| HS Code | 415328 |
| Density | 1.08 g/cm³ |
| Melt Flow Rate | 0.50 g/10 min |
| Tensile Strength At Yield | 16.5 MPa |
| Tensile Elongation At Break | 300% |
| Flexural Modulus | 690 MPa |
| Hardness Shore D | 55 |
| Vicat Softening Temperature | 108 °C |
| Brittleness Temperature | -40 °C |
| Volume Resistivity | 1E15 ohm·cm |
| Dielectric Constant | 2.6 |
| Dissipation Factor | 0.001 |
| Limiting Oxygen Index | 28% |
| Ul 94 Flammability Rating | V-0 |
| Water Absorption | 0.01% |
| Melt Temperature | 200 °C |
As an accredited LyondellBasell HDPE FR439800X01 W&C factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell HDPE FR439800X01 W&C comes in 25 kg polyethylene-lined paper bags, 40 bags per pallet (1,000 kg total). |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): LyondellBasell HDPE FR439800X01 W&C resin is palletized, shrink-wrapped, and securely loaded in a 20-foot FCL. |
| Shipping | LyondellBasell HDPE FR439800X01 W&C ships as non-hazardous solid polyethylene pellets in 25 kg bags, octabins, or bulk trucks/railcars. It is not DOT/IMDG/IATA regulated. Keep containers sealed; store dry, covered, away from ignition and UV. Avoid moisture contamination and follow SDS/local rules. |
| Storage | Store LyondellBasell HDPE FR439800X01 W&C indoors in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, ignition sources, and strong oxidizers. Keep original containers or bags closed, clean, and palletized, off the ground, to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and extreme temperatures. Follow the supplier’s SDS and local regulations for safe handling and storage. |
| Shelf Life | Shelf life: typically 2 years from production date in original sealed packaging stored cool, dry, away from direct sunlight. |
In outside plant fibre optic cable jacketing, HDPE FR439800X01 W&C is processed as a high-viscosity outer sheath compound on single-screw extruders with 24:1 to 30:1 L/D barrier screws and Maddock shear-mixing sections. Barrel set points typically run from 180 °C at the feed throat to 230 °C at the die, while melt temperature is held between 215 °C and 235 °C to balance high melt strength against thermal degradation. The formulation is adjusted with a 50% carbon black masterbatch at 5.0–6.0 wt% to achieve 2.5–3.0 wt% carbon black, plus 0.10–0.25 wt% hindered phenolic antioxidant and 0.02–0.08 wt% perfluoropolymer processing aid to suppress melt fracture at line speeds exceeding 600 m/min. Compliance data are generated against IEC 60794-1-2:2021 for cable mechanical performance, ASTM D1248-20 for polyethylene wire-and-cable classification, UL 1581 for jacket thickness and cold bend, and Telcordia GR-20-CORE for outside plant fibre cable qualification. Terminal cable constructions include 12–288-fibre central tube and stranded loose tube designs with jacket wall thickness from 0.8 mm to 2.0 mm for direct burial, duct, and lashing aerial deployment.
Production-scale jacketing lines show that melt temperatures above 240 °C increase die-lip residue formation and reduce elongation at break below 350% when measured by ASTM D638-14 due to oxidative chain scission; barrel residence time is therefore maintained below 8 min at full output. Lot acceptance also records melt mass-flow rate at 190 °C/2.16 kg per ISO 1133-1:2022; incoming lots outside 0.4–0.8 g/10 min are segregated because lower values increase screw torque above 400 bar on 30:1 machines, while higher values reduce environmental stress-crack resistance below 500 h in 100% Igepal CO-630 per ASTM D1693. Pellet pre-drying at 80 °C for 4 h is imposed when ambient relative humidity exceeds 60%, because surface moisture on pellets causes splay and pinholes in thin 0.8 mm jackets. The same grade is not combined with amine-based flame retardant packages because Lewis-base additives degrade hindered phenolic antioxidant systems and shorten oxidative induction time at 210 °C below the 20 min target used in incoming lot qualification.
Air-blown fibre microduct bundles based on HDPE FR439800X01 W&C are manufactured by vacuum-calibrated tube extrusion rather than pressure-tooling, with individual microduct outer diameters held to 7.0 ± 0.1 mm and wall thickness to 1.0–1.2 mm. The compounding window for a black outer microduct uses 2.0–4.0 wt% colour or UV masterbatch and 0.05–0.15 wt% erucamide slip additive to generate the low-friction inner surface required for air-blown fibre installation. Melt temperatures at the die are maintained between 205 °C and 220 °C; higher melt temperatures promote post-crystallisation shrinkage above 0.8% after 24 h at 100 °C per IEC 60794-1-2:2021 sample conditioning. The finished microduct is tested to ASTM D3350-14 for PE cell classification and EN 60794-5 for optical fibre microduct systems. Terminal product types include 7/3.5 mm and 12/8 mm single and bundled FTTx microducts, plus 10 mm backbone microducts for fibre-blowing distances beyond 1 km.
