wrap tubes where black pigmentation extends field storage beyond 24 months.
Corrugated cable-management conduit manufactured from black LLDPE uses die pressure as an indirect indication of carbon black agglomerate accumulation. The screw speed is indexed to maintain die pressure below 25 MPa at a melt temperature of 215 °C; pressures above this threshold indicate either an undersized screen pack or pigment tailings filling the die land. Screens of 100/80/60/20 mesh are installed, and the 20 mesh layer is replaced after 48 operating hours because backflush cannot dislodge carbon black fines from the land area. The die temperature profile runs from 180 °C at the adapter to 205 °C at the lips, while vacuum calibration holds 0.02 MPa to 0.05 MPa negative pressure to fix corrugation depth. Carbon black content is verified to ASTM D1603-14 at 2.0 wt% to 2.8 wt%. This grade is an insulating jacket material, not a semiconductive compound; volume resistivity after conditioning at 23 °C and 50% RH remains above 10¹² Ω·cm when tested to IEC 62631-3-1. Finished conduits are tested to IEC 61386-1 for compression and impact at −5 °C; compression shall not reduce inner diameter by more than 5%. RoHS recast 2011/65/EU and REACH SVHC declarations are completed on the polymer lot before conduit qualification. End products include low-smoke halogen-free conduit systems, cable protection ducts, and optical-fiber microduct outer sheaths.
The processing window in rotational moulding is bounded by the peak internal air temperature measured with a wireless probe inside the mould. The mould is charged at 3.5 kg/m² of projected area for a 6 mm wall thickness in cast-aluminium tooling. Oven setpoint is 290 °C to 310 °C with biaxial rotation at a 4:1 speed ratio and minor-axis speed of 4 rev/min to 6 rev/min. Peak internal air temperature is held at 205 °C to 215 °C for a minimum of 4 minutes. Temperatures above 220 °C cause surface oxidation that appears as black specks and reduce tensile impact strength by more than 15%; temperatures below 195 °C leave unmelted powder at the parting line. Forced-air cooling is applied for 8 minutes to 10 minutes, then water mist for 6 minutes to 8 minutes; demoulding is not started above 75 °C because warpage increases. Carbon black loading is 2.0 wt% to 2.5 wt%, and dispersion is checked on microtomed sections. Low-temperature impact is tested to ASTM D256/ISO 179 at −40 °C; mean failure energy below 12 kJ/m² is a rejection criterion for outdoor agricultural tanks. Where a tank is intended for potable water, the converter must confirm carbon black compliance under 21 CFR 177.1610 or NSF/ANSI 61; the base polyolefin alone does not establish food-contact clearance for the black concentrate. Published data for this specific grade across all mould geometries are limited; the temperature band is a process start point, not a substitute for lot-specific thermal profiling. End products include 100 L to 2,000 L chemical storage tanks manufactured to ASTM D1998-15, as well as seed hoppers and veterinary waste containers that follow the same rotational moulding practice but are outside the tank standard.
FIBC liner film and agricultural chemical bag stock made from black LLDPE separate gauge uniformity from static-load creep behaviour because both defects appear under different loading histories. The compound is cast at 220 °C to 240 °C through a 1.4 mm to 1.8 mm die gap, with chill roll temperature held at 18 °C to 22 °C to quench the black surface without blocking. For a 0.100 mm liner, web thickness tolerance is ±8%; wider variation produces fold-lines that fail during the 6:1 safety-factor drop test of filled FIBCs. Carbon black content is 2.0 wt% to 3.0 wt%. Tensile elongation is tested to ISO 527-3; machine-direction elongation below 600% is rejected because fill-and-discharge cycles impose biaxial deformation at bottom seams. Creep is measured to ASTM D2990 with a static load of 20% of film yield stress for 1,000 hours at 23 °C; creep strain above 3% before unloading indicates insufficient crystallinity from the quenched cast film. End products include polyethylene liners for FIBCs, sift-proof hazardous-goods liners, and heavy-duty sacks for polymer granules.
