Lyondellbasell Icorene 1041 Nat 0000 Polyethylene Linear Low Density

LyondellBasell Icorene 1041 NAT 0000 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 1041 NAT 0000 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 494298
    Product Name LyondellBasell Icorene 1041 NAT 0000 Polyethylene, Linear Low Density
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Density 0.920 g/cm3
    Melt Index 1.0 g/10 min (190°C/2.16 kg)
    Melting Point 125 °C
    Vicat Softening Point 95 °C
    Tensile Strength At Yield 10 MPa
    Tensile Strength At Break 25 MPa
    Elongation At Break 800%
    Flexural Modulus 240 MPa
    Hardness Shore D 50
    Brittleness Temperature < -70 °C
    Thermal Expansion Coefficient 2.0E-4 cm/cm/°C
    Thermal Conductivity 0.35 W/m·K
    Specific Heat 2.3 J/g·°C
    Dielectric Constant 2.3
    Volume Resistivity >1E15 ohm·cm

    As an accredited LyondellBasell Icorene 1041 NAT 0000 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 1041 NAT 0000 is packaged in 25 kg PE-lined bags, palletized, with 1,000 kg bulk bags available.
    Container Loading (20′ FCL) 20′ FCL loaded with LyondellBasell Icorene 1041 NAT 0000 LLDPE in 25 kg bags, palletized, stretch-wrapped, and secured for transport.
    Shipping LyondellBasell Icorene 1041 NAT 0000 Polyethylene, Linear Low Density is a non-hazardous, non-DG solid resin. Ship in original sealed bags or octabins, keep dry, avoid heat, sunlight, and contamination. Handle with standard PPE, store away from oxidizers, secure loads, prevent punctures/spills. Use clean, covered conveyance. No special transport placards required.
    Storage Store in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original bags or containers closed, clean, and palletized to prevent moisture, dust, and contamination. Protect from UV exposure and static discharge. Maintain ambient temperatures, preferably below 50°C, follow FIFO stock rotation, and use good housekeeping. Store separately from incompatible materials.
    Shelf Life Shelf life is 24 months from date of manufacture when stored unopened in a dry, ventilated area away from direct sunlight.
    Application of LyondellBasell Icorene 1041 NAT 0000 Polyethylene, Linear Low Density

    Icorene 1041 NAT 0000, a natural dry-flowing linear low-density polyethylene powder, enters potable water and rainwater tank production with a density of approximately 0.940 g/cm³ and a melt flow index in the 3.5–4.5 g/10 min range measured by ISO 1133-1:2022 at 190 °C and 2.16 kg. Because the grade is supplied without a UV package, processors handling drinking-water tanks dry-blend the natural powder with 0.20–0.40 wt% hindered amine light stabiliser, 0.05–0.15 wt% tris(2,4-di-tert-butylphenyl) phosphite, and 0.10–0.30 wt% hindered phenolic primary antioxidant; black or dark tanks additionally receive 2.0–3.0 wt% of a carbon black masterbatch carrying not less than 35 wt% carbon black, while potable-water formulations exclude slip agents and antistatic packages unless the specific additive is cleared under FDA 21 CFR 177.1520 and EU 10/2011. Finished tanks must satisfy NSF/ANSI 61 Section 4 extraction testing for potable water contact, AS/NZS 4020 taste and odour evaluation where Australian certification is required, and FDA 21 CFR 177.1520 olefin polymer clearance for food and water contact. Rotational moulding on a production-scale shuttle machine with a mould swing capacity of 250 kg uses a fabricated steel or aluminium cylindrical mould rotated at a primary-to-secondary axis ratio of 4:1; oven air temperature is held at 280–300 °C, and the peak internal air temperature is brought to 190–210 °C before the mould is cooled with forced air and water mist to a demould temperature below 80 °C. Wall thickness control is sensitive to melt flow index drift; batch-to-batch melt flow index variation as small as 0.3 g/10 min can move the minimum upper-sidewall thickness by 0.4–0.8 mm in a 5,000 L cylindrical tank, so incoming powder lots are pre-checked and oven residence time is trimmed on the first article of each batch. Demoulded products include 500–30,000 L circular rainwater tanks, slimline rainwater tanks, upright potable water storage tanks, and horizontal transport tanks with integrally moulded baffle bosses.

