Lg Chemical Keyflex Pbt Alloy Bt 3033

LG Chemical Keyflex® PBT Alloy BT-3033

    • Product Name: LG Chemical Keyflex® PBT Alloy BT-3033
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 137756
    Density G Cm3 1.18-1.22
    Tensile Strength Mpa 50
    Flexural Modulus Mpa 2100
    Flexural Strength Mpa 80
    Elongation At Break Percent 50
    Notched Izod Impact J M 50
    Hdt At 0 45 Mpa C 100
    Hdt At 1 8 Mpa C 85
    Vicat Softening Temperature C 110
    Mold Shrinkage Percent 0.4-0.7
    Water Absorption Percent 0.1
    Ul94 Flame Rating HB
    Volume Resistivity Ohm Cm 1E15
    Dielectric Constant At 1mhz 3.0
    Melting Temperature C 220

    As an accredited LG Chemical Keyflex® PBT Alloy BT-3033 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg moisture-barrier bags, LG Chemical Keyflex® PBT Alloy BT-3033 pellets are supplied on pallets for industrial handling.
    Container Loading (20′ FCL) 20′ FCL loading for LG Chemical Keyflex® PBT Alloy BT-3033: 25 kg bags, palletized, approx. 20–22 metric tons, safely secured for export.
    Shipping LG Chemical Keyflex® PBT Alloy BT-3033 is shipped as dry resin pellets in sealed moisture-barrier bags or octabins on pallets. Keep containers closed and protect from heat, sunlight, moisture, and contamination. Store in a dry, ventilated area and follow the SDS and local shipping regulations.
    Storage Store LG Chemical Keyflex® PBT Alloy BT-3033 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat sources, moisture, and strong oxidizing agents. Keep material in original sealed packaging, palletized off the floor, protected from UV, dust, and contamination. Maintain stable temperature and humidity; use first-in-first-out stock rotation and follow the supplier SDS and local regulations.
    Shelf Life Shelf life is typically 24 months when stored in original sealed packaging in a cool, dry place.
    Free Quote

    Competitive LG Chemical Keyflex® PBT Alloy BT-3033 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LG Chemical Keyflex® PBT Alloy BT-3033 is a glass-free polybutylene terephthalate alloy supplied in pellet form for injection moulding of components in which unfilled PBT exhibits excessive warpage and PC/ABS exhibits inadequate chemical resistance. The grade is supplied with a manufacturer’s certificate of analysis reporting batch-specific data under ISO 527-2, ISO 178, ISO 179-1, and ISO 75. The alloy is positioned for automotive interior switch bezels, electrical connectors, relay housings, and appliance trim where cycle time, low moisture uptake, and solvent resistance are operationally critical. Unlike reinforced PBT grades, BT-3033 contains no glass fibre, so moulded parts display lower flow-induced anisotropy; unlike unfilled PBT, the alloying phase reduces differential shrinkage between flow and cross-flow directions. In production planning, BT-3033 must be dried and processed under closed-loop melt temperature control; failure to do so manifests as surface splay, reduced Charpy notched impact, and batch-to-batch melt viscosity drift. Regulatory documentation typically covers REACH SVHC, RoHS Directive 2011/65/EU Annex II, and hazardous substance declarations, but application-specific compliance must be verified with the supplier.

    Does residual moisture in BT-3033 alter melt viscosity and impact response?

    Residual moisture is the controlling variable for melt-phase hydrolysis in PBT alloys. Desiccant drying at 120°C for 4 h with a dew point of -30°C or lower reduces pellet moisture to <0.02% by mass, measured by Karl Fischer titration according to ISO 15512. At moisture levels above 0.03%, hydrolytic chain scission lowers intrinsic viscosity and produces a measurable reduction in ISO 179-1/1eA Charpy notched impact. On production-scale dryer hoppers, return-air dew point must be monitored continuously because saturated desiccant beds allow moisture excursions above 0.05% within 30 min. For central drying systems with residence time above 6 h, drying temperature should be reduced to 100°C to avoid pellet discoloration and oxidative degradation. Single-screw injection units with L/D 20:1, compression ratio 2.5:1, and a shut-off nozzle are typical. Hot-runner manifold temperatures should not exceed 260°C to limit residence time at the hot runner. Moisture below 0.02% is not an arbitrary limit; it is the threshold below which melt viscosity remains within the specified ISO 1133-1 MVR control band. When moisture exceeds 0.05%, field observations on 80-tonne clamp injection moulding machines include gate frost, silver streaks, and a 20–30% drop in weld-line Charpy impact, even when tensile stress at yield remains within specification.

