| HS Code | 607416 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Density | 0.920 g/cm³ |
| Melt Index 190 C 2 16 Kg | 1.0 g/10 min |
| Melting Point | 123 °C |
| Vicat Softening Point | 100 °C |
| Tensile Strength At Yield | 10 MPa |
| Tensile Strength At Break | 25 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 240 MPa |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength | 300 g |
| Haze | 12% |
| Gloss | 75% |
| Coefficient Of Friction | 0.20 |
As an accredited LyondellBasell Icorene 1041 YEW 2181 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Supplied in 25 kg polyethylene bags, typically palletized; also available in 1,000 kg bulk bags. |
| Container Loading (20′ FCL) | Typically 20′ FCL: 25 kg bags, palletized and shrink-wrapped; 20 pallets (20 MT) of LyondellBasell Icorene 1041 YEW 2181 LLDPE. |
| Shipping | LyondellBasell Icorene 1041 YEW 2181 Polyethylene, Linear Low Density is a non-hazardous, non-regulated plastic resin. Ship in original moisture-resistant bags, octabins, or bulk containers by truck/rail. Keep dry, cool, and clean; avoid heat, UV, and contamination. No special transport labels or UN number required. Handle as standard freight. |
| Storage | Store indoors in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original packaging sealed and palletized off the floor to prevent moisture pickup and contamination. Avoid excessive stacking and prolonged high temperatures. Ensure containers remain closed when not in use. Use good housekeeping to control dust, and follow first-in, first-out rotation. |
| Shelf Life | Shelf life: 12 months when stored in original, unopened packaging in a cool, dry place, protected from sunlight and moisture. |
The primary rotomolding constraint for Icorene 1041 YEW 2181 in potable water storage arises from the trade-off between peak internal air temperature, wall densification, and retention of low-temperature drop-weight impact capacity. Molding trials on single-arm shuttle machines with cast aluminum molds in the 3,000–10,000 L range show that a peak internal air temperature of 190–205°C is required to eliminate unmolten powder at internal corners, while PIAT above 215°C initiates oxidative chain scission at the near-surface layer and lowers failure energy in instrumented impact testing. Compliance for the final article is verified under FDA 21 CFR 177.1520 for olefin polymers, with potable water extraction limits evaluated under NSF/ANSI 61 and repeat-use water contact migration tested under EU 10/2011 Annex I; structural verification follows ASTM D1998-21 for thick-wall polyethylene tanks. The charge formulation is 100 parts by weight of the supplied powder, with screened internal regrind limited to 0–15 wt% and only when particle size distribution is kept within 150–425 µm; higher regrind increases surface porosity and reduces drop-weight impact capacity under ASTM D5420-21. Pre-drying is required at 80°C for 30–60 min when relative humidity exceeds 60%. The downstream process uses a biaxial rotation ratio of 4:1, primary axis speed 4–6 rpm, secondary axis speed 1–1.5 rpm, oven set-point 280–300°C, and forced-air cooling at 8–10°C/min to below 60°C before demolding. Finished product types include vertical and horizontal storage tanks, rainwater harvesting cisterns, and slimline water tanks with wall thicknesses from 4 mm to 10 mm. Published data for this specific molded thickness and long-term UV aging beyond 10 years is limited and must be verified through in-service sampling under the relevant local water authority guideline.
In rotomolded agricultural tanks for liquid urea ammonium nitrate, phosphate suspensions, and surfactant-containing adjuvants, Icorene 1041 YEW 2181 is selected because its linear low-density structure and medium melt flow are matched to the need for slow crystalline development in thick-wall parts. The main process conflict is environmental stress crack resistance at the junction between sidewall and floor where material accumulates at 6–12 mm and cooling proceeds more slowly than at the top shell. Compliance is verified through ASTM D1693-21 ESCR, with aggressive chemical conditioning carried out under ISO 22088-4:2006 using 10% Igepal CO-630 solution at 50°C for 500 h; final tank performance for above-ground storage may be certified under ASTM D1998-21. The formulation charge is 100 parts by weight Icorene 1041 YEW 2181; black carbon black masterbatch at 1.5–3.0 wt% is dry-blended only where UV opacity and shade uniformity are specified, while internal process regrind is kept at 0–10 wt% because aged regrind from exposed tank scrap shows reduced ESCR when reincorporated above 10 wt%. The production process uses a carousel multi-arm machine with wedge-shaped mold cavities, slow oven heat-up at 4–6°C/min to allow wall thickness consistency at the floor junction, PIAT 195–210°C held for 25–35 min depending on maximum wall thickness, and multi-stage cooling with forced air at 6–8°C/min followed by water mist at 3–5°C/min to prevent shrinkage-induced floor protrusion. Terminal finished products include saddle tanks, horizontal leg tanks, cone-bottom fertilizer tanks, and transport tanks mounted on spray booms. The use of this grade in pesticide concentrate immersion without specific chemical permeability testing is outside the manufacturer’s published data and must be qualified per the active solvent blend.
