| HS Code | 760088 |
| Material Type | Polyethylene, Linear Low Density (LLDPE) |
| Density | 0.941 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 3.5 g/10 min |
| Melting Point | 125 °C |
| Vicat Softening Temperature | 110 °C |
| Tensile Strength At Yield | 14 MPa |
| Tensile Strength At Break | 20 MPa |
| Elongation At Break | 600% |
| Flexural Modulus | 600 MPa |
| Hardness Shore D | 60 |
| Tear Strength | 400 g |
| Dart Drop Impact | 300 g |
As an accredited LyondellBasell Icorene 1041 YEW 2176 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packed in 25 kg polyethylene bags, 55 bags per pallet, totaling 1,375 kg net weight, stretch-wrapped. |
| Container Loading (20′ FCL) | 20′ FCL loaded with LyondellBasell Icorene 1041 YEW 2176 Linear Low Density Polyethylene, palletized bags secured for ocean transport. |
| Shipping | LyondellBasell Icorene 1041 YEW 2176 Polyethylene, Linear Low Density, ships as non-hazardous LLDPE pellets in 25 kg bags, octabins, or bulk containers. Transport in cool, dry, ventilated conditions away from ignition, direct sunlight, and moisture. Keep containers closed and avoid prolonged high temperatures. No special DOT/ADR classification; normal industrial hygiene applies. |
| Storage | Store LyondellBasell Icorene 1041 YEW 2176 Polyethylene, Linear Low Density in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and strong oxidizers. Keep containers tightly closed to prevent moisture and contamination. Avoid dust generation and static discharge; use grounding. Maintain clean, dry floors to prevent slipping. Store at ambient temperature, preferably below 50°C, and follow first-in, first-out inventory practices. |
| Shelf Life | Typically two years from manufacture when stored unopened in a cool, dry, ventilated area, away from direct sunlight and heat. |
Icorene 1041 YEW 2176, a linear low density polyethylene powder with a nominal melt flow rate of 4.0 g/10 min per ISO 1133-1:2022 and a nominal density of 0.938 g/cm³ per ISO 1183-1:2019, is rotational molded for above-ground industrial tanks and containment equipment. Rotational molding operations processing the powder are typically configured around a biaxial arm speed ratio of 4:1 and primary-axis speeds between 6 rpm and 12 rpm for cylindrical tanks up to 5,000 L. Peak internal air temperature is deliberately held at 190 °C to 210 °C because the yellow-compounded LLDPE begins to emit visible decomposition volatiles above 215 °C, which creates pinhole channels along the inner melt surface. The powder is charged at a shot weight derived from the target nominal wall thickness multiplied by the mold surface area, with a 2 wt% to 3 wt% allowance for parting-line flash and vent losses. Mold surfaces are coated with a semi-permanent polysiloxane release agent at a dry film thickness below 8 µm to avoid transfer into the melt film. The cooling cycle is staged: forced-air cooling until internal air temperature reaches 80 °C to 90 °C, followed by ambient cooling to 40 °C before demolding; water quenching of walls thicker than 6 mm is avoided because differential shrinkage produces sink marks behind molded inserts. Wall thickness distribution is measured with an ultrasonic gauge at a minimum of 12 grid points per tank and checked against a minimum shell of 3.2 mm for a 1,000 L industrial water tank. When cold powder is transferred into a molding hall above 60% relative humidity, pre-drying at 70 °C for 2 hours reduces condensation-driven pinhole defects. Finished articles include above-ground agricultural water storage tanks, diesel containment bunds, and chemical dosing vessels in which high-visibility yellow asset marking is required. Applicable compliance references include ASTM D1998-15 for upright polyethylene storage tank dimensions and REACH substance registration; diesel contact requires a site-specific permeation validation because LLDPE without a barrier layer is not rated for long-term gasoline containment.
