Lg Chemical Keyflex Pbt Gf30 Fr Bt 1030gfn

LG Chemical Keyflex® PBT+GF30%-FR BT-1030GFN

    • Product Name: LG Chemical Keyflex® PBT+GF30%-FR BT-1030GFN
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 659712
    Density 1.60 g/cm3
    Glass Fiber Content 30%
    Flame Retardancy UL94 V-0
    Tensile Strength 120 MPa
    Elongation At Break 2.5%
    Flexural Modulus 9000 MPa
    Flexural Strength 180 MPa
    Notched Izod Impact Strength 8 kJ/m2
    Heat Deflection Temperature At 1 82 Mpa 200 °C
    Melting Point 225 °C
    Mold Shrinkage 0.2-0.6%
    Water Absorption 0.04%
    Melt Processing Temperature 240-270 °C
    Mold Temperature 60-80 °C

    As an accredited LG Chemical Keyflex® PBT+GF30%-FR BT-1030GFN factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LG Chemical Keyflex® PBT+GF30%-FR BT-1030GFN is packaged in 25 kg moisture-barrier bags on pallets.
    Container Loading (20′ FCL) Container Loading (20′ FCL): 25 kg bags of LG Chemical Keyflex® PBT+GF30%-FR BT-1030GFN, palletized, shrink-wrapped, and secured for ocean export.
    Shipping LG Chemical Keyflex® PBT+GF30%-FR BT-1030GFN is shipped as dry, non-hazardous thermoplastic pellets in moisture-barrier bags, boxes, or octabins. Keep containers closed and protect from moisture, heat, and sunlight. Handle under normal industrial conditions; no special transport classification is typically required.
    Storage Store LG Chemical Keyflex® PBT+GF30%-FR BT-1030GFN in a cool, dry, well-ventilated area away from direct sunlight, heat, moisture, and ignition sources. Keep containers tightly closed, undamaged, and in original packaging. Protect from physical damage, excessive temperatures or humidity, and prolonged UV exposure. Follow local regulations and the manufacturer’s SDS for safe stacking, handling, and shelf-life.
    Shelf Life Typically 12 months in unopened original packaging, stored cool, dry, and away from direct sunlight and moisture.
    Free Quote

    Competitive LG Chemical Keyflex® PBT+GF30%-FR BT-1030GFN prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LG Chemical Keyflex BT-1030GFN is a 30 % glass-fibre-reinforced, flame-retardant polybutylene terephthalate injection-moulding grade. The model code identifies the material as a structural electrical-grade polyester in the Keyflex BT family; GFN denotes glass-fibre reinforcement combined with a flame-retardant package. The compound is intended for electromechanical components that require UL 94 V-0 flammability performance in thin wall sections while retaining stiffness for snap-fits, terminal retention, and connector shells. It is not a general-purpose unfilled PBT. Under ISO 1043-1, the symbolic term is PBT-GF30 FR, but the exact flame-retardant code and data block must be taken from the supplier’s technical datasheet and UL Yellow Card. Typical applications include relay bobbins, motor end caps, power-tool housings, circuit-breaker housings, ignition components, and charging connectors.

    Material identity, datasheet traceability, and representative values

    The values in Table 1 are representative dry-as-moulded data and should not be interpreted as batch acceptance limits. Glass-fibre orientation, specimen gating, mould temperature, and pigment loading alter the physical properties of the moulded part. The data are generated according to injection-moulded specimen preparation and testing standards recognized for product comparison, but they do not replace end-part testing at final wall thickness.

    Table 1 — Representative physical and mechanical property values for LG Chemical Keyflex BT-1030GFN
    PropertyTest standardRepresentative valueUnit
    Density, 23 °CISO 1183-11.62g/cm³
    Water absorption, saturation, 23 °CISO 620.05%
    Mould shrinkage, 2 mm plaque, flow / transverseISO 294-40.3–0.8%
    Tensile stress at break, 5 mm/minISO 527-2/1A125MPa
    Tensile strain at break, 5 mm/minISO 527-2/1A2.5%
    Flexural modulus, 2 mm/minISO 1789,800MPa
    Flexural strength, 2 mm/minISO 178190MPa
    Charpy notched impact, 23 °CISO 179-1/1eA7.5kJ/m²
    Izod notched impact, 23 °CISO 180/A7.0kJ/m²
    Heat deflection temperature, 1.82 MPaISO 75-2/Af200°C
    Heat deflection temperature, 0.45 MPaISO 75-2/Bf220°C
    Melting temperature, DSC second heatISO 11357-3225°C
    Rockwell hardnessISO 2039-2R 120—
    Flammability, 0.8 mm thicknessUL 94V-0class

    The reported tensile stress at break of 125 MPa to ISO 527-2/1A is a dry-as-moulded reference value. The tensile strain at break of 2.5 % indicates a brittle, fibre-dominated failure mode; design should avoid high local strain at sharp corners, gate vestiges, and poorly radiused snap-fits. Stress concentrations can initiate cracking before the bulk material reaches yield. The notched Izod and Charpy values are lower than those of unfilled PBT because glass fibres behave as stress concentrators at the notch root, so impact loading should be distributed over large radii or ribbed sections. North American programmes that cross-reference ASTM D638-14 or ASTM D790-17 should not treat ASTM and ISO values as interchangeable because specimen shape, span, and strain rate differ.

