Lyondellbasell Cp878 01 Natural Linear Low Density Polyethylene

LyondellBasell CP878-01 Natural Linear, Low-Density Polyethylene

    • Product Name: LyondellBasell CP878-01 Natural Linear, Low-Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 836454
    Density 0.918 g/cm³
    Melt Index 0.8 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 24.1 MPa
    Elongation At Break 800%
    Flexural Modulus 207 MPa
    Vicat Softening Point 96 °C
    Melting Point 121 °C
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 350 g
    Elmendorf Tear Strength Td 600 g
    Haze 10%
    Gloss At 45 60
    Coefficient Of Friction 0.20

    As an accredited LyondellBasell CP878-01 Natural Linear, Low-Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell CP878-01 Natural Linear Low-Density Polyethylene is supplied in 25 kg polyethylene bags.
    Container Loading (20′ FCL) Container Loading (20′ FCL): LyondellBasell CP878-01 Natural Linear, Low-Density Polyethylene resin, palletized bags, securely stowed and braced for ocean freight.
    Shipping LyondellBasell CP878-01 Natural Linear Low-Density Polyethylene typically ships as non-hazardous plastic resin pellets in 25-kg bags, octabins, or bulk trucks/railcars. It is generally not DOT/IMDG/IATA regulated. Store cool, dry, away from direct sunlight, heat, ignition sources, and moisture. Use standard handling and keep containers closed/secured. Follow applicable local transport rules.
    Storage Store LyondellBasell CP878-01 Natural Linear Low-Density Polyethylene in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and moisture. Keep sealed in original packaging, on pallets, off the floor, to prevent contamination. Avoid contact with oxidizers, oils, and chemicals. Protect from UV, physical damage, and excessive stacking. Follow local regulations and the SDS. Use first-in, first-out stock rotation.
    Shelf Life Typically 24 months from date of manufacture when stored in original packaging in a cool, dry area, away from direct sunlight.
    Application of LyondellBasell CP878-01 Natural Linear, Low-Density Polyethylene

    At cast-film line speeds between 300 m/min and 600 m/min, CP878-01 natural linear low-density polyethylene is processed through a 90 mm single-screw extruder having a 30:1 L/D ratio and a five-layer feedblock fitted with a 2 400 mm flat die. The processing window requires die zone temperatures of 205 °C to 240 °C, an air gap of 25 mm to 40 mm, and a polished chill roll maintained at 20 °C to 28 °C, followed by corona treatment set to 42 mN/m to 46 mN/m on the treated web surface. In 12 µm to 23 µm stretch film, the layer formulation is 92.0 wt% to 95.0 wt% virgin CP878-01, 2.0 wt% to 3.5 wt% polyisobutylene cling masterbatch, 1.0 wt% to 2.0 wt% synthetic silica anti-block, and 0.3 wt% to 0.8 wt% erucamide slip concentrate. The cling additive becomes surface-active within 24 h to 48 h after winding, and overdosing beyond 3.5 wt% is observed as die smoke at melt temperatures above 260 °C as well as cling degradation when regrind is reintroduced at 15 wt% to 20 wt% into the main layer. Food-contact compliance is evaluated under FDA 21 CFR 177.1520(c) and Commission Regulation (EU) No 10/2011, with overall migration limits not exceeding 10 mg/dm² under the assigned food simulants; raw material registration follows REACH (EC) No 1907/2006. Terminal products include 450 mm machine rolls, 20 µm hand pallet wrap, and 23 µm agricultural bale wrap used in automated palletising warehouses, cold-storage distribution, and silage preservation.

    How Does Frost Line Height Alter Dart Impact Retention in High-Stalk Blown Film?

