| HS Code | 775840 |
| Material Type | Linear Low-Density Polyethylene (LLDPE) |
| Form | Natural Pellets |
| Density | 0.920 g/cm³ |
| Melt Index 190 C 2 16 Kg | 0.80 g/10 min |
| Melting Point | 122 °C |
| Vicat Softening Point | 100 °C |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 24.1 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 276 MPa |
| Shore D Hardness | 50 |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength | 250 g |
| Haze | 8% |
| Gloss 45 | 80% |
| Coefficient Of Friction | 0.20 |
| Blocking Strength | 100 g |
As an accredited LyondellBasell CP808-01 Natural Linear, Low-Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell CP808-01 Natural Linear, Low-Density Polyethylene comes in 25 kg polyethylene-lined bags, palletized and stretch-wrapped for shipment. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): LyondellBasell CP808-01 Natural Linear Low-Density Polyethylene supplied in standard palletized bags, secured for safe ocean transport. |
| Shipping | LyondellBasell CP808-01 Natural Linear Low-Density Polyethylene is shipped as non-hazardous resin pellets in 25-kg bags, 1,000-kg octabins, or bulk trucks/railcars. Keep containers closed, dry, and away from heat, sunlight, and ignition sources. Standard freight; no UN hazard class or placard required. |
| Storage | Store LyondellBasell CP808-01 Natural Linear Low-Density Polyethylene in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original containers or bags closed to prevent moisture and contamination. Use clean, segregated storage on stable pallets, avoid excessive stacking, and protect from physical damage. Follow the manufacturer’s SDS and local regulations. |
| Shelf Life | No specific shelf life assigned; stable under normal storage. Keep sealed, cool, dry, away from sunlight, heat, moisture, and contaminants. |
In cast-film stretch-wrap production, the base resin is dry-blended with 15–25 wt% of a lower-crystallinity ULDPE or plastomer and 1.5–3.0 wt% of a polyisobutylene tackifier masterbatch before dosing into the hopper; the natural grade CP808-01 participates at 70–85 wt%, with the remainder adjusted for cold-storage cling performance and peel-force retention over a 90-day warehouse period. Compliance for this packaging format is evaluated under FDA 21 CFR 177.1520(c) for olefin polymers, (EU) No 10/2011 Annex I and III with overall migration limit 10 mg/dm², and REACH (EC) No 1907/2006 Article 33 for SVHC disclosure. The downstream process is a single-screw extruder with 30:1 L/D, barrier screw, melt temperature 232–260 °C, die gap 0.5–0.8 mm, and chill-roll setpoint 18–24 °C; at line speeds above 250 m/min, edge instabilities emerge when the melt curtain oscillates beyond ±2 mm at the die end. The terminal products are machine stretch film, hand stretch film, and pre-stretched rewind film, with tack levels adjusted by the converter to 50–200 g peel force measured by ASTM D5458. Amine-based antifog masterbatches are not recommended in this cast-film process at melt temperatures above 240 °C because chill-roll plate-out becomes visible within 4–6 h of continuous running. Published data for this specific grade in ULDPE-rich cast-film formulations is limited, so converter trials use 100–150 kg scale-up gates before full-line adoption.
| Regulation / standard | Application exposure | Use boundary |
|---|---|---|
| FDA 21 CFR 177.1520(c) | Direct food contact olefin polymers | Natural grade without slip/antiblock is preferred for low-migration film; extractives and density limits apply |
| (EU) No 10/2011 | Plastic food contact materials | Overall migration 10 mg/dm²; specific migration limits for additive masterbatches must be verified under EN 1186 |
| REACH (EC) No 1907/2006 | All industrial conversion | Article 33 SVHC disclosure; Annex XVII restrictions for PAH or phthalate plasticisers not expected in CP808-01 |
| RoHS 2011/65/EU | Electrical/electronic equipment packaging | Applicable only when packaging is integrated into EEE after distribution |
A single-screw grooved-fed extruder with 33:1 L/D is configured for 50–125 µm industrial liner film using CP808-01 at 80–90 wt%, high-pressure LDPE at 10–20 wt%, slip masterbatch at 0.5–1.5 wt%, and synthetic silica antiblock at 0.5–2.0 wt%; the silica loading is raised when ambient warehouse humidity exceeds 60% RH because the natural grade surface is tack-sensitive on the collapsing frame after frost-line solidification. Mechanical compliance is confirmed by ASTM D882 for tensile properties, ASTM D1709 for dart impact, ASTM D1922 for Elmendorf tear, and ASTM D1003 for haze; industrial non-food exposure is documented under REACH (EC) No 1907/2006 Annex XVII and RoHS 2011/65/EU where the liner enters electrical/electronic waste streams. The blown-film process operates at a blow-up ratio of 2.0–3.0:1, die gap 1.2–2.2 mm, melt temperature 190–230 °C, and frost-line height 8–12 die diameters; converters report that gel accumulation at the die lip after 8 h of continuous operation reduces bubble symmetry and must be cleared by short shutdown cycles. Finished product types include pallet covers, heavy-duty shipping sacks, furniture covers, construction vapour barriers, and waste liners.