When 70 wt% Icorene 1041 YEW 2176 is dry-blended with 30 wt% high-pressure LDPE at a melt index of 0.8 g/10 min and density of 0.924 g/cm³, bubble stability on a 30D single-screw extruder remains acceptable only if the yellow pigment dispersion is not re-agglomerated by low hopper-mixing shear. The dry blend is metered into a low-work barrier screw with a die gap of 1.8 mm and processed at a die exit melt temperature of 210 °C to 220 °C. Die-land pressure is held between 16 MPa and 22 MPa; excursions above 24 MPa coincide with pigment agglomerates larger than 20 µm and produce visible fisheye defects. Blow-up ratio is fixed at 2.2:1, and frost line height is maintained between 3.5 and 4.0 die diameters to limit gauge variation to ±5% across a 1,600 mm web. At these settings, a 150 µm film shows a dart impact failure weight above 250 g per ASTM D1709 Method A and a machine-direction Elmendorf tear above 40 N per ASTM D1922. The finished article is typically a 6 m to 8 m wide silage clamp cover or grain overwrap used for anaerobic conservation; the yellow grade is specified for batch identification and worker visibility rather than UV-stability performance. Compliance for the agricultural film is evaluated under EN 13206, and direct food contact is not claimed under 21 CFR 177.1520 for the finished yellow article unless the pigment package is separately confirmed. Long-term outdoor weatherability requires a hindered amine light stabilizer package above 0.3 wt%; the pigment alone does not prevent surface cracking after a single season of direct solar exposure.
For tinted agricultural crates and field bins, gravimetric blending of 25 wt% Icorene 1041 YEW 2176 with 75 wt% natural LLDPE powder produces a lower-chroma yellow warning color without commissioning a separate pigment masterbatch. The powder mixture is tumbled in a low-shear conical screw blender for 15 minutes to 20 minutes; blending above 30 minutes can segregate fines and alter bulk density enough to reduce shot-to-shot consistency. The blend is then processed on an injection molding machine with a general-purpose screw of L/D 20:1, a melt temperature of 200 °C to 230 °C, and a mold temperature of 15 °C to 40 °C. Injection pressure is set between 60 MPa and 120 MPa, with holding pressure at 50% to 70% of the peak value for 6 seconds to 10 seconds depending on gate freeze time. Mold shrinkage is recorded between 1.5% and 2.2% after 48 hours at 23 °C. Color strength is checked with a spectrophotometer under CIE Lab conditions; a batch-to-batch ΔE below 0.8 is considered acceptable for non-decorative industrial components. The resulting articles are lightweight stackable field bins, farrowing boards, and livestock feed troughs with a wall thickness from 3 mm to 6 mm. Compliance is confined to industrial use; no food-contact migration testing is claimed because the yellow pigment package and possible processing aids have not been validated under EU 10/2011. Heavy-metal content in the tinted article should be checked per Directive 2011/65/EU Annex II, with lead, cadmium, hexavalent chromium, and mercury each below 100 ppm in homogeneous material.
To maintain adhesion on woven HDPE tarpaulins, Icorene 1041 YEW 2176 is extrusion-coated through a single-screw extruder with an L/D of 30:1 and a slot die set to a 0.6 mm to 0.8 mm die gap. Melt temperature at the die exit is raised to 230 °C to 245 °C to reduce viscosity and compensate for the 4.0 g/10 min melt index, which is lower than conventional extrusion coating grades. The air gap is maintained between 120 mm and 160 mm; an air gap above 180 mm increases draw resonance and creates neck-in above 12% of the die width. A fluoropolymer processing aid at 0.5 wt% is incorporated to prevent die lip drool, but it does not replace the need for oxidized melt-surface formation at the substrate interface. The coated fabric is pressed onto a chill roll at 15 °C to 20 °C with a nip pressure of 0.3 MPa to 0.5 MPa. Adhesion of the 20 g/m² to 30 g/m² coating to the woven tape is evaluated by a 180° peel test at a crosshead speed of 300 mm/min; values below 4 N/25 mm indicate insufficient oxidation or contamination from warp sizing. Web tension on the laminating line is limited to 15 N/m to 25 N/m to avoid stretching the woven tape. End products include yellow scaffolding tarpaulins, bulk bag side curtains, and temporary fencing banners requiring high-visibility color and limited water resistance. Heavy-metal compliance follows Directive 2011/65/EU Annex II; flame performance for temporary structures is assessed under the relevant local structural code rather than a single global standard.
For secondary containment liners and floating covers, Icorene 1041 YEW 2176 is sheet-extruded through a flat die at 220 °C to 240 °C and calendered to a thickness of 0.75 mm to 1.5 mm. The sheet is then cut into panels and joined by hot-wedge fusion welding at a wedge temperature of 350 °C to 450 °C, a drive speed of 0.8 m/min to 2.0 m/min, and an applied seam pressure of 0.2 MPa to 0.4 MPa. Peel and shear tests are performed according to ASTM D6392-12 on seam samples taken at intervals of every 200 m of weld; peel strength must exceed 95% of the sheet yield strength for acceptable fusion. Surface oxidation on the yellow compound is detectable as a dull haze and can reduce weld peel strength by more than 15% if the sheet is stored outdoors for more than 21 days before welding. When ambient temperature falls below 5 °C, wedge speed must be reduced because the exposed sheet surface cools too quickly to form a homogeneous melt bead. End products include lagoon floating covers, anaerobic digester covers, and secondary containment liners where yellow identification improves site safety and leak detection. Compliance for geomembrane installations is governed by site-specific project specifications and frequently references GRI GM13; published data for this specific pigmented LLDPE formulation under GRI GM13 is limited, so welding trials are required before full deployment.
