| HS Code | 331716 |
| Density Iso 1183 | 1.53 g/cm³ |
| Glass Fiber Content | 30% |
| Tensile Modulus Iso 527 1 2 | 10000 MPa |
| Tensile Strength Iso 527 1 2 | 135 MPa |
| Elongation At Break Iso 527 1 2 | 2.5% |
| Charpy Notched Impact Strength At 23 C Iso 179 1ea | 9 kJ/m² |
| Hdt A At 1 8 Mpa Iso 75 1 2 | 205 °C |
| Hdt B At 0 45 Mpa Iso 75 1 2 | 220 °C |
| Vicat Softening Temperature B120 Iso 306 | 205 °C |
| Melting Temperature Iso 11357 1 3 | 225 °C |
| Water Absorption At 23 C 24 H Iso 62 | 0.4% |
| Molding Shrinkage Parallel Iso 294 4 | 0.3% |
| Molding Shrinkage Normal Iso 294 4 | 0.9% |
| Comparative Tracking Index Iec 60112 | 600 V |
| Flammability Ul 94 | HB |
| Hydrolytic Stabilization | Yes |
As an accredited Lanxess Pocan® PBT+GF30%-Hydrolytic B3233HR factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Supplied in 25 kg moisture-resistant paper bags, palletized; store Lanxess Pocan® PBT+GF30%-Hydrolytic B3233HR dry and sealed. |
| Container Loading (20′ FCL) | Loaded in a 20-foot FCL container, Lanxess Pocan PBT+GF30%-Hydrolytic B3233HR packed in bags on pallets, secured for ocean transport. |
| Shipping | Lanxess Pocan® PBT+GF30%-Hydrolytic B3233HR is shipped as non-hazardous thermoplastic granules in moisture-proof bags or octabins. It is not classified as dangerous goods for transport and has no UN number. Keep dry, avoid excessive heat, and protect packaging from damage. |
| Storage | Store Lanxess Pocan® PBT+GF30%-Hydrolytic B3233HR in a dry, cool, well-ventilated area using original sealed packaging. Protect from moisture, direct sunlight, heat, and ignition sources. Keep away from oxidizers, acids, and bases. Maintain closed, clearly labeled compatible containers, prevent humidity ingress, avoid prolonged storage above recommended temperatures, and follow the supplier’s SDS. |
| Shelf Life | Lanxess Pocan® PBT+GF30%-Hydrolytic B3233HR shelf life is typically 12 months in unopened, dry original packaging at room temperature; protect from moisture. |
In convoluted engine-compartment wiring systems, ambient air temperature cycles between -40 °C and 125 °C. A 30 wt% glass-fibre-reinforced hydrolysis-stabilized polybutylene terephthalate such as Lanxess Pocan B3233HR is employed for connector bodies and ECU housing shells. The 30 wt% fibre fraction raises tensile modulus to 9,500–11,000 MPa when tested to ISO 527-2 at 23 °C. It also reduces mould shrinkage to 0.2–0.5 % per ISO 294-4. This shrinkage control stabilizes terminal pitch in high-count connector mouldings. Hydrolysis resistance matters because damp heat at 85 °C/85 % RH accelerates autocatalytic chain scission in unreinforced PBT. The stabilized grade is processed on a 120 t hydraulic injection moulding machine with 25 mm screw diameter and L/D 20:1. Barrel set points are 250–270 °C, nozzle 260–270 °C, and mould temperature 80–110 °C. Pre-drying at 120 °C for 4 h in a desiccant dryer to residual moisture below 0.02 % is mandatory. Moisture above this threshold hydrolyzes the melt during plastication. Regrind is restricted to a maximum of 30 % in non-appearance housings. Repeated heat history reduces hydrolysis stabilizer efficiency. Terminal parts include engine ECU housings, camshaft sensor connectors, and throttle body connectors.
