Lanxess Pocan Pbt Gf30 Laser Weld Tp150 002

Lanxess Pocan® PBT+GF30% Laser-Weld TP150-002

    • Product Name: Lanxess Pocan® PBT+GF30% Laser-Weld TP150-002
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    Trusted Payment Partner
    Secure transactions supported by VTB Bank for reliable B2B procurement worldwide.
    Specifications
    HS Code 940862
    Density 1.53 g/cm3
    Glassfibercontent 30%
    Tensilemodulus 10000 MPa
    Tensilestrength 140 MPa
    Elongationatbreak 2.5%
    Charpyimpactstrengthunnotched23c 50 kJ/m2
    Charpynotchedimpactstrength23c 10 kJ/m2
    Heatdeflectiontemperaturea 210 °C
    Meltingtemperature 225 °C
    Moldshrinkageparallel 0.3%
    Moldshrinkagetransverse 0.8%
    Waterabsorption 0.4%
    Flammabilityul94 HB
    Laserweldingsuitability Laser-transparent / laser-weldable

    As an accredited Lanxess Pocan® PBT+GF30% Laser-Weld TP150-002 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg moisture-barrier bags, palletized and labeled with product name, grade, batch number, and safety information.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Lanxess Pocan® PBT+GF30% Laser-Weld TP150-002 is securely loaded into a dry 20-foot FCL container for shipment.
    Shipping Shipping description: Non-hazardous polybutylene terephthalate (PBT) glass-fiber reinforced (30%) laser-weldable molding compound, pellet form. Package in sealed, moisture-proof bags/containers; protect from heat, moisture, and UV; store dry; handle per SDS; comply with applicable transport regulations. No UN hazardous-goods classification normally applies. Ensure labels and documentation match product name and lot.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat sources, and ignition. Keep original containers tightly closed to prevent moisture absorption and contamination. Avoid prolonged UV exposure and damp conditions. Maintain stable ambient temperature and follow first-in, first-out stock rotation. Dry according to Lanxess recommendations before processing.
    Shelf Life The shelf life is approximately 24 months in dry, sealed conditions at ≤30°C, protected from moisture and direct sunlight.
    Application of Lanxess Pocan® PBT+GF30% Laser-Weld TP150-002

    In sealed engine-control-unit cover joining, the laser-transparent cover is moulded from Pocan TP150-002 and the lower housing is moulded from a laser-absorbing PBT-GF30 compound. The joint is a full-perimeter contour weld with a nominal weld-land thickness of 2.0 mm and a pre-weld clearance of 0.05–0.10 mm between the cover and the housing. The selected beam source is a fibre-coupled diode laser operating at 980 nm. The 980 nm wavelength is preferred over 808 nm for this glass-filled grade because the longer wavelength reduces the optical loss caused by glass-fibre scattering. The weld land is positioned away from gate vestiges and ejector pin marks to prevent local reductions in transmission. Mould release agents are prohibited on the visible weld surface because silicones and waxes reduce fusion at the interface.

    Before moulding, pellets are dried in a desiccant-air dryer at 120 °C for 4 h to a residual moisture level below 0.02 wt%, measured by Karl Fischer titration according to ISO 15512:2019. Melt temperature is maintained between 250 °C and 270 °C, and the tool surface temperature is controlled between 80 °C and 120 °C. Injection speed is set in the range of 40–80 mm/s for wall thicknesses between 1.5 mm and 2.5 mm. Hold pressure is applied at 60–80 MPa hydraulic specific pressure until gate freeze is achieved. Higher mould temperatures reduce skin stress and improve weld-land flatness, which directly affects laser transmission consistency.

    Laser joining is performed with a clamping tool that transmits the beam through a glass window while applying 2–4 N/mm² of pressure along the weld seam. Weld collapse is monitored by a linear displacement sensor and held between 0.10 mm and 0.20 mm. Contour welding speed is normally 20–40 mm/s with a focused spot diameter of 1.8–2.5 mm. Finished covers are validated for ingress protection according to ISO 20653:2013 IP6K7 and for thermal shock from −40 °C to 85 °C following ISO 16750-4:2010. Published data for this specific welded configuration is limited, so leak-rate and burst-pressure thresholds are established from serial tooling trials rather than generic datasheet values.