    High-stalk blown-film extrusion of CP878-01 differs from low-stalk operation by maintaining a pronounced neck height above the die, typically 450 mm to 700 mm, on a 250 mm spiral mandrel die with a 1.6 mm to 2.2 mm die gap. Melt temperature at the die entrance is held at 210 °C to 230 °C, and the blow-up ratio is controlled between 2.5:1 and 3.2:1; lower blow-up ratios increase machine-direction orientation, while higher blow-up ratios stabilise transverse-direction tear resistance. Internal bubble cooling air at 15 °C to 20 °C reduces frost line drift during gauge variation of ±4 µm on a 75 µm heavy-sack structure. The formulation for heavy-duty sacks and industrial liners consists of 70 wt% to 85 wt% CP878-01, 15 wt% to 30 wt% LDPE, and, where outdoor exposure is specified, 2.0 wt% to 3.0 wt% carbon black masterbatch qualified under ISO 4892-2:2021 accelerated weathering conditions. Dropping CP878-01 below 70 wt% reduces dart drop energy measured under ASTM D1709-16 after specimen conditioning at 23 °C and 50% RH for 40 h; industrial acceptance criteria frequently require a minimum dart impact of 200 g at 75 µm thickness and 150 g at 50 µm. Tensile properties are measured under ASTM D882-18 at 500 mm/min, and the food-contact suitability of the finished sack liner is verifiable under EU 10/2011 and FDA 21 CFR 177.1520(c). Terminal products include flexible intermediate bulk container liners, chemical drum liners, construction vapour membranes, and heavy-duty shipping sacks.

    Extrusion coating trials with CP878-01 on 1 200 mm wide tandem laminating lines expose melt-strength limits that dictate draw-down behaviour at coating thicknesses of 15 µm to 30 µm. A 90 mm extruder with a 30:1 L/D screw feeds a slot die set to a 3.0 mm die gap, with adapter and die temperatures from 260 °C to 290 °C; the melt curtain drops through an air gap of 150 mm to 250 mm before the pressure nip, where a 42 mN/m to 46 mN/m corona-treated substrate receives the extrudate. At the nip, the blend is 80 wt% CP878-01 with 20 wt% LDPE to moderate neck-in and edge-bead instability above 350 m/min; for line speeds below 250 m/min, 100 wt% CP878-01 can be used without measurable web fluctuation. The process is verified under ASTM F88/F88M-23 seal-strength testing and ASTM D1894-14 coefficient-of-friction evaluation after conditioning at 23 °C and 50% RH. Food-contact laminates are assessed for overall migration under EU 10/2011 and FDA 21 CFR 177.1520(c); the natural resin adds no intentionally incorporated slip or anti-block substances, allowing downstream converters to adjust surface performance to filling-line coefficient requirements. At draw ratios exceeding 80:1, edge neck-in becomes severe and web tension variation above ±8 N is observed; published data for CP878-01 at full coating speeds above 600 m/min remains limited. Terminal products include multi-wall paper bag liners, sachet film for dry food powders, medical packaging overwrap, and laminated foil pouches for industrial dry chemicals.

    Selected qualification methods for CP878-01 downstream processing
    Processing segmentTest standardMeasurement conditionAttribute controlled
    Cast stretch filmASTM D882-18500 mm/min, 23 °CTensile break and elongation
    High-stalk blown filmASTM D1709-16Method A, 40 h conditioningDart drop impact energy
    Extrusion coatingASTM F88/F88M-2315 mm width, 200 mm/min peelHeat-seal strength
    Masterbatch carrierISO 1133-1:2022190 °C, 2.16 kgMelt flow rate stability

    Twin-Screw Carrier Resin Behaviour in Polyolefin Masterbatch Production

    In co-rotating twin-screw compounding, CP878-01 is melt-mixed at carrier loadings of 55 wt% to 70 wt%, with the combined pigment and additive package comprising 25 wt% to 40 wt% and a wax or polyethylene dispersant at 3 wt% to 8 wt%. The preferred machine configuration is a 32:1 L/D twin-screw extruder with side-feeding at barrel segment 6 of 10, allowing pigments to bypass the primary kneading block and reduce thermal history. Barrel temperatures are profiled at 160 °C to 200 °C, and screw speed is maintained between 500 rpm and 900 rpm; die-face pelletising uses a water-ring chamber at 35 °C to 55 °C. Insufficient melt temperature below 160 °C produces undispersed agglomerates greater than 20 µm, which manifest as surface defects when the finished masterbatch is let down into blown film at 2 wt% to 5 wt%. The carrier function is characterised by MFR stability under ISO 1133-1:2022 at 190 °C/2.16 kg, and the grade’s nominal density of 0.918 g/cm³ is confirmed under ISO 1183-1:2019 for lot-release documentation. Terminal products include UV-stabiliser masterbatches for agricultural film, processing-aid concentrates for blown film, and colour concentrates for extrusion coating and thin-gauge cast film.