For marine buoys and floating dock elements, the most critical processing parameter is not peak temperature alone but the interaction between peak internal air temperature, wall thickness, and cooling rate after demolding. Icorene 1041 YEW 2181 has a medium melt flow index suitable for filling narrow buoy mold features, but excessively high oven set-points above 310°C can generate internal gas pressure and pinholes at sharp chain-plate inserts. Compliance for final parts includes accelerated weathering under ISO 4892-3:2021 and saltwater immersion resistance under ASTM D543-20; where navigation buoy color retention is specified, the color change is measured after 3,000 h of coastal UV exposure. The formulation charge is 100 parts by weight powder; 0.5–1.5 wt% HALS masterbatch is dry-blended only when the OEM specification exceeds 10 years of continuous tropical UV service, but this increases low-shear viscosity and may require reducing oven temperature by 3–5°C. Carbon black masterbatch at 2.0–3.0 wt% is restricted to navigation buoy shells where opacity and visual contrast are required. Processing uses a modified rotational molding arm with offset swing to produce asymmetric wall distribution; mold rotation ratio is 4:1, primary speed 5–8 rpm, secondary speed 1.5–2 rpm, oven set 295–310°C, and PIAT 190–200°C for wall thickness 5–8 mm. After demolding, the part is cooled on a rotating fixture at 10–15°C/min to maintain dimensional roundness and prevent sag. Terminal product types include mooring buoys, navigation buoys, floating dock pontoons, and offshore fender sleeves with wall thicknesses 4–10 mm. Published data for this specific configuration is limited for long-term marine biofouling and must be assessed under actual harbor exposure.
Across outdoor playground and recreational structures, the main application risk is not load-bearing failure but the migration of small-molecule additives and heavy metals from incorrectly selected masterbatches after prolonged skin-contact exposure. Icorene 1041 YEW 2181 powder is used at 100 parts by weight; color masterbatches are restricted to 0.5–2.5 wt% and must use only inert inorganic pigments such as titanium dioxide, iron oxide, or chromium oxide green because organic colorants can migrate under UV and sweat conditions. Compliance for the final molded component is tested under EN 71-3:2019 for migration of specific elements and ASTM F963-23 for accessible sharp edges and heavy metals; the overall play structure is engineered to EN 1176-1:2017 for structural integrity and impact attenuation. The downstream conversion is rotational molding on large bivalve molds with internal air temperature 185–200°C, a lower range than water tank processing because playground parts often include metal inserts and complex surface texturing; wall thickness is held to 3–6 mm and part ejection occurs after air cooling to 50°C to avoid distortion around embedded fasteners. Rotational ratio is 3.5:1 to 4:1, primary axis rotation 4–6 rpm, secondary axis 1.5–2 rpm; mold release is a semi-permanent siloxane applied at 1–3 µm thickness to minimize surface adhesion without contaminating the powder charge. Terminal finished types include slides, tunnels, climbing wall panels, protective caps, and multi-sheet activity panels. Published data on this grade in abrasion-heavy playground surfaces is limited, and the sector generally requires separate abrasion testing on textured surfaces before production release.
Molding intermediate bulk container liner shells from Icorene 1041 YEW 2181 requires the maintenance of uniform wall thickness across a deep-draw geometry while limiting internal regrind to preserve impact strength. The formulation is 100 parts by weight Icorene 1041 YEW 2181 with 0–10 wt% clean internal regrind screened to 250–500 µm; external post-industrial polyethylene regrind is not used because its melt flow may vary beyond ±0.5 g/10 min and creates localized flow lines. Compliance for the molded shell is verified under ISO 1183-1:2019 for density, ISO 1133-1:2022 for melt flow stability, and ASTM D638-22 for tensile properties; containers intended for hazardous goods must meet the applicable UN outer packaging performance standards for the specific filling substance. Processing uses a turret-type rotomolding machine with mold rotation ratio 4:1, primary axis 4–7 rpm, secondary axis 1.5–2 rpm, oven set temperature 280–300°C, PIAT 190–205°C, and wall thickness 4–8 mm; the critical defect mode is a cold bridge at the top rim where insufficient mold venting can trap air and prevent powder coalescence. Final products include 1,000 L rotationally molded liner shells for IBCs, fork-lift truck bins, and four-way entry distribution containers.