    What Limits Near-Infrared Transmission Through 2.0 mm Weld-Land Sections in Transmission-Mount Sensor Housings?

    Glass-fibre orientation has the largest single effect on laser transmission in a 30 wt% glass-reinforced PBT grade. When fibres lie perpendicular to the beam path, scattering occurs at each glass-polymer interface. When the predominant fibre direction is parallel to the weld line, fewer out-of-plane fibre ends intercept the beam, and transmission improves. For this reason, gate position and flow direction are mapped before the weld land is fixed. A weld-land thickness below 2.0 mm is specified to maintain sufficient transmission for reproducible collapse. Ribs, bosses, or ejector marks below the seam are excluded within 1.5 mm of the optical path because local sink marks change the contact pattern and produce weld smoke.

    Transmission-mount sensor housings are exposed to automatic transmission fluid at intermittent peak temperatures up to 140 °C. The PBT-GF30 matrix retains dimensional stability under short-duration heat aging, but continuous exposure above 120 °C in hydrolytic media can initiate molecular-weight reduction. The weld seam is therefore located on the connector side of the housing rather than the media-contact side. A fluorosilicone seal is used at the media interface, while the laser weld provides the outer mechanical retention. Laser joining is performed after terminal-pin overmoulding with clamp pressure limited to 1.5 N/mm² to avoid bending inserted pins.

    Validation includes pressure cycling from 0.1 MPa to 1.2 MPa in automatic transmission fluid at 110 °C, followed by helium leak testing with a rejection limit of 1×10⁻⁵ mbar·l/s. The combined thermal-oil pressure cycling protocol is supplier-specific because no single ISO standard covers the exact fluid, temperature, and pressure sequence. Published data for this specific TP150-002 welded sensor configuration is limited, so weld-quality limits are established on production-representative tooling.

    In battery-management unit enclosures, TP150-002 is processed as a structural cover material where the design does not require a V-0 flame-retardant classification at the finished part thickness. The 30 wt% glass-fibre content provides a flexural modulus above 9,000 MPa when measured according to ISO 178:2019, allowing snap-fit and weld-cover geometries to be combined without separate brackets. Laser-transparent black capability permits the cover and the lower housing to be colour-matched in black without painting or secondary surface treatment, which reduces volatile organic compounds and cycle time in serial production.

    Moulding uses a two-stage injection profile. The first stage fills the part at a screw-advance speed of 60 mm/s, and the second stage packs at 50–70 MPa. The gate is placed on the long side of the cover so that glass fibres orient predominantly along the weld path. Tool temperature is held at 100 °C with oil heating. Ejection is delayed until surface temperature drops below 90 °C to reduce weld-land warpage. Pre-drying follows 120 °C for 4 h, and hot-runner residence time is kept below 5 min to limit polymer degradation that would reduce mechanical performance after welding.

    Electrical creepage is verified under IEC 60664-1:2020 for pollution degree 2. Comparative tracking index is measured according to IEC 60112:2020 on welded specimens because the weld interface can influence surface tracking behaviour. Where pack voltage exceeds 60 V DC, insulation coordination must be revalidated for the exact colour and weld configuration. The finished parts are battery slave-module covers and current-sensor retainers that require dimensional stability, low warpage, and particle-free laser joining without adhesive.

    Solenoid Valve Bodies and Helium Leak-Tightness After Contour Welding

    Hydraulic solenoid valve bodies are joined with a continuous circular weld seam between the TP150-002 cover and a laser-absorbing PBT-GF30 body. The joint uses an interference fit of 0.05 mm on the outer locating rim and a flat weld land of 3.0 mm width. A glass clamping sleeve transmits the laser beam and applies axial force up to 1.8 kN on a 40 mm diameter cover, corresponding to 1.4 N/mm² clamp pressure. The clamping force is applied before lasing begins to prevent initial weld-line flash and to ensure uniform collapse.

