| HS Code | 825327 |
| Density | 0.920 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 1.0 g/10 min |
| Tensile Strength At Yield | 10.0 MPa |
| Tensile Strength At Break | 25.0 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 200 MPa |
| Dart Drop Impact | 100 g |
| Elmendorf Tear Strength Md | 200 g |
| Elmendorf Tear Strength Td | 300 g |
| Haze | 12% |
| Gloss 45 | 80% |
| Vicat Softening Temperature | 100°C |
| Melting Temperature | 122°C |
| Coefficient Of Friction | 0.2 |
As an accredited LyondellBasell Icorene 1041 BUE 5513 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Icorene 1041 BUE 5513 LLDPE is supplied in 25 kg polyethylene bags, 55 bags per 1,375 kg pallet, or bulk. |
| Container Loading (20′ FCL) | 20′ FCL loading: LyondellBasell Icorene 1041 BUE 5513 Linear Low Density Polyethylene, 25 kg bags, palletized, shrink-wrapped, secured for ocean transport. |
| Shipping | LyondellBasell Icorene 1041 BUE 5513 Polyethylene, Linear Low Density is a non-hazardous thermoplastic resin. It is typically shipped in sealed bags, octabins, or bulk trucks/railcars. Keep containers closed, dry, and away from ignition, excessive heat, and sunlight. Store in a cool, dry, well-ventilated area. No special transport placarding required. |
| Storage | Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and flames. Keep original packaging tightly sealed, palletized, and off the floor to prevent moisture, dust, and contamination. Avoid excessive stacking and temperatures above 50°C. Maintain good housekeeping, use first-in, first-out rotation, and consult the SDS for shelf life. |
| Shelf Life | Shelf life is typically 12 months from production date when stored cool, dry, and in original unopened packaging. |
LyondellBasell Icorene 1041 BUE 5513 is a black UV-stabilized butene-1 linear low-density polyethylene powder designed for rotational moulding. The grade carries a nominal density of 0.938 g/cm³ measured according to ISO 1183-1:2019 and a melt flow rate of 4.0 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022. Tensile and flexural property data are typically generated under ISO 527-2:2012 and ISO 178:2019, respectively, after rotomoulding benchmark plaques. As a powder, it is not intended for injection moulding or blown film; the particle-size distribution and stabilizer package are tuned for dry-flow, low-shear coalescence, and ultraviolet resistance in outdoor rotomoulded parts. Powder storage must avoid condensation: if sacks are transferred from a warehouse below 15 °C to a moulding floor above 30 °C and 60 % relative humidity, surface moisture on the granules produces pinholing during first-layer coalescence; a 60–70 °C hot-air sweep of the opened charge is applied for 1 h before loading. The following application scenarios are limited to real downstream categories with industrial precedent for this grade class. Where laboratory tests are cited, they are intended as qualification protocols, not as a direct prediction of service life in aggressive chemical or marine environments.
| Application category | Nominal wall thickness | Peak internal air temperature | Oven set point | Initial forced-air cooling rate |
|---|---|---|---|---|
| Agricultural water reservoirs | 4–10 mm | 195–210 °C | 270–290 °C | 8–12 °C/min |
| Chemical storage and secondary containment | 6–12 mm | 200–210 °C | 280–300 °C | 5–8 °C/min |
| Heavy-duty industrial bins | 5–8 mm | 195–205 °C | 270–290 °C | 15–20 °C/min |
| Marine floats and fenders | 5–10 mm | 190–200 °C | 260–285 °C | 10–12 °C/min |
| Playground and street furniture | 4–8 mm | 200–210 °C | 275–290 °C | 12–15 °C/min |
| Electrical enclosures and process covers | 4–10 mm | 195–210 °C | 270–290 °C | 5–7 °C/min |
Table values are starting points, not universal recipes; rotational ratio, tool mass, shot weight, and ambient air movement require adjustment.
