Lanxess Pocan Unreinforced Pbt B1300

Lanxess Pocan® Unreinforced PBT B1300

    • Product Name: Lanxess Pocan® Unreinforced PBT B1300
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 615770
    Density 1.30 g/cm³
    Melt Volume Flow Rate 260 C 2 16 Kg 18 cm³/10 min
    Tensile Modulus 23 C 2700 MPa
    Tensile Stress At Yield 23 C 55 MPa
    Tensile Strain At Yield 23 C 3.5%
    Nominal Strain At Break 23 C >50%
    Charpy Impact Strength 23 C Unnotched 100 kJ/m²
    Charpy Notched Impact Strength 23 C 5 kJ/m²
    Vicat Softening Temperature A 180°C
    Hdt A 1 8 Mpa 55°C
    Hdt B 0 45 Mpa 150°C
    Water Absorption 23 C Saturated 0.4%
    Moisture Absorption 23 C 50 Rh 0.15%
    Molding Shrinkage Parallel 1.9%
    Volume Resistivity 1E16 Ω·cm
    Dielectric Strength 30 kV/mm
    Comparative Tracking Index Cti 600 V
    Melting Temperature 225°C

    As an accredited Lanxess Pocan® Unreinforced PBT B1300 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Lanxess Pocan® Unreinforced PBT B1300 is packaged in 25 kg moisture-barrier bags, palletized for safe industrial handling and storage.
    Container Loading (20′ FCL) 20′ FCL dry container loaded with palletized 25 kg bags of Lanxess Pocan® Unreinforced PBT B1300, shrink-wrapped and secured for ocean transport.
    Shipping Lanxess Pocan® Unreinforced PBT B1300 is shipped as solid thermoplastic pellets in moisture-proof bags, cartons, or octabins on pallets. It is not classified as dangerous goods for transport. Keep containers closed, dry, and protected from heat and direct sunlight; avoid moisture pickup during storage and handling.
    Storage Store Lanxess Pocan® Unreinforced PBT B1300 in a cool, dry, well-ventilated area away from direct sunlight, heat sources, and moisture. Keep original containers tightly closed to prevent contamination and moisture pickup. Protect from physical damage, dust, and incompatible materials. Keep away from ignition sources. Follow the supplier’s safety data sheet and local regulations. Use first-in, first-out stock rotation.
    Shelf Life Lanxess Pocan® B1300 unreinforced PBT has a shelf life of 12 months when stored dry in original sealed packaging at recommended temperatures.
    Free Quote

    Competitive Lanxess Pocan® Unreinforced PBT B1300 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Lanxess Pocan® B1300 is an unfilled polybutylene terephthalate (PBT) injection-molding resin produced from 1,4-butanediol and terephthalic acid or dimethyl terephthalate. The material carries the ISO 1043-1 designation PBT and is marked as >PBT< under ISO 11469 when molded into recoverable components. As an unreinforced grade, B1300 contains no glass fiber or mineral filler; the mechanical response is therefore isotropic in the melt and substantially less notch-sensitive than highly oriented short-glass compounds, though the structural modulus remains below that of 30 weight percent glass-fiber PBT. Typical published property values include a solid density of 1.30–1.31 g/cm³ to ISO 1183-1:2019, a melt volume-flow rate near 18–22 cm³/10 min at 250 °C under 2.16 kg load to ISO 1133-1:2022, and a tensile modulus of approximately 2,500 MPa with yield stress near 55 MPa to ISO 527-1/-2. Thermal analysis of unreinforced PBT typically identifies a crystalline melting peak at 225 °C and a glass-transition region near 45 °C. Elongation at break commonly exceeds 30%, which distinguishes the unfilled grade from glass-fiber-modified Pocan products that may fail at 2–4% nominal strain. Water absorption at 23 °C and 50% relative humidity is approximately 0.2 wt%, and saturation in water is generally below 0.5 wt%, giving B1300 stable dielectric behavior in humid service when surface contamination is controlled.

