| HS Code | 726480 |
| Materialcomposition | PBT + 15% Glass Fiber |
| Density | 1.41 g/cm3 |
| Moldingshrinkage | 0.4-0.8% |
| Tensilestrength | 95 MPa |
| Tensileelongationatbreak | 3.0% |
| Flexuralmodulus | 5000 MPa |
| Flexuralstrength | 145 MPa |
| Charpynotchedimpactstrength | 5 kJ/m2 |
| Heatdeflectiontemperatureat1 82mpa | 200 °C |
| Vicatsofteningtemperature | 210 °C |
| Rockwellhardness | M90 |
| Waterabsorption | 0.06% |
| Ul94flammability | HB |
| Volumeresistivity | 1E15 ohm·cm |
| Dielectricstrength | 20 kV/mm |
| Dielectricconstant | 3.5 |
| Dryingtemperature | 120 °C |
| Dryingtime | 3-4 h |
| Melttemperature | 240-260 °C |
| Moldtemperature | 60-80 °C |
As an accredited LG Chemical Keyflex® PBT+GF15% BT-1015GF factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LG Chemical Keyflex® PBT+GF15% BT-1015GF is packed in 25 kg moisture-proof bags, 40 bags per pallet (1,000 kg). |
| Container Loading (20′ FCL) | 20′ FCL container loaded with LG Chemical Keyflex® PBT+GF15% BT-1015GF, securely packed and stowed for export shipment. |
| Shipping | LG Chemical Keyflex® PBT+GF15% BT-1015GF is a non-hazardous thermoplastic resin (PBT with 15% glass fiber), not regulated as dangerous goods. Ship in dry, sealed bags or containers, protected from moisture, heat, and direct sunlight; no special transport requirements apply. |
| Storage | Store LG Chemical Keyflex® PBT+GF15% BT-1015GF in a cool, dry, well-ventilated area away from direct sunlight, heat, moisture, and ignition sources. Keep containers tightly closed to prevent contamination and moisture pickup. Avoid dust generation and static buildup. Use appropriate PPE and follow local regulations. For processing, dry as recommended by the manufacturer. Store only in original or compatible containers. |
| Shelf Life | Typically 12 months when stored dry, cool, and in original sealed packaging; avoid moisture and direct sunlight. |
Competitive LG Chemical Keyflex® PBT+GF15% BT-1015GF prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
The LG Chemical Keyflex® PBT+GF15% BT-1015GF grade is an injection-molding thermoplastic polyester compound in which a polybutylene terephthalate matrix is reinforced with a nominal 15 wt% short-glass-fiber loading. The grade is differentiated from unfilled PBT and GF30 polyester compounds by its intermediate modulus-to-flow balance: the 15 wt% reinforcement level increases tensile and flexural stiffness beyond unfilled PBT without the deep notch sensitivity and high melt viscosity that characterize 30 wt% glass-fiber systems on thin-wall tooling. Production handling requires moisture control below 0.02 wt% before melt processing because ester chain hydrolysis proceeds rapidly above 250°C and preferentially degrades the amorphous tie-chain population responsible for impact strength. Supplier technical literature should be consulted for certified lot-specific values; the data presented in this document are representative ranges for PBT GF15 compounds and are not substitutes for a certificate of analysis.
Melt blending of the glass reinforcement is performed by LG Chemical at the compounding stage, not by the end-user. The resulting pellets are cylindrical or cuboid granules with a density typically between 1.42 g/cm³ and 1.48 g/cm³ when measured according to ISO 1183-1:2019. On production-scale reciprocating-screw injection molding machines with a general-purpose screw L/D of 20:1 to 24:1, the material feeds best when the hopper throat is cooled to prevent bridging; glass-fiber-filled PBT pellets can compact in the feed zone if the throat temperature exceeds 60°C. Press maintenance records from connector manufacturing lines indicate that screw and barrel wear is more pronounced with GF15 PBT than unfilled PBT, and bimetallic barrels or nitride-hardened screw flights are recommended for campaigns exceeding 50,000 shots.