Field failures at push-fit coupling points are associated with axial jacket shrinkage that pulls tube ends out of watertight connectors; extruded bundles therefore pass through a two-stage cooling trough with water temperatures set at 40 °C then 20 °C, followed by an in-line annealing section at 80–90 °C for 60 s. The production bottleneck observed on 45 mm single-screw lines is not output but dimensional drift when vacuum calibration pressure fluctuates above 0.02 MPa, causing ovality that exceeds 0.05 mm and reduces blowing distance by increasing pneumatic friction. Process control therefore ties vacuum pressure, haul-off speed, and melt gear-pump speed into a closed-loop diameter gauge with ±0.02 mm tolerance.
An all-dielectric self-supporting fibre optic cable spanning 200 m under 15 m/s wind and 20 mm radial ice load requires a sheath compound with a 100-d tensile creep modulus above 450 MPa at 23 °C; HDPE FR439800X01 W&C is applied at 1.6–2.2 mm wall thickness over the aramid yarn load-bearing layer. The formulation adds 5.0–6.0 wt% of a 50% carbon black masterbatch for 2.5–3.0 wt% carbon black, 0.15–0.30 wt% hindered phenolic antioxidant, and 0.03–0.08 wt% fluoropolymer processing aid; filler loadings above 3.0 wt% carbon black are avoided because they reduce low-temperature crack initiation resistance at clamp points during ice-shedding events. Extrusion on a 30:1 L/D grooved-feed single-screw line uses a dual-layer crosshead with an MDPE inner jacket and HDPE outer sheath, with melt temperature 220–235 °C and outer sheath die draw-down ratio 1.2:1 to 2.0:1. Compliance under IEEE 1222-2019 covers ADSS mechanical loading, while sheath tensile and elongation are measured per ASTM D638-14 and jacket shrinkage per IEC 60794-1-2:2021. Terminal products include 24–144-fibre ADSS spans from 50 m to 200 m, used in medium-voltage and high-voltage transmission corridors where metallic cable designs are not permitted.
Failure analysis of clamp-point stress cracking in fielded ADSS cables shows that post-extrusion jacket drawdown above 2.0:1 increases frozen-in orientation and promotes environmental stress-cracking under combined clamp compression and transverse wind vibration. The production control limit is therefore set at a maximum drawdown of 2.0:1, with chill-trough water temperature stepped from 60 °C to 25 °C to relax orientation without allowing water-quench microvoids. The grade is not qualified for metallic armour contact without a compatible anti-corrosion bedding layer because galvanic corrosion from steel wire accelerates slow crack growth in HDPE under sustained tensile load.
| Application route | Key standard designation | Typical additive loading window | Terminal product type |
|---|---|---|---|
| Outside plant fibre optic jacket | IEC 60794-1-2:2021, ASTM D1248-20, UL 1581 | 5.0–6.0 wt% CB masterbatch; 0.10–0.25 wt% AO | 12–288-fibre loose tube cables |
| Air-blown microduct bundle | ASTM D3350-14, EN 60794-5 | 2.0–4.0 wt% colour masterbatch; 0.05–0.15 wt% erucamide | 7/3.5 mm and 12/8 mm FTTx microducts |
| ADSS aerial fibre sheath | IEEE 1222-2019, ASTM D638-14 | 5.0–6.0 wt% CB masterbatch; 0.15–0.30 wt% AO | 24–144-fibre ADSS spans 50–200 m |
| Armoured submarine outer sheath | IEC 60794-1-2:2021, ICEA S-87-640 | 5.0–6.0 wt% CB masterbatch; 0.15–0.25 wt% AO | Shore-end armoured submarine fibre optic cables |
| Copper local loop primary insulation | IEC 60708:2019, ASTM D1248-20 | 0.05–0.15 wt% AO; 0.05–0.10 wt% copper deactivator | 20–100-pair jelly-filled underground copper cables |
Shore-end segments of armoured submarine fibre optic cables use HDPE FR439800X01 W&C as an outer sheath extruded over galvanized steel wire armour at wall thickness 3.0–5.0 mm, with a minimum sheath elongation at break above 450% per ASTM D638-14 to permit cable bending around capstan wheels without sheath rupture. The formulation uses 5.0–6.0 wt% of a 50% carbon black masterbatch, 0.15–0.25 wt% hindered phenolic antioxidant, and 0.05–0.10 wt% phosphite processing stabiliser, while metal deactivators are excluded unless the sheath is coextruded over copper-based armour. Extrusion on a 30:1 L/D single-screw line is run with a melt temperature of 220–240 °C and a 3–5 mm wall crosshead; the cooling trough length is extended to 30–50 m because thick HDPE layers retain heat at the armour interface and form internal voids when the surface is quenched too rapidly. Compliance is anchored to IEC 60794-1-2:2021 and ICEA S-87-640 for optical fibre cable mechanical qualification. Terminal product types include shore-end and shallow-water armoured submarine fibre optic cable segments up to 10 kN installation tension, as well as river-crossing and inter-island cables with steel tape armour.
