| HS Code | 664540 |
| Material Type | Polyethylene, Linear Low Density (LLDPE) |
| Density | 0.921 g/cm³ |
| Melt Index 190 C 2 16 Kg | 1.0 g/10 min |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 20.7 MPa |
| Elongation At Break | 800% |
| Flexural Modulus | 241 MPa |
| Vicat Softening Temperature | 93°C |
| Melting Temperature | 122°C |
| Crystallization Temperature | 105°C |
| Shore D Hardness | 50 |
As an accredited LyondellBasell Icorene 1041 YEW 2168 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 1041 YEW 2168 Polyethylene, Linear Low Density is supplied in 25 kg polyethylene-lined paper bags, palletized and stretch-wrapped. |
| Container Loading (20′ FCL) | 20′ FCL loading for LyondellBasell Icorene 1041 YEW 2168 LLDPE: 25 kg bags, palletized/stretch-wrapped, securely loaded, approx. 20–25 MT. |
| Shipping | LyondellBasell Icorene 1041 YEW 2168 Polyethylene, Linear Low Density is a non-hazardous thermoplastic resin in pellet form. It is shipped in 25 kg bags, jumbo bags, or bulk containers/trucks. Not classified as dangerous goods. Store dry, away from heat, sunlight, and contamination; use standard industrial handling. |
| Storage | Store LyondellBasell Icorene 1041 YEW 2168 LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original containers closed, palletized off the floor, and protected from moisture, dust, UV, and contamination. Avoid excessive stacking; use first-in, first-out. Ground equipment during transfer. Inspect packages regularly for damage or leaks. No smoking. |
| Shelf Life | Store in cool, dry conditions; typical shelf life is 24 months from manufacture when unopened and protected from direct sunlight. |
Rotational moulding of transportable diesel tanks for agricultural, quarry and construction machinery places Icorene 1041 YEW 2168 powder into a processing window where peak internal air temperature rather than oven set point controls the final density profile of the wall. The grade is a butene-copolymer linear low-density polyethylene with a nominal density of 0.938 g/cm³ and a melt flow rate of 4.0 g/10 min at 190 °C/2.16 kg measured to ISO 1133-1:2022. In a carousel-type rotational moulding line with fabricated steel tools, the oven air temperature is held between 280 °C and 300 °C, while the powder tumbling inside the tool reaches a peak internal air temperature of 200 °C to 205 °C. Exceeding 210 °C accelerates thermo-oxidative chain scission in the LLDPE backbone and produces a measurable loss of low-temperature ductility after demoulding. Finished tanks in the 200 L to 1000 L class are moulded with nominal wall thicknesses of 6 mm to 10 mm and dwell times of 18 min to 28 min, with the longer dwell reserved for tools carrying thick fill-neck bosses and internal baffle inserts. The yellow pigmentation carried in the YEW 2168 designation is a supplied resin colour, not a dry-blend additive; this removes a dispersion variable during mould charging but does not contribute to hydrocarbon barrier performance. Fuel containment compliance follows ECE R34 for plastic fuel tanks on motor vehicles and, for non-road equipment sold into the United States, the evaporation and permeation limits of US EPA 40 CFR Part 1060. Environmental stress crack resistance is the controlling qualification parameter because low-sulfur diesel and biodiesel blends exert surfactant-like diffusion into amorphous tie-chain regions. Icorene 1041 YEW 2168 is tested to ASTM D1693-15e1, Condition B, 10% Igepal CO-630, with an F50 value above 1000 h; this supports use in tanks exposed to sloshing and cyclic lateral loads. Process failures observed on production lines include gas-bubble pitting on the inner surface when ambient humidity is high and cold powder is charged directly from outdoor silos; to avoid condensation, the powder is held at least 15 °C above the dew point before transfer into the tool. Demoulding temperatures above 80 °C increase the probability of warpage at the fill neck and at flat sidewalls, so forced-air cooling followed by water mist at 0.5 °C/min to 1.5 °C/min is used until the steel tool surface falls below 70 °C. The terminal product is a yellow rotationally moulded diesel tank with moulded-in threaded inserts, lifting lugs, and a wall-thickness tolerance of ±10% across the sidewall, qualified for off-road machinery rather than for sustained highway vehicle crash loading unless the specific vehicle-level certification has been completed.