| Requirement | Standard / test | Condition | Acceptance range |
|---|---|---|---|
| Damp heat cyclic | ISO 16750-4 | 85 °C / 85 % RH, 1,000 h | No visible cracking; tensile strength retention ≥ 70 % |
| Mould shrinkage | ISO 294-4 | 60 × 60 × 2 mm plaque, flow/normal | 0.2–0.5 % |
| Tensile modulus | ISO 527-2 | 23 °C, 5 mm/min | 9,500–11,000 MPa |
| Charpy impact | ISO 179-1eU | 23 °C, edgewise, unnotched | 45–60 kJ/m² |
Coolant pump impellers and thermostat covers moulded from hydrolysis-stabilized PBTP-GF30 are exposed to pressurized water-glycol. Cold-start temperatures reach -40 °C. Local hot spots reach 110 °C. The 30 wt% glass reinforcement provides creep resistance under radial pump loads when measured to ISO 899-1. The hydrolysis package retards molecular weight loss in hot water. However, PBTP remains a semi-crystalline polyester with an ester linkage. Hydrolysis is slowed but not eliminated. The continuous-use ceiling in pure water is approximately 80–90 °C depending on wall thickness and glycol concentration. In 50/50 ethylene glycol-water coolant above 110 °C, published data for this specific grade is limited. PPS or polyphthalamide grades are typically substituted above this boundary. Moulding of pump impeller tools with L/D 22:1 screws requires melt temperature 250–265 °C. Mould temperature is kept at 90–120 °C to maximize crystallinity. Holding pressure is 60–80 MPa with gate freeze times above 6 s to prevent voids in the hub. The high glass content produces anisotropic shrinkage. Impeller vane warpage is controlled with three radial gate positions rather than a single sub-gate. Failure modes observed on production-scale machines include gate blush and fibre-starved weld lines at the vane/hub junction. These defects reduce burst pressure under ISO 16750-4 pressure-temperature cycling. Coolant additives outside pH 8–9 should be validated by ASTM D543-20. Strongly alkaline heat-transfer fluids accelerate surface attack. Terminal parts include water pump impellers, thermostat housings, and heater control valves.
Where proximity sensors and inductive actuators are installed in high-pressure washdown lines, the housing must withstand repeated jet impact at 80–100 bar and 80 °C per ISO 20653 IP69K. PBTP-GF30-HR is moulded into cylindrical M12 and M18 sensor bodies with wall thicknesses of 1.5–2.0 mm. The 30 % short-glass reinforcement limits tensile creep under axial cable strain, tested to ISO 899-1 at 23 °C. Thermal expansion in the 23–60 °C washdown cycle is 40–50 × 10⁻⁶ K⁻¹ in flow direction. This value must be matched to brass threaded inserts. For insert retention, moulded-in M12 brass inserts are specified with a minimum engaged length of 6 mm. Typical pull-out force specifications range from 1,000 N to 2,000 N depending on knurl geometry. Diamond knurl is preferred because PBTP-GF30 develops lower hoop stress than unfilled PBT. Chemical exposure to alkaline foam cleaners at pH >12 and 60 °C causes surface saponification of the polyester matrix. Suitability must be tested per ASTM D543-20 for the specific cleaner. Moulding requires melt temperature 255–270 °C. Mould temperature is 100–120 °C for insert adhesion. Packing pressure is 50–70 MPa to avoid sink marks at the insert boss. Terminal parts include threaded sensor housings, washdown-rated cable glands, and mounting flanges for process automation. Published data for this specific grade under IP69K combined with alkaline cleaning is limited. Validation on production tooling is required.
Brush holder plates and motor end caps in hand-held electric tools are moulded from PBTP-GF30-HR. The 30 % glass fibres provide heat deflection temperature above 195 °C by ISO 75-2 method A at 1.8 MPa. This value is above the maximum internal winding temperature observed in locked-rotor tests. The main process conflict is weld-line formation around core pins for brush pockets. Fibre orientation normal to the weld plane reduces weld-line tensile strength to 55–70 % of the unreinforced value when tested per ISO 527-2. If the gate cannot be relocated, increasing mould temperature to 110–130 °C and injection speed beyond 300 mm/s improves molecular diffusion at the melt interface. It also raises flash risk. Hold pressure is set at 60–80 MPa for 4–6 s on tools with L/D 20:1 reciprocating screws. Terminal components include brush card carriers, motor end caps, and trigger housing halves. Compliance for hand-held tools is evaluated against EN 60745-2-1 and UL 60745-1. Ball-pressure testing is performed at 125 °C per IEC 60695-10-2 for parts in contact with current-carrying components. The grade’s HB flammability classification under UL 94 does not meet V-0 in some double-insulated designs. If a flame-retardant PBTP-GF30 variant is required, it must be qualified separately. Incoming moulding resin should be controlled by ISO 1172 glass content at 30 ± 2 %. Fibre length distribution variations alter weld-line impact.
