Lg Chemical Keyflex Pbt Alloy Bt 1200h

LG Chemical Keyflex® PBT Alloy BT-1200H

    • Product Name: LG Chemical Keyflex® PBT Alloy BT-1200H
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 796641
    Density G Cm3 1.20
    Tensile Strength Mpa 48
    Elongation At Break Percent 60
    Flexural Modulus Mpa 1900
    Flexural Strength Mpa 75
    Notched Izod Impact Kj M2 15
    Heat Deflection Temperature 1 8 Mpa C 90
    Vicat Softening Temperature C 110
    Melting Temperature C 225
    Water Absorption Percent 0.4
    Mold Shrinkage Percent 1.0-1.5
    Molding Temperature C 230-260
    Drying Temperature C 100-120

    As an accredited LG Chemical Keyflex® PBT Alloy BT-1200H factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LG Chemical Keyflex® PBT Alloy BT-1200H is packaged in 25 kg moisture-proof bags, suitable for industrial handling and storage.
    Container Loading (20′ FCL) LG Chemical Keyflex® PBT Alloy BT-1200H is loaded in a 20-foot FCL container, typically palletized in bags, ensuring secure, dry transport.
    Shipping LG Chemical Keyflex® PBT Alloy BT-1200H is shipped as thermoplastic pellets in sealed moisture-barrier bags, typically 25 kg, palletized and stretch-wrapped. Keep dry, away from direct sunlight and heat; handle as non-hazardous under normal transport regulations.
    Storage Store LG Chemical Keyflex® PBT Alloy BT-1200H in a cool, dry, well-ventilated area away from direct sunlight, heat sources, sparks, and open flames. Keep material in its original, sealed packaging to prevent moisture and contamination. Avoid prolonged exposure to high humidity and strong oxidizers. Do not stack excessively; follow the manufacturer’s SDS and local regulations. Use appropriate ventilation and housekeeping to control dust.
    Shelf Life Shelf life is generally 24 months when stored dry and cool in sealed original packaging, protected from moisture and sunlight.
    Free Quote

    Competitive LG Chemical Keyflex® PBT Alloy BT-1200H prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LG Chemical Keyflex® BT-1200H is a pelletized, unreinforced polybutylene terephthalate alloy grade positioned for injection-molded components where notch impact resistance must exceed the performance of general-purpose PBT without the sharp increase in modulus, anisotropic mold shrinkage, and surface roughness associated with glass-fiber reinforcement. The product is formulated as a PBT matrix containing a dispersed secondary polymer phase; that morphology raises energy absorption at a notch and reduces the brittle fracture tendency of the polyester. Typical published datasheets for this grade report properties after conditioning at 23 °C and 50 % RH under ISO 291, with tensile data generated to ISO 527-1/2, flexural data to ISO 178, notched Izod impact to ISO 180/1A, and heat deflection temperature to ISO 75-1/2. Users should not transfer these values to thick or highly pigmented parts without separate validation, because the alloy’s crystallinity, modifier dispersion, and skin-core structure are process-dependent.

    On production-scale injection molding cells—commonly 100–160 tonne clamp-force electric or servo-hydraulic machines using 22–30 mm diameter screws with L/D ratios of 20–24—BT-1200H is processed as a semicrystalline engineering plastic with a narrow moisture tolerance. The principal processing conflict is the combined effect of residual moisture, barrel residence time, and melt shear history. PBT ester linkages are hydrolysable at melt-processing temperatures; pellet moisture should therefore be reduced to < 0.02 wt% before melting. This is commonly achieved in a desiccant hopper dryer operating at a dew point of −40 °C to −30 °C, a pellet bed temperature of 120 °C ± 5 °C, and a minimum drying time of 4 h. When ambient relative humidity exceeds 60 %, drying should not be omitted even for freshly opened bags because surface moisture can hydrolyze the polymer during plastication. Barrel set temperatures are typically profiled from 230 °C at the rear zone to 250 °C at the nozzle; melt residence above 10 min at these temperatures may generate splay, gas streaks, and reduced notched impact values.

    Reciprocating-screw units used for this grade should employ a medium-compression screw with a compression ratio of 2.2:1–2.8:1, a hardened check ring, and a free-flow nozzle sized for crystalline PBT. Dispersive mixing elements are rarely required for an unreinforced alloy and can raise melt temperature through viscous dissipation. Hydraulic back pressure should be maintained at 3–7 bar, not elevated to promote shear heating. Shot size should remain between 30 % and 50 % of barrel capacity to avoid excessive residence time and poor melt uniformity. Screw recovery speed is typically set between 100 rpm and 150 rpm; higher speeds may generate shear heating and degrade the impact-modifier phase. Cushion control should be held to 2–5 mm, because erratic cushion creates variable residence time and can shift notched Izod results between molded parts and laboratory specimens.