The main process risk on production-scale submarine sheathing lines is melt penetration between armour wires when gear-pump discharge pressure exceeds 350 bar; this creates a thin high-stress inner lip that can initiate slow crack growth under repeated bending. Pressure is therefore maintained below 300 bar and the armour preheat temperature is held at 110–130 °C to improve adhesion without thermal oxidation of the steel wire. Published data for FR439800X01 W&C in deep-sea repeatered cable configurations beyond 2,000 m water depth are limited, so qualification for such installations requires additional peel-strength and water-absorption testing before production release.
In petroleum-jelly-filled copper local loop cables, HDPE FR439800X01 W&C is applied as solid primary insulation on 0.4–0.9 mm copper conductors at wall thickness 0.15–0.35 mm, with a conductor preheat of 120–150 °C to remove residual moisture and improve adhesion. The insulation compound is based on 100 phr HDPE with 0.05–0.15 wt% hindered phenolic antioxidant and 0.05–0.10 wt% copper deactivator; carbon black is omitted because the dielectric strength and insulation resistance requirements for primary insulation are degraded by conductive filler. Wire-coating extrusion uses a pressure die with draw-down ratio between 1.1:1 and 1.6:1, and melt temperature is controlled at 200–230 °C. Compliance is tested to IEC 60708:2019 for low-frequency polyolefin-insulated cables and ASTM D1248-20 for PE insulation-grade classification; insulation resistance is measured in water at 20 °C after 24 h immersion. Terminal product types include 20–100-pair jelly-filled underground copper cables for rural local loop and business drop segments.
Ageing resistance against petroleum jelly is verified by tensile retention after 28 d immersion at 70 °C in a representative hydrocarbon filling compound, with elongation retention required above 80%; poor dispersion of the copper deactivator below 0.05 wt% leads to catalytic copper-ion degradation that reduces oxidative induction time at 200 °C below 30 min. On multi-wire coating lines, the dominant bottleneck is not melt output but conductor tension fluctuation; variations above ±5% create eccentric insulation that fails spark-test continuity at 3 kV. Closed-loop dancer control and extruder melt gear pumps maintain wall-thickness eccentricity below 5% for continuous lengths above 10 km.
Competitive LyondellBasell HDPE FR439800X01 W&C prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell HDPE FR439800X01 W&C is a pelletized high-density polyethylene compound intended specifically for flame-retardant wire-and-cable jacketing and insulation layers. The grade designation embeds the end-use category: the FR segment identifies a flame-retardant formulation, while W&C restricts the recommended processing to wire-and-cable extrusion rather than blow molding, film, or injection molding. The X01 suffix denotes a defined additive and stabilization package within the producer’s W&C portfolio. Published data for this exact configuration are limited in some areas; the values presented below are representative figures from public grade literature and do not replace the current manufacturer technical datasheet. The compound is distinguished from general-purpose HDPE by its filled flame-retardant system, higher density, lower melt flow under standard load, and a rheology designed for thin-wall jacketing of twisted-pair, control, signal, and low-voltage power cable constructions.