Thermoforming-grade monolayer sheet from Icorene 1041 YEW 2176 is run on a 120 mm single-screw extruder with a barrier screw and a flat die width of 1,800 mm. Melt temperature at the die exit is limited to 205 °C to 215 °C; higher temperatures cause the sheet to sag before entering a three-roll polishing stack. The roll stack gaps are set to produce 1.2 mm to 4.0 mm sheet, with the middle roll temperature held at 75 °C to 85 °C to control gloss and reduce shrinkage after reheating. Reheat thermoforming uses a radiant heater setpoint of 350 °C and a sheet surface temperature of 120 °C to 135 °C before forming; below 115 °C the sheet splits at plug-assist corners and above 140 °C the yellow pigment may produce uneven draw ratios. If the sheet is stored outside shrink-wrap, it is dried at 60 °C for 30 minutes before forming to reduce steam blistering. The formed parts are trimmed on matched steel rule dies with a cutting clearance of 0.1 mm to 0.2 mm per side. End products include agricultural seedling trays, material handling trays, and machinery drip pans where chemical resistance and impact toughness at -20 °C are required. Compliance for industrial use is limited to REACH substance registration and the heavy-metal limits of Directive 2011/65/EU Annex II; no food-contact migration testing is claimed for these trays.
In low-pressure micro-irrigation conduit extrusion, the material is fed through a smooth-bore single-screw extruder with an L/D of 30:1, a mixing head temperature of 190 °C, and a die head temperature of 200 °C. The tube is calibrated in a vacuum tank at 40 kPa to 60 kPa vacuum and cooled in a water bath held at 18 °C to 22 °C. Line speed is adjusted to maintain a wall thickness of 0.8 mm to 1.5 mm for 12 mm to 25 mm outside diameter. During startup, the first 10 meters of tube can show die marks if the melt temperature is below 185 °C; this section is discarded before online ultrasonic wall monitoring. A 60 mesh stainless steel screen pack prevents die build-up from pigment agglomerates. End products include yellow marker conduit for buried irrigation lines, low-pressure drip system feeder tubes, and protective sleeving for hydraulic hoses. Dimensional compliance is verified with ISO 3126; pressure-rated service is not claimed without a hydrostatic design basis accepted by the end user. Potable water contact would require additional testing under NSF/ANSI 61, which is not automatically assigned to the yellow pigmented grade.
Competitive LyondellBasell Icorene 1041 YEW 2176 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 1041 YEW 2176 is a linear low density polyethylene powder intended for rotational moulding of medium-sized to large hollow articles, including closed tanks, agricultural hoppers, outdoor furniture, portable sanitation components, and technical enclosures. The product designation combines a base resin code, Icorene 1041, with a stabiliser suffix, YEW 2176; the suffix identifies a pre-compounded ultraviolet and thermal stabiliser system rather than a dry-blended colourant or post-moulding coating. Representative values from published LyondellBasell commercial literature for this grade include a nominal density of 0.940 g/cm³ when tested under ASTM D1505 or ISO 1183-1:2019 and a melt flow index of 4.0 g/10 min at 190 °C under 2.16 kg load under ASTM D1238 or ISO 1133-1:2022. The material is supplied as a microground powder, not as pellets, because the powder particle size distribution must permit dry-flow cavity filling during biaxial tool rotation. A typical top cut of 500 µm (35 mesh U.S. sieve) is controlled under ASTM E11. On production-scale shuttle and carousel machines, the powder requires no routine pre-drying when kept in closed silos below 50 °C; however, moisture condensed on cold powder surfaces during transfer into a warm moulding bay can generate surface voids and pinhole defects.
