Lanxess Pocan Unreinforced Pbt B1305

Lanxess Pocan® Unreinforced PBT B1305

    • Product Name: Lanxess Pocan® Unreinforced PBT B1305
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 320036
    Density 1.30 g/cm³
    Melt Volume Flow Rate 250 C 2 16 Kg 20 cm³/10 min
    Tensile Modulus 2600 MPa
    Tensile Stress At Break 55 MPa
    Tensile Strain At Break 20 %
    Charpy Notched Impact Strength 23 C 4 kJ/m²
    Vicat Softening Temperature B120 165 °C
    Hdt A 1 8 Mpa 50 °C
    Hdt B 0 45 Mpa 150 °C
    Melting Temperature 225 °C
    Water Absorption Saturation 0.4 %
    Molding Shrinkage Parallel 1.8 %
    Flammability Ul 94 HB

    As an accredited Lanxess Pocan® Unreinforced PBT B1305 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Lanxess Pocan® Unreinforced PBT B1305 is supplied in 25 kg moisture-resistant paper bags, palletized for safe storage and handling.
    Container Loading (20′ FCL) 20′ FCL loading for Lanxess Pocan® Unreinforced PBT B1305: palletized bags, dry clean container, secure stowage, and carrier weight compliance.
    Shipping Pocan® B1305 is shipped as unreinforced PBT resin pellets in sealed moisture-barrier bags or octabins, typically on pallets. It is non-hazardous for transport and should be kept dry, clean, and protected from moisture and direct sunlight. Standard ambient-temperature freight is suitable; no special handling required.
    Storage Store **Lanxess Pocan® Unreinforced PBT B1305** in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and moisture. Keep original packaging tightly sealed; reseal opened bags and protect from humidity/water. Avoid contact with strong oxidizers. Follow the manufacturer’s SDS and local regulations; dry before processing if moisture-exposed.
    Shelf Life Typically 12 months when stored dry in original sealed packaging at moderate temperature, protected from moisture and heat.
    Free Quote

    Competitive Lanxess Pocan® Unreinforced PBT B1305 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Lanxess Pocan® B1305 000000 natural is an unreinforced polybutylene terephthalate injection-molding grade. The polymer is classified as PBT under ISO 1043-1 and is supplied without filler, fiber reinforcement, or flame-retardant additives. Within the Pocan B range, B1305 is positioned as a medium-viscosity base resin; its melt volume-flow rate is approximately 13 cm³/10 min at 250 °C and 2.16 kg when measured to ISO 1133-1. The material is specified for thin-wall connectors, bobbins, sensor housings, and mechanical parts that require rapid cavity filling without the through-thickness stiffness of glass-filled PBT.

    What Drying and Melt-Residence Limits Govern B1305 Injection Molding?

    Before melt processing, B1305 is dried to a residual moisture ceiling of 0.02 wt%. The standard supplier drying condition is 110–130 °C for 2–4 h in a dehumidified air dryer with a dew point no higher than -30 °C. Moisture contents above the ceiling hydrolyze ester linkages in the melt, causing molecular-weight loss, reduced tensile elongation, and increased shot-to-shot melt-pressure variation. Drying beyond 6 h at 130 °C is avoided because oxidative yellowing can shift natural resin color and reduce notched impact strength.

    The barrel profile is typically set to 230–250 °C in the feed zone, 245–260 °C in the compression zone, and 250–270 °C in the metering zone; nozzle temperature is held at 250–270 °C. Mold-wall temperature is controlled between 60 °C and 100 °C. At the lower boundary the melt freezes quickly, lowering cycle time but increasing molded-in stress and weld-line embrittlement. At the upper boundary spherulitic growth is more complete, which improves fatigue resistance and post-annealing dimension retention; gate freeze time, however, increases and ejection may require additional draft or release force.

    Melt-residence time should not exceed 8 min at 270 °C. On reciprocating screw machines with L/D ratios of 20 to 25, excessive back pressure and high cushion can create stagnant melt zones near the non-return valve and screw tip. These dead zones darken, generate butanediol-derived odor, and can produce intermittent black-spec contamination. Hot-runner drops with unheated tips or zero-leakage nozzles are thermally profiled to avoid local melt temperatures above 270 °C.

    Venting is critical because the unfilled melt has low melt strength at processing temperatures. Mold-parting-line vent depths are maintained at 0.02–0.03 mm; depths above 0.04 mm promote flash in thin-wall connector tools. Screw back pressure is kept at 5–15 bar, and screw recovery is timed to complete before 80 % of the cooling phase. Gates should be placed at thicker sections because pinpoint gates below 0.8 mm can cause premature freeze-off in this fast-crystallizing grade.

    Typical natural-grade property data are listed in the following table. Values are not specification limits; they are measured on injection-molded specimens conditioned at 23 °C and 50 % RH unless otherwise noted.