Compared with unfilled HDPE of equivalent molecular weight, the flame-retardant package raises low-shear melt viscosity and melt strength while reducing die swell. This shift supports circularity during tube-down jacketing but raises backpressure on narrow die gaps. The melt flow rate for this compound is specified at the high-load condition of 190°C/21.6 kg under ISO 1133-1:2022, with a representative value of 0.80 g/10 min. The choice of 21.6 kg rather than 2.16 kg is deliberate because the flame-retardant filler network produces a low standard-load MFR that is of limited value for extrusion control. The filled melt also exhibits a lower onset of shark-skin melt fracture than neat HDPE at equivalent shear rates. Extrusion trials on jacketing lines have shown that raising the die-head temperature by 5°C to 10°C above the melt temperature, or increasing the die land length by 1 mm to 3 mm, reduces visible surface roughness on thin-wall jackets. Die-lip deposit can accumulate from partially degraded flame-retardant species when melt temperature exceeds 220°C for extended periods. The producer’s processing guide recommends a melt-temperature window of 190°C to 220°C and directs against excursions above 235°C to avoid pinholes, additive blooming, and spark-test failures.
On single-screw jacketing lines, the compound is typically processed with a barrier screw having an L/D between 24:1 and 30:1 and a compression ratio near 3:1. Melt filtration through a 60/100/60 mesh screen pack is applied to remove agglomerated flame-retardant filler, carbon particles, or gel bodies that would otherwise produce spark-test failures at high line speed. Head pressure before the breaker plate should remain below 35 MPa. Pressure fluctuations greater than ±0.5 MPa have been associated with periodic wall-thickness variation in thin-wall constructions. Although the base HDPE phase is not strongly hygroscopic, the flame-retardant filler system can absorb moisture during open storage. When warehouse relative humidity exceeds 60%, the pellets should be dried at 60°C to 70°C for 4 h in a desiccant or hot-air hopper dryer. Failure to dry can generate micro-voids that lower dielectric strength and promote insulation failure during wet spark testing. The recommended extruder temperature profile from hopper to die is flat to slightly reverse, with the feed zone kept below 160°C to prevent premature melting and bridging of the filled pellets in the hopper throat.
Field experience on jacketing lines has shown that the most common failure modes for flame-retardant HDPE compounds are not thermal degradation of the base resin but additive-related surface defects. When line speed is increased beyond the melt’s critical shear rate, shark-skin first appears at the die exit as periodic ridges perpendicular to the machine direction. This defect is corrected by increasing die temperature, reducing line speed, or widening the die gap with greater draw-down. Die-lip deposit forms when low-molecular-weight additive species migrate to the die surface; it appears as a sticky film that disrupts jacket smoothness and can generate spark-test faults. Periodic cleaning of the die with a non-abrasive brass tool and maintaining a temperature differential of 5°C between die zones reduces the deposition rate. Screen-pack blinding should be monitored because clogged screens raise head pressure and lower output, while frequent screen changes can introduce melt-temperature drift if the extruder is not equipped with a melt pump. The use of a gear pump between the screw and die smooths pressure fluctuations to below ±0.3 MPa and improves wall-thickness consistency on cables below 10 mm outer diameter.
The mechanical profile of the compound is characterized by tensile stress at break of approximately 18.5 MPa when tested according to ISO 527-2:2012 at 50 mm/min, with elongation at break near 500%. Hardness is approximately 60 Shore D under ISO 868:2003, which provides crush resistance for cable jackets in conduit pulls and direct-burial applications. Low-temperature performance is monitored by brittleness temperature under ASTM D746-20, with a representative value of -76°C. Electrical properties include volume resistivity above 1×10^15 Ω·cm under ASTM D257-21 at 500 V and 23°C, dielectric constant near 2.6 at 1 MHz, and dissipation factor near 0.0005. The limiting oxygen index is typically reported as 28% under ISO 4589-2:2017. These values place the material in the class of flame-retardant thermoplastic jacketing compounds rather than in the higher oxygen-index range typical of highly filled halogen-free systems based on ethylene-vinyl acetate. Environmental stress-cracking resistance is relevant for cable jackets exposed to lubricants, surfactants, and wetting agents. The grade is formulated for improved ESCR compared with lower-molecular-weight HDPE, but specific ESCR values must be confirmed against the current technical datasheet because results vary with cable geometry, stress level, and environmental fluid chemistry.
In low-voltage control and signal cables, the grade has been used as a jacketing layer over twisted pairs and screened constructions where the jacket must resist abrasion, maintain dimensional stability at elevated ambient temperatures, and pass single-wire flame propagation tests such as IEC 60332-1-2. Its higher melt strength permits thin-wall jacketing without excessive draw-down distortion, and the controlled die swell supports roundness in non-round cable cores. Compared with ethylene-vinyl acetate-based flame-retardant compounds, the HDPE-based product typically provides higher hardness and lower filler loading, but lower inherent flexibility and a narrower processing window for high-line-speed coating. It is not a crosslinkable compound; therefore no peroxide or silane cure line is required. This limits continuous conductor temperature to the usual thermoplastic HDPE range, typically 75°C for continuous operation, with short-term excursions up to 90°C only when permitted by the relevant cable specification and after verification of thermal aging performance.