Competitive LyondellBasell Icorene 1210 BLK 9001 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 1210 BLK 9001 Polyethylene, Linear Low Density is a black, UV-stabilized rotational molding powder. The base resin is an ethylene copolymer in which a short-chain α-olefin comonomer is incorporated along the backbone; this molecular architecture reduces crystallinity and density relative to a high density polyethylene homopolymer. In the LyondellBasell product code, Icorene identifies the rotational molding powder family, 1210 identifies the base resin position, and BLK 9001 denotes the black pigmentation and stabilizer package. The grade is characterized by a nominal density of 0.940 g/cm³ when tested according to ISO 1183-1 and a nominal melt flow rate of 4.0 g/10 min at 190 °C/2.16 kg when tested according to ISO 1133-1:2022. In tensile testing to ISO 527-2 at a test speed of 50 mm/min, supplier-typical values include a yield stress of 19 MPa and elongation at break above 800%. Flexural modulus determined according to ISO 178 is approximately 760 MPa. Environmental stress crack resistance, measured by ASTM D1693 in 10% Igepal CO-630, typically exceeds 1000 h at F50. These figures are class-typical for a rotomolding LLDPE at the upper density range; independent published data for this exact black 9001 configuration is limited, and the current LyondellBasell product data sheet remains the controlling reference.
On production rotational molding lines, the powder is processed in carousel or shuttle machines using cast aluminum or stainless steel molds. Dry-flow properties of the powder are as important as melt rheology: particle size distribution should be monitored to ASTM D1921 and apparent density to ASTM D1895-17. The nominal powder is ground to a sieve profile typical of rotomolding grades; fine particles passing 35 mesh (500 µm) may migrate into corners and create thin-wall regions, while coarse particles retained above 35 mesh can require longer fusion time. Oven temperatures are generally set in the range 280–320 °C, with peak internal air temperature monitored at 190–230 °C. The optimum value for this grade should be taken from supplier processing guides. If peak internal air temperature is too low, incomplete coalescence produces pinholes; if the mold is held above 250 °C for extended time, the antioxidant package can be consumed and carbon black may contribute to surface defects. Because this is a black powder, the carbon black increases radiant heat absorption in the oven, but it also reduces the visibility of early yellowing. Once the optimum peak internal air temperature is established for a specific mold, control limits of ±5 °C are typical in production to avoid pinhole formation at low temperature and overbake at high temperature. A deviation of 10 °C may be sufficient to change part appearance, cause internal surface roughness, or reduce impact performance without a visible color shift in black parts. Therefore, process validation should include impact testing of rotomolded plaques, not oven time alone.
The BLK 9001 designation is not solely a pigment change. Carbon black is introduced during compounding or as a fully developed masterbatch prior to grinding; its dispersion quality affects ultraviolet screening and mechanical continuity. In rotomolding, carbon black raises the absorption of radiant heat, which can shorten oven residence time relative to a natural powder of the same melt flow rate. However, carbon black can act as a nucleating agent, shifting the crystallization temperature upward and increasing the risk of nonuniform shrinkage in thick parts. The stabilizer component is designed for prolonged outdoor exposure, but accelerated weathering to ISO 4892-3 should be used to compare retention of tensile elongation rather than color change alone. Because black grades absorb heat more efficiently, cooling time may need to be extended to bring thick sections below the recrystallization range before demolding. A molder transferring from a natural Icorene 1210 powder to the BLK 9001 grade should not assume identical cycle time or warpage behavior without trial on the specific mold.
Thermo-oxidative stability of the black powder can be screened by oxidative induction time (OIT) using ISO 11357-6 or ASTM D3895. LLDPE rotomolding grades with standard antioxidant packages often exhibit OIT values above 20 min at 200 °C, but the black 9001 system may shift the value depending on carbon black interaction with phenolic antioxidants. Because the carbon black masks yellowing, retained tensile elongation after oven aging is a more reliable degradation indicator. For outdoor parts, black UV-stabilized polyethylene can retain a substantially higher fraction of elongation after 4000 h xenon-arc exposure under ISO 4892-3 than unstabilized natural LLDPE; however, published data for this exact Icorene 1210 BLK 9001 configuration is limited, and users should request weathering curves from LyondellBasell. Continuous service under load above 60 °C is generally not recommended for LLDPE parts because creep becomes the limiting design condition.
