| HS Code | 761733 |
| Polymer Type | PBT (polybutylene terephthalate) |
| Glass Fiber Content | 30% |
| Flame Retardant System | Halogen-free |
| Ul 94 Flammability Rating | V-0 |
| Density | 1.53 g/cm³ |
| Tensile Modulus | 9500 MPa |
| Tensile Strength At Break | 120 MPa |
| Elongation At Break | 2.5% |
| Charpy Impact Strength Unnotched | 40 kJ/m² |
| Charpy Notched Impact Strength | 8 kJ/m² |
| Hdt A 1 8 Mpa | 205 °C |
| Hdt B 0 45 Mpa | 220 °C |
| Melting Temperature | 225 °C |
| Comparative Tracking Index Cti | 600 V |
| Volume Resistivity | 1E15 Ω·cm |
| Dielectric Strength | 30 kV/mm |
| Molding Shrinkage | 0.2-0.8% |
| Melt Temperature Processing | 260-280 °C |
| Mold Temperature | 80-100 °C |
As an accredited Lanxess Pocan® PBT+GF30%-FR-NF-CTI BFN4230 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packed in 25 kg moisture-proof bags, 40 bags per pallet (1,000 kg), with product identification and safety labels. |
| Container Loading (20′ FCL) | Lanxess Pocan® PBT+GF30%-FR-NF-CTI BFN4230 is palletized and securely loaded into a 20-foot FCL container for dry, ambient transport. |
| Shipping | Lanxess Pocan® PBT+GF30%-FR-NF-CTI BFN4230 is shipped as solid thermoplastic pellets in moisture-proof bags or cartons, palletized and stretch-wrapped. It is not classified as dangerous goods for transport. Store dry, cool, ventilated, away from direct sunlight, and handle with standard industrial precautions. |
| Storage | Store **Lanxess Pocan® PBT+GF30%-FR-NF-CTI BFN4230** in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and moisture. Keep in original sealed packaging, off the floor, and protect from UV exposure. Follow first-in/first-out stock rotation and consult the SDS for any additional local requirements. |
| Shelf Life | Store sealed in original packaging, dry and below 30°C; typical shelf life is 12 months from production date. (20 words) |
In low-voltage terminal blocks and busbar supports, the Lanxess Pocan® BFN4230 grade is moulded to reconcile three competing constraints: CTI retention after thermal cycling, flame retardance at minimal wall thickness, and screw-clamp torque resistance across a multi-tier cavity layout. The grade is formulated with a nominal glass-fiber loading of 30 % by mass according to ISO 3451-1, with the remaining PBT matrix carrying a non-halogen flame-retardant package and a CTI-selective mineral system that raises the tracking index measured under IEC 60112 to 600 V. This combination is relevant for terminal blocks evaluated under IEC 60947-7-1 and UL 1059, where moulded barriers must survive screw torque without cracking and must maintain insulation integrity after contamination. Production-scale injection moulding on clamp-force machines in the 800–1,200 kN range requires pre-drying at 120 °C for 4 h in a desiccant dryer until residual moisture is below 0.02 %; hydrolysis above that threshold produces silver streaking on visible surfaces and a measurable reduction in melt viscosity due to PBT chain scission. The recommended melt temperature is 250–270 °C, while the mould temperature should be held at 80–100 °C to promote crystallization and minimize post-shrinkage in a 12-way block. Screw geometry should be a general-purpose reciprocating screw with an L/D ratio of at least 20:1 and a compression ratio of 2.0:1–2.5:1; back pressure of 30–60 bar and screw surface speed of 0.05–0.15 m/s keep glass-fiber attrition low while maintaining dispersion of the flame-retardant package. Regrind from runners and sprues may be re-introduced up to 20 % by mass if dried identically; higher levels reduce CTI consistency and notched impact because of progressive fibre-length reduction. Moulds should use corrosion-resistant tool steel because halogen-free flame-retardant decomposition by-products can attack chrome-plated cores during high-temperature purging or extended residence. Gate placement at the thickest busbar support section reduces jetting and allows a uniform flow front into thin terminal barriers; post-mould annealing at 120 °C for 2 h is used by some processors when warpage has to remain below 0.05 mm across a 50 mm sealing face. Finished components include multi-tier screw terminal blocks, fuse holders, cross-connector insulation plates, and busbar supports rated for low-voltage switchgear.
