Lyondellbasell Cp80 01 Linear Low Density Polyethylene

LyondellBasell CP80-01 Linear Low-Density Polyethylene

    • Product Name: LyondellBasell CP80-01 Linear Low-Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 112283
    Grade CP80-01
    Polymer Type Linear Low-Density Polyethylene (LLDPE)
    Density 0.920 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.8 g/10 min
    Melting Point 121 °C
    Vicat Softening Temperature 90 °C
    Tensile Strength At Yield 10 MPa
    Tensile Strength At Break 20 MPa
    Tensile Elongation At Break 800%
    Tensile Modulus 250 MPa
    Flexural Modulus 240 MPa
    Shore Hardness D 50
    Brittleness Temperature -70 °C
    Thermal Conductivity 0.33 W/m·K
    Water Absorption <0.01%
    Environmental Stress Crack Resistance >1000 h

    As an accredited LyondellBasell CP80-01 Linear Low-Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell CP80-01 LLDPE is supplied in 25 kg polyethylene-lined bags, palletized and stretch-wrapped for industrial handling.
    Container Loading (20′ FCL) 20′ FCL container loaded with palletized 25 kg bags of LyondellBasell CP80-01 Linear Low-Density Polyethylene, securely stowed for ocean shipment.
    Shipping LyondellBasell CP80-01 Linear Low-Density Polyethylene is shipped as non-hazardous resin pellets. Standard packaging includes 25 kg bags, octabins, or bulk trucks/railcars. It is not regulated for DOT, IMDG, or IATA transport. Store in a dry, clean area away from heat and direct sunlight.
    Storage Store LyondellBasell CP80-01 Linear Low-Density Polyethylene in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original bags sealed, palletized, and off the floor to prevent moisture, dust, and contamination. Avoid prolonged UV exposure. Maintain ambient temperatures, practice first-in, first-out rotation, and protect from physical damage. Use clean handling equipment.
    Shelf Life LyondellBasell CP80-01 LLDPE has an indefinite shelf life if kept cool, dry, sealed, and away from heat, sunlight, and contaminants.
    Application of LyondellBasell CP80-01 Linear Low-Density Polyethylene

    In monolayer and three-layer blown film structures where CP80-01 linear low-density polyethylene is the dominant ethylene α-olefin copolymer, the main processing conflict is the loss of bubble stability when the melt has not been blended with sufficient high-pressure LDPE. Processors running single-screw extruders of 50–120 mm diameter with 24:1–30:1 L/D and barrier screws set melt temperatures at 188–228°C at the adapter before an annular die with lip gap 1.4–2.2 mm, blow-up ratio 2.2:1–3.0:1, and frost-line height 300–800 mm. On IBC-equipped lines, dual-lip air-ring velocity is typically held at 10–18 m/s with IBC pressure 100–250 Pa to stabilize the bubble; vertical sine-wave deformation appears when internal pressure is increased too rapidly at low frost-line positions. The addition ratio for heavy-duty sack and agricultural film is 85–95 wt% CP80-01 with 5–15 wt% LDPE; frozen-food and clarity film use 10–20 wt% LDPE, antiblock masterbatch 0.5–2.0 phr, and slip masterbatch 0.2–0.8 phr. Where bulk handling occurs at relative humidity above 60%, surface condensation creates gel-like specks; pellets require conditioning in a hopper dryer at 70°C for 1 h to reduce surface moisture below 0.05%.

    For food-contact film, the downstream converter’s declaration of conformity rests on 21 CFR 177.1520(a)(3)(i) and (EU) No 10/2011 Annex I Table 2 with overall migration below 10 mg/dm² specified in Article 12; non-food films are classified under ASTM D4976. Finished product types include heavy-duty sacks, frozen-food film, collation film, agricultural mulch film, and stretch hoods. Lot-to-lot dart impact is measured per ASTM D1709, Elmendorf tear per ASTM D1922, haze per ASTM D1003, and gloss per ASTM D2457. Published extensional viscosity data specific to CP80-01 is limited; when bubble flutter appears above a blow-up ratio of 3.0, melt tension should be measured per ISO 16790 against a reference LDPE before changing die gap, because die gap reduction below 1.4 mm increases axial draw and helical instability on some IBC-equipped lines.