The stabiliser package in YEW 2176 is dispersed into the polymer matrix before grinding, meaning each powder particle carries the additive load. In dry-blended UV concentrate systems, particle segregation can occur during transport from the feed hopper into the rotating mould, creating zones with uneven stabiliser concentration and variable weathering life. The compounded approach reduces that segregation risk but does not eliminate the need to control powder handling. The stabiliser system may slightly extend the tack phase at mould surface temperatures below 105 °C because of low-molecular-weight additive migration to the particle surface. Rotational moulding processors using shuttle machines with unheated moulds should therefore establish a minimum demoulding temperature based on the part skin, not the mould exterior. Oxidative induction time measured by differential scanning calorimetry under ASTM D3895 or ISO 11357-6:2022 is an appropriate incoming quality-control indicator for stabiliser consistency, although it is not a direct outdoor weathering test. The hindered amine light stabiliser component functions by free-radical scavenging during ultraviolet exposure, while a phenolic antioxidant protects the melt during the long oven residence time typical of rotomoulding.
The heating cycle for an LLDPE rotomoulding grade is best controlled by internal air temperature rather than oven set temperature alone. For Icorene 1041 YEW 2176, a peak internal air temperature between 190 °C and 220 °C is commonly used on single-skin parts; thick-walled parts above 12 mm may require a longer plateau at the upper end of that range. During the initial heating stage, the powder begins to sinter when the air temperature reaches the melting onset of the LLDPE, which for a density of 0.940 g/cm³ is around 105 °C to 115 °C depending on short-chain branching distribution. Powder particles adhere at contact points, then coalesce into a porous bed. Bubble removal is governed by melt viscosity and the internal pressure difference across each bubble; residual nitrogen from the mould cavity can diffuse into the polymer and create voids if the part is held too long at low temperature. The peak internal air temperature must therefore be high enough to reduce melt viscosity but low enough to prevent oxidative chain scission. A plateau at 190 °C to 220 °C is usually maintained for 1 min to 3 min for wall thicknesses up to 10 mm; thicker sections may require longer plateaus. Major-axis to minor-axis rotation speed ratios in the range of 4:1 to 8:1 are typical, but deep corners or narrow necks may force a ratio outside that range. Tooling with cast aluminium contact surfaces should be conditioned with a semi-permanent release agent at a film thickness below 10 µm; solvent-based release agents may leave skin residues that reduce stress crack resistance. Cast aluminium moulds have higher thermal conductivity than stainless steel, so they heat and cool faster. For thin-walled parts, cast aluminium is preferred where cycle time is critical; sheet steel tools produce longer heating rates and may require a lower oven set point to avoid skin overheating.
Cooling rate controls the crystalline structure and therefore the mechanical properties of rotomoulded parts. Forced air cooling after demoulding increases the skin crystallisation rate and can produce a hard outer layer over a softer core with lower density. If the part is ejected before the inner surface cools below 80 °C, warpage in flat panels and top decks can become permanent. Water mist cooling shortens cycle time but may raise the brittleness temperature of the skin because of rapid nucleation. The material’s low-temperature ductility, evaluated by ASTM D746 or ISO 974:2000, is retained only if the cooling profile avoids severe quench gradients greater than 15 °C/min. For thick-walled tanks, published data for this specific configuration is limited; controlled trials with thermocouple arrays are therefore required to link cooling rate to part warpage and impact retention. Wall-thickness uniformity is controlled less by the resin melt index than by rotation ratio, tool symmetry, oven airflow, and the thermal mass of the mould. Production-scale failure modes observed on carousel machines include wall-thickness thinning at the top of closed tanks, powder bridging in narrow sections, and inner-surface oxidation when the oven temperature is increased to compensate for short cycle times. Bridge formation occurs when the powder no longer flows across the rotating tool surface because the internal air temperature is too high and the outer layer fuses prematurely. Reducing oven set point or increasing major-axis speed can restore powder tumbling.
ESCR testing by ASTM D1693-21 in 10% Igepal CO-630 at 50 °C reports failure time under constant strain; values above 1000 h are typical for the base grade. The result is highly sensitive to surface defects, frozen-in strain, and the chemical nature of the release agent. Silicone-bearing release agents can mask surface cracks during testing and are not recommended for fuel or detergent containers because they can migrate into the product and alter surface sealing. In rotomoulded agricultural tanks, stress cracking failures usually initiate at the inside corner where the wall is thinnest and residual stress is highest. Environmental stress crack resistance in rotomoulded LLDPE is controlled by molar mass, short-chain branch distribution, crystal tie-chain density, and processing-induced residual stress. The slow crack growth mechanism proceeds from surface defects or internal voids when a stress-cracking fluid lowers the surface energy of the plastic. Igepal CO-630 is a nonylphenoxy poly(ethyleneoxy) ethanol used in ASTM D1693; the 10% solution at 50 °C is an aggressive but reproducible stress-crack agent. A result above 1000 h does not classify the part as universally compatible with all chemicals; it specifically indicates resistance to that test fluid. A mould release system that allows easy part removal without excessive build-up is therefore part of the ESCR control strategy, not a cosmetic choice.