Under IEC 62196-2 for Type 2 charging interfaces and UL 2251 for EV plugs and receptacles, the connector housing must pass dielectric withstand after thermal cycling and must resist tracking under condensation, salt mist, and dust. The material’s CTI of 600 V under IEC 60112 supports pollution degree 3 creepage distances specified in IEC 60664-1, reducing the need for enlarged creepage slots that would otherwise weaken latch features. Moulding trials on 1.2–1.8 mm wall sections show that flow balance between core and cavity is critical: glass-fibre orientation in a non-uniform melt front creates differential shrinkage in the longitudinal and transverse directions, producing latch flatness deviation. Valve-gated hot runners with sequential opening per cavity are applied to keep the flow front symmetrical; the hot-runner manifold is externally heated and the nozzles are sized to avoid dead spots where flame retardant can degrade during colour changes. Pre-drying must be at 120 °C for 4 h to a residual moisture below 0.02 %, and melt temperature should be limited to 255–270 °C at the nozzle. Mould temperature between 90 °C and 100 °C is specified to crystallize the thin lip around the terminal socket; lower mould temperature produces an amorphous skin that can fail glow-wire testing at the same wall thickness. Injection speed is profiled high during the first 70–80 % of fill, then reduced at the latching boss to prevent flash on the parting line, which is unacceptable in connector faceplates. Back pressure should remain below 50 bar to avoid over-shearing the flame-retardant package. Regrind usage is limited to 15 % because the combination of thin-wall flow length and GF30 reduces weld-line strength; published data for this specific configuration is limited, so processors commonly qualify each sprue/runner ratio with a puncture impact test according to ISO 6603-2. Finished parts include charging plug body shells, inlet socket housings, locking ring carriers, and internal insulation shields. Material compliance statements should be verified against the current EU RoHS Directive 2011/65/EU and REACH regulation 1907/2006 SVHC list.
| Requirement | Test method | Material condition |
|---|---|---|
| Tracking resistance | IEC 60112 | CTI 600 V |
| Vertical burn at reduced wall | UL 94 | V-0 at 0.75 mm |
| Hot-wire ignition | UL 746A | PLC category per current UL Yellow Card |
| Relative thermal index, electrical | UL 746B | Value per current UL Yellow Card; end-system insulation class prevails |
| Glow wire flammability index | IEC 60695-2-12 | To be confirmed at final component wall thickness |
| Glow wire ignition temperature | IEC 60695-2-13 | To be confirmed at final component wall thickness |
A photovoltaic combiner enclosure moulded from this non-halogen flame-retardant PBT grade must satisfy glow-wire and track-resistance requirements while supporting copper busbars, DC disconnect switches, and array wiring terminals under IEC 62790 and UL 373. The 30 % glass-fibre reinforcement supplies sufficient flexural stiffness for a 2.0–2.5 mm housing wall, and the CTI of 600 V under IEC 60112 permits compact creepage distances inside the enclosure without sacrificing busbar clearance. Moulding is performed with a steel-safe tool that gates into a thick boss beneath the internal busbar support; this gate position avoids a weld line crossing the cable-entry aperture, where flame-retardant skin orientation is weakest. Drying follows the same desiccant-dryer regime, 120 °C for 4 h to 0.02 % or less residual moisture, because photovoltaic components often have long melt residence times in multi-cavity tools. Melt temperature is set at 250–265 °C, and the mould temperature is held at 80–95 °C to balance flatness against cycle time. Because PBT is not inherently UV-stable, black enclosures intended for outdoor direct-sunlight installation require either a carbon-black masterbatch or a co-stabilized UV additive package; non-black parts exposed to 1,000 h xenon-arc aging per ISO 4892-2 may show surface chalking and a measurable drop in CTI unless specifically validated. Regrind is generally limited to 20 % and must be dried identically; higher regrind accelerates hydrolysis and reduces tensile modulus under ISO 527-2. Finished products include combiner-box bases, DC disconnect enclosures, opaque terminal covers, and busbar isolation plates for photovoltaic arrays.
Insert moulding of coil bobbins around laminated steel or copper terminals introduces a differential-shrinkage risk that is managed by preheating the inserts and by reducing shear work in the melt. The grade is processed on a reciprocating-screw machine with a low-compression screw, typically 2.0:1 compression and 20:1 L/D, to limit additional glass-fibre breakage around brass terminal pins. Melt temperature is maintained at 250–265 °C; mould temperature is raised to 95–105 °C so that the polymer crystallizes uniformly around the insert and does not form a low-density amorphous layer that can crack under thermal cycling. Pre-drying at 120 °C for 4 h to residual moisture below 0.02 % is essential because insert tools have long flow lengths around pin-side walls. Clamp force is selected on the basis of projected area and flash risk: valve-gate nozzles are recommended to shut off cleanly at the cavity edge, preventing stringing across the bobbin flange. The electrical insulation system is evaluated under UL 1446 together with enamelled wire and varnish; the end-use thermal class depends on the complete insulation system, not on the moulded resin alone. The comparative tracking index of 600 V under IEC 60112 is relevant for coil forms exposed to humid environments under IEC 60335-1 and IEC 60730-1, where creepage currents must not lead to carbon tracks. Published data for this specific insert-moulded configuration is limited; processors typically rely on insulation-system approvals from UL or an equivalent third-party test house. Finished components include stator bobbins, coil forms for solenoid valves, relay coil carriers, and terminal boards for fractional-horsepower motors.
