| HS Code | 122216 |
| Materialtype | PBT + 30% glass fiber |
| Glassfibercontent | 30 % |
| Hydrolysisresistance | Improved (XHR) |
| Density | 1.52 g/cm3 |
| Tensilemodulus | 9500 MPa |
| Tensilestrength | 135 MPa |
| Elongationatbreak | 2.5 % |
| Charpyimpactstrengthnotched 23c | 9 kJ/m2 |
| Hdt A 1 8mpa | 205 °C |
| Meltingtemperature | 225 °C |
| Moldingshrinkage | 0.3-0.6 % |
| Waterabsorption | 0.4 % |
| Ul94flammability | HB |
| Volumeresistivity | 1E15 ohm·cm |
| Dielectricstrength | 30 kV/mm |
| Processingmethod | Injection molding |
As an accredited Lanxess Pocan® PBT+GF30%-XHR B3233XHR factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Supplied as pellets in 25 kg moisture-proof bags, 40 bags per pallet, total quantity 1,000 kg per pallet. |
| Container Loading (20′ FCL) | 20-foot FCL container loaded with palletized Lanxess Pocan® PBT+GF30%-XHR B3233XHR, properly secured and stowed for ocean transport. |
| Shipping | Shipping description: Lanxess Pocan® PBT+GF30%-XHR B3233XHR, a non-hazardous polybutylene terephthalate compound with 30% glass fiber and flame-retardant properties, is supplied as pellets in moisture-proof bags or octabins. Protect from moisture, heat, sunlight, and ignition sources; no UN/DG classification under normal transport conditions. |
| Storage | Store in a cool, dry, well-ventilated area in original sealed packaging. Keep away from moisture, direct sunlight, heat sources, open flames, and strong oxidizing agents. Prevent contamination by dust or other materials. Maintain moderate temperature and low humidity; use first-in, first-out. For prolonged storage, reseal containers tightly to limit moisture pickup. Do not store near food or feed. |
| Shelf Life | Lanxess Pocan PBT+GF30%-XHR B3233XHR has a shelf life of 24 months when stored dry, cool, and in original sealed packaging. |
Within engine-compartment electrical packaging where ambient air temperature cycles between −40 °C and 125 °C, relative humidity exceeds 85 % during tropical damp-heat soak, and salt spray from winter road service reaches connector housings, Pocan® B3233XHR is processed as supplied. The glass fiber content is fixed at 30 wt%; no additional glass reinforcement is compounded on site because fiber-length attrition during plastication already establishes the balance between tensile modulus and notch sensitivity in snap-fit regions. Regrind addition is limited to ≤20 wt% for non-locking connector bodies and ≤10 wt% for snap-fit latch features, with regrind lot fraction controlled under ISO 11469 marking. Material is predried at 120 °C for 4 h in a desiccant-bed dryer to residual moisture <0.02 %. Injection molding on a 20:1 L/D general-purpose screw uses a barrel profile of 245–270 °C, nozzle at 255–265 °C, mold temperature 80–100 °C, and injection pressure 800–1,200 bar; hold pressure is maintained at 50–70 % of peak injection pressure for 6–10 s per mm of nominal wall thickness. Gate position is shifted away from the pin retention zone to avoid weld-line formation in high-stress snap-fit areas. Venting depth is kept at 0.01–0.02 mm to prevent burn marks without flash. Compliance testing uses SAE/USCAR-2 for thermal cycling, terminal retention, and mating force, with damp-heat aging per IEC 60068-2-30 at 85 °C/85 % RH for 1,000 h; dimensional stability is checked after temperature-humidity cycling according to LV214 OEM schedules. Terminal finished product types include engine position sensor housings, MAP sensor sockets, camshaft sensor mounting flanges, ignition coil low-voltage connector bodies, and underhood relay plugs.
Pressurized coolant housings manufactured from Pocan® B3233XHR replace PA66 in thermostat bodies and water pump impellers where glycol-water immersion at 130 °C combined with vibration fatigue produces property cliffs and dimensional instability. Qualification requires tensile property retention after immersion in 50/50 ethylene glycol/water at 130 °C for 1,000 h per ISO 175:2010 and ISO 527-1:2019, with impact retention measured by ISO 179-1/1eA. The compound is used at 100 % virgin for pressure-bearing housing walls; regrind is accepted up to ≤15 wt% only in non-wetted mounting brackets. Predrying at 120 °C for 4–6 h to <0.02 % moisture is mandatory because residual water above 0.05 % accelerates hydrolysis at the gate interface. Melt temperature is held at 250–270 °C, mold temperature at 90–100 °C; sequential valve-gate hot-runner filling is used to locate the weld line away from the thermostat seat and impeller hub. Packing pressure of 55–75 MPa is applied for 8–12 s per mm to compensate for fiber-orientation shrinkage. Screw rotation is limited to 60–100 min⁻¹ to reduce glass-fiber breakage. Operational boundaries: continuous exposure to coolant pH >9.0 at >110 °C is not recommended; amine-based corrosion inhibitors can attack the PBT ester linkage if concentration exceeds the coolant manufacturer’s specified range. Terminal finished product types include thermostat housings, coolant pump impellers, coolant distribution flanges, and thermal management valve bodies.