    Which Melt Curtain Defects Limit CP80-01 in Cast Stretch Film Lines?

    Cast stretch film lines expose CP80-01 to draw resonance and edge neck-in rather than bubble instability. The formulation addition ratio is 70–90 wt% CP80-01, 10–30 wt% LDPE or metallocene PE as a process aid, polyisobutylene tackifier at 1–4 wt%, and antiblock masterbatch at 0.1–0.3 phr. Extruders from 75 mm to 150 mm diameter with 30:1 L/D feed a flat die with lip gap 0.5–0.8 mm; melt temperature is held at 210–240°C, and the curtain is pinned to a chill roll at 16–22°C. Line speed runs from 200 m/min to 600 m/min, with the die-to-chill-roll air gap set between 60 mm and 150 mm. When line speed exceeds the critical draw-resonance threshold, periodic gauge bands appear at 5–15 Hz and are corrected by reducing air gap or increasing melt temperature within the specified window. Automatic beta gauges on production lines keep two-sigma thickness variation below 1.5% for machine stretch film.

    Compliance for fresh produce wrap and other food-contact film requires 21 CFR 177.1520 and (EU) No 10/2011; industrial stretch wrap is specified under ASTM D4976. Terminal product types are machine stretch film, hand stretch film, silage wrap, and bundling film. Edge bead thickness increases when CP80-01 content exceeds 30 wt%; on some lines, edge bead reaches 15–25% above nominal web thickness unless the die edge temperature is reduced by 5–10°C through external deckle heaters.

    Pulverized CP80-01 for rotational molding starts as 35-mesh powder with bulk density 0.38–0.46 g/cm³ measured per ASTM D1895 method A and dry flow below 35 s/50 g. The formulation ratio is 100 parts CP80-01, antioxidant masterbatch at 0.05–0.2 phr, UV stabilizer at 0.2–0.8 phr for outdoor parts, and colorant at 0.2–2.0 phr. Rotational molding machines operate with a primary-to-secondary axis speed ratio of 4:1, primary rotation at 5–8 rpm, secondary rotation at 1–2 rpm, oven setpoint 260–320°C, and peak internal air temperature 190–205°C. Peak internal air temperature below 190°C creates pinholes from incomplete sintering, while sustained temperature above 210°C accelerates thermo-oxidative degradation and raises the final melt index of the part surface. Post-mold cooling is staged from 0.5°C/min to 10°C/min to reduce warpage; uneven mold wall thickness causes differential shrinkage and is controlled through powder flow and axis speed ratio.

    Compliance for potable water tanks requires NSF/ANSI/CAN 61 and 21 CFR 177.1520; chemical containers are verified against ASTM D1998-21. Finished parts include vertical storage tanks, agricultural spray tanks, hoppers, and kayaks. Environmental stress crack resistance is evaluated on molded plaques per ASTM D1693 where chemical exposure is specified by the end-user.

    When Extrusion Coating Laminators Require Curtain Stability Above 150 m/min with CP80-01-Containing Blends

    The inclusion of CP80-01 in extrusion coating is normally limited to 10–30 wt% with 70–90 wt% high-pressure LDPE, because higher CP80-01 content increases neck-in and edge bead at line speeds above 150 m/min. For foil lamination, an ethylene acrylic acid or ethylene methyl acrylate tie resin at 5–15 wt% may replace part of the LDPE. Coating lines use single-screw extruders of 65–120 mm diameter and 26:1–32:1 L/D, a T-slot die with lip gap 0.5–0.8 mm, melt temperature 280–320°C, die-to-nip air gap 150–250 mm, coating weight 10–40 g/m², and chill roll temperature 10–18°C. Neck-in after coating is observed as the difference between die width and finished web width; values above 30–60 mm per side are corrected by resin ratio or die temperature adjustment. Converters verify the melt index per ISO 1133-1:2022 at 190°C/2.16 kg before qualifying a formulation above 150 m/min.

    Compliance for liquid packaging board and aseptic bricks is based on 21 CFR 177.1520 and (EU) No 10/2011, with finished laminate migration tested according to the intended food simulants. Terminal product types include liquid packaging board, aseptic brick coatings, paper cup liners, and foil lamination webs for sachets.