In carousel and shuttle rotational moulding operations, agricultural water reservoirs produced from this powder are processed with cast aluminium or fabricated mild-steel tools. The black BUE 5513 formulation provides the ultraviolet resistance required for exposed outdoor tank walls, while the butene-1 comonomer content maintains impact strength at the sub-zero temperatures encountered in high-altitude and continental irrigation districts. For compliance, above-ground static tanks for aqueous service are qualified under EN 13575:2012 and, where North American specification applies, ASTM D1998-21; installations that can be connected to potable networks require additional evaluation under NSF/ANSI 61 or AS/NZS 4020 because carbon black formulations must meet national purity criteria before potable-water contact is permitted. The powder is used at 100 % as supplied for black single-layer tanks. Post-industrial trim from the same grade may be dry-blended up to 15 wt% when the regrind is sieved through a 500 µm screen and dried to a surface moisture content below 0.05 wt%; higher regrind loadings reduce the slow crack growth resistance measured under ASTM D1693-15 and are not recommended for long-term hydrostatic service. Production uses a biaxial rotation ratio of 4:1 to 5:1, together with sealed tooling and an internal air temperature target of 195–210 °C; the oven set point is maintained at 270–290 °C. Demoulding below 60 °C prevents distortion of threaded bungs and side-wall stiffeners. Typical end products are 2,000–15,000 L vertical cylindrical storage tanks, rectangular irrigation reservoirs, fertigation day tanks, and transportable water carts for horticultural nurseries.
Chemical containment shells produced from this grade are specified for secondary spill control and dosing-tank service because butene-1 LLDPE retains environmental stress-cracking resistance beyond high-pressure LDPE under intermittent polar-agent exposure. Qualification for stationary tanks in European chemical service follows EN 13575:2012, with the Annex B chemical resistance declaration for each stored substance; in the United States, polyethylene upright tanks are designed and tested under ASTM D1998-21, and environmental stress-cracking resistance is assessed by ASTM D1693-15 condition B at 50 °C with 100 % Igepal CO-630. Secondary containment installations fall under EPA 40 CFR 112.7 where the aggregate storage volume exceeds the reportable quantity. Formulation for chemical service remains at 100 % virgin powder. Recycled material is limited to 0–5 wt% and only after full ESCR validation because reprocessing shortens the tie-molecule population at the crystalline interface, which governs slow crack growth in rotomoulded LLDPE. The downstream rotor cycle uses machined aluminium tools with corner radii of at least 25 mm and wall thickness of 6–12 mm; peak internal air temperature is held at 200–210 °C for 10–15 min after the thermocouple signal stabilizes, reducing pinholing at the peel-off region of the mould parting line. Slow cooling between 5–8 °C/min improves dimensional stability of large sidewalls but must not fall below 3 °C/min where thicker bosses create differential crystallinity. Operational boundaries exclude continuous contact with aromatic solvents, chlorinated hydrocarbons, and oxidizing acids above 10 % concentration at temperatures above 40 °C; swelling and loss of ESCR have been observed in production-scale tanks used for sodium hypochlorite dosing where internal weld-line porosity introduced crack initiation sites. End products are 500–20,000 L vertical storage tanks, double-wall secondary containment sumps, acid/alkali dosing cabinets, and pump containment bunds.
Under steam-clean duty cycles, industrial bins and pallet boxes moulded from this powder are used where cleaning with steam or dilute caustic detergents occurs between batch cycles, and where the material must withstand fork impacts at warehouse temperatures. The governing performance specifications for palletized containers are ISO 8611-1:2021 for flat pallet test methods and ISO 445:2013 for pallet terminology; end-product dimensions in the 600 × 800 mm to 1200 × 1000 mm envelope are validated for racking load capacity with a 1.5:1 safety factor. Dry-blend formulation uses 20–30 wt% post-industrial regrind from the same black grade only when the regrind is passed through a 600 µm sieve and processed below 0.05 wt% surface moisture. Higher regrind above 30 wt% reduces notched impact under ISO 179-1:2010 at -20 °C and causes melt-flow inhomogeneity at steel corner inserts; this is a practical processing boundary observed in production-scale shuttle machines. The rotor process for bins uses a peak internal air temperature of 195–205 °C, lower than that used for large tanks, because thinner 5–8 mm walls reach full densification sooner. After the internal air temperature peaks, forced-air cooling at 15–20 °C/min is applied until the mould skin reaches 90 °C, followed by water-mist cooling at 8–12 °C/min; demoulding above 55 °C on flat sidewalls causes warp and permanent set. End products include distribution totes, tilt trucks, livestock feed troughs, wash-down trays, and 800 × 600 × 650 mm Euro-pallet containers.