    The base B1300 product is neither impact-modified nor flame-retarded; property improvements such as low-temperature notched toughness or V-0 flammability require a different Pocan grade or an additive package. This distinction matters in substitution reviews because adding halogen-free flame retardants can shift CTI, relative permittivity, and density, while impact modification lowers tensile modulus and HDT-A. Typical downstream uses include relay bases, bobbins, power-tool housings, automotive connector bodies, sensor mounts, LED frames, and appliance control modules. The selection of B1300 for these parts depends on the combination of easy flowing melt, high elongation, good surface appearance, and resistance to fuels, greases, and dilute aqueous acids. It is not generally selected for load-bearing brackets or structural housings because the heat deflection temperature under 1.8 MPa to ISO 75-1/-2 is in the range 55–65 °C, far below the 200–210 °C typical of a 30% glass-fiber-reinforced PBT. Unfilled PBT also has higher isotropic mold shrinkage, commonly 1.4–2.0% in flow and 1.8–2.2% transverse to flow as measured on 2 mm plaques to ISO 294-4, which makes tool compensation more demanding than with mineral-filled or glass-filled grades. The absence of fiber bloom and the lower melt viscosity allow finer surface replication and more precise short-shot control in multi-cavity molds, but the processing window must still be controlled because PBT is subject to hydrolysis and thermal chain scission above the upper melt-temperature limit.

    How Does B1300 Differ from Low-Viscosity PBT, Extrusion-Grade PBT, and Glass-Fiber-Reinforced Pocan Products?

    The medium-flow MVR of B1300 places it between low-viscosity rapid-cycle PBT grades used for large-area thin-wall parts and high-viscosity extrusion PBT grades used for tubing and cable sheathing. Lower-viscosity grades may provide shorter fill times in sub-millimeter walls, but their lower molecular weight often translates to lower notched impact strength and reduced melt strength, which can cause drooling at the nozzle and poor hot-runner balance. Higher-viscosity extrusion grades provide greater melt strength and toughness but can require elevated melt temperatures or increased injection pressure in thin-wall connector molds. B1300 is designed for injection molding where fill ratios are moderate and where balanced hot-runner flow is required without excessive shear heating. Compared with glass-fiber-reinforced Pocan PBT, B1300 exhibits lower density, lower tensile modulus, higher elongation, and lower HDT-A. A 30 wt% glass-fiber PBT typically has a tensile modulus of 9,000–11,000 MPa and a Charpy notched impact strength at 23 °C near 8–12 kJ/m² by ISO 179-1/1eA, while B1300 is generally reported near 2,400–2,600 MPa and 3–5 kJ/m² under the same notched conditions. Fiber-reinforced grades provide higher creep resistance and lower shrinkage but introduce anisotropic warpage and tool wear; B1300 avoids fiber-induced surface roughness and is preferable where electrical tracking, paint adhesion, or ultrasonic welding are critical. The absence of mineral or glass also reduces melt density and simplifies regrind handling, though unfilled PBT remains notch-sensitive at low temperatures.

    Desiccant drying is the first critical operation in production-scale molding of B1300. Residual moisture above 0.02 wt% at hopper entry causes hydrolytic cleavage of ester linkages during plastication, leading to splay, lowered molecular weight, increased MVR, and a measurable reduction in weld-line strength. Pre-drying at 120 °C for 4 h in a desiccant dryer with dew point below −40 °C is recommended for virgin pellets; regrind containing prior thermal history may require an additional hour. A closed hopper feed with dry-air purge reduces moisture re-uptake between drying and the feed throat. Melt-temperature control is bounded at the lower end by incomplete melting and unmelted pellets, and at the upper end by thermal degradation. The usual melt-temperature range is 250–270 °C for injection molding; mold temperatures from 60 °C to 100 °C are used to balance crystallization, surface gloss, and cycle time. In hot-runner tools with valve-gate nozzles, melt residence time above 270 °C should not exceed 8–10 min because chain scission shifts the MVR upward by more than 2 cm³/10 min, reduces Charpy notched impact strength, and produces yellowing in unpigmented parts. Screw geometry of 18:1 to 22:1 L/D ratio with a compression ratio near 2.0:1 to 2.5:1 and a low back pressure of 0.5–1.0 MPa hydraulic is typical for unreinforced PBT. High compression or high back pressure generates excessive shear heating and may mask a poorly dried feedstock by lowering melt viscosity that is already shifting from hydrolytic degradation.