    Injection moulding parameter selection for BT-3033 follows a descending barrel profile from 250°C at the rear zone to 240°C at the nozzle, with melt temperature measured at the nozzle between 240°C and 255°C. Mould temperature is set at 60–80°C for dimensional stability; raising the mould to 100°C increases crystallinity, lowers post-shrinkage, and raises heat deflection temperature under ISO 75-2/B but extends cycle time. Holding pressure is typically 50–70% of injection pressure; inadequate holding pressure causes sink marks and voids in thick sections. Screw speed should be limited to 100–150 mm/s to avoid shear heating above 270°C, which triggers thermal degradation and yellowing. On hot-runner systems, valve-gate sequencing is preferred over open hot tips because PBT alloy solidifies rapidly and freezes hot tips after 3–5 s of interruption. During switchover, the use of position or velocity transfer with a 0.5–1.0 mm cushion prevents pressure spikes at the check ring. Mould venting channels of 0.01–0.02 mm depth are required on the parting line to evacuate gases; insufficient venting causes burn marks in blind ribs and bosses. For multicavity tools, flow balancing by runner diameter adjustments reduces cavity-to-cavity weight variation to <1.5%, which is necessary to maintain ISO 179-1 impact consistency.

    Mechanical property classes under ISO 527 and ISO 178 establish the structural window

    Test data are generated on dry, injection-moulded Type 1A specimens after 40 h conditioning at 23°C and 50% relative humidity. The following table lists property classes and test methods used for glass-free PBT alloy systems; product-specific values must be read from the BT-3033 certificate of analysis.

    Property classTest methodTypical glass-free PBT alloy range
    Tensile stress at yieldISO 527-2/1A40–55 MPa
    Tensile modulusISO 527-2/1A1800–2400 MPa
    Flexural modulusISO 1781700–2200 MPa
    Charpy notched impact at 23°CISO 179-1/1eA4–15 kJ/m²
    Heat deflection temperature at 0.45 MPaISO 75-2/B80–120°C
    DensityISO 1183-11.25–1.35 g/cm³

    Thermal and dimensional stability are governed by the coexistence of crystallizable PBT segments and an amorphous alloy phase. In thermomechanical analysis under ISO 11359-2, unfilled PBT typically exhibits a coefficient of linear thermal expansion of 80–100 µm/m/°C below the glass transition; the alloying modification narrows the differential between flow and cross-flow directions. Parts moulded from BT-3033 should be annealed at 120°C for 2 h when service temperatures exceed 100°C, otherwise post-crystallization shrinkage of 0.1–0.3% may occur. Dimensional acceptance should be based on 24-h room-temperature conditioning after moulding, not on hot dimensions measured at the press.

    Chemical resistance and environmental stress-cracking response

    PBT alloys display low equilibrium moisture uptake, typically <0.1% at 23°C and 50% RH, which confers dimensional stability in humid environments compared with PA66. Resistance to aliphatic hydrocarbons, engine oil, transmission fluids, alcohols, and dilute acids is retained at temperatures up to 60°C. Immersion testing according to ISO 22088-3 in brake fluid at 70°C can be used to qualify stressed connector housings. The grade is not recommended for continuous exposure to hot >80°C aqueous alkaline solutions, ketones, chlorinated solvents, or strong mineral acids; such media induce ester hydrolysis or environmental stress cracking at moulded-in stress concentrations. When solvent contact is intermittent, stress relief annealing reduces craze initiation at weld lines.

    Differentiation from unfilled PBT, glass-reinforced PBT, PC/ABS, and PA66 is primarily expressed in moisture uptake, anisotropy, and chemical resistance. Unfilled PBT crystallizes rapidly and offers good solvent resistance but can produce out-of-round cylindrical parts due to differential shrinkage measured under ISO 294-4. Glass-reinforced PBT raises flexural modulus to 6000–9000 MPa but introduces flow-direction anisotropy and surface glass bloom. PC/ABS has higher notched impact at -30°C but is vulnerable to stress cracking in toluene and certain plasticizers. PA66 absorbs 2.5–3.0% moisture at saturation under ISO 62, causing tensile modulus to fall by 30–40% and dimensions to shift by 0.5–0.7% in service. BT-3033, as a glass-free PBT alloy, occupies a middle position: lower moisture shift than PA66, better chemical resistance than PC/ABS, and lower warpage than unfilled PBT, but lower heat deflection than glass-filled PBT. This balance is selected for connectors exposed to automotive interior heat, low moisture, and cleaning agents.