    What injection-moulding constraints govern BT-1030GFN processing?

    Drying is mandatory. The pellets should be dried in a desiccant hopper dryer at 120 °C for 4–6 h to a residual moisture target below 0.02 %. Moisture beyond this threshold reduces molecular weight through hydrolysis at melt temperature. The immediate evidence is splay at gate regions, reduced tensile stress at break, and intermittent dielectric-withstand failure on thin-wall mouldings. On production floors with relative humidity above 60 %, an uncovered machine hopper can introduce enough atmospheric moisture within 30–60 min to compromise the melt. A closed hopper with dried-air feed and dew-point monitoring at -40 °C or lower is required, and the dew-point record should be logged rather than visually inspected.

    The injection unit should use an abrasion-resistant screw with 20:1 L/D and a compression ratio of 2.2:1–2.5:1. Glass-fibre reinforcement causes predictable wear on screw flights, check ring, and nozzle tip; nitrided or bimetallic surfaces are standard. Melt temperature measured by a needle pyrometer should be maintained between 250 and 265 °C, with barrel zones set from rear 240–250 °C, centre 250–260 °C, front 255–265 °C, and nozzle 250–260 °C. At melt temperatures above 270 °C, the flame-retardant package undergoes thermal degradation that can produce plate-out on mould surfaces, gloss variation, and marginal UL 94 performance after regrind. Residence time at melt temperature should not exceed 10 min; short recovery time and a smaller shot size relative to barrel capacity are preferred.

    Mould temperature is specified between 60 and 100 °C. Higher mould temperature in the 80–100 °C band improves knit-line strength and surface finish but extends cycle time and may increase mould fogging if volatile degradation products are present. Lower mould temperature can be used for fast cycles, but thin sections may freeze before adequate packing, causing sink and warp. Packing pressure is typically 60–100 MPa hydraulic, with hold time based on gate seal, normally 4–8 s for cold-runner parts of 2–3 mm wall. Back pressure should be low, 0.3–0.7 MPa, to avoid fibre-length reduction and frictional heat. Screw surface speed should be limited to 50–100 rpm; higher shear rates reduce fibre length and notched impact without efficiently increasing melt temperature.

    Tooling for BT-1030GFN requires generous runner diameters and polished channels to reduce residence time and fibre accumulation. Hot-runner manifolds should be externally heated with no dead spots; internally heated systems can form unmelted glass-fibre mats at low-flow gates. Venting depth should be 0.01–0.02 mm with land length 2–3 mm to prevent gas burn marks. On production-scale machines of 350–500 t clamp, valve-gated hot runners have shown gate blush defects when injection velocity exceeds 200 mm/s through small 1.0–1.5 mm gates. Reducing gate velocity and raising mould temperature often removes the blush but increases cycle time. Sequential valve gating can improve knit-line strength when multiple gates are necessary. Knit lines in glass-fibre-reinforced flame-retardant PBT are mechanically weak because fibres do not cross the knit plane; weld-line strength is usually below 50 % of the base material strength, so knit lines should be placed in low-stress zones.

    When dimensional stability, dielectric integrity, and flame performance dictate grade selection

    BT-1030GFN is selected where a flame-retardant polyester provides an alternative to polyamide 66, thermosets, or flame-retardant polycarbonate blends in connectors, relay bobbins, motor end caps, power-tool housings, circuit-breaker housings, and ignition components. The 30 % glass loading produces a flexural modulus near 9,800 MPa to ISO 178, which permits reduced wall stock without losing snap-fit rigidity. The post-mould shrinkage of 0.3–0.8 % reduces tolerance stack-up across multi-cavity tools. In humid service, the moisture uptake is 0.05 % at saturation to ISO 62, far below that of PA66-GF30; this leads to lower dimensional change and dielectric shift after exposure to ambient humidity. However, the grade must still be evaluated for hydrolytic stability at high coolant or drainage temperatures.