| Characteristic | BT-1015GF representative range | Unfilled PBT | PBT GF30 | Test method |
|---|---|---|---|---|
| Density | 1.42–1.48 g/cm³ | 1.30–1.32 g/cm³ | 1.52–1.56 g/cm³ | ISO 1183-1:2019 |
| Tensile strength at break | 85–100 MPa | 50–60 MPa | 120–140 MPa | ISO 527-2:2012 |
| Flexural modulus | 4,000–5,500 MPa | 2,200–2,700 MPa | 7,500–9,000 MPa | ISO 178:2019 |
| Izod notched at 23°C | 4.5–6.5 kJ/m² | 4–6 kJ/m² | 8–11 kJ/m² | ISO 180/A:2000 |
| Heat deflection temperature at 0.45 MPa | 195–210°C | 150–160°C | 210–220°C | ISO 75-2:2013 |
| Mold shrinkage, flow direction | 0.4–0.7% | 1.5–2.0% | 0.2–0.5% | ISO 294-4:2018 |
| Mold shrinkage, transverse direction | 0.8–1.2% | 1.5–2.0% | 0.6–0.9% | ISO 294-4:2018 |
The ranges for BT-1015GF represent the expected band for a 15 wt% glass-fiber PBT compound; certified values vary by color, regrind content, and processing conditions. Compared with GF30, the GF15 formulation typically reduces melt pressure at the machine nozzle by an amount that becomes significant in multi-cavity tools with hot-runner manifolds. The exact pressure drop is mold-specific and should be derived from flow simulation or pressure transducer data, not from a single published value.
In practice, the choice of BT-1015GF over unfilled PBT is typically made when a part requires reduced warpage in flat connector bodies and better creep resistance at elevated automotive underhood temperatures. The GF15 system provides a flexural modulus roughly 80–100% higher than unfilled PBT and better dimensional stability in humid environments, while the flow length in a 1 mm wall-thickness spiral flow mold is longer than for a GF30 compound at the same melt temperature and injection pressure. Published data for this specific configuration is limited because spiral flow results depend on tool geometry, gate design, and machine response time; mold trials on the intended production tool are required before gate sizing is finalized.
In injection molds with abrupt thickness changes, glass fibers orient along flow lines and can cause differential shrinkage between flow and transverse directions. For BT-1015GF, the flow-direction coefficient of linear thermal expansion may be around 50–70 µm/m/°C between 23°C and 80°C when tested according to ISO 11359-2:2021, while transverse CLTE values may be 80–110 µm/m/°C. This anisotropy is lower than unfilled PBT but should be modeled using Moldflow or Moldex3D with measured shear viscosity data rather than generic isotropic assumptions. Mold designers typically use a gate land length of 0.5–1.5 mm and a gate diameter not less than 60% of the part wall thickness to avoid premature freeze-off.
The melt viscosity of BT-1015GF exhibits shear-thinning behavior. Apparent melt viscosity at a shear rate of 1,000 s⁻¹ and 250°C typically falls between 60 Pa·s and 120 Pa·s depending on drying and colorant package. At 10,000 s⁻¹, corresponding to thin-wall gate shear, the apparent viscosity may decrease to 15–35 Pa·s. These are presentation ranges for glass-filled PBT and are not a substitute for capillary rheometry on the actual lot; an in-line rheological measurement using a slit die or injection pressure transducer provides more reliable control.
The melt-processing window for BT-1015GF is constrained by two boundaries: the crystallization temperature of the PBT matrix and the onset of hydrolytic decomposition. Barrel temperature profiling from feed to nozzle is typically set at 240°C, 250°C, 260°C, 250°C, with nozzle temperature not exceeding 270°C. Mold temperature is controlled between 60°C and 100°C to permit adequate crystallinity while avoiding post-ejection dimensional drift. Hold pressure is typically 40–80 MPa, with screw back pressure of 2–5 MPa. The use of a reverse-taper nozzle and free-flow non-return valve is recommended because short-glass fibers can trap in standard ball-check valves and cause inconsistent shot weights. Vented barrel zones are not recommended for this polyester grade unless vacuum is applied to minimize oxidative yellowing; polyester degradation products can deposit on vent ports and require periodic cleaning.
Desiccant drying is mandatory for BT-1015GF following storage in ambient relative humidity above 60%. The pellets are typically dried at 120°C for 3–4 hours to reduce residual moisture to 0.02 wt% or less when measured by Karl Fischer titration according to ISO 15512:2019. Drying-air dew point should be maintained at -30°C or lower, and hopper residence time should not exceed 8 hours at temperature to limit thermo-oxidative discoloration. In production-scale operations with central drying systems, the conveying distance between dryer and machine throat should be kept below 10 m if unheated air lines are used; otherwise moisture re-uptake in the pellets can exceed 0.01 wt% within 30 minutes.