For mooring buoys and dock floats, the shell is required to retain impact-toughness after prolonged water absorption, cyclic flexure from wave action, and continuous ultraviolet exposure. The relevant weathering protocol for the black UV-stabilized formulation is ISO 4892-2:2013 cycle 1 with a 0.35 W/m² irradiance at 340 nm, black-panel temperature 65 ± 3 °C, and water spray; outside of accelerated ageing, published full-scale marine weathering data for this specific grade is limited, so product approval should include salt-spray preconditioning under ASTM D1141-98(2021) for 1000 h followed by Charpy impact testing under ISO 179-1:2010. The powder is not formulated for permanent antifouling performance; marine growth must be controlled by mechanical cleaning or external coatings after verifying adhesive compatibility. Formulation for the outer shell remains at 100 % as-supplied black powder. Regrind is limited to 10 wt% maximum and only for non-load-bearing buoyancy blocks because repeated thermal history reduces low-temperature impact at the -30 °C service limit observed in northern waters. Production is carried out on rock-and-roll machines with an arm speed ratio of 5:1 and a peak internal air temperature of 190–200 °C; shell cooling to 40 °C is required before injection of a 45–60 kg/m³ closed-cell polyurethane foam core. The mould seam on cylindrical floats must be positioned away from the rope-attachment eye to avoid weld-line stress concentration. End products include 150–800 mm diameter mooring buoys, dock floats, cable floats, and fender shells.
Playground decking panels and street-furniture shells moulded in this material operate under a combination of cyclic mechanical loading, impact at sub-zero ambient temperatures, and ultraviolet irradiance. The material is applied as a 100 % as-supplied black powder for shells, panels, and structural hides; no pigmented masterbatch is used because the carbon black loading already governs the colour and attempts to lighten the surface require loadings that degrade impact under ISO 179-1:2010. Compliance for children’s equipment follows EN 1176-1:2017 for common play structures, while accessible plastic surfaces are tested for heavy-metal migration under EN 71-3:2019; installers additionally verify that migration data for the black formulation meet the national REACH Annex XVII entry 50 restrictions where applicable. The rotomoulding process uses fabricated aluminium tools with multi-part cores for hollow crawl-tunnel sections; peak internal air temperature is controlled at 200–210 °C, and the oven residence time is extended until the internal air temperature remains stable for 8–12 min, ensuring full densification at rib intersections. Cooling is performed in forced-air stations at 12–15 °C/min until the part reaches 70 °C, then restrained in a fixture to control shrinkage on flat seating surfaces. Operational limits include surface temperatures under direct solar load, which can exceed 70 °C on black parts in hot climates; ventilation holes or perforated panels are introduced to reduce third-degree contact risk. End products include slide hoods, tunnel sections, seating shells, litter bins, bollards, and modular climbing panels.
Because polyethylene is an electrical insulator, rotational moulding of industrial enclosures in this grade is restricted to non-live electrical compartments where the UL 94 classification of the selected black formulation is accepted by the end-use electrical standard. Typical enclosures are qualified for ingress protection under IEC 60529:1989+A2:2013, commonly IP65 or IP66, depending on the moulded gasket seat geometry and insert adhesion. Mechanical properties are specified under ISO 178:2019 for flexural modulus and ISO 527-2:2012 for tensile yield; flame propagation tests under UL 94 generally yield a horizontal-burn classification for unfilled polyethylene, and live electrical components must be separated by a UL-recognised insulating barrier rather than relying on the moulded wall. The powder is processed at 100 % as supplied for enclosure shells; antistatic additive masterbatches may be dry-blended up to 3 wt% only when static dissipative performance is specified and after verifying that the selected additive does not reduce ISO 4892-2:2013 weathering retention. Shuttle or carousel rotomoulding machines with preheated metal inserts at 120 °C are used to mould threaded brass or stainless-steel inserts into bosses; peak internal air temperature is maintained at 195–210 °C, with a slow cooling step from 120 °C to 80 °C at 5–7 °C/min to reduce flatness deviation on gasket flanges. End products include water-meter boxes, valve protection housings, telecommunication node covers, chemical dosing pump enclosures, and process-control cabinet lids.