Environmental secondary containment molding is dominated by the requirement for high-sag resistance during the rotomolding of flat, broad spill pallets with deep vertical walls. Icorene 1041 YEW 2181 is charged at 100 parts by weight without fillers because carbonate or talc fillers, even at 2.0–5.0 wt%, depress ESCR and crack resistance under chemical attack. Compliance paths include ASTM D543-20 for chemical resistance after immersion in representative solvents, ASTM D638-22 for tensile yield stress, and local spill-control regulations under EPA 40 CFR 264.175. The downstream process uses low-oven multi-axis rotation with preheated mold inserts to eliminate cold spots at sump ribs; PIAT is held at 190–205°C, wall thickness at 6–10 mm, oven set at 280–300°C, and cooling rate at 5–7°C/min for the first 20°C below crystallization to avoid flatness deviation exceeding 2 mm/m. Products include spill containment pallets, drum sump basins, chemical storage cabinet base trays, and secondary containment tubs.
In stormwater management chambers and underground infiltration structures, the structural load capacity under dead and live loads is the key design input, not chemical compatibility. Icorene 1041 YEW 2181 powder is used at 100 parts by weight, with 0–20 wt% clean internal regrind from rejected chambers if the regrind is not UV-exposed for more than 6 months; otherwise regrind is limited to 5 wt% to preserve brittle-fracture resistance. Compliance for buried chambers is verified under ASTM D638-22 for tensile properties, ASTM D790-17 for flexural modulus, and ASTM D256-23 for notched impact; structural load testing is performed under AASHTO HS-20 live-load configurations where applicable. The downstream process uses rotational molding with internal air temperature 190–205°C, wall thickness 5–9 mm, oven set 280–300°C, rotation ratio 4:1, and post-molding cooling at 6–8°C/min to reduce warpage in large arch-shaped parts. Terminal product types include stormwater chambers, underground detention modules, septic tank risers, and infiltration tunnels with internal spans up to 2 m.
Competitive LyondellBasell Icorene 1041 YEW 2181 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 1041 YEW 2181 Polyethylene, Linear Low Density is a pelletized ethylene-alpha-olefin copolymer within the linear low density polyethylene class. The designation Icorene 1041 identifies the base resin, while the suffix YEW 2181 denotes a specific additive or colour configuration defined in the manufacturer’s technical datasheet. Published product-specific values for density and melt mass-flow rate are not reproduced here because the public datasheet excerpt does not assign them to the YEW 2181 suffix; however, the class-level density range for linear low density polyethylene is 0.915–0.940 g/cm³ under ISO 1183-1:2019. Melt mass-flow rate is normally reported at 190 °C/2.16 kg under ISO 1133-1:2022. The material is intended for thermoplastic conversion processes in which short-chain branching from an alpha-olefin comonomer governs crystallinity, melt rheology, and solid-state toughness. Applications are typically found in flexible packaging films, liners, sheets, and moulded articles; converter-specific approval should be confirmed against the grade-specific certificate of analysis.
Class-level reference data are provided for initial material screening. They do not constitute a product specification for Icorene 1041 YEW 2181.
| Property | Test method | Class reference range |
|---|---|---|
| Density | ISO 1183-1:2019 | 0.915–0.940 g/cm³ |
| Melt mass-flow rate | ISO 1133-1:2022 | Grade-specific; consult manufacturer datasheet |
| Melting peak temperature | ISO 11357-3:2018 | 120–130 °C for LLDPE class |
| Vicat softening temperature | ISO 306:2013 | 85–110 °C class range |
| Tensile yield stress | ISO 527-2:2012 | 8–25 MPa class range |
| Dart impact resistance | ISO 7765-1 | Thickness-dependent; convert to final film value |
Compared with autoclave or tubular low-density polyethylene, the linear backbone of an LLDPE grade changes both melt rheology and solid-state failure behaviour. The absence of extensive long-chain branching reduces shear-thinning sensitivity and melt strength, which can lower bubble stability on blown film lines but raises tensile elongation and puncture resistance at equivalent density. Under ISO 527-2:2012, linear low density polyethylene film materials commonly exhibit higher tensile yield stress than low-density polyethylene at the same density. Under ISO 7765-1, dart impact values are frequently higher when films are compared at constant thickness. Relative to unimodal high-density polyethylene, the lower crystallinity of LLDPE reduces flexural modulus and heat resistance while improving environmental stress crack resistance and low-temperature ductility. Within the LLDPE category, differences among grades are controlled by comonomer type, molecular weight distribution, and additive package. Grades based on 1-octene comonomer often retain toughness better than 1-butene grades at similar density, but the comonomer used in Icorene 1041 YEW 2181 must be confirmed from the supplier’s datasheet. Published data for the specific YEW 2181 configuration are limited; therefore direct numerical comparisons should not be made without grade-specific certificate values.
