Lyondellbasell Cp842 01 Hexene Copolymer Lldpe Resin

LyondellBasell CP842-01 Hexene Copolymer LLDPE Resin

    • Product Name: LyondellBasell CP842-01 Hexene Copolymer LLDPE Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 249152
    Product Name LyondellBasell CP842-01 Hexene Copolymer LLDPE Resin
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Hexene
    Melt Index 190c 2 16kg 1.0 g/10 min
    Density 0.918 g/cm3
    Melt Flow Ratio 28
    Tensile Strength At Yield Md 10.3 MPa (1500 psi)
    Tensile Strength At Break Md 27.6 MPa (4000 psi)
    Tensile Strength At Break Td 24.1 MPa (3500 psi)
    Elongation At Break Md 700%
    Elongation At Break Td 800%
    Elmendorf Tear Strength Md 300 g
    Elmendorf Tear Strength Td 400 g
    Dart Drop Impact 150 g
    Haze 10%
    Gloss 45 Deg 60
    Vicat Softening Point 108 °C
    Melting Point 124 °C
    Brittleness Temperature -70 °C
    Coefficient Of Friction 0.2

    As an accredited LyondellBasell CP842-01 Hexene Copolymer LLDPE Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg polyethylene bags, palletized, or bulk trucks/railcars for LyondellBasell CP842-01 Hexene Copolymer LLDPE Resin.
    Container Loading (20′ FCL) 20′ FCL loading for LyondellBasell CP842-01 Hexene Copolymer LLDPE Resin: palletized 25 kg bags, shrink-wrapped, strapped, evenly distributed for safe export.
    Shipping LyondellBasell CP842-01 Hexene Copolymer LLDPE Resin is a non-hazardous thermoplastic pellet, not classified as dangerous goods. It is typically shipped in moisture-barrier bags, octabins, or bulk trucks/railcars. Store cool, dry, ventilated, away from heat, sunlight, moisture, and oxidizers. Follow SDS and transport regulations.
    Storage For LyondellBasell CP842-01 Hexene Copolymer LLDPE Resin, store in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original containers closed, elevated off floors, and protected from moisture, dust, and contamination. Avoid excessive stacking and high temperatures to prevent blocking. Do not smoke. Follow SDS and local regulations.
    Shelf Life Shelf life is 2 years from date of manufacture when stored in original packaging, dry, cool, well-ventilated area, away from sunlight.
    Application of LyondellBasell CP842-01 Hexene Copolymer LLDPE Resin
    In high-output cast stretch film conversion for automated pallet unitization, CP842-01 hexene copolymer LLDPE is introduced into the extruder at **70–85 wt%** with **15–30 wt%** metallocene LLDPE in monolayer formulations, or at **100 wt%** where cling modification is applied via migratory additives rather than resin blending. The C6 short-chain branching distribution produces a tie-chain concentration that supports protrusion puncture resistance under **ASTM D5748** at film thicknesses of **12–30 μm**; butene-grade LLDPE of equivalent nominal density and melt index generally requires a **15–20%** increase in gauge to match the puncture energy dissipation of the hexene comonomer at equal elongation. Published property data for CP842-01 in this specific monolayer stretch film configuration is limited; the ranges cited here represent field-observed norms for hexene copolymer LLDPE film grades. Processing runs on a cast film line configured with a **30:1 L/D** barrier-type single-screw extruder, a static mixer, an automatic gauge-control flat die with a **0.7–0.9 mm** die gap, and a matt-finish chill roll held at **15–25 °C**. Melt temperature is maintained within **245–265 °C** to suppress gel formation from localized thermal degradation of the narrow molecular weight distribution, while the chill roll surface temperature is kept below **25 °C** to avoid chill roll release failure and film blocking on the winding core. The film enters a pre-stretch unit operating at **200–300%** mechanical elongation; exceeding **300%** extension at gauge bands created by inherent die lip variation produces localized tear initiation and catastrophic web breaks, a failure mode documented on production lines where oscillating haul-off was disabled. Winding occurs at **400–450 m/min** with tension control and corona treatment at **38–44 dyne/cm** to prepare the film surface for optional label adhesion. Compliance for this application rests on **FDA 21 CFR 177.1520** paragraphs pertaining to olefin polymers, which govern the suitability of the resin for indirect and direct food-contact packaging in secondary distribution, and migration testing under **EU Regulation No 10/2011** applies for films entering the Single Market where overall migration must not exceed **10 mg/dm²**. End products include machine stretch film rolls at **8–30 μm** gauge slit to **450 mm** and **500 mm** widths, hand stretch film rolls, and pre-stretched film for low-tension manual applications. The formulation gradient governing pre-stretch stability is summarised in Table 1.
    CP842-01 loading (wt%)mLLDPE loading (wt%)LDPE loading (wt%)Maximum stable pre-stretch (%)Puncture force trend at 20 μm, ASTM D5748 (N/mm)
    10000220–25010–13
    85150250–2809–12
    702010260–3008–11
    603010280–3207–10