In extrusion coating for paperboard and aluminium foil liquid packaging, CP808-01 is melt-blended or co-fed with high-pressure LDPE at a ratio of 60–80 wt% CP808-01 to 20–40 wt% LDPE; an ethylene-acrylic acid or maleic anhydride tie concentrate at 5–10 wt% is introduced only when peel adhesion falls below 3 N/15 mm on metallised substrates. The coated structure is tested under FDA 21 CFR 177.1520(c) and (EU) No 10/2011, with migration testing according to EN 1186 and barrier testing according to ASTM F1249 for water vapour and ASTM D3985 for oxygen. The process uses a coat-hanger die with die gap 0.8–1.2 mm, melt temperature 275–320 °C, coat weight 12–20 g/m², and chill-roll temperature 10–18 °C; neck-in from the die edge is measured optically at 10–25 mm per side and is reduced by increasing the LDPE fraction to 40 wt% when line speed exceeds 200 m/min. Terminal products include gable-top cartons, aseptic brick sachets, paper cups, and composite can liners. At melt temperatures above 320 °C, oxidation and odour generation on the extrudate surface become detectable, so the upper setpoint is pinned to 320 °C for taste-sensitive liquid packaging.
| Process | CP808-01 addition ratio | Co-resin / functional additive | Process limit reference |
|---|---|---|---|
| Cast film | 70–85 wt% | ULDPE/plastomer 15–25 wt%; PIB tackifier 1.5–3.0 wt% | Line speed 250 m/min |
| Blown film | 80–90 wt% | LDPE 10–20 wt%; slip masterbatch 0.5–1.5 wt% | BUR 2.0–3.0:1 |
| Extrusion coating | 60–80 wt% | LDPE 20–40 wt%; tie concentrate 5–10 wt% if adhesion < 3 N/15 mm | Melt temp 320 °C |
| Thin-wall injection | 90–100 wt% | EVA/plastomer 0–10 wt%; nucleating agent 0.05–0.15 wt% | Wall thickness 1.5 mm |
| 5-layer coextrusion | 60–80 wt% in skin layers | EVA tie 5–10 wt%; antifog 500–1,500 ppm | Frost-line height 5–8 die diameters |
| Agricultural sheeting | 70–85 wt% | EVA/plastomer 10–20 wt%; carbon black 5–12 wt%; HALS 1,000–3,000 ppm | Screen-pack change 6–8 h |
Thin-wall injection moulding of CP808-01 at shot weights of 15–35 g typically requires the resin to be blended with 0–10 wt% EVA or polyolefin plastomer, 0.05–0.15 wt% nucleating agent, and 0–1.0 wt% slip/antiblock masterbatch for closures; the nucleating agent is omitted for transparent lids because haze measured by ASTM D1003 rises by 2–5 percentage points at 0.15 wt%. Compliance for direct food contact is controlled by FDA 21 CFR 177.1520(c) and (EU) No 10/2011, with mechanical performance measured by ISO 178 flexural modulus and ASTM D638 tensile yield stress; the latter falls below 11 MPa when mould temperature is kept below 10 °C. The injection machine is set with barrel temperatures 180–230 °C, mould temperature 15–30 °C, injection pressure 60–100 MPa, and clamp force 80–150 tonnes depending on cavity count; cooling time for 1.0–1.5 mm walls is 6–12 s, above which sink marks become visible on the flat lid surface. The finished products are thin-wall food containers, margarine tubs, snap-over lids, and dosing closures. Published data for CP808-01 in thin-wall injection moulding is limited, so production validation uses short-shot studies and gate-seal time checks on each mould change.