Because appliance pressure vessels are subjected to repeated thermal quench from 90 °C wash liquor to 20 °C rinse water while maintaining dimensional seal integrity against alkaline detergents, B3233XHR is selected for pump bodies and internal impellers. Formulation addition ratio uses the compound as supplied with 30 wt% glass fiber; no post-compounding fiber addition is used. Regrind is limited to ≤20 wt% in pump impeller hubs only if impact data after 1,000 h humid aging per ISO 179-1/1eA remain within the application acceptance window; for sealing valve seats, regrind is excluded. Predrying to <0.015 % moisture is performed at 120 °C for 5 h in a desiccant-air dryer. Injection molding uses a 22:1 L/D barrier screw with melt temperature 245–265 °C, mold temperature 80–95 °C, and injection speed 50–100 mm/s through edge gates entering at the hub to minimize radial fiber orientation. Cooling time is 8–12 s per mm for sections up to 3 mm; thick bosses above 4 mm require a second packing stage to avoid internal voids. Compliance evaluation follows IEC 60335-1:2020 moisture resistance tests and IEC 60730-1:2020 control component endurance, with end-product water ingress checks per IEC 60529 IPX4/IPX7. Terminal finished product types include washing machine drain pump housings, dishwasher circulation pump impellers, water inlet valve bodies, and steam iron pump bases.
In tropical and subtropical low-voltage distribution equipment, internal support plates and terminal block housings are exposed to 85 % RH at 40 °C for extended periods under IEC 60068-2-30 and must maintain creepage distances without warpage. Pocan® B3233XHR is processed at 30 wt% glass loading; for switchgear non-live structural parts, regrind addition is capped at ≤15 wt% because recycled glass fiber shortens and affects comparative tracking index values. Masterbatch addition is limited to ≤1 wt% to preserve CTI values measured under IEC 60112. Melt temperature is set at 240–260 °C, mold temperature at 85–95 °C, and injection speed is reduced in sections exceeding 4 mm wall thickness to avoid sink marks at boss intersections. For thick ribs, hold pressure is staged at 60 MPa for 10 s, then 35 MPa for 6 s to balance shrinkage without overpacking. Compliance testing is performed according to IEC 60112 for comparative tracking index, IEC 60695-2-11 for glow wire flammability at end-product thickness, IEC 60529 for ingress protection, and IEC 62208:2011 for empty enclosure mechanical properties. Molded parts are not post-annealed except in threaded brass insert regions, where selective induction pre-heating to 140 °C is used before insert placement. Terminal finished product types include terminal block housings, busbar supports, miniature circuit breaker covers, relay sockets, and distribution box internal partitions.
| Application segment | Primary standard | Test condition |
|---|---|---|
| Underhood connectors | SAE/USCAR-2, IEC 60068-2-30 | 85 °C/85 % RH, 1,000 h |
| Coolant housings | ISO 175:2010, ISO 527-1:2019 | 50/50 glycol/water, 130 °C |
| Appliance pumps | IEC 60335-1:2020, IEC 60730-1:2020 | thermal quench 90 °C/20 °C |
| Low-voltage switchgear | IEC 60112, IEC 60695-2-11 | CTI and glow wire at end-product thickness |
| Solenoid bobbins | UL 1446, IEC 60216-1 | Class F 155 °C |
| Charging infrastructure | IEC 62196-1:2014, IEC 62196-2:2016 | damp heat per IEC 60068-2-30 |
Coil formers for transmission-control solenoids operate under a combination of continuous winding tension, hot ATF vapor, and current-induced self-heating that raises the bobbin flange temperature toward 155 °C. B3233XHR is supplied at 30 wt% glass reinforcement; for thin-wall bobbins with wall thickness 0.6–1.0 mm, regrind is limited to ≤10 wt% and material is dried to <0.02 % moisture at 120 °C for 6 h before molding. High injection speed of 80–120 mm/s with melt temperature 250–270 °C and mold temperature 90–100 °C is used to fill the core-pulled spool geometry; hold pressure is 60–80 MPa for 0.5–1.0 s/mm to prevent short shots between core pins. A 25:1 L/D mixing screw with compression ratio 3:1 improves glass distribution in the thin flange-to-body transition. Gate vestige is machined or sheared below 0.02 mm to avoid wire enamel abrasion during winding. Compliance evaluation uses UL 1446 insulation system tests only after complete insulation system approval, with thermal endurance data generated under IEC 60216-1. Dimensional checks after damp heat aging per IEC 60068-2-30 are required because bobbin flange warpage above 0.05 mm disrupts winding tension and increases coil stack height. Operational boundaries: the grade is not suitable where cyclic temperatures exceed 170 °C peak or where ATF is combined with strong amine-based additives. Terminal finished product types include transmission shift solenoid coil formers, ABS/ESP pressure modulator bobbins, variable valve timing actuator bobbins, and fuel injection metering unit coil carriers.