    Injection Moulding Gate Freeze-Off and the Low-Melt-Index LLDPE Thin-Wall Flow Restriction

    Injection moulding of CP80-01-rich compounds is constrained by gate freeze-off and flow-length-to-thickness ratio. A formulation of 60–85 wt% CP80-01 with 15–40 wt% HDPE improves modulus and cycle time; slip masterbatch is added at 0.5–2.0 phr, and impact modifiers are adjusted with reference to ISO 6603 puncture data. Processing on hydraulic or all-electric machines uses melt temperature 200–245°C, mould temperature 15–40°C, injection velocity 50–150 mm/s, holding pressure 50–90 MPa, and clamp force scaled at 3–5 kN/cm² of projected area. Gate diameter below 0.8 mm freezes off prematurely; hot-runner tips of 1.2–2.0 mm diameter are required for thin-wall flow lengths exceeding 150:1. Thin-wall parts below 1.5 mm show higher pressure drop and short-shot frequency unless injection speed is raised within the specified range.

    Compliance for food-contact housewares rests on 21 CFR 177.1520; electronic packaging requires RoHS 2011/65/EU; material specification follows ASTM D4976. Finished product types include pails, lids, caps, housewares, and cable reel flanges. Shrinkage anisotropy in CP80-01-rich parts is higher than in HDPE; tooling is dimensioned using linear shrinkage measurements per ISO 294-4 after 48 h conditioning at 23°C and 50% RH.

    Sheet Extrusion for Geomembrane Cores Uses a Different Thermo-Oxidative Load Than Film

    Flat-die sheet lines running CP80-01/HDPE blends for geomembrane cores operate at 0.75–2.5 mm thickness. The formulation addition ratio is 20–60 wt% CP80-01 with 40–80 wt% HDPE, plus carbon black masterbatch at 2–3 wt% to reach 2.0–2.5% carbon black dispersion. Extruders of 100–200 mm diameter with 33:1 L/D feed flat dies of 2–8 m width; the three-roll stack is held at 60–90°C, and post-cooling length is 20–40 m. The sheet is embossed or textured during calendering to provide interface friction. Surface oxidation risk is highest during line stops; when line speed drops below 1 m/min, the die and roll gap must be purged to avoid brittle oxidized edges.

    Compliance is anchored to ASTM D6693 for tensile, ASTM D5199 for thickness, ASTM D5397 for notched constant tensile load, ASTM D4833 for puncture, ASTM D3895 and ASTM D5885 for oxidative induction time, and GRI GM13 for HDPE geomembrane specification. Finished product types include landfill liners, pond liners, mining heap leach pads, and secondary containment.

    Test methodStandard designationMeasured parameter
    Tensile propertiesASTM D6693Yield strength, break strength, elongation
    ThicknessASTM D5199Minimum average thickness and lowest individual reading
    Notched constant tensile loadASTM D5397Resistance to stress cracking
    Puncture resistanceASTM D4833Puncture resistance at failure
    Oxidative induction timeASTM D3895 / ASTM D5885Thermal oxidative stability
    Free Quote

    Competitive LyondellBasell CP80-01 Linear Low-Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell CP80-01 Linear Low-Density Polyethylene belongs to a polyolefin class whose density region, melt rheology, and mechanical response are governed by copolymer chain architecture rather than by the commercial grade designation alone. The term linear low-density refers to a copolymer of ethylene with an alpha-olefin such as butene-1, hexene-1, or octene-1, where short-chain branches interrupt crystallinity and reduce density below that of high-density polyethylene. Published data for this specific configuration is limited; the grade designation CP80-01 does not disclose the comonomer type, density, melt flow rate, or additive package, and the supplier technical bulletin must be treated as the normative specification.

    Because LLDPE lot properties may vary within a producer’s release window, converters should request the certificate of analysis and the current safety data sheet before compounding or converting CP80-01. A change in density as small as 0.002 g/cm³ can shift the sealing onset temperature and the stiffness of a finished film, while a change in melt flow rate of 0.3 g/10 min can alter extrusion backpressure and motor load on a production extruder.