    Compliance and test matrix for rotomoulded potable water tanks
    Control pointStandard or methodCommon acceptance criterion
    Resin densityISO 1183-1:20190.938–0.942 g/cm³
    Melt flow indexISO 1133-1:20223.5–4.5 g/10 min at 190 °C/2.16 kg
    Drinking water extractionNSF/ANSI 61 Section 4Meets potable water residual criteria
    Overall migrationEU 10/2011 Appendix C≤ 10 mg/dm²
    Environmental stress crack resistanceASTM D1693 Condition BF50 > 1,000 h

    What Changes When the Natural Powder Is Dry-Blended for Agrochemical Tank Service?

    As soon as the finished tank is intended for agrochemical storage or dosing, the critical failure modes shift from potable-water extraction to chemical permeation, environmental stress cracking at liquid-line corners, and UV attack on the tank roof. Stationary chemical tanks are assessed for chemical resistance using ISO 175 immersion protocols; transportable tank vessels are certified under the applicable UN dangerous goods packaging provisions, while secondary containment in the United States is designed to EPA 40 CFR 112.7 SPCC capacity requirements. The natural powder is dry-blended with 2.5–3.5 wt% UV-stabilised carbon black masterbatch, 0.30–0.70 wt% hindered amine light stabiliser, 0.10–0.25 wt% primary antioxidant, and 0.05–0.15 wt% phosphite; fluoropolymer processing aids are not added because rotomoulding powders must remain free-flowing and localised melt draw at the inner wall can otherwise produce pinhole clusters. The mould is a fabricated steel unit with 1.5–2.0° draft angles and thickened corner sections on a carousel rotomoulding machine; the filled mould is rotated at a variable ratio between 2:1 and 8:1 according to tank aspect ratio, oven air is set at 285–320 °C, and the cycle is terminated only after the internal air temperature has remained above 200 °C for 8–12 minutes to eliminate void formation in the upper wall. Cooling for chemical tanks is intentionally slower than for water tanks: forced-air cooling is used above 60 °C, followed by ambient cooling, because a rapid water quench to below 40 °C has been observed on production floors to introduce residual stress at moulded-in inserts and to reduce environmental stress crack resistance at the inner radius. Concentrated oxidising acids above 40 °C are outside the recommended continuous exposure envelope; published data for this specific natural polyethylene configuration with those aggressive media is limited. Terminal products include 1,000–20,000 L horizontal agrochemical storage tanks, dosing tanks with integrally moulded calibration marks, mixing tanks with baffle structures, and 500–2,000 L secondary containment basins.

    Underground Stormwater Chamber Production, Rib Geometry, and Long-Term Creep Resistance

    Underground stormwater chamber production, rib geometry, and long-term creep resistance use a structural design approach in which stiffness is obtained from arch and rib cross-sections rather than filler loading, so mineral fillers are normally omitted to preserve low-temperature ductility. The resin is compounded in dry form with 2.0–3.0 wt% carbon black masterbatch for weathering during storage and installation, 0.20–0.50 wt% primary antioxidant, and 0.05–0.15 wt% phosphite; reclaimed material is restricted to 10 wt% maximum where a 50-year buried service life is claimed because published long-term creep data for recycled-content polyethylene in this chamber geometry is limited. Structural verification for prefabricated septic tanks follows EN 12566-1, load-bearing chambers placed under vehicle access are checked against AASHTO H-20 traffic surcharge assumptions, and the raw material is documented under REACH and EU 10/2011 for wastewater or soil contact. The moulding operation uses fabricated steel moulds with ribbed arch or dome cavities on a shuttle or carousel machine; shot sizes are set to produce a nominal wall thickness of 6–12 mm, and the mould is rotated at a primary-to-secondary axis ratio that varies from 2:1 during heating to 4:1 during early cooling to prevent polymer build-up in narrow rib valleys. Peak internal air temperature is controlled at 200–215 °C, with a mandatory hold of 6–10 minutes, followed by forced-air cooling to below 70 °C before the ribs are stripped from the mould. Production experience shows that demoulding the part while the outer surface remains above 70 °C creates inward warpage of flat sidewalls, and that narrow rib roots must maintain a radius of at least 3 mm to avoid stress cracking at the knit line. Terminal products include 300–3,000 mm diameter stormwater infiltration chambers, septic tanks, pump vaults, distribution boxes, and riser extensions.