When a battery management system carrier integrates cell-voltage sense leads, temperature sensor guides and busbar retention ribs, the polymer must resist creep under vibration. It must also manage dimensional change after thermal cycling from -40 °C to 85 °C and condensation caused by module temperature swings. In this configuration, PBTP-GF30-HR is moulded at wall thickness 1.2–1.8 mm. Melt temperature is 250–265 °C. Mould temperature is 90–120 °C. High mould temperature creates spherulitic crystallinity that reduces post-mould shrinkage to 0.15–0.35 % per ISO 294-4. Terminal product includes low-voltage BMS carrier frames, cell monitoring unit housings, and connector alignment plates. Compliance validation follows ISO 6469-1 for on-board electrical energy storage. Vibration and mechanical integrity are assessed under UN ECE R100 Rev.3. Creepage and clearance are evaluated per IEC 60664-1. The grade is not intended for high-voltage insulation barriers where UL 94 V-0 at 0.8 mm and comparative tracking index above 600 V per IEC 60112 are mandatory. A flame-retardant PBTP-GF30 or PBT/ASA blend must be used for those parts. On production-scale hot-runner tools, uneven heating above 270 °C at the valve-gate tip causes localized black specks. Barrel residence time is limited to 5 min. Screw rotation speed is set to 80–120 min⁻¹. Incoming resin moisture below 0.02 % after drying at 120 °C for 4–6 h in a desiccant dryer is mandatory.
In HVAC actuator housings and condensate drain valves, repeated condensation cycling between 5 °C chilled water and 60 °C coil air induces differential expansion stresses at gear pins and drive shafts. PBTP-GF30-HR is selected when mineral-filled polyamide absorbs excessive moisture and loses dimensional control. The PBT grade exhibits water absorption below 0.5 % by ISO 62 after 24 h immersion at 23 °C. Moulded parts are gasket-sealed against a flat face. Flatness of 0.15 mm over 100 mm length is maintained by holding pressure 50–70 MPa and cooling time 20–30 s for a 2.0 mm wall. Terminal application includes damper actuator covers, condensate valve bodies, and humidity sensor housings. Compliance is evaluated under EN 60730-1 for automatic electrical controls. Ball-pressure testing at 125 °C is performed per IEC 60695-10-2. The ester matrix is susceptible to surface attack by strongly alkaline coil cleaners at pH >11. Compatibility with specified maintenance chemicals should be validated using ASTM D543-20. Published data for this specific grade in open condensate systems is limited. Material selection should be confirmed by test coupons on the actual moulding line.
Competitive Lanxess Pocan® PBT+GF30%-Hydrolytic B3233HR prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Lanxess Pocan® PBT+GF30%-Hydrolytic B3233HR is a hydrolysis-stabilized polybutylene terephthalate compound reinforced with 30 % glass fiber by mass. The material is supplied in natural color and is referenced as B3233HR 000000 in the Lanxess product range. The grade is formulated for injection-molded components exposed to hot water, aqueous coolant media, condensation, or repeated high-humidity thermal cycling where conventional PBT-GF30 compounds can undergo chain scission, surface embrittlement, and loss of impact strength. The compound combines the stiffness and creep resistance of 30 % short-glass reinforcement with a stabilization package intended to retard ester hydrolysis in the polymer matrix. Typical applications include automotive cooling-circuit connectors, sensor housings, water pump impellers, appliance pump bodies, and electrical enclosures. Processing requires pre-drying to a residual moisture content of 0.02 % or lower before melt processing.
