LyondellBasell Aquathene FR420000 W&C, LLDPE
-
Product Name:
LyondellBasell Aquathene FR420000 W&C, LLDPE
-
Factroy Site:
Yinchuan, Ningxia, China
-
Price Inquiry:
sales8@ascent-chem.com
-
Manufacturer:
Ascent Petrochem Holdings Co., Limited
-
CONTACT NOW
-
LyondellBasell Aquathene FR420000 W&C, LLDPE is typically used in formulations when melt flow index and density, and processing temperature and extrusion pressure must be controlled within specific ranges.
Specifications
|
HS Code
|
177998
|
| Density |
1.28 g/cm³ |
| Melt Flow Rate |
0.5 g/10 min |
| Tensile Strength At Break |
13.8 MPa |
| Elongation At Break |
200% |
| Flexural Modulus |
483 MPa |
| Hardness Shore D |
50 |
| Melting Point |
125 °C |
| Vicat Softening Point |
90 °C |
| Brittleness Temperature |
-40 °C |
| Volume Resistivity |
1.0E15 ohm·cm |
| Dielectric Constant |
2.6 |
| Dissipation Factor |
0.002 |
| Limiting Oxygen Index |
32% |
| Ul 94 Rating |
V-0 |
| Halogen Content |
0% |
| Smoke Density |
Low |
| Water Absorption |
0.1% |
| Flame Retardant |
Yes |
| Low Smoke Zero Halogen |
Yes |
| Moisture Curable |
Yes |
As an accredited LyondellBasell Aquathene FR420000 W&C, LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
Packing & Storage
| Packing |
Supplied in 25 kg moisture-barrier bags, palletized for storage and transport: LyondellBasell Aquathene FR420000 W&C LLDPE. |
| Container Loading (20′ FCL) |
20′ FCL container loaded with LyondellBasell Aquathene FR420000 W&C LLDPE in palletized 25 kg bags, securely stowed and sealed for export. |
| Shipping |
LyondellBasell Aquathene FR420000 W&C, LLDPE typically ships as a non-hazardous, moisture-sensitive wire-and-cable compound in sealed moisture-barrier bags or boxes on pallets. It is generally not DOT/IMDG/IATA regulated. Protect from moisture, heat, and contamination; use standard dry freight and material-handling equipment. |
| Storage |
Store LyondellBasell Aquathene FR420000 W&C, LLDPE in original, sealed packaging in a cool, dry, well-ventilated warehouse. Keep away from direct sunlight, heat, moisture, ignition sources, and incompatible materials. Protect from contamination, punctures, and excessive stacking. Store on pallets off the floor with adequate spacing. Use first-in-first-out rotation and follow supplier SDS/local regulations. |
| Shelf Life |
Shelf life: 6 months from manufacture when stored unopened in a cool, dry area, away from moisture and direct sunlight. |
Application of LyondellBasell Aquathene FR420000 W&C, LLDPE
In single-core low-voltage cable insulation lines, Aquathene FR420000 W&C LLDPE is introduced after conductor preheating, with the preheater set to a surface temperature between 60 °C and 90 °C for bare copper and up to 110 °C for tinned copper, depending on line speed. The compound is fed into a single-screw extruder with an L/D ratio of 24:1 to 30:1, a barrier screw with a compression ratio of 2.5:1 to 3.5:1, and a screen pack of 80/100/120 mesh. Melt temperature at the die is maintained in the 160–180 °C band, measured by infrared thermocouple at the breaker plate; head pressure is normally 10–25 MPa depending on die land length and line speed. The insulation enters a segmented water trough with first-stage temperature at 20–30 °C and second-stage at 10–15 °C to limit frozen-in stress. Spark testing is performed online per IEC 62230 or UL 1581 after the cooling section, because flame-retardant fillers can introduce micrometer-scale pinholes that are not visible to manual inspection. Tensile verification is carried out per IEC 60811-501, with elongation measured on dumb-bell specimens conditioned at 23 °C for 24 h. Where a colour concentrate must be introduced, it is metered at 2–3 wt% using a gravimetric feeder; the concentrate carrier must be LLDPE-compatible and should not contain stearate lubricants above 0.5 wt%. The compound is not used above its voltage rating unless the design passes partial discharge testing; published data for this specific configuration is limited, so each conductor size must be qualified on the production crosshead rather than transferred from a different tooling set.