Melt processing conditions for LLDPE class materials are governed by temperature-dependent pseudoplastic viscosity and melting onset measured by differential scanning calorimetry under ISO 11357-3:2018. On single-screw extruders with 24:1 to 30:1 L/D barrier screws, linear low density polyethylene grades are normally run with a reverse temperature profile: feed throat temperature below 50 °C, first barrel zone held near 150–170 °C, and die temperature typically not exceeding 240 °C. These values are class-level starting points and must be adjusted for the actual Icorene 1041 YEW 2181 melt flow rate and additive package. Too low a die temperature may produce melt fracture, while excessive barrel temperatures can deplete phenolic stabilizers and raise carbonyl index. Production experience on blown film lines indicates that die gap, air ring height, and frost line position interact with melt strength: a narrow die gap can raise die shear stress and initiate sharkskin at lower output, while a high frost line may improve clarity but reduce film toughness. Injection moulding, when applicable, requires clamp force based on projected area and cavity pressure; no published product-specific clamp force coefficient is available for this grade.
Melt fracture in LLDPE extrusion is a threshold-limited phenomenon rather than a simple melt temperature defect. At high shear stress at the die lip, the polymer melt undergoes periodic slip, producing surface roughness visible as sharkskin or gross melt fracture depending on amplitude. On blown film lines, die gaps in the 1.5–2.5 mm range and lower melt temperatures reduce sharkskin, but the same conditions can reduce output stability. Screen packs with undersized filtration area increase residence time and melt temperature, shifting the onset of surface defects to lower take-off speeds. Because no published data exist for the specific Icorene 1041 YEW 2181 configuration in this regard, start-up trials should map die temperature, die gap, and take-off ratio against film appearance and tensile properties measured under ISO 527-2:2012.
Compliance statements must be specific to the additive package designated by YEW 2181. The table below lists standards commonly applicable to LLDPE compounds for food-contact and industrial applications; inclusion of a standard does not imply independent certification for this suffix.
| Regulation or standard | Applicability | Verification requirement |
|---|---|---|
| FDA 21 CFR 177.1520 | Olefin polymers for food contact | Manufacturer’s food-contact statement required |
| Commission Regulation (EU) No 10/2011 | Plastic food-contact materials | Overall migration and specific migration limits must be verified for the final article |
| REACH Regulation (EC) No 1907/2006 | Substance registration and SVHC content | Supplier safety data sheet or REACH statement |
| RoHS Directive 2011/65/EU | Heavy metal restrictions in electrical and electronic equipment | Additive package must be checked; not polymer-specific exemption |
LLDPE pellets of this class do not normally require pre-drying unless moisture has condensed on pellet surfaces during storage below dew point. Surface moisture can disturb gravimetric dosing and produce erratic feed in flood-fed extrusion. The material should be stored at ambient temperatures below 30 °C and relative humidity below 60 % unless the manufacturer’s packaging label specifies otherwise. Avoid combination with amine-based additives, certain flame retardants, or metal deactivators unless oxidative stability is re-evaluated by oxidative induction time under ISO 11357-6:2018. Such combinations may deplete the phenolic antioxidant package or alter processing colour.
Post-consumer recyclate addition changes the molecular weight distribution and contaminant profile of the melt. Melt flow rate under ISO 1133-1:2022 should be measured on the blend rather than assumed from the virgin product. Tear and dart impact properties under ISO 6383-2 and ISO 7765-1 may decline nonlinearly as recyclate content increases, particularly if the recyclate contains degraded high-density polyethylene or print residues. Process validation should include a production-scale extrusion trial of at least 4 h at the intended recyclate loading to detect pressure drift, plate-out, and screen pack blinding. No universal recyclate loading limit applies to Icorene 1041 YEW 2181 because the additive package and final end-use requirements govern stability and taste/odor transfer. Published data for this specific configuration with post-consumer recyclate are limited.
Application evaluation should follow the intended thickness and end-use test protocol. For flexible packaging films, tensile strength, elongation, and dart impact are measured under ISO 527-2:2012 and ISO 7765-1; sealing performance is evaluated on a laboratory heat sealer with temperature, dwell time, and pressure controlled according to ASTM F2029-16. For rotomoulding or injection-moulded articles, slow crack growth resistance and impact properties are assessed under ISO 22088-1:2006 and ISO 179-1:2010. The specific product must be qualified on the actual mould because wall thickness and cooling rate alter crystallinity, and grade-specific processing windows must be derived from the manufacturer’s certificate of analysis and application trial data.