    What Processing Window Governs Thin-Gauge Dart Impact Retention in FFS Sack Blown Film?

    Form-fill-seal tubular blown film for **25 kg** and **50 kg** granular chemical and polymer resin sacks is produced on monolayer or three-layer blown film lines with a die diameter of **200–350 mm**, **2.0–2.5 mm** die gap, and a blow-up ratio of **2.0–2.8**. CP842-01 is blended at **80–100 wt%** with LDPE at **0–20 wt%** in monolayer constructions; in three-layer coextrusions, the virgin hexene LLDPE forms the outer skins at **25–35 wt%** of total layer distribution on each surface, while the core may carry **20–30 wt%** of closed-loop edge-trim regrind without measurable loss of dart drop performance when measured under **ASTM D1709**. Melt temperature is held at **195–215 °C**; exceeding **215 °C** accelerates oxidation-induced gel formation in the narrow-molecular-weight polymer and produces film defects that translate directly into form-fill-seal weld failures at the bag top and bottom seals. Internal bubble cooling is required for throughput stability above **1.5 kg/h per mm of die circumference**, and the frost line height is controlled at **2–4 times the die diameter** to balance machine-direction and cross-direction elongation characteristics. The finished film, at **80–160 μm** gauge, is slit and wound into form-fill-seal roll stock, then fed through a tubular bagging machine operating at **1,800–2,400 bags/h** where the sack is formed by impulse or hot-bar welding, filled with granular product, and sealed under top-closure welding. The critical threshold governing this application is the frost line position: a frost line displaced below the lower limit of the specified range produces excessive cross-direction shrinkage that closes the gusseted opening and interrupts the bag-filling cycle, while an elevated frost line reduces machine-direction tear resistance and generates split defects at the top seal. Compliance for this application depends on customer-specific drop test and stacking specifications derived from **ISO 21898** for flexible intermediate bulk containers, while the film resin itself may require **FDA 21 CFR 177.1520** registration where the sack contacts food-grade granular goods. End products include **25 kg** FFS sacks for petrochemical resin pellets, fertilizer compounds, salt granules, and flour; the sack length-to-width ratio and closure geometry are determined by the filling line spout configuration and the bulk density of the packed product.Flexible geomembrane sheeting fabricated from hexene copolymer LLDPE in flat-die and blown-sheet configurations depends on the elastic recovery and environmental stress crack resistance provided by the C6 comonomer. CP842-01 is compounded at **97–98 wt%** with **2–3 wt%** carbon black masterbatch when a **0.5–2.0 mm** monolithic black sheet is specified; where a hybrid stiffness-flexibility profile is required, the resin is blended with HDPE at **50/50 wt%** to **80/20 wt%** LLDPE/HDPE ratios, and additional stabilizer packages are added at **0.3–0.5 wt%** to protect against thermal oxidation during high-output sheet extrusion at **215–230 °C**. A blend ratio beyond **80/20** LLDPE/HDPE is rarely specified because the flexural modulus rises steeply and the puncture elongation retention measured under **ASTM D4833** declines to values approaching HDPE monolayer sheeting, negating the hexene LLDPE flexibility advantage. Production uses a flat-die sheet extruder of **30:1–33:1 L/D** with a chill roll stack held at **60–80 °C** or a blown-film line operating at a blow-up ratio of **1.5–2.0** for narrower seamless sheeting; thickness is monitored continuously by beta or X-ray gauging with tolerance maintained at **±5%**. The critical process threshold is cooling uniformity: differential shrinkage across the sheet width caused by chill roll temperature gradients exceeding **5 °C** produces edge curl and planar distortion that compromises subsequent field welding. Compliance is governed by **GRI-GM17** for LLDPE geomembranes, which specifies minimum values for thickness, tensile strength under **ASTM D638**, tear resistance under **ASTM D1004**, puncture resistance under **ASTM D4833**, and stress crack resistance under **ASTM D1693**; field seam evaluation follows **ASTM D4437** and **ASTM D6392** for peel and shear properties. End products include pond liners, canal linings, secondary containment basins for chemical storage areas, landfill capping membranes, and temporary storm water retention cells.