What Limits the Extruder Envelope When Hydrated Mineral Flame-Retardant Fillers Are Present?
Extruder throughput is governed less by torque than by the decomposition threshold of the flame-retardant system. If the compound contains hydrated mineral fillers, chemically bound water is released at approximately 180–220 °C; at melt temperatures above 190 °C, the resulting water vapour forms micro-voids that lower dielectric strength and produce surface roughness on the jacket. The safe operating melt temperature on production equipment is normally 155–175 °C at the die, with the screw zones set at 140 °C in the feed section, 150 °C in the compression section, 160 °C in the metering section, 160 °C at the head, and 165 °C at the die. This is not a universal setting; it describes the boundary condition for hydrated mineral-filled flame-retardant LLDPE compounds of this product category. A deviation of ±5 °C is tolerable at the die; overshoot beyond 170 °C may not appear immediately but can emerge during 72 h humidity ageing as a reduction in breakdown voltage. Residence time above 170 °C should be kept below 15 min. If relative humidity exceeds 60%, the granulate is pre-dried at 70–80 °C for 3–4 h in a desiccant hopper dryer. The vent port is operated open to atmosphere rather than under vacuum; vacuum can pull water out of the filler inside the barrel and create melt fracture. Capillary rheometry data on unfilled LLDPE show a pseudoplastic plateau at apparent shear rates below 100 s−1, but the filled material requires shear rates of 200–1000 s−1 in the die land to prevent shark-skin. When die lip temperature fluctuates more than 3 °C within one minute, the output may show periodic diameter variation. Processors should record melt temperature, head pressure, and screw speed at 5 min intervals, because flame-retardant filler dispersion degrades if the screw and barrel are worn; the acceptable screw/barrel clearance is below 0.3 mm for a 90 mm extruder. The product should not be diluted with unfilled LLDPE above 10 wt% unless the cable standard allows a lower flame classification, because dilution reduces oxygen index in a non-linear manner and may create batch-to-batch combustion variability.When FR420000 W&C Replaces Unfilled LLDPE Jacketing in Control Cable Lines
In control cable sheathing, replacement of an unfilled LLDPE with a flame-retardant LLDPE compound requires recalibration of die draw-down ratio, cooling length, and print adhesion. Because the flame-retardant filler increases melt density and decreases die swell, the outer diameter may differ at the same tip and die settings. Processors usually adjust draw-down ratio by 5–15% relative to the unfilled compound, or change the die orifice according to the supplier batch certificate. The extruded jacket is cooled in a segmented water trough with first-stage water temperature at 20–25 °C and second-stage at 10–15 °C; higher first-stage temperature reduces frozen-in stress but slows heat removal for thick jackets. Shrinkback is checked per IEC 60811-508 on a 1 m sample placed in a forced-air oven at 100 °C for 1 h; flame-retardant LLDPE commonly shows higher shrinkback than unfilled LLDPE when the draw-down ratio is excessive. Flame propagation is evaluated on the finished cable per IEC 60332-1-2; if the specification requires low-smoke zero-halogen performance, acid gas is measured per IEC 60754-2 and smoke density per IEC 61034-2. Not all flame-retardant LLDPE grades pass these three tests simultaneously; batch selection should be confirmed with the supplier certificate of analysis. Pulling lubricants used during cable installation must be silicone-free; silicone can migrate into the flame-retardant jacket surface and reduce ink adhesion. Printing is done with an ink system based on a cyclohexanone-free, non-aromatic vehicle and an adhesion promoter approved for polyolefin jackets. A surface energy sufficient for ink adhesion is verified by ISO 8296 test inks; typical polyolefin jacket surfaces require at least 38–42 mN/m after flame or corona treatment. The final product is a control cable jacket with printed identification and bundle flame performance, intended for conduit and tray installation.Armored cable bedding lines encounter a different first-order constraint: melt fracture at low line speed and incomplete filling of interstices between steel wire armoring and the outer jacket. The bedding compound is extruded through a crosshead with a pressure-relief die having a land length ratio of 10:1 to 15:1; the inner die diameter is selected at least 0.5 mm larger than the maximum cable core diameter to prevent wiping and orientation of the bedded layer. Because the steel armor acts as a heat sink, melt temperature at the die is held at 150–165 °C and the steel wire is preheated with induction heating to 40–60 °C before entering the crosshead. The screw is set with a rear barrel temperature 5–10 °C lower than the front zones; this reduces surging caused by filler compaction in the feed section. A vented barrel with open vent is preferred, but the vent must be checked for filler buildup every 8 h. The bedding layer is typically applied at 1.5–2.5 mm nominal thickness for steel wire armored cables; the ratio of bedding thickness to armour wire diameter is kept above 0.8:1 in cable plants to prevent outer jacket penetration. Incomplete penetration into the armour interstices creates air gaps that increase flame spread in bundle testing; bundle combustion performance is verified per IEC 60332-3-24 or EN 50266-2-4. Diameter control is measured with a laser gauge and logged continuously; variation above ±0.05 mm on a 2 mm bedding wall usually indicates screen pack blockage or unstable hopper bridging. The compound is not a substitute for water-blocking filling compounds; if longitudinal watertightness is required, a separate water-swellable tape or yarn must be used. The end product is the bedded core assembly that passes into the outer jacket head without intermediate reheating.UV-Exposed Jacket Qualification in Photovoltaic Array Interconnects
In outdoor photovoltaic array interconnects, ultraviolet exposure, wet heat, and low-temperature bending are evaluated simultaneously. A flame-retardant LLDPE base compound is not inherently UV stable; the outdoor grade must incorporate a carbon black or hindered amine stabiliser package. For PV array interconnects, the cable standard EN 50618 requires long-term thermal endurance at 120 °C, weather resistance per EN 50396 or UL 4703 sunlight resistance, and wet electrical testing after conditioning in 85 °C / 85% RH. The jacket compound is tested for tensile strength and elongation at break per IEC 60811-501 before and after ageing; oxidation is indicated by loss of elongation beyond the standard limit. The extrusion line for PV jacket must avoid copper contamination; transition metal impurities catalyse degradation and are checked by a melt filtration test or by IEC 60811-410. Because halogen-free flame-retardant LLDPE compounds often contain mineral fillers, insulation resistance is measured at 500 V DC for 1 min after water immersion. If the compound is not specified for direct burial, a separate mechanical protection layer is required. The outdoor service boundary for this material class is typically -25 °C to +70 °C at the conductor unless the manufacturer’s certificate of analysis states a higher continuous temperature rating. Carbon black content, when required for UV stabilisation, is maintained at 2.0–3.0 wt% in the final jacket compound and must be pre-dispersed rather than added as a powder at the hopper.Instrumentation and Communication Cable Sheathing in Process Automation
Process automation networks route cables through cable trays, conduits, and junction boxes in refineries and pharmaceutical plants where flame-retardant jackets must survive mechanical abrasion and exposure to cleaning chemicals. The LLDPE-based compound provides higher environmental stress crack resistance than HDPE and is therefore evaluated by ASTM D1693-15, condition B, with a 10% Igepal CO-630 solution. Sheathing extrusion is performed on a 20:1 to 25:1 L/D single-screw extruder at melt temperature 150–175 °C; the jacket is applied over twisted pairs or triads with an overall screen. The flame-retardant filler changes the effective dielectric environment of the cable, so electrical performance is measured per IEC 60502-1 for low-voltage power control cables or per IEC 61156-1 for digital communication cables. Cold bend testing at -25 °C is conducted per IEC 60811-504; no cracks are allowed when the mandrel diameter matches the declared cable diameter. The material is not suitable for continuous contact with strong acids, ketone-based solvents, or chlorinated hydrocarbons; incidental splash resistance should be confirmed by immersion testing per ISO 1817. Where low-smoke zero-halogen performance is required, flame propagation, smoke density, and acid gas are tested on the complete cable rather than on the jacket alone because the bedding, screen tape, and insulation contribute to the fire load. The batch-to-batch MFI variation should be checked by ISO 1133-1:2022 at 190 °C / 2.16 kg against the supplier value; deviations above ±0.2 g/10 min may require screw speed adjustment to maintain jacket wall thickness. A colour masterbatch for identification is limited to 1–2 wt% addition in this sheathing grade; higher addition levels can reduce tensile elongation below the acceptance criterion for flexible automation cables.