    What set of property trade-offs separates BT-1200H from neat PBT and glass-filled PBT?

    Neat PBT homopolymer is characterized by a relatively high tensile strength and flexural modulus but a low notched Izod impact strength, often cited in the 20–40 J/m range under ISO 180/1A. A 30 % glass-fiber-reinforced PBT grade raises flexural modulus to roughly 8,000–10,000 MPa and tensile strength to 120–140 MPa, but it increases flow-direction/transverse shrinkage anisotropy and reduces surface appearance. A high-impact PBT alloy such as BT-1200H shifts the balance toward notch insensitivity and lower stiffness: published ranges for unreinforced impact-modified PBT grades typically include notched Izod values of 500–800 J/m at 23 °C, flexural modulus of 1,500–2,000 MPa, and tensile strength of 30–45 MPa. The consequence is that BT-1200H is selected for snap-fit housings, clips, and enclosure covers rather than for dimensionally stable structural supports. Published data specific to the BT-1200H lot under evaluation should be obtained from the manufacturer’s certificate of analysis, because alloy modifier content and molecular weight can shift these values between production campaigns.

    Representative comparative property bands for material classes, not a substitute for BT-1200H lot data
    PropertyStandardUnmodified PBTHigh-impact PBT alloy class30% glass-filled PBT
    Notched Izod impact, 23 °CISO 180/1A20–40 J/m500–800 J/m60–90 J/m
    Flexural modulusISO 1782,300–2,800 MPa1,500–2,000 MPa8,000–10,000 MPa
    Tensile strengthISO 527-1/250–60 MPa30–45 MPa120–140 MPa

    Within the Keyflex PBT alloy range, a high-impact alloy such as BT-1200H is typically chosen over general-purpose PBT for thin-walled electrical housings, relay sockets, sensor bodies, and snap-fitted covers. The improvement in notched impact comes at the expense of flexural stiffness and solvent resistance. For load-bearing frames or pump housings where creep resistance and dimensional stability under load are more important than impact, a glass-filled PBT or a glass-filled polyamide may be more appropriate. BT-1200H should not be automatically substituted into a glass-filled PBT tool without recalculating gate size, shrinkage, and ejection draft.

    Weld-line toughness is a recognized operational boundary for this product class. When two melt fronts meet at angles below 45°, the dispersed impact-modifier phase can orient along the weld interface and produce a plane of reduced interdiffusion. On multi-gate housing molds, tensile strength at a weld line may be only 50–70 % of the base value measured on a single-gate specimen under ISO 527-2. The effect is most severe when the weld line falls at the base of a cantilever snap-fit or at the root of a screw boss. For such designs, increasing the local wall section by approximately 30 %, relocating the gate to raise the meeting angle, or raising mold temperature to 80 °C improves melt-front interdiffusion. Mold flow simulation with lot-specific PVT and viscosity data is required for quantitative prediction.

    Mold shrinkage after demolding is not instantaneous. The crystalline portion of the PBT phase continues to densify as the part cools; for BT-1200H parts with a flow-length-to-thickness ratio above 150:1, flow-direction and transverse shrinkage can differ by 0.2–0.5 % absolute. Dimensional audits should be postponed for a minimum of 24 h after demolding, with specimens stored at 23 °C and 50 % RH. If parts are measured immediately after ejection, the recorded dimensions may overstate final size and lead to incorrect press-fit interferences. Automotive OEM dimensional control plans often require 48 h aging for unreinforced PBT alloys before CMM verification. Demolding from a cold tool below 40 °C may shorten cycle time but increases molded-in stress and reduces impact performance; mold temperature should therefore be maintained at 60–80 °C rather than reduced solely to increase output.

    When hot-runner valve gates and thin-wall sections impose high shear on BT-1200H

    Hot-runner systems with valve-gate diameters below 0.8 mm or edge gates below 0.5 mm can subject the melt to calculated wall shear rates exceeding 100,000 s⁻¹. In such circumstances, shear-induced phase segregation may be observed as a dull halo or surface blush around the gate boundary. Field observations on multi-cavity connector molds using 2.5 mm nominal wall stock suggest that increasing gate diameter from 0.5 mm to 1.0 mm can reduce peak injection pressure by 20–30 % and reduce cavity-to-cavity mass variation from approximately ±1.5 % to ±0.5 %. The melt-temperature window for the alloy is often 230–250 °C, with the nozzle set to the upper end for thin sections and the lower end for thick-wall parts to limit residence-time degradation. Mold temperature should be held within 60–80 °C for dimensional stability; lower mold temperatures shorten cycle time but increase internal stress and weld-line fragility. Hold pressure should be set to 60–80 % of peak injection pressure, and gate freeze should be verified by part-weight stability rather than visual sprue appearance alone.