    The preferred laser source is a direct diode laser at 980 nm with a top-hat intensity distribution. A top-hat profile reduces peak thermal degradation at the weld centre compared with a Gaussian beam, which is more critical in glass-filled PBT because the heat-affected zone is shallower and carbon-black absorber response is rapid. Weld speed is set between 15 mm/s and 25 mm/s, and collapse is controlled to 0.08–0.12 mm to retain port flatness. The beam is defocused to a 2.2 mm spot to widen the melt pool without increasing peak irradiance.

    After welding, parts are stabilised at 23 °C and 50 % RH for 24 h before leakage testing. Helium leak detection is performed according to ISO 20485:2017 or the customer-specific equivalent; a typical rejection limit is 1×10⁻⁵ mbar·l/s. Sample burst-pressure testing is conducted at 3× working pressure but must remain below the design limit of the valve body. Published data for this specific TP150-002 top-hat welded configuration is limited, so serial production parameters require validation on the final valve-body geometry.

    ApplicationWeld land thicknessWavelengthWeld speedClamp pressureCollapseAcceptance reference
    ECU cover2.0 mm980 nm20–40 mm/s2–4 N/mm²0.10–0.20 mmISO 20653:2013 IP6K7
    Transmission-mount sensor1.8 mm980 nm15–25 mm/s1.5 N/mm²0.08–0.12 mmHelium leak 1×10⁻⁵ mbar·l/s
    Battery-management cover2.0 mm980 nm25–35 mm/s2–3 N/mm²0.12–0.18 mmIEC 60664-1:2020
    Solenoid valve3.0 mm980 nm top-hat15–25 mm/s1.4 N/mm²0.08–0.12 mmISO 20485:2017

    Because hand-held power-tool trigger modules require black-on-black joints with high impact resistance, TP150-002 is used for the laser-transparent upper module and is paired with a laser-absorbing PBT-GF30 lower module. The part design includes a 1.2 mm-wide weld rib and a 0.3 mm collapse stop. The stop prevents over-welding when clamp force is applied and avoids excessive molten polymer ejection into the trigger cavity. The weld seam is placed around the cable exit and along the outer retention edge, away from the moving trigger surfaces.

    Impact performance is measured by notched Charpy according to ISO 179-1:2020. Glass-fibre orientation at the weld seam is controlled by a film gate at the cable exit, which creates longitudinal flow along the weld path. This orientation increases impact strength in the weld zone but can reduce near-infrared transmission, so laser power is raised while weld speed is held constant. Moulding uses a melt temperature of 260 °C and a tool temperature of 100 °C. Pre-drying follows 120 °C for 4 h with residual moisture below 0.02 wt%.

    Laser welding is performed by contour welding with two passes at 30 mm/s to widen the melt pool without increasing peak temperature. The resulting trigger module is tested for mechanical impact and drop performance under IEC 62841-1:2014. The black-on-black joint eliminates adhesive bond lines and allows downstream assembly of the switch module without additional sealant. Published process data for this specific combination is limited, so weld-strength and drop-test results are confirmed on serial mouldings.

    When an 85 °C / 85 % RH Damp-Heat Sequence Is Required for Outdoor Enclosures

    Outdoor telecommunication enclosures with laser-welded access covers are sometimes moulded from glass-reinforced PBT for dimensional stability under solar load. TP150-002 should be used only after verifying damp-heat endurance because PBT is susceptible to hydrolytic molecular-weight reduction above 60 °C in moist environments. Test programmes follow IEC 60068-2-78:2013 at 85 °C and 85 % RH for 1,000 h, followed by impact testing under ISO 179-1:2020 and flexural modulus measurement under ISO 178:2019. Published data for TP150-002 under this exposure is limited, and batch-specific validation is required before series approval.

    If damp-heat qualification is required, injection moulding must minimise moisture entrapment and surface defects. Pellets are dried to 0.015 wt% residual moisture, melt temperature is held below 270 °C, and hot-runner residence time is kept below 5 min to limit hydrolytic chain scission during processing. Laser welding is performed within 72 h of moulding or after drying at 80 °C for 8 h to remove surface moisture that can form steam bubbles under the weld interface. The weld seam is placed on a vertical wall rather than a horizontal surface to limit water pooling at the joint.