Outdoor wallbox interior supports and charging plug shells manufactured from Pocan® B3233XHR are processed without the unmodified PBT grades that fail hydrolytically after monsoon-season humidity cycling. The compound enters at 30 wt% glass loading; for closed-loop production, regrind addition is ≤12 wt% and is sourced only from sprues and runners verified by ISO 3451-1 ash content at 30 ± 2 wt% glass. Pre-drying at 120 °C for 4–6 h maintains residual moisture below 0.02 %; hopper capacity is matched so material residence time at drying temperature does not exceed 8 h to avoid oxidative yellowing. Injection molding uses melt temperature 245–265 °C, mold temperature 80–100 °C, and injection pressure 700–1,000 bar; multi-cavity tooling uses geometrically balanced runner systems because glass-fiber orientation disparity above 5 % across cavities creates bow in plug shell latches. End product testing is referenced to IEC 62196-1:2014 for charging connector mechanical load, IEC 62196-2:2016 for interface dimensions, and IEC 60068-2-30 for damp heat exposure; smoke and flammability requirements are end-product dependent and must be confirmed because this grade is not a flame-retardant PBT compound. Terminals finished product types include wallbox internal mounting plates, charging plug latch shells, charging inlet support rings, and power module busbar spacers.
Competitive Lanxess Pocan® PBT+GF30%-XHR B3233XHR prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Lanxess Pocan® PBT+GF30%-XHR B3233XHR is a 30% glass-fibre-reinforced polybutylene terephthalate compound. Its ISO 1043 designation is PBT-GF30, and the XHR suffix identifies the hydrolysis-resistant modification. The datasheet profile is organised around ISO 1183, ISO 527-1/-2, ISO 179-1/1eA, ISO 75-2 and ISO 1133-1. The product is supplied as pellets for reciprocating-screw injection moulding and is used where standard PBT GF30 would fail prematurely in hot water/glycol service. Dry-state mechanical values occupy the normal range for glass-filled PBT; the core difference is retention of tensile and impact properties after hydrolytic ageing. Current manufacturer documentation should be consulted for lot-specific release values because pigmentation, regrind level and moulding conditions can shift property results within the specification tolerance.
Hot water and water–glycol mixtures attack the ester linkages of polybutylene terephthalate through random chain scission. The reaction liberates carboxylic acid end groups, producing an autocatalytic degradation front once the acid concentration rises. In glass-filled PBT, this process acts on both the matrix and the interfacial region around the fibre sizing, leading to brittle failure at weld lines, bosses and sharp transitions. The XHR package is formulated to reduce the rate of ester hydrolysis, typically through end-group capping or chain-extension chemistry; the manufacturer does not publish a kinetic model for B3233XHR. Qualification therefore requires immersion testing in the actual coolant fluid rather than reliance on dry-state tensile data. Screening programs commonly use ISO 175 immersion in 50:50 ethylene glycol/water at 120–135°C for 1,000–3,000 h, with tensile testing after exposure according to ISO 527-2. Published comparative data for this specific grade in every coolant chemistry is limited; component-level validation remains necessary.
Before melt processing, the pellets require predrying in a dehumidified hopper dryer with a dew point no higher than −30°C. A residual moisture content below 0.02% should be achieved, typically after 4–6 h at 120°C in dry air. Residual moisture above this threshold promotes hydrolytic chain scission inside the barrel and can generate surface splay on moulded parts. Melt temperature is maintained at 250–270°C at the nozzle, while mould wall temperature is held between 80°C and 100°C to support crystallinity development and dimensional consistency. On standard reciprocating-screw machines, moderate back pressure and controlled screw rotation are used to limit glass-fibre attrition because severe shear shortens fibre length distribution and reduces weld-line strength. Gates should be located in the thickest section, and flow length-to-wall-thickness ratios must be more conservative than for unfilled PBT because the 30% glass content raises melt viscosity and increases anisotropic frozen-in stress. Mould release is generally unnecessary for simple geometries; external release agents may be applied only if ejection marks or sticking are observed.