    During cavity filling, the melt front solidifies against the tool wall within 1–3 s; sequential valve gates prevent cold slug formation at the sprue. For parts with wall thickness below 1.5 mm, injection velocity should be raised to 80–120 mm/s and mould temperature to 90°C, but shear rates above 50000 s⁻¹ in thin-wall sections may induce melt fracture and visible flow marks. In thick sections above 4 mm, holding time is determined by gate freeze time, which can be estimated by pressure-drop measurement: when cavity pressure ceases to decay after holding pressure removal, the gate has frozen. Gate sizing below 0.8 mm for a 2 mm wall creates jetting; gate depths of 1.0–1.5 mm produce plug flow and reduce blush. For connector housings with multiple pins, flow leaders and pin-gates are preferred over edge gates to reduce gas entrapment at the core side.

    If low-temperature impact retention is required, moulded-in stress and weld-line position override resin selection

    Low-temperature ductility is measured with ISO 179-1/1eA at -30°C; for unfilled PBT alloys, notched Charpy values typically fall to 20–40% of the 23°C value. The ductile-to-brittle transition is sensitive to gate location because weld lines act as stress concentrators. In production evaluation on a 120-tonne injection moulding machine, moving the weld line from the centre of a boss to a non-stressed outer wall raised -30°C Charpy notched impact from 4 kJ/m² to 7 kJ/m², an improvement that cannot be achieved by drying alone. Packing pressure decay after gate freeze must be controlled; excessive packing creates residual hoop stress in cylindrical parts, lowering cold-temperature resistance. When the application requires cold impact below -40°C, published data for this specific configuration is limited, and validation must include component-level drop tests at the lowest service temperature.

    Electrical connector housings require tracking resistance and dielectric strength under IEC test conditions. Comparative tracking index is evaluated according to IEC 60112; glass-free PBT alloys often fall within PLC 2 to PLC 3 depending on pigment and conductive contamination. Dielectric strength is measured under IEC 60243-1 on 3.0 mm plaques; values above 20 kV/mm are typical for unfilled PBT systems. For glow-wire requirements, ignition temperature and flame spread are assessed under IEC 60695-2-12; unfilled PBT alloys are classified as HB under UL 94 unless flame retardant additives are used. When BT-3033 is selected for EV charging connectors, the design must consider creepage and clearance distances under IEC 60664-1, because tracking resistance is inferior to thermoset electrical grades. Surface contamination from mould release or silicone-based assembly lubricants alters CTI and should be avoided.

    Regrind use is constrained by hydrolysis and thermal history. Production-scale trials indicate that up to 20 wt% clean regrind from dried sprues can be reintroduced if granulate particle size is 3–5 mm and the blend is dried to <0.02% moisture. Above 30 wt% regrind, batch-to-batch melt viscosity drift under ISO 1133-1 becomes measurable; tensile elongation at break under ISO 527-2/1A can fall by 10–15% after three regrind cycles. Regrind containing oil, mould release, or dust must be excluded because contamination reduces tracking resistance and weld-line strength.

    Post-mould dimensional control of BT-3033 is influenced by both primary cooling shrinkage and secondary crystallization. ISO 294-4 specimens show that mould temperature at 80°C reduces 24-h shrinkage by 0.1–0.2% absolute compared with 40°C. For parts with flatness requirements below 0.3 mm over 100 mm, fixture cooling is required after ejection because free cooling produces bow from asymmetric heat removal. Annealing at 120°C for 2 h stabilizes crystallinity and reduces subsequent exposure shrinkage; annealing should be performed after all machining on the part is complete to avoid stress relief deformation.

    Rheologically, BT-3033 is a shear-thinning melt; melt volume-flow rate under ISO 1133-1 at 250°C/2.16 kg is used for lot release. MVR values outside the supplier’s control band, typically 10–25 cm³/10 min for medium-flow PBT alloys, indicate moisture, regrind contamination, or thermal degradation. For thin-wall parts, apparent viscosity at 1000 s⁻¹ can be determined by capillary rheometry according to ISO 11443; this data is required for Moldflow simulation but is not part of standard certificates. In hot-runner systems, residence time at melt temperature above 250°C should be limited to <10 min to avoid non-Arrhenius thermal degradation.

    Application qualification for under-hood brackets and sensor housings uses a combined test sequence: 1000 h heat aging at 120°C, thermal shock from -40°C to 100°C for 500 cycles, and exposure to 50°C engine oil for 7 days. Property retention is assessed by ISO 527-2 tensile tests before and after aging. In such environments, BT-3033 is positioned against glass-filled PA66 where moisture-induced dimensional change is unacceptable, and against PC/ABS where oil stress cracking is a known failure mode. Published data for this specific configuration is limited; component-level validation remains mandatory.