The five downstream segments that follow impose different qualification matrices on the same base resin because the failure modes are not identical. Table 1 extracts the controlling test methods and acceptance corridors used in production qualification.
| Application segment | Controlling standard | Method or clause | Production acceptance corridor |
|---|---|---|---|
| Diesel fuel tanks | ASTM D1693-15e1 | Condition B, 10% Igepal CO-630 | F50 above 1000 h |
| Agricultural sprayer tanks | EN 907:1997 / ISO 16119-2:2013 | Chemical immersion at 23 °C and 40 °C | No visible attack; no post-test impact loss above 15% |
| Marine buoy shells | ISO 4892-2:2013 / ISO 6603-2:2023 | Xenon-arc 3500 h; puncture at -20 °C | No surface cracks; ductile failure mode |
| Rainwater tanks | AS/NZS 4766:2021 | Hydrostatic test at 1.1 rated capacity | No leakage |
| Insulated fish boxes | EU Regulation 10/2011 / FDA 21 CFR 177.1520 | Overall migration and food simulant contact | Below 10 mg/dm² |
| Material handling bins | ISO 8611-1:2021 / ISO 2248:1985 | Rated load and drop impact | No permanent deformation at 1.25 rated load |
Mounted and trailed agricultural sprayer tanks in the 600 L to 3000 L class are rotationally moulded from Icorene 1041 YEW 2168 because the end-use environment combines hydrostatic loading, ultraviolet exposure, and continuous contact with dilute pesticide and surfactant formulations. The product sidewall is specified at 8 mm to 12 mm at the lower chime and 6 mm to 8 mm on the upper cylinder, with the transition zone thickened to avoid stress concentration at the baffle weld line. Formulation for this segment is intentionally simple: 100 wt% of the supplied yellow powder, with no additional filler or impact modifier, because inert fillers raise low-temperature brittleness and reduce the melt-flow homogeneity required for consistent corner formation. If ultraviolet stabilisation beyond the resin package is required for prolonged tropical exposure, a hindered amine light stabiliser masterbatch is dry-blended at 0.3 wt% to 0.6 wt%, and the blend is tumbled for 15 min to 20 min in a low-shear ribbon mixer before charging. Process conditions on a shuttle-type rotational moulding machine set the oven air temperature to 290 °C to 310 °C, with a peak internal air temperature of 195 °C to 210 °C. The secondary-to-primary rotation ratio is 4:1 for vertical cylindrical tools, and the tool is rotated through a full 360° primary axis to prevent pooling at the sump. Cooling is performed in two stages: forced ambient air to 0.5 °C/min until the tool reaches 90 °C, followed by water mist to 1.0 °C/min to 1.5 °C/min until demoulding at 65 °C. Compliance for chemical resistance is established by immersion testing of machined tensile bars in the actual tank-mix formulation at 23 °C and 40 °C for 28 days, with acceptance requiring no visible surface attack and no loss of elongational break below 15% of the as-moulded value. EN 907:1997 and ISO 16119-2:2013 provide the mechanical and safety frame for the finished sprayer, while the resin-level stress crack resistance is monitored by ASTM D1693-15e1 using 10% Igepal CO-630. The terminal product is a yellow tank with a baffled interior, rotationally moulded sump, threaded inserts for boom mounts and sight gauges, and a wall-thickness distribution that remains above 80% of the nominal sidewall at the corner radii.
A 25-L marine buoy shell moulded from Icorene 1041 YEW 2168 is a spherical or elliptical hollow body in which the minimum wall thickness is set not by hydrostatic pressure but by puncture and abrasion during dock contact. The powder charge for a 25-L spherical tool is calculated to produce a wall thickness of 4 mm to 6 mm; the tool is rotated at a 7.5:1 secondary-to-primary ratio to prevent equatorial thickening and pole thinning. Oven air temperature is held at 285 °C to 305 °C, with a peak internal air temperature of 195 °C to 205 °C. The primary failure mode in marine service is not thermal oxidation but low-temperature embrittlement after ultraviolet exposure; tests are therefore run to ISO 4892-2:2013 for 3500 h of xenon-arc weathering, followed by ISO 6603-2:2023 puncture testing at -20 °C. The acceptance criterion is a ductile failure with radial cracking rather than shattering; a brittle response requires reformulation with an additional UV absorber or a reduction in peak internal air temperature to avoid over-cure. Formulation for buoy shells uses 100 wt% Icorene 1041 YEW 2168, with a stabiliser package already supplied in the resin; if a separate UV masterbatch is added, it is limited to 0.5 wt% to avoid lowering the melt-flow index below the level needed for complete mould filling at the poles. After demoulding at 60 °C to 65 °C, the shell is filled with closed-cell polyurethane foam at a density of 40 kg/m³ to 60 kg/m³ to provide reserve buoyancy and to dampen impact energy. The terminal product is a yellow foam-filled buoy with moulded-in rope eyes and a wall thickness tolerance of ±0.8 mm, suitable for marked navigation buoys, fender shells, and floating dock separation elements. Published data for this specific Icorene grade in sub-zero seawater immersion is limited; qualification is therefore conducted on representative moulded dome sections rather than by extrapolation from neat resin data.