    Injection speed, hold pressure, and gate freeze are coupled in B1300 because the higher volumetric shrinkage of unfilled PBT requires adequate packing. Short hold-pressure time produces sink marks, internal voids, and post-mold shrinkage beyond the tool design allowance. Production-scale molds for connector insulators typically run hold pressures of 50–80 MPa at the cavity, with total cycle times of 20–40 s depending on wall thickness and mold temperature. Screw recovery speeds of 150–250 rpm are common for medium-flow PBT, but high recovery speeds combined with wet material produce visible silver streaks at the gate and lower weld-line burst strength. Mold-filling simulation should set gate dimensions; submarine or tunnel gates below 0.8 mm diameter may cause jetting in unfilled PBT, especially in thin-wall sections near 0.6 mm flow length. Ventilation depth of 0.02–0.03 mm is standard for PBT to prevent gas burn without flash.

    Shrinkage, Weld-Line Behavior, and Dimensional Tolerance Constraints in Unfilled Parts

    Post-mold shrinkage of B1300 is more pronounced than in glass-filled Pocan grades, and the difference must be accounted for in multi-cavity tools and overmolded assemblies. The use of 60 mm × 60 mm × 2 mm plaques to ISO 294-4 gives typical parallel shrinkage of 1.4–2.0% and perpendicular shrinkage of 1.8–2.2%. Higher mold temperatures near 100–120 °C increase crystallinity, reduce post-mold shrinkage, and improve dimensional stability but lengthen cycle time and alter surface gloss. Differential shrinkage between flow and transverse directions is smaller in unfilled PBT than in short-glass compounds but still sufficient to warp flat parts if gate locations produce asymmetric orientation. Weld lines in multi-gate switch housings are locations of reduced elongation and notched impact. Their strength depends on melt temperature, moisture level, and venting; wet material lowers weld-line strength more than general tensile properties because moisture-induced hydrolysis products concentrate at the flow front. The design of ribs, bosses, and snap-fits in B1300 should include radii of at least 0.5 mm at the base to limit notch-sensitive brittle failure, particularly at use temperatures below 0 °C. Annealing of molded parts at 120 °C for 2 h is sometimes applied to relax molded-in stress before secondary operations such as ultrasonic welding or painting.

    Electrical connector designs benefit from the unfilled morphology of B1300 because glass fibers are absent from the surface, reducing the risk of conductive fiber bridges after abrasion or hot-stamping. Volume resistivity of unfilled PBT is commonly reported at 1×1016 Ω·cm to IEC 62631-3-1, dielectric strength at 30 kV/mm on 1.6 mm specimens to IEC 60243-1, and comparative tracking index in the 400–600 V range to IEC 60112. These values describe the unfilled PBT family, and lot-specific certificates should be required when CTI above 400 V is a design limit. The grade is typically rated UL 94 HB at 1.6 mm; it does not contain a flame-retardant package and therefore should not be substituted for Pocan V-0 grades in unattended electrical equipment. The relative permittivity of unfilled PBT is approximately 3.2–3.5 at 1 MHz, with a dissipation factor near 0.02, making B1300 suitable for insulating parts where low loss is more important than high-temperature load-bearing performance.

    PropertyTest methodB1300 unreinforced PBT30% glass-fiber PBT reference
    Density, g/cm³ISO 1183-11.30–1.311.53–1.56
    Tensile modulus, MPaISO 527-1/-22,400–2,6009,000–11,000
    Yield stress, MPaISO 527-1/-252–57120–140
    Nominal strain at break, %ISO 527-1/-2>302–4
    Charpy notched impact, kJ/m²ISO 179-1/1eA3–58–12
    HDT-A, 1.8 MPa, °CISO 75-1/-255–65200–210
    MVR, 250 °C, 2.16 kg, cm³/10 minISO 1133-118–228–15

    The comparative table above represents a general property envelope for unreinforced B1300 and a short-glass-reinforced PBT reference. Actual datasheet values may differ by pigment, lot, specimen thickness, and conditioning history; the values are not design allowable without supplier confirmation.