Free Quote
Competitive LyondellBasell Aquathene FR420000 W&C, LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at
+8618005193850
or mail to
sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Inquiry
Get Free Quote of Ascent Petrochem Holdings Co., Limited
Flexible payment, competitive price, premium service - Inquire now!
Certification & Compliance
-
LyondellBasell Aquathene FR420000 W&C, LLDPE is manufactured under an ISO 9001 quality system and complies with relevant regulatory requirements.
-
COA, SDS/MSDS, and related certificates are available upon request.
For certificate requests or inquiries, contact: sales8@ascent-chem.com.
More Introduction
LyondellBasell Aquathene FR420000 W&C is identified in supplier-controlled documentation as a linear low-density polyethylene (LLDPE) formulation intended for wire and cable manufacturing. The suffix W&C denotes a wire-and-cable-specific grade within the Aquathene family, while the FR prefix indicates a flame-retardant additive package; the numerical designation 420000 separates the product from adjacent lower- and higher-filled grades. Engineering evaluation is conditioned on the current LyondellBasell technical data sheet, because independent public reproductions of the product’s full property set are limited. The material is supplied in pellet form and processed on conventional polyolefin extrusion lines; however, the presence of flame-retardant additives alters melt-phase rheology relative to unfilled LLDPE resins. Lot acceptance testing references ISO 1133-1:2022 for melt mass-flow rate and ISO 1183-1:2019 for density. The grade is not intended for thin film, blow molding, or injection molding applications; its additive package and melt stability are tuned for cable jacket and insulation extrusion.
Melt rheology and barrel temperature governance on single-screw extrusion lines
On conventional single-screw extruders with L/D 24:1 to L/D 30:1 and compression ratios from 2.5:1 to 3.5:1, a filled LLDPE compound requires a reverse or flat temperature profile rather than a steep positive ramp. Melt temperature at the die must remain within the limits printed in the grade-specific processing guide; for many flame-retardant LLDPE systems, the upper control limit is 230 °C, although exact boundaries depend on additive chemistry. Barrel zones may be set at 160 °C in the feed section, rising to 200 °C to 220 °C at the metering section, with die head pressure controlled by staged screen packs. These values define a processing envelope for minimization of screw-slip and melt-fracture in mineral-filled polyolefins; they are not substitutes for the supplier’s certificate. Batch-to-batch variation in flame-retardant filler particle size distribution can shift melt pressure at constant screw speed; a 0.5 MPa upward trend is often used as a control alarm limit on production-scale equipment.
What limits extrusion throughput when running Aquathene FR420000 W&C?
Throughput in flame-retardant LLDPE is governed less by motor amperage than by the melt-pressure boundary at the breaker plate. Because the melt contains dispersed flame-retardant particles, a screen pack with 20/40/60/80 mesh staged layers can raise head pressure relative to unfilled resin; the pressure increase is a function of filler loading and screen retention, and no universal value applies. Production-scale observations on single-screw machines show that pressure oscillations above 1.0 MPa per 10 rpm increment often indicate insufficient screw recovery in the feed zone and incipient melt fracture at the die lip. The limiting screw speed is therefore set by the maximum acceptable melt temperature and the pressure drop across the filtration stack, not by theoretical conveying capacity. Melt filtration is critical because flame-retardant particle agglomerates larger than 0.25 mm produce surface teardrops and spark-test failures on finished cable. Shear heating in the metering section scales with screw speed squared; when adiabatic temperature rise exceeds 15 °C above the barrel setpoint, the excess energy can degrade the LLDPE backbone and release volatile additive fragments. Twin-screw compounding lines with L/D 40:1 and side feeders are used for concentrate dilution; if the compound is run as a ready-to-use pellet on a single-screw line, downstream melt pumps are not normally required unless line speeds exceed 300 m/min.