The dry-state tensile modulus and flexural modulus of the XHR grade are close to those of a standard 30% glass-filled PBT. The separation occurs after hot aqueous exposure. Unstabilised PBT GF30 grades typically lose molecular weight more rapidly under acidic end-group accumulation, reducing weld-line strength, elongation at break and impact resistance before visible surface degradation appears. The XHR modification slows this sequence by shifting the chemical balance away from acid-catalyzed chain scission. The comparison should be made on stabilised property retention, not on initial dry values, and should include notched impact testing under ISO 179-1/1eA after fluid ageing because impact sensitivity often precedes gross tensile failure.
| Property | Test condition | Representative range | Standard |
|---|---|---|---|
| Density | 23°C | 1.53–1.56 g/cm³ | ISO 1183 |
| Melt volume-flow rate | 250°C / 2.16 kg | 9–16 cm³/10 min | ISO 1133-1 |
| Tensile modulus | 1 mm/min | 9,000–10,500 MPa | ISO 527-1/-2 |
| Tensile stress at break | 5 mm/min | 120–140 MPa | ISO 527-2 |
| Nominal strain at break | 5 mm/min | 2.0–3.0% | ISO 527-2 |
| Flexural modulus | 2 mm/min | 8,500–9,500 MPa | ISO 178 |
| Flexural strength | 2 mm/min | 180–210 MPa | ISO 178 |
| Charpy notched impact strength | 23°C | 7–11 kJ/m² | ISO 179-1/1eA |
| Heat distortion temperature A | 1.8 MPa | 195–215°C | ISO 75-2 |
| Melting temperature | DSC | 220–230°C | ISO 11357-3 |
| Mould shrinkage, flow | 60×60×2 mm plaque | 0.2–0.6% | ISO 294-4 |
| Water absorption saturation | 23°C | 0.3–0.5% | ISO 62 |
The table above is a release-orientation matrix rather than a certified specification. Differences between B3233XHR and standard PBT GF30 should be evaluated through paired ageing studies, with test specimens moulded under the same conditions and tested after exposure to controlled coolant chemistry. Unfilled PBT offers lower continuous-use stiffness and greater moisture-induced dimensional movement, while polyamide 66 GF30 can show higher dry heat resistance but generally absorbs more moisture and displays broader moulding shrinkage. The hydrolytically stabilised PBT GF30 therefore sits between those material options: it retains the low-moisture character of PBT while addressing a primary failure mode in hot water/glycol service.
For injection-moulded coolant valves, thermostat housings and electric water-pump components, the dominant failure mode is often not uniform tensile overload but the combination of hoop stress, pressure cycling and hydrolytic wall thinning at weld lines. In a 30% glass-filled PBT, fibre orientation is highly planar; regions where two flow fronts meet produce a knit line with lower load-carrying capacity. Under hot coolant pressure cycling, cracks can initiate at the knit line even when the bulk tensile strength appears adequate. Qualification protocols should therefore include pressure cycling from 0 to 2 bar at 120°C, followed by burst testing and sectioning at suspected gate and weld-line locations. The XHR grade is intended for this application class, but published data for cyclic-pressure performance in production-scale parts is limited outside specific OEM validation programs.
In tool design, wall thickness should not fall below 2.5–3.0 mm in load-bearing sections of glass-filled PBT unless mold-flow and fibre-orientation simulation confirm adequate packing. Sharp internal corners should be radiused at 0.5 mm or greater. Gate placement should push the weld line away from sealing lips and threaded bosses. Hot-runner systems require sufficiently large flow channels to limit shear heating and fibre attrition; valve gates may create local fibre alignment defects if the gate diameter is undersized. Cooling circuit layout must keep mould surface temperature uniform within ±5°C across the cavity, because uneven crystallinity changes shrinkage and creates post-demoulding warpage after moisture equilibration.
Mold-flow analysis for this compound should not be restricted to fill time and pressure curves. Fibre orientation tensor prediction is required because local stiffness and failure strain are anisotropic. The datasheet tensile values assume homogeneous injection-moulded test specimens with preferential orientation; they do not represent the transverse direction at a weld line. A structurally weak knit line can pass initial dimensional inspection and fail later under thermal shock. Qualification should therefore include tensile coupons cut transverse to the principal flow direction, not only standard ISO 527-2 Type 1A specimens. Thermal cycling between −40°C and 140°C, followed by coolant immersion at 120°C, provides a more meaningful indicator of service capability than dry-room tensile testing alone.
Final acceptance criteria must be established against the actual service fluid, because coolant additive packages differ in pH, buffer capacity and corrosion-inhibitor chemistry. Phosphate-based, organic-acid and hybrid coolants can produce different hydrolysis acceleration factors for polyester matrices. The use of reclaimed coolant, chloride-contaminated water or extended drain intervals can shift degradation beyond the range covered by standard laboratory screening. No universal retention percentage can be assigned to B3233XHR across all coolant systems; design release should be based on component-specific immersion, pressure cycling and mechanical property retention data generated under production-representative tooling and processing conditions.