Competitive LyondellBasell Icorene 1041 BUE 5513 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 1041 BUE 5513 is a linear low-density polyethylene grade identified by the 1041 base resin designation and the BUE 5513 ultraviolet-stabilised black formulation code. The polymer backbone is an ethylene/α-olefin copolymer with short-chain branching introduced during low-pressure polymerisation. This configuration produces lower crystallinity than high-density polyethylene and higher tensile strength than high-pressure low-density polyethylene at comparable density. The producer’s certificate of analysis is the controlling specification document for lot acceptance. Characterisation of this material class is normally performed under ISO 1183-1:2019 for density and ISO 1133-1:2022 for melt mass-flow rate at 190 °C/2.16 kg. Class-typical rotational moulding grades of this architecture may occupy a density band of 0.930–0.940 g/cm³ and an MFR band of 3.5–4.5 g/10 min, but these figures are class-typical control windows and must not be substituted for lot-specific certification. Published data for this specific configuration is limited to the producer’s revision-dated datasheet and batch certificate, and no service-life or mechanical limit should be transposed from adjacent Icorene series grades without verification.
Where the grade is processed by rotational moulding, the powder is charged into steel or cast aluminium tools and biaxially rotated through forced-air ovens. Production-scale carousel and shuttle machines commonly operate at oven set temperatures from 280 °C to 310 °C and peak internal air temperatures from 200 °C to 240 °C. Actual cure-cycle requirements depend on wall thickness, powder bulk density fill ratio, tool mass, and plant humidity. A fill ratio of 0.85–0.95 by volume is typical for uniform wall formation, while ribbed sections, inserts, and undercuts can force adjustments to charge mass and rotation ratio. Because thermal lag between oven indication and mould centre can exceed 30 °C on heavy steel tools, centre-axis internal air temperature is monitored rather than oven temperature alone. Failure to compensate for this lag produces cold spots, incomplete particle coalescence, and visible weld lines at thin-section intersections.
The BUE 5513 suffix indicates an ultraviolet-stabilised formulation intended for exterior service, but designation alone does not establish a service-life class. Accelerated weathering is evaluated under ISO 4892-2:2013 or ASTM G154-23, and correlation with field data is required before a warranty period is defined. During outdoor exposure, polyethylene photo-oxidation proceeds through chain scission and carbonyl formation; the black pigment and stabiliser system present in such formulations retard that mechanism but do not eliminate surface chalking or eventual mechanical property decay. The grade should not be specified for continuous hot-water oxidative loading unless hydrostatic stress testing under ISO 9080:2012 and oxidative stability testing under ISO 11357-6:2018 confirm the service condition. For potable-water contact, certification under BS 6920 or equivalent national requirements is separate from ordinary polyethylene food-contact statements.
During the sintering stage, adjacent powder particles densify by surface-tension-driven coalescence and gas diffusion. The lower zero-shear viscosity of linear low-density polyethylene, compared with an equivalent-melt-flow high-density resin, promotes bubble coalescence and gas escape, but it also increases sensitivity to pinhole formation when peak internal air temperature is reached before uniform coating of the tool surface. The cure phase is normally terminated when centre-axis internal air temperature reaches the predetermined value; extending the cycle beyond that point by 5–8 °C increases oxidative degradation and can reduce elongation at break under ISO 527-2:2012 even when no visible discolouration occurs.
Rotational moulding shops using carousel machines with independent arm speed control adjust biaxial speed ratios between 4:1 and 6:1 to manage thickness distribution. A speed ratio that is too low leaves heavy heel sections at the bottom of the mould, while a ratio that is too high can starve polar regions and produce thin sidewall areas. On multicavity tools with differing cross-sections, the same arm ratio may not be applicable across all cavities; converter trials are required to balance fill ratio, oven residence time, and cooling rate. Cooling is equally consequential: rapid water-mist cooling reduces cycle time but freezes in residual thermal stress, whereas slow air cooling improves flatness but increases total cycle duration.