    Standard or regulationScopeApplicability to B1300
    ISO 1043-1Polymer abbreviationPBT
    ISO 11469Molding identification>PBT<
    ISO 1133-1:2022Melt volume-flow rateQuality-control verification
    ISO 1183-1:2019DensityMaterial identification and part weight control
    ISO 527-1/-2Tensile propertiesDesign and incoming inspection
    ISO 179-1/1eACharpy notched impactImpact-sensitive snap-fit evaluation
    ISO 75-1/-2Heat deflection temperatureLoad-bearing thermal limit assessment
    IEC 60112Comparative tracking indexElectrical connector creepage design
    IEC 60243-1Dielectric strengthInsulation thickness selection
    UL 94Flammability classHB at 1.6 mm; not V-0
    RoHS 2011/65/EURestricted substances in electrical equipmentFinal part compliance depends on colorants and additives
    REACH 1907/2006SVHC communicationSupply-chain declaration required per lot

    Under-hood sensor housings in polyamide-free zones exploit the low moisture uptake of PBT relative to polyamide 66; dimensions remain more stable in humid engine-bay air because B1300 absorbs approximately 0.2 wt% at 50% relative humidity, whereas polyamide 66 can absorb more than 2 wt% in conditioned service. Fuel-resistance tests in gasoline, diesel, and engine oil show negligible mass change after 500 h at 60 °C in typical PBT grades; published B1300-specific data for all fuel blends is limited, and exposure to ethanol- or methanol-containing fuels requires component-level validation due to potential stress cracking. Domestic appliance modules and power-tool housings use B1300 for its surface hardness and dimensional stability after conditioning, but the resin should not be exposed to hot water above 80 °C for extended periods because hydrolysis accelerates. The unfilled grade is also susceptible to strong alkalis, hot concentrated acids, and chlorinated solvents; compatibility should be tested with production cleaning agents before use.

    Production-scale failure modes observed with unfilled PBT include gate blush from excessively high injection velocity, jetting from undersized gates, splay from wet material, and sink over bosses from short hold pressure. In a 16-cavity hot-runner relay-base tool with valve-gate sequences, melt fill imbalance of 1–2% in cavity weight is typically corrected by nozzle tip temperature adjustment or hold-pressure profiling rather than by raising barrel temperature, because the latter reduces viscosity but narrows the thermal safety margin. Batch-to-batch MVR variation should be monitored by incoming inspection to ISO 1133-1:2022; a shift of ±1.5 cm³/10 min may require revalidation of the process window in thin-wall tools.

    Chemical resistance of B1300 is governed by the semicrystalline PBT matrix. The resin withstands aliphatic hydrocarbons, greases, mineral oils, and many dilute aqueous acids, but environmental stress cracking can occur in contact with strong mineral acids at elevated temperature, hot concentrated sodium hydroxide, and certain chlorinated solvents. Paint adhesion and ultrasonic welding are generally easier on unfilled PBT than on glass-filled grades, but surface preparation such as plasma or primer may be required after mold release agents. Welding amplitude, force, and weld time should be developed on molded parts, not on dry plaques, because moisture equilibrated at 0.2 wt% changes damping behavior.

    Long-term thermal aging of unreinforced PBT above 140 °C is generally not recommended without grade-specific stabilizer data; at 160 °C air-oven aging can embrittle unfilled PBT within 1,000 h, depending on specimen thickness and antioxidant package. Published data for B1300 at 150 °C in specific automotive under-hood configurations is limited; service life calculations should be based on actual part testing under load and temperature cycling rather than on generic PBT Arrhenius projections. Lot-specific data sheets and certificates should be obtained before designing release approval tests because values for CTI, UL 94 thickness, and food-contact status vary with colorant and additive package.

    Top