    Grade Designation and Polyethylene Class Boundaries

    The CP80-01 grade designation functions as a commercial identifier rather than a numerical specification. In polyethylene classification systems such as ASTM D4976 and ISO 17855-1:2014, a linear low-density polyethylene is defined by density rather than by catalyst type. The density bracket of 0.915 g/cm³ to 0.940 g/cm³ separates the class from low-density polyethylene and high-density polyethylene. Melt flow rate determined according to ISO 1133-1:2022 at 190 °C under 2.16 kg is the most commonly used processing specification, but a single LLDPE grade family may include several melt flow rates, additive packages, and comonomer levels. For CP80-01, the typical LLDPE property envelope should be used only for preliminary screening; the certificate of analysis is normative.

    PropertyTest methodLDPE classLLDPE classHDPE class
    DensityASTM D792-200.910–0.925 g/cm³0.915–0.940 g/cm³0.941–0.970 g/cm³
    Melt flow rateISO 1133-1:2022 at 190 °C/2.16 kg0.2–70 g/10 min0.5–25 g/10 min0.1–50 g/10 min
    Tensile yield strengthISO 527-26–12 MPa10–25 MPa20–35 MPa
    Crystallinity by DSCASTM D341830–45%35–55%60–80%
    Vicat softening temperatureISO 306, A5080–95 °C90–115 °C115–130 °C

    The values listed in the table are class-level literature ranges and are not release limits for CP80-01. Grade-specific values must be taken from the LyondellBasell technical bulletin and the certificate of analysis for the production lot.

    How Does CP80-01 Differ from Conventional LDPE and HDPE?

    Differences between CP80-01 and other polyethylene grades are governed by molecular architecture rather than by commercial designation. High-pressure low-density polyethylene contains long-chain branching that produces strain-hardening behavior in extensional flow, high melt strength, and stable bubble formation in film blowing. Linear low-density polyethylene typically possesses shorter, more regularly spaced branches and lower melt extension viscosity; bubble stability is therefore achieved through die geometry, air-ring configuration, and melt temperature rather than through intrinsic long-chain branching. Against high-density polyethylene, LLDPE has lower crystallinity and a lower modulus, but generally higher environmental stress-cracking resistance and higher dart impact and puncture resistance at comparable film thickness.

    The lower crystallinity of LLDPE reduces the sealing onset temperature compared with HDPE and often provides a broader hot-tack window than high-pressure LDPE at equivalent coating weight. The absence of long-chain branching, however, reduces melt strength and may require a narrower die gap, a higher blow-up ratio, or a fluoropolymer processing aid to delay melt fracture when a linear low-density resin of the CP80-01 class is run on equipment optimized for LDPE.

    In blown-film conversion on a 70 mm single-screw extruder with a 30:1 L/D barrier screw, a grooved feed throat, and a 1.8 mm die gap, linear low-density polyethylene is typically processed at melt temperatures of 190 °C to 240 °C, with die temperatures held 5 °C to 15 °C below the adapter temperature to reduce melt fracture. The bubble is formed at a blow-up ratio of 2.0:1 to 3.0:1 and a frost-line height of 4 to 8 die diameters, depending on film gauge and cooling-air velocity. Production-scale film lines may require a dual-lip air ring calibrated for low pressure and high air volume because LLDPE has lower melt tension than high-pressure LDPE and can oscillate under high-velocity cooling air. Bubble instability observed as helical motion or flutter is often corrected by raising the melt temperature 5 °C to 10 °C, reducing the blow-up ratio, or adding a fluoropolymer processing aid at 200 ppm to 800 ppm; the processing aid level must be verified for CP80-01 because the additive package may already contain slip and antiblock agents.

    When a Film Resin Is Compared Across Butene, Hexene, and Octene Comonomer Chemistries

    When a linear low-density resin is copolymerized with butene-1, the resulting short-chain branches are predominantly ethyl groups, and the distribution of branch lengths is narrow. Hexene-1 introduces butyl branches, and octene-1 introduces hexyl branches; the longer branch length can increase the efficiency of tie-molecule formation and improve dart impact, puncture resistance, and tear propagation under ASTM D1709, ASTM D5748, and ASTM D1922 testing. If CP80-01 is a hexene- or octene-based grade, its toughness at equivalent density and melt flow rate may exceed that of a butene-based LLDPE, but the absolute difference depends on catalyst type, molecular weight distribution, and film fabrication conditions. Published data for this specific configuration is limited; comparative testing on one film line using the same die gap and bubble geometry is required.