The following values are typical for natural-color specimens injection-molded in accordance with ISO 294-1 and conditioned at 23 °C/50 % RH according to ISO 291. These are not specification minima; colorants, regrind content, and molding conditions can shift the measured result.
| Property | Test method | Typical value |
|---|---|---|
| Glass fiber content | ISO 3451-1 | 30 % |
| Density | ISO 1183-1 | 1.53 g/cm³ |
| Tensile modulus | ISO 527-1/-2 | 10,500 MPa |
| Tensile stress at break | ISO 527-1/-2 | 135 MPa |
| Nominal strain at break | ISO 527-1/-2 | 2.5 % |
| Flexural modulus | ISO 178 | 9,800 MPa |
| Flexural strength | ISO 178 | 215 MPa |
| Charpy notched impact, 23 °C | ISO 179/1eA | 8.0 kJ/m² |
| Melt volume-flow rate, 260 °C/2.16 kg | ISO 1133-1:2022 | 15 cm³/10 min |
| Heat deflection temperature, 1.8 MPa | ISO 75-1/-2 | 200 °C |
| Vicat softening temperature, VST/B50 | ISO 306 | 220 °C |
| Comparative tracking index | IEC 60112 | 250 V |
| Water absorption, saturation at 23 °C | ISO 62 | 0.4 % |
The primary difference is not dry-state tensile strength or modulus. Standard PBT-GF30 and the B3233HR hydrolysis-resistant variant can exhibit similar initial mechanical values at 23 °C. The functional difference appears after exposure to hot water, wet heat, or condensation. In a non-stabilized PBT-GF30, ester bond cleavage during wet aging produces new carboxyl end groups. These end groups can autocatalyze further hydrolysis, accelerating molecular weight reduction and converting a ductile glass-reinforced polymer into a brittle material with low elongation at break and low notched impact. B3233HR is formulated to suppress this autocatalytic pathway. The exact stabilizer chemistry is proprietary, and published data on the specific additive composition is limited, but the effect is measured as a slower loss of strain at break and notched Charpy impact after humid aging compared with conventional PBT-GF30.
Compared with heat-stabilized PBT-GF30 grades intended for dry hot-air service, B3233HR is specifically targeted at aqueous media. A grade stabilized for oxidation may retain stiffness in dry heat but still fail through hydrolysis when water is present. Compared with unreinforced hydrolysis-resistant PBT, the 30 % glass fiber content raises tensile modulus by a factor of approximately 4 and reduces isotropic mold shrinkage, but it also introduces anisotropic shrinkage and a greater sensitivity to weld-line strength reduction. Compared with mineral-filled PBT grades, the glass-fiber variant provides higher load-bearing stiffness at elevated temperature, but it has more pronounced fiber orientation effects in thin-walled parts.
Hydrolytic degradation in PBT proceeds through ester-bond cleavage in the presence of water. Each cleavage event creates a new acid end group, which can protonate additional ester linkages and accelerate the reaction. In an unstabilized PBT matrix, this autocatalytic cycle causes a nonlinear loss of molar mass. Hydrolysis-resistant grades such as B3233HR are formulated to interrupt the cycle, either by limiting the active carboxyl end-group concentration or by scavenging acidic species. The result is not complete immunity to hydrolysis; it is a delay in the transition from ductile fracture to brittle fracture.
At 85 °C/85 % RH, glass-fiber-reinforced PBT absorbs moisture at the fiber-matrix interface. Capillary transport along exposed glass fibers can deliver water to the interior of a molding more rapidly than matrix-controlled Fickian diffusion. This is particularly important at knit lines, gate regions, and machined surfaces where cut fibers are open to the environment. A part can therefore show surface whitening or microcracking earlier than a homogeneous tensile bar from the same material. Comparative aging data for this specific B3233HR configuration is limited, but the grade is routinely specified where tensile strength retention and notched impact retention after 85 °C/85 % RH exposure are the acceptance criteria.
Water-glycol mixtures above 100 °C increase the hydrolysis rate. Continuous exposure to pressurized hot water above 100 °C, concentrated acids, strong alkalis, or long-term contact with amines should be validated for each part design. Amine-based additives can catalyze ester cleavage and should be avoided unless compatibility has been demonstrated.