At a density of 0.940 g/cm³, Icorene 1210 BLK 9001 occupies the upper end of the LLDPE spectrum, close to medium density polyethylene. The flexural modulus of approximately 760 MPa is lower than the 1050–1200 MPa typical of high density polyethylene rotomolding grades. This lower modulus reduces load-bearing capacity but improves stress distribution and environmental stress crack resistance. For rotationally molded tanks and containers, environmental stress crack resistance rather than stiffness often determines service life. Under ASTM D1693, class-typical LLDPE in this density range exceeds 1000 h; high density polyethylene rotomolding resins of similar melt flow rate may fail at 50–200 h. The low-temperature impact resistance of LLDPE is also higher because short-chain branching lowers the ductile-to-brittle transition temperature. Molders should still obtain notched Izod or instrumented impact values from the supplier data sheet for design calculations.
| Property | Icorene 1210 BLK 9001 (LLDPE) | HDPE rotomolding | MDPE rotomolding |
|---|---|---|---|
| Density, ISO 1183-1 | 0.940 g/cm³ | 0.953 g/cm³ | 0.935 g/cm³ |
| Melt flow rate, ISO 1133-1 | 4.0 g/10 min | 5.0 g/10 min | 4.0 g/10 min |
| Flexural modulus, ISO 178 | 760 MPa | 1100 MPa | 650 MPa |
| ESCR, ASTM D1693, 10% Igepal | >1000 h | 100 h | >1000 h |
Powder particle geometry also affects dry flow. The particles are not spherical; pulverized LLDPE particles have irregular surfaces that can bridge in narrow hopper outlets. Bulk density measured to ASTM D1895-17 typically falls within 0.35–0.45 g/cm³ for rotomolding powders; low bulk density increases the volume needed to fill a given mold and may reduce the maximum fill factor. Flow through a standard funnel test may require a 10 mm orifice; powders that fail a 25 mm orifice may need mechanical vibration or auger feeding. On carousel machines, multi-shot loading and in-mold blending with other pigments are common. When dry blending, particle size distribution differences between the blend components can cause segregation because finer particles concentrate in the lower hopper region. For Icorene 1210 BLK 9001, the recommended approach is to test the as-received powder for sieve retention and apparent density before adding recycled material. Rotomolding regrind changes particle shape and may raise the fines fraction, affecting dry flow and wall thickness control.
Unlike injection molding, rotational molding does not apply external shear after melting; therefore, the zero-shear viscosity controls bubble removal. For an LLDPE with melt flow rate 4.0 g/10 min, the zero-shear viscosity at 190 °C is approximately 10⁴ Pa·s; this is lower than a 0.5 g/10 min HDPE rotomolding grade and allows bubble dissipation at lower peak internal air temperature. The trade-off is a lower resistance to gravity-induced flow on vertical walls before solidification, which can cause uneven wall thickness in chimney-like projections. Molds with tall vertical sections may require rotation ratio adjustment or blend with a lower MFR resin.
Applications for this grade include rotationally molded water tanks, agricultural chemical storage, marine buoys, outdoor furniture, insulated cooler bodies, and agricultural equipment enclosures. The black UV-stabilized package is intended for exterior service, but design calculations should use tensile and flexural data generated on rotomolded specimens, not only compression molded sheets. The polyethylene matrix is not resistant to strong oxidizing acids, aromatic hydrocarbons, or esters. Food-contact status is not automatic; the finished part must comply with FDA 21 CFR 177.1520(c) for the specific pigment and antioxidant loading. The powder should be stored in closed containers at ambient temperature below 40 °C and protected from moisture and direct sunlight. The product is supplied in powder form, not pellets, and should not be injection molded or extruded without reprocessing; injection molding grades have different stabilizer and lubricant packages.
| Requirement | Standard/Regulation | Verification approach |
|---|---|---|
| Olefin polymer food contact | FDA 21 CFR 177.1520(c) | End-test migration under intended conditions of use |
| Authorization and SVHC communication | REACH EC 1907/2006 | Safety data sheet and Article 33 declaration |
| Heavy metal and brominated flame retardant restrictions | RoHS Directive 2011/65/EU | XRF screening and certificate of analysis |
Substitution of the LLDPE grade into an HDPE mold should be handled as a requalification. Because the flexural modulus drops from about 1100 MPa to 760 MPa, the part may deflect more under service load; wall thickness may need to be increased or ribs added. LLDPE at 0.940 g/cm³ typically shows lower overall mold shrinkage than HDPE, but black pigmentation can increase differential shrinkage between thick and thin sections because cooling is slower. The lower zero-shear viscosity of the LLDPE may improve fill in deep pockets at lower peak internal air temperature, reducing pinhole frequency. However, the lower crystallization temperature extends the tacky state; demolding should be delayed until the mold surface has cooled below 70–80 °C to prevent post-mold distortion. In biaxial carousel machines, oven dwell may be reduced by 5–10% relative to HDPE because the black powder absorbs radiant heat more efficiently, but the change should be confirmed by peak internal air temperature measurement rather than oven time alone. Switching to Icorene 1210 BLK 9001 therefore requires cycle re-validation, not a simple drop-in replacement.