    Filling speed should be profiled so that the melt front advances within 0.5–1.5 s for small connector housings, with the initial stage at lower velocity to avoid jetting and the final stage at higher velocity to prevent surface freeze-off. High-speed injection without profiling raises shear at the gate and can produce delamination at the surface. Screw recovery throttle should be set to allow screw retraction to finish before cooling time ends, avoiding cylinder over-ride and inconsistent plastication. These settings are machine-specific and should be adjusted by short-shot series and cavity pressure measurements using sensors mounted behind the ejector pin or in the hot runner.

    Lot-to-lot variation in melt viscosity can be detected by monitoring injection peak pressure and screw recovery torque. A shift in melt volume-flow rate outside the supplier’s specification band may indicate improper drying, blend separation, or raw-material lot change. Incoming resin should be tested for melt volume-flow rate under ISO 1133-1:2022 at 250 °C/2.16 kg and for moisture content; typical unreinforced PBT alloy grades fall within a melt volume-flow rate band of 15–35 g/10 min, but the BT-1200H specification must be taken from the manufacturer’s certificate.

    Electrical enclosure and connector applications involving BT-1200H must be evaluated against flammability and tracking resistance requirements that are not automatically satisfied by the base alloy. Unreinforced PBT alloys are usually classified as UL 94 HB; a V-0 rating should not be inferred unless the supplier provides a specific yellow card for the BT-1200H formulation. Comparative tracking index values can span from below 400 V to above 600 V depending on heat stabilizer and impact-modifier selection, and glow-wire testing to IEC 60695-2-12 must be conducted on the finished part thickness. For low-voltage appliance housings intended for unattended use, the final part must be tested at the minimum wall thickness and with the same color concentrate, because pigment packages can alter tracking resistance and flame behavior.

    Regulatory documentation boundaries under REACH, RoHS, and food-contact assumptions

    BT-1200H is not self-certifying for food-contact, medical, or potable-water service solely on the basis of its PBT backbone. Under REACH, a registration number should be obtained from the safety data sheet for the EU-manufactured or imported material. RoHS compliance is assessed against Directive 2011/65/EU as amended by Delegated Directive (EU) 2015/863, and requires laboratory verification of restricted phthalates and heavy metals using methods such as IEC 62321. Food-contact suitability under EU 10/2011 or FDA 21 CFR 177.166 depends on the specific formulation, migration testing under OM2 or OM3 conditions, and an explicit supplier declaration. In the absence of such documentation, the material is limited to non-food industrial and electrical applications.

    For load-bearing covers and fixtures exposed to continuous stress at 60 °C, the creep modulus of an unreinforced PBT alloy is significantly lower than that of a glass-filled PBT and lower than its short-term flexural modulus would suggest. Published creep data for BT-1200H-specific formulations is limited; designers should apply a creep modulus reduction factor based on the manufacturer’s isochronous stress-strain curves. Snap-fit geometries cycled more than 10 times should be designed with outer-fiber strain below 2 % to avoid stress-whitening and progressive permanent set. For bolted joints, molded-in inserts should be designed to avoid hoop stresses exceeding the stress-cracking threshold when exposed to automotive fluids.

    Continuous-use temperature for unreinforced PBT alloys is often specified by the supplier relative to a 50 % retention of tensile strength after 1000 h heat aging. For general PBT alloy systems, this can lie near 110–130 °C, but BT-1200H lot-specific data should be confirmed. Above 140 °C, oxidative embrittlement may reduce elongation rapidly; components exposed to under-hood heat spikes above this threshold require additional stabilizers or a different polymer.

    What are the chemical resistance boundaries of BT-1200H in hydrocarbon and under-hood environments?

    The PBT matrix in BT-1200H retains polyester resistance to many aliphatic hydrocarbons at room temperature, but it is less resistant to hot aqueous acidic or alkaline media, ketones, and certain chlorinated solvents. In under-hood environments, continuous exposure to motor oil at 80–100 °C may plasticize or stress-crack the alloy when tensile stresses exceed 10–20 MPa, and the impact-modifier phase can further reduce solvent resistance relative to neat PBT. The material is not a substitute for polyamide in glycol-continuous cooling systems or for PPS in sustained fuel-contact service. For any chemical environment, part testing should be performed on molded specimens with the actual molded-in stress state, using tensile bars exposed under ASTM D543 or ISO 22088-2 conditions. Published data for BT-1200H in specific fluids is limited to the supplier’s chemical resistance table; if a fluid is not listed, the grade should be validated under use temperature and exposure time.