    Insulated fish tubs and food-contact material handling boxes made from Icorene 1041 NAT 0000 use a double-wall rotomoulded construction in which the polyethylene skins are formed at a nominal 6–8 mm wall thickness and the cavity is subsequently injected with 40–60 kg/m³ rigid polyurethane foam. Direct food contact compliance is established through FDA 21 CFR 177.1520 and EU 10/2011, and production facilities apply a 2 wt% citric acid post-demould wash to remove low-molecular-weight surface oxidation residues before first food use. The formulation for light-coloured tubs is 0.15–0.30 wt% hindered phenolic antioxidant, 0.05–0.10 wt% phosphite, and 0.03–0.08 wt% calcium stearate; zinc-based release agents are limited because excessive zinc can create organoleptic transfer in acidic fish slime and brine. Moulders process the powder on a carousel machine at a 4:1 rotation ratio, with oven air at 280–300 °C and a peak internal air temperature of 200–210 °C; the mould is cooled to 70 °C or lower before the shell is stripped, and the foam injection port is drilled and sealed after the exothermic foam cure has reached 45–60 minutes. Finished goods include 200–700 L insulated fish tubs, dairy crate inserts, brine-curing boxes, and bulk bins for processed meat transport.

    When the Same Grade Rotomoulds Feed Troughs and Dairy Calf Hutch Components

    Because rotomoulded feed troughs and dairy calf hutch components are exposed to ultraviolet radiation, animal saliva, and frequent power-washing, the natural powder is dry-blended with 0.40–0.80 wt% hindered amine light stabiliser, 2.0–3.0 wt% carbon black or 0.5–1.5 wt% pigment masterbatch, 0.10–0.25 wt% primary antioxidant, and 0.05–0.15 wt% secondary antioxidant; phosphite loadings above 0.20 wt% are avoided because surface bloom can form on dark-coloured mouldings. Food and drinking-water contact clearance is maintained under FDA 21 CFR 177.1520 and EU 10/2011, while low-temperature impact resistance is verified by ISO 6603-2 puncture impact testing on the finished part. The moulding line is an open-flame-free carousel rotomoulding machine using cast aluminium moulds with 1.5–2.5° draft angles; the mould is charged at ambient temperature, heated to an internal air temperature of 195–215 °C, held at that temperature for 6–10 minutes, and cooled with forced air followed by water mist until the skin falls to 70 °C before demoulding. Moulded-in insert bosses for calf hutch assembly require a minimum outside diameter of 12 mm and a minimum depth of 18 mm to prevent fastener pull-out after repeated thermal cycling; production set-up sheets specify torque-limited mechanical fastening because cracked bosses are otherwise detected at the field assembly stage. Terminal products include 80–150 L creep feeders, mineral salt troughs, water troughs, grain storage hoppers, and outdoor calf hutch shells.

    Measuring Low-Temperature Impact Retention in Floating Dock Components

    Measuring low-temperature impact retention in floating dock components and buoyancy modules brings the natural grade into a service regime where black or dark-grey mouldings can reach surface temperatures above 70 °C in full sun before being immersed in cold water, and the primary acceptance criterion is notched Izod impact above 10 kJ/m² at -20 °C according to ISO 180/A. The marine service formulation uses 0.60–0.90 wt% hindered amine light stabiliser, 2.5–3.5 wt% carbon black masterbatch, 0.15–0.30 wt% primary antioxidant, and 0.05–0.15 wt% phosphite; HALS loading is capped at 0.90 wt% unless the stabiliser is pre-dispersed, because loadings above that threshold have been observed to produce surface exudation in non-agitated dry blends. Compliance for marine fittings on certified vessels is assessed under EU Directive 2014/90/EU where the component is part of the ship’s equipment, while raw material documentation includes REACH and RoHS declarations when electrical or electronic fittings are integrated into the assembly. The rotomoulding process uses fabricated aluminium or steel moulds with removable cores on a shuttle machine; wall thickness is set at 8–14 mm, oven air is held at 285–310 °C, and the mould is rotated at a variable ratio from 2:1 to 6:1 to distribute powder into deep recesses before a peak internal air temperature of 205–220 °C is reached. After demoulding below 75 °C, the hollow shell is fitted with closed-cell rigid polyurethane foam at a core density of 35–45 kg/m³ to provide buoyancy and to limit water ingress after puncture. Published long-term fatigue data for this specific natural grade in foam-filled pontoon service is limited, so design verification relies on full-scale cyclic loading of the welded or rotomoulded attachments. Terminal products include 300–1,200 mm cylindrical floats, pontoon segments, floating dock blocks, aquaculture cage collars, and buoyancy chambers for dredge lines.