Flame-retardant performance in LLDPE wire-and-cable compounds is influenced by the decomposition endotherm of the mineral hydrate phase when the route is non-halogenated; the release of water absorbs heat and dilutes fuel gases, but it also generates internal pressure in the melt if extrusion temperatures exceed the dehydration onset, typically 180 °C to 200 °C for aluminum trihydrate-based systems. For halogenated systems, the active chemistry operates through gas-phase radical scavenging, and acid-gas emission during combustion is measured under IEC 60754-2. In either case, the exact additive package in Aquathene FR420000 W&C is not stated in all public documents, so emission class, oxygen index, and smoke density must be confirmed from the supplier safety data sheet and performance certificate. Cable evaluations generally require vertical flame propagation testing under IEC 60332-1-2, with smoke density evaluated to IEC 61034-2 and pH/conductivity by IEC 60754-2 when halogen-free classification is sought. The presence of LLDPE as the base polymer provides lower flexural modulus than HDPE-based alternatives and improved stress-crack resistance relative to LDPE, but the flame-retardant additive increases compound density and reduces melt elongation compared to unfilled LLDPE. Storage at relative humidity above 60 % can raise moisture uptake in filled systems; drying to residual moisture below 0.05 wt% is required before extrusion to avoid pinholes.
When replacing unfilled LLDPE jacketing with a flame-retardant grade
Substitution is not a drop-in viscosity change. Unfilled LLDPE processes with stable melt strength at die temperatures from 190 °C to 220 °C, but the filled grade may require a higher die temperature to reduce surface roughness because mineral particles disrupt the melt-fracture boundary. Shrinkage after extrusion also changes; filled compounds typically exhibit lower longitudinal shrinkage but higher transverse die swell, requiring calibration of the cooling trough. Mechanical properties shift: tensile elongation at break generally falls from values above 600 % for unfilled LLDPE to a lower interval in filled systems, while tensile strength may remain in the 10 MPa to 15 MPa range, but the exact values depend on filler type and loading. These comparisons are generic to LLDPE wire-and-cable compounds; published data for this specific configuration is limited and must not be inferred as grade-specific.
Comparative evaluation against unfilled LLDPE jacket material
| Attribute | Unfilled LLDPE | Flame-retardant LLDPE grade | Reference method |
| Melt mass-flow rate | Resin-dependent, generally higher | Lower due to filler | ISO 1133-1:2022 |
| Density | Base resin range near 0.918–0.935 g/cm³ | Elevated by flame-retardant filler | ISO 1183-1:2019 |
| Tensile strength at break | Upper range for neat LLDPE | Reduced or similar depending on adhesion | ISO 527-2:2012 |
| Elongation at break | Above 600 % | Lower, application-dependent | ISO 527-2:2012 |
| Flame propagation | No inherent vertical-flame rating | Evaluated to cable flame standards | IEC 60332-1-2 |
In quality-control laboratories, lot acceptance for a flame-retardant wire-and-cable LLDPE compound is structured around three classes of measurement: melt-flow stability, mechanical properties, and flame performance. Melt mass-flow rate is measured at 190 °C under 2.16 kg in accordance with ISO 1133-1:2022; density is measured by ISO 1183-1:2019; tensile properties by ISO 527-2:2012 using type 1A specimens. The supplier’s certificate of analysis should be matched to the production lot and stored for regulatory inspection. Processing incompatibilities arise when the compound is mixed with other wire-and-cable materials containing peroxide crosslinking agents; premature crosslinking during extrusion can produce gels and screen-pack pressure spikes. Avoid direct combination with amine-based stabilizer packages when halogenated flame retardants are present, because amine-halogen interactions can generate corrosive species and reduce long-term thermal stability. Regulatory documentation for supply into the European Union should include REACH registration and RoHS Directive 2011/65/EU statements where applicable; these are not product specifications but compliance markers.