    Where Coextruded Sealant Layers Require Low Migration Concurrent with High Abuse Resistance

    In **5-layer** and **7-layer** barrier coextrusions, CP842-01 functions as the sealant skin at **20–40%** of total film thickness, with the core barrier layer of EVOH or polyamide accounting for **5–10%** and tie layers of maleic anhydride-grafted polyethylene at **5–8%**. The hexene LLDPE provides seal initiation at **105–115 °C** on the outer skin while maintaining hot-tack strength under the rapid jaw closure times of vertical form-fill-seal machines operating at **80–120 packages/min**. A critical threshold risk exists at the sealant layer gauge: reducing CP842-01 below **20%** of total thickness increases the probability of seal-through failures at contaminated seal surfaces, while exceeding **40%** displaces barrier layer thickness and elevates oxygen transmission rates beyond product shelf-life limits. The production process uses blown film coextrusion with die gaps of **1.6–2.2 mm** and individual extruder zones maintained at **190–220 °C**; the bubble is internally cooled and the film is drawn through an oscillating haul-off to randomize gauge bands before reaching a reversing winder. Formulation compliance is anchored to **FDA 21 CFR 177.1520** for the olefin polymer sealant layer and **EU Regulation No 10/2011** for overall migration testing not exceeding **10 mg/dm²** of food-contact surface, with specific migration limits for any antioxidants or process stabilizers retained in the resin from upstream pelletization. The compliance matrix governing this application is summarised in Table 2. End products include frozen food pouches, cereal box liners, dried soup mix films, confectionery overwraps, and bag-in-box inner liners. Published data for CP842-01 in high-barrier food-contact coextrusions with EVOH is limited; converter qualification trials are normally required to establish seal initiation curves against specific jaw profiles and contamination conditions.
    RequirementStandard / RegulationTest methodControl limit
    Olefin polymer suitability for food contactFDA 21 CFR 177.1520Extractive analysisAs specified in clause (c)
    Overall migrationEU Regulation No 10/2011EN 1186-110 mg/dm²
    Tensile properties of thin sheetingASTM D882Machine and transverse directionCustomer-defined
    Dart drop impact resistanceASTM D1709Method A, free-falling dartCustomer-defined
    Hot-tack strengthASTM F1921Method A, parallel plateCustomer-defined