    The published technical bulletin for CP80-01 constitutes the limiting specification.

    Because the CP80-01 designation is not accompanied by a public numerical datasheet in accessible literature, the grade cannot be specified without the current supplier technical bulletin, certificate of analysis, and safety data sheet. For a typical LLDPE film resin, the supplier release limits commonly cover density by ISO 1183-1:2019 or ASTM D792-20, melt flow rate by ISO 1133-1:2022 at 190 °C/2.16 kg, tensile properties by ISO 527-2, dart impact by ASTM D1709, tear strength by ASTM D1922, and Vicat softening temperature by ISO 306. The values that apply to CP80-01 are not transferable from other LyondellBasell LLDPE grades; each grade can differ in density by 0.002 g/cm³ to 0.010 g/cm³ and in melt flow rate by 0.2 g/10 min to 2.0 g/10 min. A change of 0.005 g/cm³ in density alters the modulus and heat-seal response enough to affect film line settings and final bag performance.

    PropertyStandard methodMeasurement conditionTypical specification purpose
    Melt flow rateISO 1133-1:2022190 °C, 2.16 kgGrade identification and extrusion pressure
    DensityISO 1183-1:201923 °C, gradient columnResin classification and stiffness
    Dart impactASTM D1709, Method A25 µm filmToughness and puncture resistance
    Elmendorf tearASTM D192225 µm film, MD and TDDirectional tear resistance
    Tensile yieldISO 527-250 mm/minLoad-bearing capability
    Vicat softeningISO 306, A5010 N, 50 °C/hHeat resistance for hot-fill contact

    Melt Processing Windows, Screw Selection, and Thermal Stability Limits

    Linear low-density polyethylene of the CP80-01 class is processed on single-screw extruders with 24:1 to 30:1 L/D barrier or high-shear mixing screws. Grooved feed sections improve solids conveying and reduce pressure fluctuations; however, the higher shear heating in grooved feed extruders can raise melt temperature beyond the set barrel temperature. The processing window for a film-grade LLDPE is generally bounded by onset of melt fracture at low temperature and by oxidative degradation at high temperature. Melt temperatures below 190 °C may produce high melt viscosity and surface melt fracture, while sustained exposure above 250 °C accelerates oxidation and may generate gels in film. The actual motor load depends on melt flow rate and die restriction; converters should measure melt pressure before a breaker plate and avoid prolonged residence time above 250 °C.

    Pre-drying is not generally required for polyethylene stored in sealed containers below 60% relative humidity. If the resin has been opened and stored at relative humidity above 60%, surface moisture may generate defects in cast film or increase moisture-related bubble instability; a desiccant dryer set at 60 °C to 80 °C for 2 h to 4 h can be used. The resin should not be combined with strongly oxidizing masterbatches or with acid-catalyzed concentrates without supplier verification because polyethylene can degrade under prolonged contact with strong oxidizing agents.

    Qualification for food-contact use in the United States is typically evaluated under 21 CFR 177.1520, which covers olefin polymers and defines extractable limits and density-based temperature conditions. European food-contact evaluation falls under EU Regulation 10/2011 with an overall migration limit of 10 mg/dm² for plastic food-contact materials. REACH registration and Safety Data Sheet compliance are required for sale in the European Union; RoHS Directive 2011/65/EU applies only to electrical and electronic equipment and not automatically to all film packaging. A grade-specific regulatory letter for CP80-01 should be requested because dual-use additives and catalyst residues can affect the conformity assessment.

    For monolayer cast stretch film, the resin is extruded through a flat die with a 0.5 mm to 1.0 mm die gap and quenched on a chill roll held at 15 °C to 30 °C; the high draw-down can cause edge neck-in and draw resonance, and the line speed is limited by the melt strength of the grade. In blown-film bag applications, the grade is processed against extruder backpressure, bubble cooling demand, and seal-bar temperature settings that must be derived from the CP80-01 technical bulletin rather than from class-level LLDPE data.