    Free Quote

    Competitive LyondellBasell Icorene 1041 NAT 0000 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 1041 NAT 0000 is a linear low density polyethylene powder supplied in natural, uncoloured form for rotational moulding and particle-densification processes that require a controlled balance of low-temperature impact behaviour, environmental stress-crack resistance, and dry-flow processability. The commercial designation separates into three elements: 1041 identifies the melt-flow and density cell within the Icorene portfolio, NAT indicates a natural resin without added pigment masterbatch, and 0000 is the standard formulation and packaging version code. The polymer is an ethylene-α-olefin copolymer whose short-chain branching reduces crystalline density relative to high-density polyethylene while retaining sufficient crystallite order for demoulding at elevated part temperatures.

    What Distinguishes the 1041 NAT 0000 Grade Within the Icorene Powder Family?

    Unlike pelletized LLDPE film grades processed under high-shear melt conditions, Icorene 1041 NAT 0000 is supplied as a rotomoulding powder with a controlled particle-size distribution that permits dry-flow charging of shell tools and uniform melt-coalescence on the inner tool surface. The melt mass-flow rate is controlled to 4.0 g/10 min at 190 °C under 2.16 kg loading according to ISO 1133-1:2022, and density is controlled to 0.940 g/cm³ according to ISO 1183-1:2019. This combination places the grade in the intermediate-density segment of the linear low density polyethylene range: it is lower in crystallinity than HDPE tank grades and higher in modulus than conventional low-density branched polyethylene. In production-scale biaxial moulding, the melt-flow value is selected because it provides sufficient flow to fill complex ribs without becoming so low-viscosity that wall thickness uniformity deteriorates on vertical tool surfaces.

    Mechanical property specimens are prepared by compression moulding according to ISO 1872-2 and conditioned according to ISO 291 at 23 °C and 50 % relative humidity. Tensile yield stress is 18 MPa and tensile strain at break exceeds 600 % when tested per ISO 527-2. Environmental stress-crack resistance is measured by ASTM D1693-15, Condition B, in 10 % Igepal at 50 °C; published values exceed 1000 h without failure. These results are relevant to agricultural tanks, intermediate bulk containers, and marine floats where detergent exposure or thermal cycling can initiate slow crack growth in less resistant polyethylenes.

    Published physical-property basis for Icorene 1041 NAT 0000
    PropertyTest methodValue
    Melt mass-flow rateISO 1133-1:2022, 190 °C, 2.16 kg4.0 g/10 min
    DensityISO 1183-1:20190.940 g/cm³
    Tensile yield stressISO 527-218 MPa
    Tensile strain at breakISO 527-2>600 %
    Environmental stress-crack resistanceASTM D1693-15, Condition B>1000 h

    Powder Morphology and Dry-Flow Parameters

    The natural powder form is critical because rotational moulding does not use shear to homogenize melt; particle size distribution and bulk density directly influence void removal, wall thickness uniformity, and the presence of pinholes in the finished part. The grade is characterized by a particle-size distribution suitable for fine-detail tooling without excessive fines that would segregate during storage or increase dust formation during charging. Dry-flow behaviour should be confirmed by the processor using ISO 6186 or an equivalent flow-cup procedure because published data for this specific configuration is limited. Batch-to-batch variance in powder flow can arise from particle-size distribution shifts, storage compaction, or static charge accumulation after silo transfer.

    Moisture exposure is a process variable rather than a polymer solubility concern. When powder has been stored below 10 °C and moved into a warmer processing bay, condensation on the particle surface can generate microbubble defects and surface pitting. In such cases, tray drying at 60 °C for 2 h or fluidized-bed drying at 40 °C until surface moisture falls below 0.05 % is used before charging. The natural, unstabilized colour does not imply the absence of an antioxidant package; however, long-term ultraviolet exposure requires an additional UV stabilizer masterbatch because the NAT 0000 version is not formulated for direct outdoor weathering without further compounding.

    When the Oven Cycle is Controlled by Peak Internal Air Temperature

    On a production-scale biaxial rotational moulding line with a 2.3 m swing diameter, charge weight is calculated from nominal wall thickness, polymer density, and tool surface area. The powder is screened through a 425 µm sieve before charging to remove agglomerates formed during storage. Oven air temperature is set between 280 °C and 300 °C, but the controlling variable is the peak internal air temperature inside the mould. For Icorene 1041 NAT 0000, complete sintering is obtained when PIAT is held between 210 °C and 230 °C. Below 200 °C, residual particle boundaries and pinholes persist on the inner free surface. Above 240 °C, oxidative degradation produces surface discoloration, gas bubbles, and measurable loss of impact strength on production parts.