    Tunnel Film Tear Propagation and UV Stabilizer Retention Mechanics

    Because seed oil migration and condensation cycling impose specific surface energy requirements, three-layer greenhouse glazing and silage stretch film constructions position CP842-01 in the core layer at **60–70%** of total film mass, with the skin layers reserved for EVA or metallocene LLDPE to carry the high-loading additive packages. The core placement leverages the hexene comonomer's resistance to tear propagation under **ASTM D1922**, while the skins contain UV stabilizer masterbatch at **0.2–1.5 wt%** depending on expected field service life; a **12-month** silage film typically requires **0.2–0.5 wt%**, while a **36-month** greenhouse glazing film demands **1.0–1.5 wt%** HALS and UV absorber combinations. The production process uses a three-layer blown film line with die diameters of **250–400 mm** and die gaps of **1.8–2.4 mm**, with internal bubble cooling and melt temperatures maintained at **190–210 °C**. A process conflict emerges at loading levels above **2.0 wt%** additive masterbatch: screw slippage in the skin extruders caused by lubricity of the carrier resin reduces throughput stability and causes layer-to-layer interfacial instability, observable as wavy film bands and thickness oscillation. Compliance measurements follow **ASTM G154** for accelerated weathering and **ASTM D4329** for UV exposure testing, with retained tensile elongation monitored under **ASTM D882**; European agricultural film specifications may additionally cite **EN 13206:2017** for covering films used in agriculture and horticulture. End products include greenhouse glazing sheets at **150–200 μm**, silage stretch wrap at **25–50 μm**, tunnel crop covers, and soil mulch films where the gas permeability of the hexene LLDPE is tuned through layer arrangement.Where waste containment liners demand a combination of dart drop resistance, seal integrity at folded gussets, and compatibility with post-consumer recyclate streams, blown film converters blend CP842-01 at **70–80 wt%** with **20–30 wt%** post-consumer recyclate LLDPE in the core layer of a three-layer coextrusion, with virgin resin skins at **10–15 wt%** each to preserve surface sealability and odour containment. The film is produced on a blown film line at **190–210 °C** melt temperature and **2.5–3.0** blow-up ratio, with gauge targets of **50–120 μm** and dart drop resistance measured under **ASTM D1709** method A as the primary acceptance criterion. Compliance for healthcare waste liners references **ASTM D1709** for impact failure weight, while municipal waste collection specifications may cite **ASTM D1922** tear resistance and **ASTM D882** tensile properties; if the liners are used for food-soiled waste in a food processing facility, **FDA 21 CFR 177.1520** applies to the virgin food-contact side. End products include institutional can liners, regulated medical waste bags in red and yellow markers, and industrial refuse sacks for hotels and commercial facilities.
    Free Quote

    Competitive LyondellBasell CP842-01 Hexene Copolymer LLDPE Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell CP842-01 is a linear low-density polyethylene resin produced with 1-hexene as the α-olefin comonomer rather than the 1-butene used in conventional C4-LLDPE. Published grade data place the nominal density at 0.918 g/cm³ when measured by ASTM D1505 or ISO 1183, and the nominal melt mass-flow rate at 1.0 g/10 min under ASTM D1238 at 190 °C/2.16 kg or ISO 1133-1:2022; the certificate of analysis remains the controlling document for commercial material. The resin is supplied with a stabiliser package suitable for pelletised handling and film conversion. In film applications, the hexene-derived ethyl side branches introduce a different short-chain branching distribution than butene-derived methyl side branches, producing a polymer architecture that alters tear resistance, dart impact, seal behaviour, and orientation effects relative to C4-LLDPE grades of equivalent density and melt index.

    Why Hexene Comonomer Selection Changes Solid-State Performance

    In ethylene/α-olefin copolymers, the branch length controls the efficiency of crystallinity disruption and the probability of stress-bearing tie-chain formation between adjacent lamellae. 1-Butene contributes a methyl branch, whereas 1-hexene contributes an ethyl branch. The longer C6 branch introduces a higher local free-volume perturbation per comonomer unit, which reduces lamella thickness more effectively and supports a higher population of load-bearing interlamellar tie molecules. The practical consequence is that C6-LLDPE film frequently displays higher dart impact values than C4-LLDPE film at the same density and gauge. Comparative blown-film data for Ziegler-Natta C4 and C6 resins of approximately 0.918 g/cm³ density and 1.0 g/10 min melt index commonly place the C6 dart impact F50 result 30–50% higher when tested by ASTM D1709 method A at 25 µm gauge. This relationship is not a guaranteed property conversion; film processing, die gap, frost line height, and blow-up ratio can narrow or widen the difference.

    The same architectural difference changes Elmendorf tear balance. Values measured by ASTM D1922 typically show C6 films with a more balanced machine-direction and transverse-direction tear ratio than C4 films, provided the bubble is operated at a blow-up ratio above 2.0:1. At low blow-up ratio, machine-direction orientation dominates and can depress machine-direction tear, creating a property cliff-edge that is not visible in standard tensile data alone. Environmental stress crack resistance under ASTM D1693, conditioned in 10% Igepal CO-630 at 50 °C, also separates C6 and C4 products: the hexene architecture extends failure times because the tie-molecule network delays brittle crack propagation through the amorphous phase. For converters, the most useful specification checks are dart impact F50, tear balance at the intended blow-up ratio, and seal initiation temperature rather than a single tensile yield value.