Representative published values for the base Icorene 1041 grade include a tensile strength at yield of 14.0 MPa under ASTM D638 or ISO 527-2:2012, an elongation at break above 800%, and a flexural modulus near 650 MPa under ASTM D790 or ISO 178:2019. The Vicat softening point reported for the base resin is approximately 112 °C under ASTM D1525 or ISO 306:2022 method A50. These values are obtained on compression-moulded or injection-moulded test specimens and should not be read as guaranteed rotomoulded part properties. The rotomoulding process generates fewer molecular orientations than injection moulding but produces a broader range of wall-thickness uniformity, so tensile and impact results can vary with wall thickness, cooling rate, and tooling condition. For specification work, melt flow index is not the only flow parameter. The low-frequency complex viscosity measured by parallel-plate rheometry in a nitrogen atmosphere is more informative for sintering time than melt index alone. Published data for the melt flow ratio at 21.6 kg versus 2.16 kg for this specific subgrade is limited outside the manufacturer’s technical documents.
Compared with highly branched low density polyethylene rotomoulding grades, the linear low density backbone of Icorene 1041 provides higher stiffness and improved environmental stress crack resistance, but the melt is more sensitive to slow bubble removal if the peak internal air temperature is too low. Compared with a lower melt index LLDPE, this grade offers easier densification and shorter cycle time on thin-walled parts, while a higher melt index grade would flow faster but sacrifice ESCR and low-temperature impact. The YEW 2176 suffix distinguishes the product from weather-unprotected natural powder and from dry-blend UV masterbatch systems because the stabiliser is present in each powder particle. This is particularly relevant in electrostatic powder handling where additive dust separation can occur with dry blends.
OIT by differential scanning calorimetry under ASTM D3895 or ISO 11357-6:2022 offers a quantitative comparison of the active antioxidant and UV stabiliser content in incoming powder. A decrease in OIT from the supplier’s certificate of analysis can indicate improper storage, excessive exposure to sunlight, or contamination with regrind of unknown history. The test is performed at elevated temperature under oxygen; it does not replicate outdoor weathering but is sensitive to antioxidant depletion. When the powder is stored in ventilated silos below 50 °C and protected from direct UV exposure, the stabiliser package remains active for the supplier-stated shelf life. If a bag is opened and partially consumed, the remaining powder should be resealed because the outer layer of bagged powder can oxidise faster than the bulk. In closed-tool moulding with a small vent, the oxygen concentration inside the cavity is gradually depleted, reducing oxidative stress; in open-arm machines with large vents, continuous oxygen ingress can increase antioxidant consumption at the inner air-polymer interface.
For regulatory compliance, the base LLDPE is typically positioned under U.S. FDA 21 CFR 177.1520, but the finished rotomoulded article is not automatically compliant because end-use migration testing depends on wall thickness, contact duration, and food simulant. European food-contact applications must be assessed under Regulation (EU) No 10/2011 with specific migration limits relevant to the finished article. REACH compliance is supply-chain-specific and requires SVHC content confirmation from the supplier. RoHS 2011/65/EU is not normally applicable to unpigmented polyethylene substrates, but pigmented dry blends may require separate evidence. Finished potable water tanks must comply with ANSI/NSF 61 or the applicable national drinking-water regulation; base resin FDA status is not sufficient for the fabricated article.
Icorene 1041 YEW 2176 is intended for non-pressure hollow articles and is not designed for continuous exposure to strong oxidising acids, aromatic hydrocarbons, or chlorinated solvents. Stress crack resistance data obtained with Igepal CO-630 solutions do not predict performance in these aggressive media. Dry blending with recycled LLDPE or HDPE regrind above 20 wt% can reduce ESCR and low-temperature impact because of high-density domains and particle-size segregation; processors should screen recycled powder through an ASTM E11 35 mesh sieve and verify the final blend melt index before full-scale production. Peak internal air temperature should not exceed 260 °C because surface oxidation accelerates and gas bubbles may remain trapped in the melt. Combination with amine-based external additives not covered by the stabiliser formulation should be avoided unless the additive supplier provides oxidative induction time data demonstrating no antagonism.