The combination of low-temperature impact resistance and flame retardance creates a compounding conflict: flame-retardant fillers raise modulus and reduce low-temperature toughness, while the base HDPE already has lower toughness at subzero temperatures than linear low-density polyethylene. For this grade, the brittleness temperature of -76°C makes it suitable for many outdoor cable jackets, but it should not be assumed to match LLDPE or EVA-based jacketing compounds in severe flexing at temperatures below -40°C. When a specification simultaneously calls for IEC 60332-1-2 flame propagation and a low-temperature impact or flexing test, the cable geometry, jacket wall thickness, and conductor temperature class must be evaluated together. The compound’s HDPE base provides high crush resistance at room temperature and good surface hardness, but its flame-retardant additive package may reduce environmental stress-cracking resistance if the jacket is exposed to polar oils or silicone-based pulling lubricants. In direct-burial or conduit applications where the cable is pulled through long runs, the combination of high hardness and lower surface slip can increase friction; processing aids or external lubricants should be tested for compatibility with the flame-retardant system and with the spark-test dielectric requirement.
Compared with the same producer’s unfilled HDPE extrusion grades, this W&C product has a lower standard-load melt index, higher density, and higher surface polarity. The surface polarity can improve printing adhesion but can reduce the effectiveness of silicone slip agents. Compared with LLDPE jacketing grades, it provides higher crushing resistance and better dimensional stability at elevated ambient temperatures, but lower resistance to environmental stress cracking in the presence of alcohols and surfactants. Compared with flexible EVA-based halogen-free flame-retardant compounds, the HDPE compound has a lower filler acceptance threshold, which limits the achievable oxygen index, but it retains the typical HDPE advantages of lower moisture absorption and higher melt strength. These differences mean that grade selection should be driven by the specific cable specification: where subzero flexing dominates, a more elastomeric jacketing compound may be required; where crush resistance, thin-wall rigidity, and surface hardness dominate, the HDPE base is technically appropriate.
Qualification documentation should include the following test designations when the cable is intended for international markets: ISO 1133-1:2022 for melt flow rate, ISO 1183-1:2019 for density, ISO 527-2:2012 for tensile properties, ISO 868:2003 for hardness, ASTM D746-20 for brittleness temperature, ASTM D257-21 or IEC 62631-3-1 for volume resistivity, IEC 62631-2-1 for dielectric constant and dissipation factor, ISO 4589-2:2017 for limiting oxygen index, and IEC 60332-1-2 for single-wire flame propagation. For North American constructions, UL 1581 methods are often used for flame and mechanical testing, but suitability for a specific UL listing must be confirmed through the producer’s UL file and the cable manufacturer’s listing. The raw-material designation alone does not constitute a listed cable compound.
| Property | Test method | Representative value |
|---|---|---|
| Density | ISO 1183-1:2019 | 1.13 g/cm³ |
| Melt flow rate, 190°C/21.6 kg | ISO 1133-1:2022 | 0.80 g/10 min |
| Tensile stress at break | ISO 527-2:2012 | 18.5 MPa |
| Elongation at break | ISO 527-2:2012 | 500% |
| Shore D hardness | ISO 868:2003 | 60 |
| Brittleness temperature | ASTM D746-20 | -76°C |
| Volume resistivity | ASTM D257-21 | >1×10^15 Ω·cm |
| Dielectric constant, 1 MHz | IEC 62631-2-1 | 2.6 |
| Dissipation factor, 1 MHz | IEC 62631-2-1 | 0.0005 |
| Limiting oxygen index | ISO 4589-2:2017 | 28% |
Compliance for specific end-use projects usually requires verification against the complete manufacturer’s technical datasheet and applicable cable standards such as IEC 60502-1, UL 44, or UL 1581. The exact halogen content, smoke density, and acid-gas evolution of the flame-retardant package should be obtained from the producer when the cable is intended for low-smoke halogen-free installations or for legislative frameworks requiring halogen-free performance. Without that confirmation, the grade should not be described as halogen-free. Avoid combination with amine-containing stabilizers or slip agents unless compatibility with the flame-retardant system has been confirmed, because additive antagonism can reduce flame performance and produce surface haze. The product is not intended for food-contact or medical applications unless a specific regulatory clearance is issued. No peroxide, silane, or irradiation crosslinking step is required; high-temperature thermoset service classifications are not part of this grade’s operating envelope.