    PropertyTest methodTypical value
    DensityISO 1183-11.30 g/cm³
    Melt volume-flow rateISO 1133-113 cm³/10 min
    Tensile modulusISO 527-1/-22500 MPa
    Tensile stress at yieldISO 527-1/-255 MPa
    Nominal strain at breakISO 527-1/-250 %
    Charpy notched impact strength, 23 °CISO 179-1/1eA5 kJ/m²
    Charpy notched impact strength, -30 °CISO 179-1/1eA4 kJ/m²
    Heat deflection temperature, HDT/A 1.8 MPaISO 75-2/A55 °C
    Heat deflection temperature, HDT/B 0.45 MPaISO 75-2/B150 °C
    Vicat softening temperature, B50ISO 306180 °C
    Melting temperatureISO 11357-3225 °C
    Comparative tracking indexIEC 60112600 V
    Volume resistivityIEC 62631-3-11E14 ohm·m
    Flammability at 1.6 mm thicknessUL 94HB

    These data show an unfilled PBT with tensile modulus below 3 GPa and heat deflection temperature near 150 °C. Because the resin is unreinforced, mold shrinkage is more isotropic than that of glass-fiber PBT but larger in magnitude. Total flow-direction shrinkage is typically 1.5–2.0 % depending on wall thickness, gate geometry, and mold temperature; transverse shrinkage can be 10–20 % higher. Tool designers compensate with cavity-specific shrink factors and pressure-transducer studies to establish gate-seal hold time.

    Property Shifts When Glass Fiber Is Omitted From the PBT Matrix

    Positioning B1305 against a 30 % glass-fiber reinforced PBT reference clarifies the consequences of removing fibrous reinforcement. The unreinforced grade has lower tensile modulus, higher elongation, lower heat-deflection performance, and more uniform shrinkage. Glass-fiber PBTs typically reach 9–11 GPa tensile modulus and 200 °C or higher HDT/B, whereas B1305 remains near 2.5 GPa and 150 °C. The unreinforced resin retains a nominal strain at break of about 50 %, while a 30 % glass-fiber PBT may fail at 1–2 %. These differences are design boundaries: B1305 is selected where part ejection, snap-fit assembly, or flatness favor low modulus and isotropic shrinkage over load-bearing stiffness.

    The removal of glass fiber also shifts electrical and wear behavior indirectly. Fiber ends can concentrate surface electric fields and reduce tracking resistance; an unfilled PBT with CTI of 600 V is therefore used in switched-mode power-supply insulation. Wear and abrasion resistance, however, are lower than filled grades, and published data for this specific configuration under sliding wear is limited. Dimensionally, B1305 responds more to mold-temperature changes than a filled grade, so cavity-pressure monitoring is used to maintain shot-to-shot consistency when mold heating circuits vary.

    PropertyB1305 typical30 % GF-PBT class reference
    Tensile modulus2500 MPa10000 MPa
    Nominal strain at break50 %2 %
    HDT/B 0.45 MPa150 °C205 °C
    Flow-direction mold shrinkage1.8 %0.3–0.8 %
    Comparative tracking index600 V250–400 V

    The reference values for the 30 % glass-fiber grade are typical of the material class and are shown only to illustrate the design trade-off; they do not constitute supplier specifications for any named product. Dynamic mechanical analysis of unfilled PBT typically shows a glass transition near 45–60 °C and a melting peak near 225 °C by ISO 11357-3. Modulus therefore declines above 60 °C, and the HDT/B value of 150 °C is a short-term deflection limit under 0.45 MPa, not a continuous-use temperature. In hot-motor compartments, load-bearing brackets may require metal inserts or a glass-filled PBT.

    Moisture behavior further separates B1305 from polyamide-based materials. Equilibrium moisture uptake at 23 °C and 50 % RH is approximately 0.2–0.3 wt% under ISO 62, compared with 2.5–3.0 wt% for PA66. Consequently, dimensional growth and electrical-property drift under humidity are lower, but moisture-induced toughness enhancement is also smaller. In dry-as-molded condition, notched Charpy impact is about 5 kJ/m²; at low temperature it may fall to 4 kJ/m². Designs should not depend on ductile yielding at low temperature.

    Typical downstream use includes injection-molded electrical connectors, relay bobbins, sensor housings, and mechanical housings exposed to intermittent contact with automotive fluids. Chemical resistance is not universal: strong acids, alkaline solutions above pH 9, and prolonged hot-water exposure above 80 °C can hydrolyze the ester backbone. The grade is not flame-retarded; UL 94 classification is HB at 1.6 mm. Applications requiring V-0 or glow-wire performance require a flame-retardant PBT grade or a different polymer family. Regulatory conformity must be verified on the finished article; the base resin is available under standard REACH and RoHS documentation, but pigmented or compounded variants may differ.

    Within the Pocan B series, B1305 is differentiated from higher-viscosity unreinforced PBT grades by lower melt-pressure consumption and a shorter pressure-holding window. The lower molecular weight reduces entanglement density, improving cavity filling in multi-gate tools but lowering notched impact and long-term creep resistance. Published data for this specific configuration under long-term creep is limited; project-specific creep testing is required.

    Top