At 260 °C/2.16 kg, the melt volume-flow rate of 15 cm³/10 min permits filling of wall sections down to about 1.5 mm in most cold-runner molds. For wall sections below 0.8 mm, high injection speed, adequate venting, and gate diameters of at least 60 % of part wall thickness are required. The glass fiber content also raises thermal conductivity relative to unfilled PBT, but the melt remains shear-thinning; therefore gate shear rate should be kept below 100,000 s⁻¹ to avoid excessive fiber breakage and surface defects. Fiber length preservation is critical because notched impact and fatigue resistance decline when glass fiber length falls below approximately 300 µm after plastication.
If barrel residence time exceeds 8 min, melt temperature should be reduced toward 250 °C, and shot size should be increased or cycle time reviewed. Thermal degradation of PBT above 270 °C generates tetrahydrofuran and additional carboxyl end groups. The carboxyl end groups then accelerate wet-aging hydrolysis even after the molded part has cooled. On production-scale injection molding machines with a 22:1 L/D three-zone screw, nozzle melt temperature variation greater than ±5 °C can produce visible gloss variation and shift post-mold shrinkage by more than 0.1 % absolute. Such variation is often caused by incorrect back pressure, worn check ring, or excessive screw recovery speed.
The recommended screw configuration is a general-purpose three-zone screw with a compression ratio of 2.5:1, a non-return valve, and no sharp dead spots. Back pressure of 5–10 MPa supports glass-fiber dispersion without excessive shear heating. Screw speed should be set between 50 min⁻¹ and 150 min⁻¹ depending on screw diameter; small-diameter screws should use the lower range. The holding-pressure profile should be set to deliver cavity pressure of 40–60 MPa and to hold gate freeze. Premature gate freezes below 80 °C mold temperature can produce sink marks and dimensional instability.
Pre-drying is mandatory. The compound should be dried in a desiccant dryer at 120 °C for 4–6 h to a residual moisture content of 0.02 % or less. The dew point of the drying air should be −30 °C or lower. If bags have been opened and exposed to 60 % RH for more than 24 h, the drying time should be extended to 6 h. Residual moisture above 0.02 % causes silver streaks, reduced notched impact, and hydrolysis during plastication.
| Parameter | Recommended range | Unit |
|---|---|---|
| Pre-drying temperature | 120 | °C |
| Pre-drying time | 4–6 | h |
| Drying air dew point | ≤ −30 | °C |
| Maximum residual moisture | 0.02 | % |
| Melt temperature | 250–270 | °C |
| Mould temperature | 80–100 | °C |
| Maximum barrel residence time | 8 | min |
Regrind use should be limited to 25 % by mass with virgin material. Higher regrind fractions reduce notched impact and increase lot-to-lot shrinkage variability. Hot-runner manifolds should be externally heated with no dead spots; internal runner diameters below 6 mm can produce excessive shear heating and fiber damage. Gate size should be at least 60 % of the nominal wall thickness, and gate location should place knit lines away from pressure-loaded or wet-exposed regions. Mold shrinkage is anisotropic because of glass-fiber orientation. For an edge-gated plaque, machine-direction linear shrinkage is typically 0.2–0.3 %, while transverse shrinkage is 0.6–0.8 %. Mold designers should apply these ranges in flow simulation rather than using a single isotropic shrinkage factor.
In production, the grade is used for injection-molded automotive cooling-circuit connectors, sensor housings, water pump impellers, and appliance pump bodies. These applications impose wet environments and dimensional constraints. The limiting criterion is usually not initial tensile strength but retention of notched Charpy impact after hot, humid aging. Compliance with Directive 2011/65/EU and Regulation (EC) No 1907/2006 should be verified for the specific colorant package, because additives can affect RoHS and REACH conformity. The material is not marketed as a flame-retardant grade; if a UL 94 V-0 classification is required, a different Pocan® grade should be selected. Published data for specific long-term hot-water life in complex parts is limited; component-level validation under actual coolant chemistry, pressure cycling, and wall thickness is required.