    Edge thickness is increased to 2.5 mm to compensate for modulus loss after damp-heat aging. If continuous outdoor exposure includes ultraviolet radiation, a UV-stabilised cover grade or opaque topcoat should be used because unreinforced PBT surface layers can chalk after prolonged weathering. These restrictions define the operational boundary for TP150-002 in outdoor enclosures where hydrolytic stability and UV resistance are part of the acceptance specification.

    Validation areaStandardCondition or limitPurpose
    ECU cover sealingISO 16750-4:2010−40 °C to 85 °C thermal shockWeld-seam integrity under thermal cycling
    Transmission-mount sensorISO 20485:20171×10⁻⁵ mbar·l/s heliumLeak tightness after fluid exposure
    Battery-management coverIEC 60664-1:2020Pollution degree 2Clearance and creepage verification
    Solenoid valveISO 20485:2017Helium leak after contour weldingPressure-retention validation
    Power-tool trigger moduleIEC 62841-1:2014Drop and mechanical impactHand-held tool safety
    Outdoor enclosureIEC 60068-2-78:201385 °C / 85 % RH, 1,000 hHydrolytic stability assessment
    Free Quote

    Competitive Lanxess Pocan® PBT+GF30% Laser-Weld TP150-002 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Lanxess Pocan® PBT+GF30% Laser-Weld TP150-002 is a 30 wt% glass-fiber-reinforced polybutylene terephthalate compound supplied as black granules and formulated with an infrared-transparent black pigment package for through-transmission laser welding. The grade is intended for injection-moulded covers, housings, brackets, and sensor bodies in which a clean, particle-free weld plane is required without adhesives or mechanical fasteners. Published nominal density is 1.57 g/cm³ per ISO 1183, the melting temperature is 225 °C per ISO 11357-1/-3, and the melt volume-flow rate is 15 cm³/10 min at 260 °C under a 5 kg load per ISO 1133. The following table lists the nominal dry-as-moulded property set at 23 °C.

    Nominal property profile
    PropertyNominal valueTest method
    Density1.57 g/cm³ISO 1183
    Tensile modulus, 1 mm/min9200 MPaISO 527-1/-2
    Tensile stress at break130 MPaISO 527-1/-2
    Nominal strain at break2.5%ISO 527-1/-2
    Charpy unnotched impact, 23 °C45 kJ/m²ISO 179/1eU
    Charpy notched impact, 23 °C8 kJ/m²ISO 179/1eA
    Heat-deflection temperature, 1.8 MPa200 °CISO 75-1/-2
    Vicat softening temperature, B120210 °CISO 306
    Moulding shrinkage, flow/transverse0.2/0.8%ISO 294-4

    At 30 wt% glass-fiber reinforcement, the compound occupies a stiffness class above unfilled laser-welding PBT grades and below high-fiber alternatives. The tensile modulus of 9200 MPa is significantly higher than that of an unfilled PBT formulation, while the heat-deflection temperature of 200 °C at 1.8 MPa supports applications requiring short-term thermal load resistance. The glass fiber also reduces isotropic shrinkage and increases load-bearing capacity, but it introduces optical scattering and anisotropic mechanical behavior. The published property values are single-point nominal figures, not design minima, and the specific pigment lot may shift laser transmission without changing the visible black colour.

    What Limits Laser Transmission in a 30% Glass-Fiber PBT Joint?

    Through-transmission laser welding requires the upper component to transmit sufficient incident diode-laser energy at 808–980 nm to melt the absorbing lower component at the faying surface. Conventional black PBT compounds containing carbon black absorb strongly across the near-infrared spectrum; the outer surface heats before the interface reaches the PBT melting temperature. TP150-002 substitutes an infrared-transparent black pigmentation package, so the moulded part remains visually black while allowing near-infrared radiation to reach the joint plane. The glass-fiber phase complicates this transmission path. The refractive index mismatch between PBT and E-glass causes multiple internal reflections and beam divergence, and the degree of divergence depends on fiber orientation, thickness, and local moulded-in stress. Transmission measured on polished plaques is therefore not directly transferable to textured, grained, or weld-line-containing production parts. In a production laser-welding cell, the transparent-shell transmission should be mapped on the actual moulded part with a diode laser at the intended wavelength and an integrating sphere or power meter.