The process windows for the six described conversion routes are not interchangeable because tool geometry and required final wall thickness shift the PIAT tolerance. Table 2 consolidates representative machine settings observed on shuttle, carousel, and rock-and-roll lines.
| Segment | Oven air temperature | Peak internal air temperature | Rotation ratio | Demoulding temperature |
|---|---|---|---|---|
| Diesel fuel tanks | 280 °C to 300 °C | 200 °C to 205 °C | 4:1 | Below 70 °C |
| Agricultural sprayer tanks | 290 °C to 310 °C | 195 °C to 210 °C | 4:1 | 65 °C |
| Marine buoy shells | 285 °C to 305 °C | 195 °C to 205 °C | 7.5:1 | 60 °C to 65 °C |
| Rainwater tanks | 280 °C to 300 °C | 200 °C to 210 °C | 4:1 | Below 60 °C |
| Insulated fish box shells | 290 °C to 315 °C | 200 °C to 210 °C | 4:1 | 60 °C |
| Material handling bins | 290 °C to 320 °C | 200 °C to 215 °C | 4:1 | Below 80 °C |
Rainwater harvesting tanks and process-water buffer vessels rotomoulded from Icorene 1041 YEW 2168 are produced as vertical cylinders with capacities between 1000 L and 5000 L and wall thicknesses from 6 mm at the upper shell to 10 mm at the bottom chime. The yellow pigmentation is acceptable for non-potable rainwater and process water service; for potable water contact, the specific YEW 2168 pigment must be verified against the positive-list requirements of EU Regulation 10/2011 and the food-contact polymer provisions of FDA 21 CFR 177.1520, and where that verification is not available, a natural over-mould layer or an alternative approved grade is specified. The resin is processed as supplied without regrind in the first-quality wall layer; closed-loop regrind from the same yellow powder may be incorporated at up to 20 wt% in the outer shell layer only, because a regrind-rich inner layer can carry oxidised gel particles that initiate pinhole leaks under cyclic roof loading. The rotational moulding cycle uses an oven air temperature of 280 °C to 300 °C, a peak internal air temperature of 200 °C to 210 °C, and a rotation ratio of 4:1 for cylindrical tools. Cooling is deliberately slow at 0.3 °C/min to 0.8 °C/min through the recrystallisation range to control shrinkage of the large flat base; demoulding is performed only when the tool surface temperature is below 60 °C. Compliance follows AS/NZS 4766:2021 for polyethylene storage tanks, with hydrostatic testing at 1.1 times the rated capacity and a post-test inspection for leakage or visible distortion. The terminal product is a yellow above-ground tank with moulded-in inlet and outlet bosses, a removable lid, and a sidewall that retains at least 75% of the nominal wall thickness at the bottom knuckle radius.