    When MFR 1.0 g/10 min Meets Thin-Wall Injection Moulding

    When the 1.0 g/10 min melt flow rate of CP878-01 is retained through barrel profiling, thin-wall injection moulding is feasible only with the mould temperature and injection speed held within a narrow envelope. The material is blended at 50 wt% to 70 wt% CP878-01 with 30 wt% to 50 wt% HDPE to raise modulus and shorten sink-mark recovery; colour masterbatch is added at 1.5 wt% to 2.5 wt%, while release-agent concentration remains below 0.2 wt% to preserve weld-line strength. A 25 mm barrier screw with a 20:1 L/D feed section and a 1 200 kN clamp force machine delivers shot-weight consistency when the barrel is zoned from 190 °C to 240 °C, the nozzle is held at 220 °C, and the mould is cooled to 20 °C to 35 °C using a turbulent-flow thermolator. Injection pressure of 700 bar to 900 bar and holding pressure of 350 bar to 500 bar are monitored against cavity filling times of 0.4 s to 0.7 s; failure to maintain high-speed filling produces flow hesitation lines on flat surfaces at wall thickness below 1.2 mm. Mechanical acceptance is tested under ISO 294-1:2017 specimen preparation, ISO 527-2:2012 tensile modulus, and ISO 180:2023 Izod impact; food-contact parts are validated under EU 10/2011 and FDA 21 CFR 177.1520(c). For configurations requiring flow paths longer than 400 mm or wall thickness below 0.8 mm, published industrial data for CP878-01 remains limited. Terminal products include collapsible liquid-handling containers, laboratory drainage fittings, caps for chemical pails, and reusable shipping plugs.

    Free Quote

    Competitive LyondellBasell CP878-01 Natural Linear, Low-Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell CP878-01 Natural is a linear low-density polyethylene (LLDPE) delivered as natural-colored pellets. The chain architecture is based on ethylene copolymerized with a short-chain α-olefin, producing a predominantly linear backbone with controlled short-chain branching. That structural feature distinguishes the grade from high-pressure LDPE, which contains both short-chain and long-chain branches. The natural designation indicates that the formulation does not include a pre-dispersed pigment, carbon black, or titanium dioxide; downstream processors may add a masterbatch or mold translucent unpigmented parts. Water absorption of the matrix remains below 0.01% when tested under ISO 62:2008, so the major processing risk is not hygroscopic hydrolysis but surface moisture from humid storage.

    Melt mass-flow rate and density are the primary lot-release controls. Melt mass-flow rate is determined at 190 °C under a 2.16 kg load with ISO 1133-1:2022 or ASTM D1238-20. Density is measured by ASTM D1505-18 or ISO 1183-1:2019. For CP878-01 Natural, the certificate of analysis is the binding specification; class-level density for injection-molding LLDPE generally sits between 0.916 g/cm³ and 0.940 g/cm³, and melt mass-flow rate commonly falls between 2 g/10 min and 30 g/10 min. Published data for this specific grade in blown film, extrusion coating, or rotational molding are limited; grade-specific pilot trials are required before substituting CP878-01 Natural outside injection molding.

    What Test Methods Govern Mechanical and Thermal Specifications?

    Tensile yield stress, tensile stress at break, and elongation at break are measured on injection-molded Type IV or ISO 1A dumbbells at a crosshead speed of 50 mm/min using ASTM D638-14 or ISO 527-2:2012. Flexural modulus is obtained by three-point bending at 2 mm/min according to ISO 178:2019 or ASTM D790-17. Notched Izod impact is generated on Type 1 specimens under ISO 180/A:2019. Because polyethylene notched impact at 23 °C often reports partial break or no break, tensile and flexural data are more discriminating for lot-to-lot control. Vicat softening temperature is measured under 10 N load at a heating rate of 50 K/h per ISO 306:2013. Melting peak temperature is recorded by differential scanning calorimetry at 10 K/min under ISO 11357-3:2018; for LLDPE, the melting peak typically falls between 120 °C and 127 °C depending on comonomer content.

    For CP878-01 Natural, class averages are not a substitute for certified values. Part-specific qualification should use the same gate type, cavity texture, and packing pressure as production tooling because weld lines, flow orientation, and frozen-in stress alter tensile and impact results. When certified values are unavailable, incoming resin audits should include melt-flow testing under ASTM D1238-20 and density measurement under ASTM D792-20.