    At the joint interface, the melt film must exceed 225 °C to achieve PBT melting, but it should remain below 260–270 °C because prolonged exposure above that range causes thermo-oxidative and hydrolytic chain scission, surface yellowing, and void formation. The practical process window is narrow. At 2 mm wall thickness, glass-fiber scattering may reduce transmitted power to a low single-digit percentage of the incident beam, forcing higher laser power or longer dwell. Excessive power creates surface blistering, fiber bloom, and weld flash; insufficient power creates a cold joint with minimal interfacial healing. Production trials therefore require destructive tensile-pull or burst testing and cross-section microscopy to establish part-specific limits, because published data for this specific configuration are limited. Weld-collapse displacement is often controlled in the range of 50–200 µm to avoid dimensional shift while ensuring molten material at the interface.

    Three common scanning modes are contour welding, quasi-simultaneous welding, and simultaneous welding. In contour welding, a focused beam traverses the joint line once or several times; the local heating spike is short, and fibre-filled PBT can cool before the next pass unless the scan speed and power are matched. Quasi-simultaneous welding scans the beam at high speed around the weld path multiple times, integrating heat and allowing more even collapse. Simultaneous welding uses an array of diode laser emitters around the weld line and is preferred where flatness errors from fibre-induced warpage must be compensated by the clamp. For this 30 wt% glass-fiber grade, quasi-simultaneous welding is often selected because it reduces the influence of local transmission variation, but the final selection depends on part geometry and leak-rate requirements.

    The weld joint should be a lap-shear or tongue-and-groove configuration with a defined melt-collapse path. A flat energy-director style rib used in ultrasonic welding is generally not appropriate for through-transmission laser welding; instead, the upper and lower parts should contact uniformly under a defined clamping force. Glass-fiber-filled PBT requires close tolerances on the mating surfaces because high fiber content reduces melt-flow and prevents large collapse from filling gaps. Gaps below 0.05 mm are commonly targeted, but achievable values depend on mould accuracy and part size. Larger gaps require excessive local melting and can cause weld flash or displacement of the transparent layer.

    Hydrolytic degradation and mould-based contamination can also reduce laser transmission. Dust, mould release migration, and silicone-based parting agents absorb or scatter the beam and should be kept off the weld surface. The grade should not be welded to itself if both halves are laser-transparent; one mating surface must be laser-absorbing. A common production configuration uses TP150-002 for the transparent upper shell and a carbon-black PBT GF30 for the absorbing base.

    Moisture Conditioning and Injection-Moulding Window

    Before melt processing, the polymer must be dried because PBT is hydrolytically sensitive at processing temperature. A desiccant dryer with a dew point below -30 °C and drying at 120 °C for 4 h reduces residual moisture below 0.04% as measured by Karl Fischer titration per ISO 15512. Higher residual moisture produces viscosity loss, splay on the visible surface, and reduced weld strength because steam porosity can form during the laser heat pulse. Melt temperature is normally controlled between 260 °C and 280 °C, and mould temperature between 80 °C and 100 °C. The upper mould-temperature boundary increases crystallinity and reduces residual stress on the weld plane, but it extends cooling time and may reduce productivity. Barrel residence time should be kept short; accumulated hot residence beyond approximately 8–10 min can yellow the material and degrade infrared transmission. Injection speed, hold pressure, and gate position must be tuned for fiber orientation. Flow-direction moulding shrinkage is approximately 0.2%, while transverse shrinkage is approximately 0.8% per ISO 294-4. This difference means that gate location changes the fiber orientation field and the local transmission, producing anisotropic weld strength in the final assembly.

    Multi-cavity tools for this compound should use generous gates and a hot-runner manifold designed for glass-fiber-filled PBT. Screw geometry with a low compression ratio and hardened barrel components is preferred because glass fiber accelerates abrasive wear. Back pressure is typically held at 2–5 MPa hydraulic to maintain melt homogeneity, but excessive back pressure can overheat the heat-sensitive pigment package. If recycled regrind is used, laser transmission must be revalidated on samples containing the actual regrind ratio.