In five-layer blown-film lines producing 25–80 µm fresh-cut salad bags and frozen vegetable films, CP808-01 is distributed in the skin layers at 60–80 wt% of the layer, with an EVA-based tie or plastomer at 5–10 wt% in adjacent layers; the core may contain 20–30 wt% of recycled reprocessed trim that is food-contact approved under FDA 21 CFR 177.1520(c) and (EU) No 10/2011. Antifog masterbatch is added to the inner skin at 500–1,500 ppm by mass, and migration limits are verified with EN 1186 overall migration testing at 10 mg/dm²; gas barrier is measured by ASTM F1249 and ASTM D3985 with oxygen transmission below 2,500 cm³/(m²·day·atm) for the target polyolefin-only structure. The coextrusion process uses a 5-layer annular die with gap 1.6–2.4 mm, melt temperature 190–230 °C, blow-up ratio 2.0–2.8:1, and frost-line height deliberately maintained at 5–8 die diameters because lower frost lines increase haze by 3–6 percentage points on the outer skin. Terminal product types include fresh-cut salad bags, frozen vegetable films, cheese shrink bags, and polyolefin lidding film. Avoid fluorinated processing aids in the food-contact skin layers unless covered by a valid FCN or equivalent national authorisation.
Conversion of CP808-01 into 200–500 µm agricultural silage sheeting begins with pellet blending of the resin at 70–85 wt%, an EVA or plastomer at 10–20 wt%, carbon black masterbatch at 5–12 wt%, and hindered amine light stabiliser at 1,000–3,000 ppm; the carbon black loading is pushed above 8 wt% only when UV protection requirements are specified under ISO 4892-2 for greater than 3,000 h of accelerated weathering. Regulatory compliance for this non-food application is documented under REACH (EC) No 1907/2006 Annex XVII, and if the film is used in facilities covered by RoHS 2011/65/EU, the carbon black masterbatch must be checked for restricted PAH content. The extrusion process is a flat-die or blown-film line with melt temperature 190–240 °C, die gap 2.0–3.0 mm, blow-up ratio 2.0–2.8:1 for blown film, and haul-off speed set to deliver 200–500 µm gauge; at carbon black loadings above 8 wt%, melt pressure rises by 15–25% and screen-pack changes are required every 6–8 h to prevent gel breakdown. Terminal product types include silage stretch film, greenhouse covers, temporary enclosure film, and geomembrane base sheets for vapour barriers.
Competitive LyondellBasell CP808-01 Natural Linear, Low-Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell CP808-01 Natural is identified by the manufacturer as an uncolored linear low-density polyethylene pellet grade. The material is a copolymer of ethylene and an α-olefin; because the short product designation does not identify the comonomer type, the branching architecture and catalyst residue profile must be confirmed from the lot-specific technical datasheet. The “Natural” designation refers to the absence of colorant, not to the absence of stabilizers, neutralizers, or processing-aid packages. In the absence of a lot certificate, no slip agent, antiblock agent, or ultraviolet stabilizer should be assumed. The grade is generally assigned to the conventional Ziegler-Natta LLDPE class, distinguished from metallocene-catalyzed LLDPE by broader molecular weight distribution and higher extrusion stability under shear. CAS registration for the final polymer depends on the comonomer and is therefore lot-dependent; the ethylene homopolymer CAS registry number 9002-88-4 is not sufficient to describe the copolymer. Packaging is typically 25 kg polyethylene-lined bags, octabins, or bulk silo containers. Because LLDPE is nonhygroscopic, routine predrying is unnecessary for surface moisture; however, storage at relative humidity above 60 % can increase surface moisture and should be managed by controlled warehouse conditions.
The density and melt flow rate of CP808-01 define the grade’s position between low-density polyethylene and high-density polyethylene. A nominal density of 0.918 g/cm³ measured according to ISO 1183-1:2019 or ASTM D1505-18 places the material in the linear low-density range and limits crystallinity to approximately 35–40 % by differential scanning calorimetry. The melt flow rate determined at 190 °C with 2.16 kg load is approximately 1.0 g/10 min under ISO 1133-1:2022 and ASTM D1238-23. Melt flow rate in this range corresponds to a high-viscosity film resin with sufficient melt strength for blown-film bubble stability but too high for thin-gauge cast film without a higher melt temperature or processing aid. The density controls the balance between stiffness and puncture resistance: higher density increases the flexural modulus and lowers environmental stress-cracking resistance, while lower density increases impact resistance but reduces tensile strength and film blocking resistance. Converters should not substitute a similar melt index LLDPE from another supplier without comparing the full molecular weight distribution, because viscosity-shear response and back-pressure behavior diverge even at equivalent melt flow rate.