The double-wall insulated fish box converts the same LLDPE powder into two rotationally moulded shells that are joined and filled with rigid polyurethane foam. Each shell is moulded at 4 mm to 5 mm wall thickness, with the inner shell carrying a smooth food-contact surface and the outer shell providing abrasion resistance and stacking strength. The moulding process uses oven air temperatures of 290 °C to 315 °C and a peak internal air temperature of 200 °C to 210 °C; the higher oven set point is permitted because the thinner wall section shortens the dwell time to 12 min to 16 min and reduces the total thermal history. The outer shell is demoulded at 60 °C and transferred to the foaming station, where a two-component rigid polyurethane foam with a free-rise density of 40 kg/m³ to 60 kg/m³ is injected into the cavity at 0.2 MPa to 0.5 MPa; injection pressure above 0.5 MPa can deform the outer shell if the shell surface temperature remains above 65 °C. The thermal conductivity of the foam core is specified at 0.022 W/(m·K) to 0.026 W/(m·K), which is the controlling variable for ice-retention performance in the 300 L to 1000 L box class. Food-contact compliance for the inner shell is tested under EU Regulation 10/2011 overall migration limits of 10 mg/dm² and under FDA 21 CFR 177.1520 for olefin polymers in contact with aqueous and fatty food simulants; the YEW 2168 yellow pigment must be confirmed as a permitted colorant under the applicable national food-contact legislation for the intended market. The terminal product is a yellow insulated box with moulded-in hinge blocks, drain plug thread, and stacking lugs, used for fish landing, meat transport, and chilled pharmaceutical logistics. A known processing limitation is the dimensional growth of the outer shell after demoulding; post-mould shrinkage continues for 24 h to 48 h, so the foam injection step is delayed until the outer shell has stabilised at ambient temperature.
Warehouse and logistics bins moulded from Icorene 1041 YEW 2168 are produced as thick-wall open-top containers with fork pockets and base runners, requiring a different balance between melt-flow, impact resistance, and long-term creep than thin-wall tanks. Nominal sidewall thickness is 8 mm to 14 mm, with the base thickened to 15 mm to 20 mm at the fork-entry pads. The resin is processed without dilution, and regrind from trimmed holes and rejected parts is limited to 15 wt% of the total charge to preserve the low-temperature ductility required for cold-store use; when regrind exceeds this fraction, ISO 6603-2 puncture energy at -20 °C falls below the production acceptance floor established for the specific bin design. The moulding cycle on a rock-and-roll machine uses oven air temperatures of 290 °C to 320 °C, a peak internal air temperature of 200 °C to 215 °C, and a rotation ratio of 4:1 for rectangular tools. The higher peak internal air temperature is tolerated because the thick base section must sinter fully without leaving powder-rich cores at the fork-pocket corners. Cooling is performed with forced air at 0.4 °C/min until the tool reaches 80 °C, followed by water mist at 1.0 °C/min to 1.5 °C/min; demoulding above 80 °C is avoided because residual heat softens the base runners and leads to localised creep under the first stacking load. Rated-load testing follows ISO 8611-1:2021 for pallet-like bases, with no permanent deformation at 1.25 times the rated load, and drop impact testing follows ISO 2248:1985 at 0 °C to -20 °C. The terminal product is a yellow moulded bin with integral forklift pockets, drainage holes, and stacking ribs, used in fruit and vegetable field logistics, seafood processing, and refrigerated warehouse order picking.
Competitive LyondellBasell Icorene 1041 YEW 2168 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 1041 YEW 2168 is classified as a linear low density polyethylene (LLDPE) rotational moulding grade supplied as a free-flowing powder. The material designation combines the base resin Icorene 1041 with the package code YEW 2168, which identifies the compounded stabilizer and colour configuration. The base resin is specified for outdoor structural parts requiring resistance to environmental stress cracking, sub-zero impact, and ultraviolet weathering. Because the product is delivered as a powder rather than pellets, it can be charged directly into rotational moulding equipment without an additional grinding step. Typical base-resin lot values used for preliminary material selection include a density of 0.925 g/cm³ determined according to ISO 1183-1:2019 and a melt flow rate of 1.0 g/10 min under ISO 1133-1:2022 at 190 °C and 2.16 kg. The final YEW 2168 compound may show measurable shifts in density, melt flow, and tensile response after colourant and stabilizer incorporation; the supplier’s certificate of analysis supersedes generic datasheet values for lot acceptance.
Application selection for this class of UV-stabilised LLDPE includes chemical storage tanks, agricultural spraying equipment, traffic-control panels, outdoor equipment enclosures, and leisure-vehicle bodies. The short-chain branching distribution of the LLDPE backbone increases tie-chain concentration relative to low density polyethylene at equivalent density, improving slow crack growth resistance under repeated hydrostatic or mechanical loading. Published data for the exact Icorene 1041 YEW 2168 compound are limited; replacement of an incumbent rotational moulding grade should therefore be validated by moulded-part testing rather than by powder property comparison alone.