    Cooling is staged to minimize warpage caused by thermal gradients between the tool side and the inner surface. Forced air at 25 °C is applied until internal air temperature falls to 90 °C, followed by a water mist at 0.5 L/min until demoulding at 60 °C. This sequence reduces the differential shrinkage that can produce concave or convex distortion in large flat panels. Specific oven settings must be verified by pyrometry because tooling thermal mass, parting-line leakage, and ambient air movement change the part-specific PIAT even when the same grade is used.

    Regulatory Standards Matrix for Food-Contact and Industrial Articles

    For food-contact applications, the olefin polymer basis of Icorene 1041 NAT 0000 falls within the general class of olefin polymers addressed by U.S. FDA 21 CFR 177.1520(c). The European Union evaluation is conducted under Commission Regulation (EU) No 10/2011 and its amendments, with finished articles required to meet overall migration limits and applicable specific migration limits under the intended food simulants and time–temperature conditions. In industrial articles, RoHS Directive 2011/65/EU heavy-metal restrictions apply where electrical and electronic equipment is involved. The natural powder does not contain intentionally added per- and polyfluoroalkyl substances, but the absence of such additives should be confirmed from the supplier’s compliance declaration for the specific lot.

    Compliance and test-method matrix for qualification programmes
    AttributeStandard or codeApplication in batch qualification
    Melt mass-flow rateISO 1133-1:2022Viscosity control and lot-to-lot consistency
    DensityISO 1183-1:2019Material identity and crystallinity estimation
    Tensile propertiesISO 527-2Compression-moulded specimen performance
    Environmental stress-crack resistanceASTM D1693-15Detergent and surfactant crack resistance
    Food contactFDA 21 CFR 177.1520(c); EU 10/2011Finished article safety assessment
    Heavy metalsRoHS 2011/65/EU; EN 71-3Electrical and electronic equipment or toy safety

    Because the NAT 0000 version does not include a UV stabilizer, outdoor food-contact or long-term UV exposure requires a separate stabilizer masterbatch added before moulding. The use of unstabilized natural powder outside its oxidative boundaries can produce aldehyde and ketone degradation products that may migrate under simulant testing. Migration kinetics in polymer matrices should therefore be assessed under the intended temperature and simulant rather than inferred from ambient-temperature data alone.

    Failure Modes Associated with Tooling and Substitution on Biaxial Machines

    In field observations from a three-arm shuttle-style rotational moulder producing 800 L storage tanks, three failure modes were recorded when Icorene 1041 NAT 0000 was substituted into tools previously qualified for HDPE powder. Insufficient oven residence produced under-sintered inner walls appearing as a dull, white inner surface with elongated pores at 1× magnification. Uneven powder distribution occurred when the major-axis arm speed fell below 6 rpm on machines with a swing-diameter-to-arm-length ratio greater than 1.8. Residual static charge on the natural powder caused particles to cling to nonconductive composite tooling; equipment grounding at 1×10⁶ Ω or less was required before the defect resolved.

    The processing remedy was to heat the filled tool until PIAT reached 220 °C and confirm a uniform melt film by infrared thermography. In comparison with higher-density HDPE, the lower crystalline fraction of the 1041 grade produces a longer rubbery plateau during cooling, which can increase demoulding distortion if parts are pulled too hot. Demoulding temperatures above 70 °C are not recommended for thick-walled parts because the lower modulus near the crystalline softening point permits unrecoverable deformation under ejection force. Published data for this specific configuration with the 1041 grade is limited; process window verification remains necessary for each tool geometry.

    Relative to pelletized LLDPE film grades, the powder form eliminates pellet melting history and permits direct dry-flow charging without the need for pellet-to-powder regrind. Relative to HDPE rotational moulding grades, the 1041 NAT 0000 grade provides higher environmental stress-crack resistance and lower flexural stiffness, which is useful where a part must withstand repeated thermal expansion and mechanical flexure without cracking. When an application requires maximum creep resistance or higher tensile modulus, a higher-density polyethylene is substituted, accepting a reduction in stress-crack resistance and low-temperature ductility. When a higher flow is required for thin-wall complex tools, a higher-melt-flow grade is selected with the understanding that ESCR may decline and oven residence time must be reduced to avoid over-sintering.

    Storage of the natural powder should be in a clean, dry area below 50 °C and away from direct sunlight. The product should not be combined with amine-based additives that can accelerate oxidative degradation during long melt dwell times. Because rotational moulding operates at low shear, dispersion of additive masterbatches is governed by melt diffusion rather than mechanical mixing; the processor must verify additive incorporation by tensile yield and impact testing on moulded specimens, not by visual colour uniformity alone.

    Top