| Property | Standard method | Unit | Typical value |
|---|---|---|---|
| Density at 23 °C | ISO 1183-1:2019 / ASTM D1505-18 | g/cm³ | 0.918 |
| Melt flow rate 190 °C/2.16 kg | ISO 1133-1:2022 / ASTM D1238-23 | g/10 min | 1.0 |
| Tensile yield stress | ISO 527-2:2012 / ASTM D638-22 | MPa | 11 |
| Elongation at break | ISO 527-2:2012 / ASTM D638-22 | % | 800 |
| Flexural modulus, 1 % secant | ISO 178:2019 / ASTM D790-17 | MPa | 260 |
| Dart drop impact, 50 µm blown film | ASTM D1709-22 | g | 250 |
| Elmendorf tear strength MD, 50 µm film | ASTM D1922-23 | N/mm | 20 |
| Haze, 50 µm film | ASTM D1003-21 | % | 12 |
| Vicat softening temperature A/50 | ISO 306:2022 / ASTM D1525-17e1 | °C | 100 |
| Melting peak temperature | ISO 11357-3:2018 / ASTM D3418-21 | °C | 122 |
On production-scale blown-film lines with grooved-feed single-screw extruders of 25:1 to 30:1 L/D and barrier screw designs, CP808-01 Natural is processed at adapter melt temperatures between 190 °C and 220 °C. Barrel profiles should be flat to reverse profile to control shear heating; screw speeds on a 60 mm extruder are typically 40–80 min⁻¹, with observed melt pressure at the breaker plate from 250 bar to 350 bar depending on screen pack condition. Die gaps for low-density linear film are commonly set between 1.2 mm and 2.5 mm, and blow-up ratios of 2.0:1 to 3.0:1 balance tensile properties and bubble stability. Frost-line height should be maintained at 5 to 9 die diameters; a low frost-line height increases quench rate and improves dart impact but may reduce tear strength in the machine direction. When high outputs are required, internal bubble cooling and dual-lipped air rings reduce bubble instability, but the higher shear viscosity of LLDPE can increase motor load by 10–20 % relative to a comparable LDPE of the same melt index. Screen-pack filtration of 100–250 µm and purging with a film-grade LDPE or a dedicated LLDPE purge compound is recommended before shutdown; extended residence time above 180 s at melt temperatures above 240 °C promotes gel formation and accumulation on die lips.
Cast film and extrusion-coating operations with CP808-01 Natural are constrained by the grade’s conventional LLDPE melt strength, which is lower than LDPE. On a 75 mm or 90 mm extruder feeding a slot die at 230–260 °C, output above 250 kg/h can induce draw resonance if the draw ratio exceeds approximately 20:1 or if the die-to-chill-roll air gap exceeds 100 mm. Draw resonance appears as periodic gauge bands in the machine direction and is measured by ±2 % or larger deviation in film thickness using an online beta gauge. To suppress thickness oscillations, the air gap is reduced to 60–100 mm, the chill-roll temperature is held at 15–25 °C, and edge pinning is set at ±15 mm outside the die width. Neck-in at the die edges is typically higher for LLDPE than LDPE; on a 900 mm die, neck-in values of 25–50 mm per edge are observed depending on melt temperature and draw distance. LLDPE also produces lower odor and lower heat-seal initiation temperature than HDPE but requires higher motor torque than LDPE. A fluoropolymer processing aid or an LLDPE-compatible processing additive at 0.02–0.05 wt% is effective in delaying melt fracture and reducing die lip build-up. The use of a chilled air knife or vacuum box at the chill roll improves contact and reduces air entrainment, but the grade’s natural slip and antiblock levels are insufficient for high-speed cast film needing low coefficient of friction.
Compliance for CP808-01 Natural must be established through the manufacturer’s lot certification because the natural designation does not automatically confer food-contact status. In the United States, olefin polymers may be evaluated under FDA 21 CFR 177.1520; the regulation covers ethylene-α-olefin copolymers and permits use in food contact when the density and melt flow criteria and overall and specific migration limits of the final article are met. The converter is responsible for demonstrating that the finished structure, including any added masterbatch, adhesive, or tie resin, meets the applicable conditions of use. For the European Union, plastic food-contact materials are assessed under EU Regulation 10/2011, which requires overall migration testing in simulants and specific migration limits for monomers and additives. No SVHC disclosure under REACH Regulation (EC) No 1907/2006 should be assumed without a written supplier declaration. The polymer itself is usually exempt from REACH registration, but monomers and intentionally added substances require registration or authorization. For electrical and electronic applications, RoHS Directive 2011/65/EU restricts levels of lead, cadmium, mercury, hexavalent chromium, PBB, and PBDE in homogeneous materials; LLDPE may comply when the total formulation is free of these substances above the specified 0.1 wt% or 0.01 wt% cadmium threshold. A certificate of analysis for each lot is required because natural grades can contain catalyst residues, neutralizers, and processing stabilizers that affect product conformity.