The primary distinction is molecular architecture. High-pressure LDPE contains long-chain branches that increase melt elasticity but limit ultimate tensile and environmental stress-cracking resistance at equal density. LLDPE grades obtained by low-pressure catalyst-mediated ethylene/α-olefin copolymerization have short-chain branches that distribute lamellar thickness and increase tie-molecule connectivity. In practice, LLDPE rotational moulding grades with densities between 0.920 g/cm³ and 0.930 g/cm³ typically show tensile yield stresses from 10 MPa to 14 MPa under ISO 527-2:2012, while LDPE grades of comparable density often fall between 8 MPa and 11 MPa.
Compared with HDPE rotational moulding powders in the 0.940–0.955 g/cm³ density range, Icorene 1041 YEW 2168 sacrifices flexural stiffness and surface hardness to obtain a wider impact and cracking resistance envelope. HDPE rotational moulding grades commonly exceed 800 MPa flexural modulus under ISO 178:2019, whereas LLDPE grades of this class generally fall between 300 MPa and 500 MPa. The lower crystallinity suppresses yield strength but retards environmental stress cracking in detergent, polyol, and agricultural chemical environments; ASTM D1693-21 ESCR values above 1000 h are typical for such LLDPE structures in 100% Igepal CO-630.
Within the LLDPE range, comonomer type determines low-temperature performance. Butene-based copolymers generally exhibit lower impact strength at -40 °C than hexene- or octene-based equivalents at the same melt flow rate and density. Because the specific comonomer of Icorene 1041 YEW 2168 should be confirmed from the manufacturer’s technical literature, users comparing grades should fix density, melt flow rate, and impact test protocol before material substitution. Under ISO 6603-2:2023 instrumented puncture, candidate materials should be moulded in identical tools because wall thickness and cooling-induced crystallinity directly affect the ductile-to-brittle transition.
On production-scale carousel or shuttle machines with 1.0–2.0 m³ steel tools, powder dry-flow, bulk density, and particle-size distribution govern wall-thickness uniformity in narrow ribs and bridge sections. Powder fractions below 150 µm improve surface detail but can reduce bulk density and increase dusting, while fractions above 600 µm can produce voids in thin webs. A dry-flow time lower than 25 s/100 g using the ASTM D1895 test cup is generally preferred for automated charging; however, the exact value for the Icorene 1041 YEW 2168 lot should be measured because antistatic and colour concentrates modify flow behaviour.
During heating, the powder sinters, coalesces, and densifies. For this LLDPE class, peak internal air temperature is typically controlled at 190–210 °C. Oven set-point temperatures of 280–300 °C are used for steel tools with wall thicknesses of 6–10 mm, but cast aluminium tools heat more rapidly and may require lower set points to prevent over-heating. Oven residence times for 6 mm walls generally range from 12–20 min under forced convection. Insufficient peak internal air temperature yields pinholes and poor impact; excessive peak internal air temperature consumes the stabilizer package and can shift colour in the YEW 2168 configuration.
The 1.0 g/10 min melt flow rate reflects a relatively high viscosity that limits flow into ribs thinner than 3 mm but prevents sagging of thick sections during long powder-bed rotation. Dynamic oscillatory data for comparable LLDPE rotational moulding bases at 190 °C typically show complex viscosity at 0.1 rad/s between 2.0×10³ Pa·s and 4.0×10³ Pa·s. The broad molecular weight distribution produces shear-thinning that compensates partially for the low flow index, but narrow cavities and mould seams require sufficient internal air temperature and tool rotation speed to develop full wall density.
The following properties are representative for a UV-stabilised LLDPE rotational moulding compound in this density class. They should not be used as minimum lot acceptance values; mechanical data depend on moulded wall thickness, cooling rate, and mould contact surfaces.
| Property | Value | Method |
|---|---|---|
| Density | 0.925 g/cm³ | ISO 1183-1:2019 |
| Melt flow rate | 1.0 g/10 min | ISO 1133-1:2022, 190 °C/2.16 kg |
| Tensile stress at yield | 12 MPa | ISO 527-2:2012 Type 1B, 50 mm/min |
| Elongation at break | >800% | ISO 527-2:2012 |
| Flexural modulus | 400 MPa | ISO 178:2019 |
| Vicat softening temperature | 95 °C | ISO 306:2022 Method A50 |
| Brittleness temperature | < -60 °C | ASTM D746-20 |
| Environmental stress-cracking resistance | >1000 h | ASTM D1693-21, 100% Igepal CO-630, Condition A |
Published data for the exact YEW 2168 stabilizer and colour configuration are limited; therefore, the table above should be treated as a material-class reference rather than a product-specific guarantee. When comparing with another Icorene grade, the lot-specific melt flow and powder particle-size data must be used because the additive package can shift fusion time and part density.