Porosity in linear low-density polyethylene rotomoulded parts is often the result of moisture, particle size distribution, or premature skin formation. Powder with higher fines content can entrain air between grains, and if surface densification occurs before gas diffusion is complete, the resulting voids remain in the finished wall. Moisture contents above 0.05 wt% may generate steam porosity; therefore stored powder should be protected from condensation at relative humidity above 60%. The use of dry-air silos, moisture analysers, and sieve analysis under ISO 4610:2001 or equivalent powder-flow measurement is common on lines producing technical parts.
Compared with high-pressure LDPE, Icorene 1041 BUE 5513 contains fewer long-chain branches. The absence of a substantial long-chain branching fraction lowers melt tension and strain-hardening response. In extrusion processes this can reduce bubble or parison stability, but in rotational moulding the more Newtonian flow character can improve detail reproduction in narrow ribs and sharp corners. The corresponding trade-off is vertical-wall sag on large flat panels and greater thickness variation if rotation parameters are not tuned. High-pressure LDPE, by contrast, exhibits stronger strain hardening and better sag resistance at similar melt index, but generally lower tensile strength and lower low-temperature impact resistance.
Against high-density polyethylene, the linear low-density architecture of Icorene 1041 BUE 5513 lowers crystallinity and flexural modulus while improving impact toughness and resistance to slow crack growth. The difference is significant in outdoor structural parts subjected to sub-zero impact; brittle fracture in HDPE may be replaced by large-deformation yielding in LLDPE. However, the lower modulus requires thicker wall sections for equivalent stiffness, and creep behaviour must be checked under the intended load. For cyclic loading, design data should be generated under ISO 899-1:2023 and compared against the required deformation limit.
Compared with metallocene-catalysed LLDPE, a conventional Ziegler-Natta linear low-density polyethylene of this type typically has a broader molecular weight distribution and a broader short-chain branching distribution. That broadening improves processability and tolerates wider mould temperature ranges, but it reduces clarity and dart impact in film applications. For black ultraviolet-stabilised rotomoulded parts, optical properties are less relevant, and the broader process window can reduce cycle-time variability across multicavity production tools. The narrower composition distribution of metallocene grades can produce higher impact and better consistency, but often at higher melt elasticity and greater sensitivity to processing temperature deviations.
Food-contact status is not automatic for the formulated black grade. The base resin may be covered by FDA 21 CFR 177.1520 and EU Regulation 10/2011 as amended, but the carbon black and ultraviolet additive package requires end-use migration testing under the relevant specific migration limits. Articles for electrical and electronic equipment must be checked against RoHS 2011/65/EU restricted substance concentrations. Under REACH EC 1907/2006, the polymer itself is exempt from registration, but the monomer and additive substances must be registered by their respective suppliers for the stated tonnage band.
| Purpose | Standard or regulation | Operational boundary |
|---|---|---|
| Density | ISO 1183-1:2019 | Lot acceptance against producer specification; affects crystallinity and stiffness |
| Melt mass-flow rate | ISO 1133-1:2022 | Mould filling and coalescence control |
| Tensile properties | ISO 527-2:2012 | Yield stress and elongation at break after processing |
| Flexural properties | ISO 178:2019 | Structural stiffness comparison |
| Impact strength | ISO 179-1:2023; ISO 180:2023 | Low-temperature service evaluation |
| Accelerated weathering | ISO 4892-2:2013 | UV exposure ranking, not a direct service-life claim |
| Oxidative stability | ISO 11357-6:2018 | Thermal-oxidative resistance characterisation |
| Food contact | FDA 21 CFR 177.1520; EU 10/2011 | Requires end-use migration testing for the formulated grade |
The material should not be blended with strongly acidic or oxidising processing aids, and extended residence time above 260 °C should be avoided because chain degradation accelerates sharply and can generate odorous volatiles. In rotational moulding, direct flame impingement on the powder must be prevented before the mould enters the oven, and nitrogen purging of the feed hopper is used in humid plants. The physical form and packaging code must be verified against the bill of lading because suffix variations in the Icorene range can indicate different additive packages or logistics forms. Rotomoulders using thin-walled tools with high surface-to-volume ratios frequently observe greater sensitivity to oven-temperature overshoot, requiring segmented heating profiles and real-time internal air temperature feedback rather than fixed timer control.