For semi-crystalline PBT GF15, the gate freeze time at a 1.5 mm wall thickness and mold temperature of 80°C is commonly 2–4 s; packing time should extend beyond gate freeze by 1–2 s to avoid sink marks at bosses. Short shots followed by controlled overpacking are not recommended because glass-fiber breakage at the flow front cannot be reversed. Multi-cavity connector tools with 16 or 32 cavities running on 80–120 t clamp force machines have used BT-1015GF with mold temperature control units set to 80°C. The injection speed is usually profiled with an initial 100–200 mm/s screw front velocity to fill the runner, followed by a controlled deceleration to 30–60 mm/s at the gate to avoid jetting. Packing pressure is often 50–70% of the peak fill pressure, with total cycle times ranging from 25–40 s for wall stocks of 1.5–2.5 mm. These figures are observed production ranges; machine-specific optimization is required.
The addition of regrind to BT-1015GF alters fiber length distribution and matrix molecular weight because each melt pass subjects the polyester chains to shear and thermal history. A regrind content of 20% by weight is generally considered the upper practical limit for dimensional tolerance classes below ±0.05 mm according to ISO 20457:2018. At regrind levels above 20 wt%, glass-fiber attrition in the check ring and screw compression zone reduces average fiber length, causing a measurable drop in notched impact strength and an increase in flow-direction shrinkage anisotropy. Press-side audits on multi-cavity tooling have reported shot-to-shot weight variance exceeding 0.15% when regrind fraction exceeds 30%, especially with hot-runner systems that impose additional shear heating in the manifold. Fillers should not be added downstream; BT-1015GF is delivered as a ready-to-mold compound and there is no published evidence that blending with unfilled PBT improves processability without disproportionately sacrificing modulus.
Masterbatch addition should be limited to carrier systems compatible with PBT. Polyolefin-based color masterbatch can delaminate at the interface and reduce weld-line strength; polyester or PBT-based carrier masterbatches are preferred. Loading of color masterbatch should not exceed 2 wt% unless approved by the compound supplier, and titanium dioxide levels above 1 wt% can shift melt viscosity and require a revised processing window.
Electrical interconnects, relay bases, sensor housings, and exterior mirror mounts are among the production areas where GF15 PBT compounds are selected. In these applications, the material must maintain electrical insulation resistance through thermal cycling and humid exposure. PBT GF15 typically has a dielectric strength around 20–25 kV/mm at 2 mm thickness when tested according to IEC 60243-1:2013, and comparative tracking index values commonly fall in the 250–300 V range under IEC 60112:2020. These values are not exclusive to BT-1015GF and must be confirmed on the final molded part because glass-fiber orientation at the weld line can reduce local dielectric strength by 10–20%.
Chemical compatibility is limited by the polyester backbone. Strongly alkaline cleaners, amine-based mold releases, and hot water systems above 70°C can attack the ester linkages through hydrolysis or aminolysis, lowering molecular weight and creating surface hazing. If contact with automotive coolants is required, testing according to ASTM D543-21 at the expected service temperature is recommended, as published multi-fluid compatibility data for BT-1015GF specifically are not widely available. Continuous exposure to hot water above 70°C should be considered a service boundary unless the part is redesigned or the material is replaced with a hydrolytically stabilized grade.
| Requirement | Relevant standard | Verification point |
|---|---|---|
| RoHS Directive 2011/65/EU | IEC 62321-5:2013 | Supplier declaration required for each color lot |
| REACH SVHC candidate list | EC 1907/2006 | Certification required from LG Chemical |
| UL 94 flammability | UL 94 | HB at 0.8 mm typical for PBT GF compounds unless FR-modified |
| Moisture content after drying | ISO 15512:2019 | <0.02 wt% |
| Melt volume-flow rate | ISO 1133-1:2022 | Reported at 250°C/2.16 kg, value depends on grade color and drying history |
Because BT-1015GF is not a flame-retardant compound, end-use requirements of V-0 or V-2 at 0.75 mm under UL 94 are not met by this grade; the material is normally rated HB up to 3.0 mm. For connector applications with glow-wire requirements according to IEC 60695-2-11, a separate evaluation on the final part is required because wall thickness and colorants influence the result.