| Regulation / standard | Scope | Status |
|---|---|---|
| FDA 21 CFR 177.1520 | Olefin polymers for food contact; natural grade evaluation | Candidate for use; must be listed in lot certification |
| EU Regulation 10/2011 | Plastic materials and articles intended for food contact | Overall migration and SML compliance required per final article |
| REACH Regulation (EC) No 1907/2006 | SVHC disclosure and registration | Polymer exempt from registration; monomers/intermediates require supplier confirmation |
| RoHS Directive 2011/65/EU | Restriction of hazardous substances in electrical and electronic equipment | Pb, Cd, Hg, Cr(VI), PBB, PBDE limits apply |
In blown-film conversion for high-strength industrial liners, CP808-01 Natural is utilized in monolayer and coextruded structures at film thicknesses from 50 µm to 200 µm. The film exhibits an Elmendorf tear strength in the machine direction above 20 N/mm at 50 µm and a dart drop impact above 250 g when tested under ASTM D1709-22, which supports applications such as frozen vegetable bags and heavy-duty sacks. In form-fill-seal packaging, seal initiation temperatures are measured on a laboratory heat sealer at 95–115 °C at 0.5 MPa seal pressure and 0.5 s dwell; seal strength above 10 N/15 mm is attainable when the film contains no antiblock particle that reduces seal integrity. The grade is also processed as a core layer in stretch film where the surface layers contain cling additives; because the natural resin contains no tackifier, the core layer contributes puncture resistance measured by ASTM F1306 while the skin layers govern unwind characteristics. Agricultural silage film and greenhouse film are viable only with ultraviolet stabilizer masterbatch addition; unstabilized LLDPE loses mechanical integrity after outdoor exposure and is not suitable for multi-season use. For extrusion coating and laminating, the resin is processed at melt temperatures of 230–260 °C onto paper, board, or aluminium foil, with adhesion controlled by the substrate’s surface treatment and the resin’s thermal oxidative stability. Published data for this specific CP808-01 configuration in coextruded barrier film is limited; conversion trials with the final structure are required to establish seal performance, gauge uniformity, and coefficient of friction.
The main differentiation of CP808-01 Natural from high-pressure LDPE is molecular architecture. LDPE contains long-chain branching and has higher melt strength, lower tensile yield, lower dart impact, and lower environmental stress-cracking resistance than a linear short-chain-branched LLDPE of comparable density. Typical LLDPE tensile yield stress is in the 10–12 MPa range versus 8–10 MPa for LDPE, while flexural modulus is usually 200–300 MPa versus 150–250 MPa depending on crystallinity. HDPE, with density above 0.940 g/cm³, provides higher modulus and higher upper service temperature but inferior slow-crack-growth resistance; CP808-01 Natural is therefore selected for applications requiring low-temperature impact and stress-crack resistance rather than maximum stiffness. Compared with metallocene-catalyzed LLDPE, a conventional Ziegler-Natta LLDPE typically has broader molecular weight distribution, which reduces extrusion pressure at high shear and improves bubble stability but may produce lower clarity and lower dart-impact values. In addition, mLLDPE grades usually have narrower melting distribution and lower extractable content. CP808-01 Natural, if processed without a slip or antiblock package, may exhibit higher film-to-film blocking than formulated grades; coefficient of friction measured under ASTM D1894-14 may exceed 0.6 on natural monolayer film. This limitation requires addition of a slip masterbatch or use in a coextruded structure. Other polyethylene products containing pre-dispersed slip, antiblock, or ultraviolet stabilizer packages should not be replaced by CP808-01 Natural on a weight-for-weight basis without reformulation. Lot-to-lot variation in melt flow rate and density is controlled by the manufacturer but should be monitored by melt flow rate and density testing per ISO 1133-1:2022 and ISO 1183-1:2019 during incoming inspection.
Storage at ambient temperatures below 40 °C and relative humidity below 60 % is recommended to prevent moisture pickup and additive migration. The resin should be introduced into the extruder hopper at 20–30 °C to avoid condensation and screw bridging. Predrying is not normally required; if surface moisture is observed after outdoor storage, a desiccant dryer at 60–70 °C for 2–4 hours may be applied, but higher temperatures or longer residence can cause pellet agglomeration. The melt should not exceed 280 °C; above this threshold, oxidative degradation generates low molecular weight fractions, visible gels, and odor. The grade is incompatible with strong oxidizers and with processing conditions that create long adiabatic residence times. Combination with amine-based additives in masterbatches requires verification because of potential interactions with residual catalyst and stabilizer systems; thermal stability of the final compound may be assessed by ISO 11357-6 or ASTM D3895.