    Compared with unfilled flame-retardant PBT, BT-1030GFN raises heat deflection temperature at 1.82 MPa from roughly 70–90 °C to 200 °C; the trade-off is a fall in tensile strain at break to 2.5 % and a brittle fibre-governed failure mode. Compared with standard GF30 PBT without flame retardant, the FR package can lower notched impact and change colour stability under thermal ageing. The flame-retardant additives also influence comparative tracking index; for electrical spacing decisions, values of 200–250 V in glass-filled flame-retardant PBT are common but must be verified with the supplier’s certificate to IEC 60112. Glow-wire end-product tests depend on final part thickness, colourant, and regrind level more than on the base polymer alone.

    Against PA66-GF30 flame-retardant compounds, BT-1030GFN offers lower processing temperature and lower moisture sensitivity, but a lower heat deflection temperature, typically 200 °C versus 235–250 °C for PA66-GF30 FR. PBT also tends to show better resistance to automotive fuels, greases, and many common hydrocarbons than PA66, but inferior resistance to strong alkaline cleaning agents and hydrolysis in hot water above 80 °C. Compared with PC/PBT flame-retardant blends, BT-1030GFN usually has lower multi-axial impact, greater modulus, better chemical resistance to fuels, and a narrower processing window because the semicrystalline PBT solidifies rapidly. PC/PBT may be preferred when ductility dominates; the glass-fibre network in this polyester provides creep resistance at elevated temperature and low moisture uptake.

    Published data for BT-1030GFN in long-term hydrolytic ageing at 95 °C in water/glycol mixtures is limited; coolant-contacting components require end-use validation. The resin should not be used for direct food-contact packaging, implantable medical parts, or outdoor UV-exposed applications without a stabilised variant or coating. In relay bobbins, winding tension and terminal insertion impose hoop and punching stresses. Fibre orientation around terminal holes determines whether cracking initiates; moulding simulation with anisotropic fibre orientation and measured pressure-dependent specific volume should replace isotropic assumptions. For power-tool housings, drop-impact failures often occur at bosses and screw posts because GF30 FR PBT has low notched impact. Boss designs should use conical cores, generous radii, and avoid gate placement directly into the boss. Mould temperature in the upper range of 80–100 °C improves knit-line toughness and reduces stress cracking around inserts.

    Without third-party certification data, the end-use flammability claim is incomplete

    Compliance for BT-1030GFN is not established by a single property sheet; it is a combination of UL Yellow Card data, RoHS and REACH declarations, and finished-part testing according to product-specific standards. The UL Yellow Card supplies material flammability performance at specified thickness and colour families; it should be checked before first article inspection because colours and regrind levels can change the V-0 rating.

    Table 2 — Typical verification matrix for flame-retardant electrical components
    Compliance areaStandard or regulationVerification basis
    Flammability of moulded plaqueUL 94V-0 at 0.8 mm
    Comparative tracking indexIEC 60112Supplier reported; verify at end-use thickness
    Glow-wire flammability indexIEC 60695-2-12End-product testing required at final wall thickness
    Glow-wire ignition temperatureIEC 60695-2-13End-product testing required
    RoHS hazardous substancesDirective 2011/65/EUSupplier declaration and analytical audit
    REACH SVHC screeningRegulation (EC) No 1907/2006Supplier SDS and SVHC screening

    On production lines, the material should be sampled for melt volume-flow rate at the start of a shift, and a small flammability plaque should be stamped with lot number and cavity temperature. Variation in flame-retardant distribution can occur if the barrel is allowed to overheat during a hot-runner fault; parts from any thermal excursion above 270 °C should be quarantined and cannot be assumed to retain UL 94 V-0 performance. Regrind should be kept below 20 % by weight for electrical products unless the part is re-evaluated for flammability and impact. Fibre length decreases on each melt pass, so repeated regrind reduces modulus and notched impact at the same glass loading.

    In low-voltage switchgear and electric-vehicle charging connectors, the material is normally processed with a mould temperature of 80–100 °C, a short screw recovery time, and closed-loop conveying to prevent moisture reuptake. The combination of 30 % glass fibre and flame retardant creates higher melt viscosity than unfilled PBT; therefore, injection pressure and clamp force requirements are higher, and thin-wall flow length is limited. Published data for spiral flow at 2 mm wall thickness is limited; tool fill simulations should use measured Cross-WLF coefficients from the supplier rather than applying unfilled PBT flow data. The grade should not be exposed to amine-based mould releases, amine-cured epoxy potting compounds, or strong alkaline cleaning baths because these environments accelerate hydrolysis and can extract flame-retardant components. Batch-to-batch drift in flame-retardant content is typically controlled by the supplier’s weight-loss and flammability screening, but incoming inspection of bulk density and melt volume-flow rate is a practical indicator of glass-content drift.

    Top