Non-isothermal crystallization by differential scanning calorimetry at 10 K/min shows onset crystallization near 105–110 °C for this density class, with peak crystallization around 95 °C. Slow cooling in thick sections shifts the exotherm to higher temperatures, increasing lamellar thickness and reducing toughness. Fast water-spray quenching depresses crystallinity and raises impact but can freeze in surface stresses. These trade-offs are typical of LLDPE rotational moulding and require the processor to validate wall-thickness-specific properties.
Oven residence time is also limited by oxidative induction time. Thermogravimetric analysis under nitrogen and air at 200 °C shows that unstabilized LLDPE loses 5% mass at 360–380 °C, while the stabilizer package decomposes or volatilizes gradually before the polymer backbone. Isothermal oxidative induction time at 210 °C by ISO 11357-6:2018 for UV-stabilized LLDPE rotational grades often exceeds 60 min before weathering but falls below 5 min after 3000 h of accelerated xenon-arc exposure. This depletion pattern indicates that the primary antioxidant package is consumed by surface radical generation before visible embrittlement appears.
Olefin polymer food-contact clearances such as FDA 21 CFR 177.1520 apply primarily to the base polyolefin; the final compounded product may also be subject to migration limits for stabilizers, pigments, and processing aids. Compliance with Commission Regulation (EU) No 10/2011 should be verified for the complete Icorene 1041 YEW 2168 formulation. Under REACH (EC) No 1907/2006, the supplier’s safety data sheet lists the registration status and any substances of very high concern. For electrical and electronic equipment applications, RoHS Directive 2011/65/EU thresholds for cadmium, lead, mercury, and hexavalent chromium apply; the YEW 2168 colour package should be screened when the moulded part falls within the directive’s scope.
Outdoor qualification of the YEW 2168 package normally combines accelerated weathering with mechanical property retention. Xenon-arc exposure under ISO 4892-2:2013 cycle 1 or fluorescent UV exposure under ISO 4892-3:2016 is followed by tensile testing per ISO 527-2. Retention of at least 75% of initial elongation after 3000 h is a common internal benchmark for UV-stabilised LLDPE rotational moulding compounds, though published values for this specific product are limited. Oxidative induction time measurement by ISO 11357-6:2018 is used to monitor remaining stabilizer after weathering; a large decrease in oxidative induction time indicates depletion of the radical-scavenging package before visible embrittlement appears.
Lot-to-lot variation in colour and stabilizer concentrates can shift fusion time by 2–5 min at a constant oven set point. Because the YEW 2168 designation may include a colour package, processors should not transfer moulding parameters from natural Icorene 1041 without verifying minimum wall thickness and drop-impact response. The material should be stored in closed containers below 50 °C and dried if moisture content exceeds 0.05% by weight; wet powder produces steam bubbles and porosity in thick walls.
Chemical compatibility for tanks is evaluated by immersion in representative media at 23 °C and 60 °C for periods of 30–90 days. For diesel, detergent, and sodium hypochlorite solutions, environmental stress-crack resistance measured by ASTM D1693 or the bent-strip method in ISO 22088-1:2006 provides a relative ranking. The lower crystallinity of LLDPE is generally advantageous in alkaline solutions but can be softened by aromatic hydrocarbons; the specific fluid compatibility of the YEW 2168 grade must be confirmed before service.
Bonding and welding of Icorene 1041 YEW 2168 parts require removal of mould-release residues and oxidative surface treatment. For adhesive joints, surface energy after flame treatment or plasma treatment should exceed 40 mN/m; otherwise polyurethane and epoxy adhesives may fail cohesively at the interface. Rotational moulded LLDPE surfaces are inherently low-energy, generally below 32 mN/m as moulded. For mechanical fasteners, bosses should be designed with generous radii, and metallic inserts should be isolated from cyclic thermal stresses because the coefficient of linear thermal expansion is typically 1.5×10⁻⁴ K⁻¹.