    When CP878-01 Natural Is Processed by Injection Molding

    A reciprocating-screw machine with a general-purpose polyolefin screw of 20:1–25:1 length-to-diameter ratio and a compression ratio of 2.5:1–3.5:1 is suitable. A non-return valve is used to reduce cushion variation. Barrel temperature profiles from feed to nozzle may be set at 160 °C, 190 °C, 210 °C, 220 °C, and 230 °C, with actual melt temperature maintained between 200 °C and 250 °C. Above 260 °C, thermal oxidative degradation becomes rapid; in high-shear thin-wall tools with long hold times, the practical window can be as narrow as ±5 °C around setpoint.

    Injection velocity should be moderate to high to prevent flow hesitation in thin sections, but excessive velocity causes jetting and gate blush. Injection pressures are typically 30–80 MPa hydraulic pressure, with holding pressure at 50–70% of peak injection pressure and back pressure at 0.3–1.5 MPa. Mold temperature is controlled between 15 °C and 60 °C; lower temperatures reduce cycle time but may increase frozen-in stress and sink marks. Linear mold shrinkage for LLDPE injection-molding grades typically spans 1.0–2.5% after 24 h when measured per ASTM D955-21. Gate placement should avoid weld lines in high-stress regions; runner diameters between 3.0 mm and 6.0 mm and a cold slug well are typical starting points. For gate design, edge gate thickness of 50–70% of nominal wall thickness helps keep the gate open during packing; premature gate freeze-off leads to sink marks and excessive flow-direction shrinkage.

    Surface moisture can cause splay defects after silo storage at relative humidity above 60%. A desiccant-bed hopper dryer at 70–80 °C for 1–2 h with a dew point of −20 °C is recommended. Residence time in the barrel should be kept below 5–10 min; if an interruption exceeds this limit, the barrel should be purged with a low-viscosity polyethylene purge compound. On a 1,200 kN toggle-clamp machine with a 25 mm screw, screw speed is initially set at 60–100 rpm. Higher speeds can raise melt temperature by 15–25 °C through viscous dissipation, requiring a lower barrel setpoint.

    During mold filling, a single melt-flow value is insufficient to predict pressure drop because gate shear rates in injection molding can reach 1,000–10,000 s⁻¹. Capillary rheometry at 190 °C across apparent shear rates from 10 s⁻¹ to 1,000 s⁻¹ generates a viscosity curve that can be fitted to a Carreau–Yasuda model. LLDPE exhibits shear thinning, but less than high-pressure LDPE with long-chain branching; this means injection pressure may remain higher at thin-wall gates. A spiral-flow test in the intended tool steel at the intended wall thickness is preferable for evaluating lot-to-lot processability.

    Shrinkage is anisotropic. Flow-direction shrinkage is usually lower than cross-flow shrinkage because of molecular orientation. A preliminary mold design may start at 1.5% linear shrinkage, but the actual molded part can vary by 0.8–2.5% depending on wall thickness, packing pressure, and gate location. Shrinkage should be measured on a plaque with the same gating as the production part; ASTM D955-21 provides a standardized method but does not capture complex geometry effects.

    Natural LLDPE injection-molding grades are used in thin-wall containers, caps, closures, housewares, and industrial components requiring stress-crack resistance and low-temperature toughness. In closure development, environmental stress-crack resistance is measured with notched bent specimens immersed in nonylphenol ethoxylate at 50 °C under ASTM D1693-15; time to failure is the response, and higher short-chain branching generally improves it. CP878-01 Natural in unpigmented form is not inherently stabilized for long-term ultraviolet exposure; outdoor service life requires a UV stabilizer package or protection by painting. The absence of carbon black removes opacity but can increase photodegradation in direct sunlight.

    Compared with high-pressure LDPE, the linear backbone of CP878-01 as an LLDPE increases tensile strength and puncture resistance at equivalent density but lowers melt extensibility and bubble stability in film. Compared with HDPE, the lower density of CP878-01 reduces flexural modulus and continuous-use stiffness but may improve notched impact and environmental stress-crack resistance. Compared with metallocene-catalysed LLDPE, a conventional Ziegler-Natta grade may have a broader comonomer distribution, which can improve high-shear processability but reduce clarity and increase extractables; if CP878-01 Natural is metallocene-catalysed, the reverse may apply, and supplier documentation must be consulted.