    Tensile properties measured by ASTM D882 on 25 µm blown film provide only a first-pass indication of grade differences because hexene LLDPE and butene LLDPE can have similar yield and ultimate tensile values while differing strongly in impact and tear. Typical C6 film at 0.918 g/cm³ density exhibits machine-direction yield tensile strength in the range of 10–13 MPa, transverse-direction ultimate elongation above 500%, and 1% secant modulus between 140 MPa and 180 MPa. These values do not replace a full qualification on the production line. The most discriminating test set for film applications combines dart impact F50 under ASTM D1709, Elmendorf tear under ASTM D1922, puncture resistance under ASTM D5748, and slow-rate penetration under ASTM D5458 if the article is used in stretch-film or pallet-wrap service.

    Thermal analysis by ASTM D3418 shows a broad endotherm with peak melting between 120 °C and 124 °C for this density class. The associated crystallinity, determined using the 290 J/g reference enthalpy, is usually in the 45–50% range. The reduced peak melting and crystallinity relative to homopolymer high-density polyethylene lower the seal initiation temperature and increase the available hot-tack window on form-fill-seal lines, but they also reduce maximum service temperature.

    In blown-film conversion, CP842-01-class hexene resins are processed on single-screw extruders with 24:1 to 30:1 L/D and barrier or Maddock mixing screws. Temperature profiles usually progress from 170 °C in the feed zone to 190–210 °C in the compression zone, 210–230 °C in the metering zone, and 220–240 °C at the die. Die gaps of 1.8 mm to 2.2 mm are typical for gauges below 50 µm; heavier films may use 2.5 mm gaps to control shear stress at the die lip. If the die gap is reduced below 1.5 mm while output is held constant, shear stress at the die lip can reach the critical level for sharkskin melt fracture. The initial corrective action used in production audits is to increase die temperature or widen the gap rather than to reduce screw speed, because a lower screw speed reduces throughput but may not reduce die-lip shear stress sufficiently. Blow-up ratios from 2.0:1 to 2.5:1 and frost line heights of 8–12 die diameters balance bubble stability, dart impact, and extraction force. Frost line height has a direct effect on residual orientation: a frost line that is too low traps amorphous orientation and may elevate machine-direction shrink measured by ASTM D2732 above the level required for the end-use.

    For cast film operation, chill roll temperatures of 15–25 °C are commonly employed. Faster quench increases film clarity by reducing spherulitic scattering, but excessive quench can increase residual stress and reduce flatness during slitting. The resin does not require routine drying because polyolefins have negligible equilibrium moisture uptake. However, storage at relative humidity above 60% can deposit surface moisture on pellets; a desiccant hopper at 80 °C for 2 h removes surface splay defects in cast film dies and reduces the risk of hydrolysis in any acid-neutralising additive package.

    Roll hardness and slit-edge quality are influenced by the balance of machine-direction and transverse-direction modulus. C6 LLDPE films with higher dart impact may still exhibit lower machine-direction modulus than C4 at the same density, so winding tension should be profiled by roll diameter rather than held constant. Constant-tension winding can create telescoped rolls when the film has a low coefficient of friction measured by ASTM D1894, especially after corona treatment. Corona treatment level, measured in mN/m according to ASTM D2578, is often specified at 38–44 mN/m for lamination and printing grades, but surface treatment does not substitute for proper film formulation.

    When Downstream Converters Substitute C6 Resin into Existing C4 Film Lines

    A change from butene-based LLDPE to CP842-01 should not be treated as a drop-in exchange because melt rheology and solid-state properties shift simultaneously. On single-screw cast film extruders, process logs from comparable C6 grades show that screw torque and die head pressure can differ by 5–10% at constant screw speed and output. The direction of the pressure change depends on molecular weight distribution and shear thinning. A broader-distribution C6 resin may reduce die head pressure relative to a narrow-distribution C4 resin; a narrow-distribution hexene grade may increase pressure. Converter-specific pressure and torque baselines should therefore be recorded before adjusting gear pump speed or melt temperature.