    For electrical housings, the relevant performance indicators are comparative tracking index, glow-wire flammability, and surface resistivity. Published data for this specific grade should be taken from the manufacturer’s product data sheet; general PBT GF30 grades often exhibit a comparative tracking index around 250 V and a glow-wire ignition temperature in the range of 650–750 °C, but pigment and fibre packages shift these values. Users should not transfer a UL Yellow Card from a carbon-black grade to this laser-welding variant without verifying the specific colour and wall thickness. Dielectric strength and arc resistance are also thickness-dependent and should be measured on the final moulded part per IEC 60243 and IEC 61621 respectively.

    When Through-Transmission Welding Replaces Ultrasonic or Hot-Plate Joining

    In clean-room sensor assembly, laser welding is selected where ultrasonic welding would transfer mechanical vibration to pressure sensors, crystal oscillators, or sealed electronic circuits, and where hot-plate welding would generate macroscopic melt flash or require heated-tool contact with the exposed part surface. TP150-002 enables black-on-black joints: the infrared-transparent black upper component can be welded to a laser-absorbing lower body without sacrificing uniform exterior colour. This is the principal difference from standard carbon-black PBT GF30 grades, which cannot serve as the laser-transparent component because carbon black absorbs the incident beam at the outer surface. Compared with unfilled laser-welding PBT, the 30 wt% glass-fiber grade raises the tensile modulus to 9200 MPa and the heat-deflection temperature to 200 °C, which supports brackets and housings that must retain dimensional accuracy under thermal load. The trade-off is reduced near-infrared transmission and higher melt viscosity, which makes thin-wall filling more difficult and requires larger gates or higher injection pressure than an unfilled grade.

    Relative to a chemically identical glass-fiber PBT without the laser-welding pigment, the mechanical property envelope is comparable, but ultraviolet weathering and colour stability may differ because the non-carbon-black pigment system does not provide the same UV screening as carbon black. Applications with long-term outdoor exposure require additional UV stabilization or opaque coating. The grade is also not a hydrolysis-stabilized PBT; continuous hot-water or high-humidity service above 60 °C should be evaluated separately. Contact with strong alkaline solutions, amines, or certain strong acids can attack the surface and should be avoided. For chemical exposure, users should test the final welded assembly under the actual fluid, temperature, and stress state because residual weld stress accelerates environmental stress cracking in some media.

    Automotive sensor housings moulded from TP150-002 are typically produced in multi-cavity hot-runner tools with clamp forces in the range of 80–120 t for cavity counts of 8–16, depending on shot volume. A representative manufacturing sequence involves drying the granules in a wheel desiccant dryer at 120 °C, injecting at a melt temperature of 270 °C and a mould temperature of 90 °C, then holding until gate freeze to minimize sink and warpage. After ejection, parts are stored in moisture-barrier packaging until welding because moisture uptake above 0.04% can produce steam porosity during the laser heat pulse. The laser cell may use a 940 nm diode laser with a clamping pressure of 0.5–2 MPa; the transparent shell is placed over the absorbing base, and clamp force is applied normal to the welding plane. Destructive testing of welded assemblies is conducted by hydraulic burst or tensile pull-off, and acceptance criteria are typically defined according to part-specific leak-rate requirements rather than a universal material specification.

    Documentation for this grade should include the latest REACH SVHC declaration, the EU RoHS certificate for Directive 2011/65/EU with delegated amendment (EU) 2015/863, and a lot-specific certificate of analysis. The material is not typically supplied as a food-contact grade; users requiring food-contact status should request a separate declaration. The UL Yellow Card rating, if cited, applies only to the tested wall thickness and colour; the laser-welding pigment can alter flammability and glow-wire performance relative to a standard carbon-black PBT GF30. Published data for this specific configuration are limited for laser transmission through textured or grained surfaces; grain depth and orientation can scatter the incident beam and reduce transmitted power relative to a smooth polished surface.

    Top