    Mechanical Property Differences Across Polyethylene Families

    The table below reports class-level property envelopes for initial material screening. These ranges are not CP878-01 certifications and should not replace the certificate of analysis.

    FamilyDensity (g/cm³)Tensile Yield (MPa)Flexural Modulus (MPa)Melt/Process Character
    High-pressure LDPE0.915–0.9358–12200–400High long-chain branching; stable blown-film bubble
    LLDPE class0.916–0.94010–18300–700Linear backbone; higher tensile and ESCR; lower melt extensibility
    HDPE0.940–0.96520–32800–1500High stiffness and heat resistance; ESCR depends on comonomer
    Metallocene LLDPE0.915–0.94010–15300–600Narrow MWD/comonomer distribution; high clarity; lower melt strength

    The selection drivers for CP878-01 Natural over LDPE are higher tensile yield and puncture resistance at similar density; over HDPE, improved impact and stress-crack behavior at the cost of stiffness; over metallocene LLDPE, a potentially broader processing window on older injection molding machines at the cost of clarity and possibly higher extractables.

    Molecular architecture is the underlying cause. High-pressure LDPE carries long-chain branches that entangle in the melt, giving high melt strength, high die swell, and low shear thinning. LLDPE prepared by catalytic coordination polymerization has short-chain branches without the same degree of long-chain entanglement, so melt extensional behavior is lower. This can reduce flow marks in large flat parts but limits bubble stability in blown-film and lowers melt strength in blow molding.

    Weld lines in LLDPE are typically stronger than in filled crystalline polymers but remain initiation points. In a multiple-gated part, weld-line tensile strength can be tested with a double-gated tensile bar under ASTM D638-14; the reduction relative to a single-gated bar may be 20–50%. Melt temperature, mold temperature, and holding pressure have the largest influence on weld-line strength because they control molecular interdiffusion across the flow front.

    Melt Temperature and Time Interact Through a Kinetic Degradation Boundary

    Surface moisture is not a bulk absorption problem for LLDPE, but condensation can create splay defects. Thermal stability is controlled by free-radical oxidation with hydroperoxide intermediates; measurable degradation begins above 200 °C and accelerates sharply above 260 °C. A melt held at 250 °C for 5 min may degrade less than a melt held at 230 °C for 30 min under shear. Oxidation induction time measured by differential scanning calorimetry at 200 °C per ISO 11357-6:2018 provides a comparative measure of the stabilizer package.

    In high-shear molds with 0.5 mm wall sections and multiple hot drops, viscous heating can raise the actual melt temperature above the barrel setpoint. If nozzle melt temperature exceeds the barrel setpoint by more than 10 °C, shear heating is excessive; screw speed, back pressure, or screw geometry should be adjusted. On a 25 mm mixing screw, high screw speed can add 15–25 °C to the melt temperature, so the upper barrel setpoint should be reduced accordingly. The usable processing window is a time-temperature-shear envelope rather than a single setpoint.

    For compounding or masterbatch addition, a twin-screw extruder with 28:1–48:1 length-to-diameter ratio and distributive mixing elements can be used. High-intensity kneading blocks should be limited because LLDPE is shear-sensitive; excessive mechanical work can reduce molecular weight and shift melt flow rate. If regrind is used, the virgin-to-regrind ratio should be fixed at the qualification level because repeated thermal history can narrow molecular weight distribution and reduce impact resistance.

    For food-contact applications, unmodified olefin polymers may be subject to 21 CFR 177.1520; compliance is article-specific and must be documented by the supplier. In the European Union, food-contact plastics are evaluated under EU No 10/2011, with overall migration and specific migration limits linked to food simulant and contact temperature. REACH registration under EC 1907/2006 and RoHS restrictions under 2011/65/EU apply to the finished electrical or electronic article. Processors should not rely on raw-material compliance alone; article-specific verification is required.

    Storage should be in original sealed packaging at 10–35 °C and relative humidity below 60%. Once opened, re-sealing and use within 6 months is a reasonable housekeeping practice. Bulk material in sealed bags is stable against ambient oxidative degradation; exposed surfaces should be minimized before processing.

    Top