    In blown film, bubble stability may improve because the C6 branch architecture increases strain-hardening during inflation, although it does not match the long-chain branching of autoclave or tubular LDPE. The improvement usually permits a lower LDPE addition in blends than a comparable C4-LLDPE, but the converter should verify dart impact and haze because LDPE addition affects both. The optical values measured by ASTM D1003 and gloss at 60° measured by ASTM D2457 are generally similar for C4 and C6 films at equal density and gauge when the die lip is clean and the frost line is below the point of crystallization-induced surface roughness.

    The primary conflict is tear balance. Dart impact gains under ASTM D1709 are frequently accompanied by a machine-direction tear decline under ASTM D1922 if the blow-up ratio is kept below 2.0:1. Production trials often correct this by increasing blow-up ratio to 2.3:1–2.5:1 and raising frost line height by 10–20% to rebalance transverse orientation. In multi-layer structures, the C6 resin is used in high-toughness sealant plies, while the substrate may remain a C4-LLDPE or HDPE. Seal initiation temperature measured by ASTM F1921 is generally lower for C6 than C4 of equal density because the reduced crystallinity permits molecular diffusion at lower interface temperature. Hot-tack performance in vertical form-fill-seal packaging improves when the sealant layer contains C6 LLDPE, but the exact hot-tack window is line-specific because it depends on dwell time, sealing pressure, and film gauge.

    Compared with metallocene-catalysed hexene LLDPE, conventional C6 grades such as CP842-01 class resins typically display a wider molecular weight distribution. The practical differences are lower die-lip build-up, reduced melt pressure at the same output, and better processing tolerance, but lower dart impact and lower ultimate optical clarity than a well-formulated metallocene LLDPE. The converter’s choice between conventional C6 LLDPE and mLLDPE is therefore controlled by available extruder pressure margin, die gap capability, and whether the film specification values dart impact or haze more heavily.

    Regulatory Compliance Under 21 CFR 177.1520 and EU 10/2011

    In the United States, linear low-density polyethylene copolymers based on ethylene and 1-hexene are addressed by 21 CFR 177.1520(c) 3.1b when the density is below 0.940 g/cm³. Compliance is not granted by resin type alone; the finished article must meet the extraction limits specified in 21 CFR 177.1520(d), and the converter must hold a supplier food-contact statement because additive levels and catalyst residues affect the regulatory determination. In the European Union, the controlling framework is Regulation (EU) No 10/2011. The consolidated regulation lists 1-hexene as an authorised comonomer in Annex I, Table 1. Overall migration testing under EN 1186 and specific migration testing under EN 13130 are applied to the final article, with overall migration limits of 10 mg/dm² or 60 mg/kg depending on packaging geometry and the food-contact surface-to-volume ratio.

    Regulation or standard Scope Key value or test condition
    FDA 21 CFR 177.1520(c) 3.1b Ethylene/1-alkene copolymers for food contact Density 0.905–0.940 g/cm³; extraction per paragraph (d)
    EU 10/2011 Annex I Table 1 Authorised monomer and additive list 1-Hexene listed; SML to be confirmed from consolidated text
    EN 1186 Overall migration in food simulants 10 mg/dm² general; 60 mg/kg infant food
    EN 13130 Specific migration of monomers and additives Simulant selection per food type; time and temperature per contact conditions
    REACH 1907/2006 SVHC declaration < 0.1% w/w candidate list substance
    RoHS 2011/65/EU Homogeneous material heavy metals Pb < 1000 ppm; Cd < 100 ppm; Hg < 1000 ppm; Cr(VI) < 1000 ppm

    Operational boundaries are set by stabiliser chemistry and comonomer architecture. The material should not be held at melt temperatures above 250 °C for extended residence time because oxidative degradation of the phenolic stabiliser can increase yellowness index measured by ASTM E313 and reduce dart impact retention. Abrasive fillers are not recommended in dry blends without hardened screw and barrel metallurgy because film dies operate at narrow gaps where wear becomes a gauge-control problem. Direct copper-alloy contact in high-temperature hot runner components should be avoided where residence times are long because copper ions can catalyse thermo-oxidative chain scission. Published data for CP842-01 in rotational molding, blow molding, or foam extrusion are limited; those processes are outside the documented film application envelope unless the converter performs separate validation on the target machine.

    Top