Relay bases and contactor supports require a balance between high CTI for arc-induced carbon tracking and flatness after prolonged exposure to contact heat. Under IEC 61810-1 and UL 508, moulded relay sockets must retain their screw-terminal electrical clearances and not warp beyond the contact-strip insertion tolerance. The 30 % glass-fibre loading reduces thermal expansion in the plane of the base plate, but the anisotropy of fibre orientation creates a tendency to bow if the part is moulded with large flat faces and uneven wall thickness. A mould temperature of 95–100 °C is specified to maximize crystallization and shift the moulded-in stress to a level that survives 85 °C continuous-use testing under IEC 60068-2-14 thermal shock. Melt temperature should not exceed 270 °C; higher nozzle settings degrade the halogen-free flame retardant, resulting in a drop in UL 94 V-0 performance at 0.75 mm. Pre-drying follows 120 °C for 4 h to 0.02 %. The tooling often uses a cold sub-runner with a tunnel gate into a ribbed non-critical surface to keep the visible base plate free of gate vestiges; however, cold-runner scrap must be dried before regrind at no more than 20 %. On production lines, cavity pressure is monitored with piezoelectric sensors, and hold pressure is switched when cavity pressure reaches 450–600 bar in the gate-adjacent zone to prevent overpacking and plate distortion. Finished products include power relay sockets, contactor base plates, arc chamber supports, and auxiliary contact housings.
In industrial control-gear insulation plates and switch-disconnector components, the main failure mode is not initial flammability but progressive carbon tracking after repeated micro-arcing at 250 V AC across contaminated surfaces. The grade is used for insulating panels, arc chutes, and partition plates that must comply with IEC 60947-3 and IEC 60664-1 pollution degree 3 requirements. Its CTI of 600 V under IEC 60112 is critical for compact switchgear, but moulders must control processing to avoid surface carbonization from overheated melt. Drying is at 120 °C for 4 h to 0.02 % or less moisture, and melt temperature is kept in the 245–260 °C band to avoid plate-out from the flame retardant on vent pins. Mould temperature is set at 80–90 °C for non-load-bearing insulated plates where flatness tolerance is less severe. Injection velocity is profiled to fill the plate edge last, moving air through generous vent grooves of 0.01–0.02 mm depth; insufficient venting causes burn marks that act as local tracking initiation sites under high-voltage test. The terminal products include insulating barriers, switch-disconnector partitions, phase separation plates, and fuse switch bases.
Competitive Lanxess Pocan® PBT+GF30%-FR-NF-CTI BFN4230 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Lanxess Pocan® BFN4230 is a polybutylene terephthalate (PBT) injection-moulding compound containing 30% glass fibre by mass. The FR-NF-CTI suffix identifies a flame-retardant formulation whose comparative tracking index is elevated relative to conventional PBT-GF30 FR products. Published supplier documentation positions the grade for thin-wall electrical insulating parts that operate in polluted, humid, or high-voltage environments. The glass-fibre content raises tensile modulus and heat deflection temperature; the CTI modification changes the surface failure mode from slow electrolyte-induced tracking to a stable insulating surface at 600 V when tested under IEC 60112. The grade is marketed under the Pocan® trade name of LANXESS. Public datasheets describe the grade primarily through its flammability rating, CTI value, and mechanical properties rather than through a single proprietary composition statement.
The polymer base is semi-crystalline PBT, which provides rapid crystallisation and lower moisture uptake than polyamide. The 30% glass-fibre reinforcement creates anisotropic moulding shrinkage, typically lower parallel to flow and higher transverse to flow. That anisotropy must be considered when the moulded geometry defines creepage and clearance distances. Differential shrinkage in a 50 mm connector span can alter the position of metal inserts, busbar pockets, and mating faces by several tenths of a millimetre. For electrical assemblies designed under IEC 60664-1, such dimensional movement changes the final insulation coordination and must be compensated in tooling through flow-pattern simulation and measured shrinkage data. The difference from unreinforced PBT is substantial: glass fibre raises tensile modulus from approximately 2,800 MPa to 11,000 MPa and raises heat deflection temperature under 1.8 MPa from approximately 60°C to 200°C in reinforced formulations. The penalty is reduced elongation at break, usually below 3%, and pronounced notch sensitivity in snap-fit features.
Standard PBT-GF30 FR compounds often use brominated flame retardants with antimony trioxide or phosphorus-nitrogen systems. Under IEC 60112, conventional flame-retarded grades can exhibit comparative tracking index values in the 200–250 V range because the flame-retardant system or its decomposition products form conductive carbonaceous tracks under electrolyte droplets. Pocan® BFN4230 is formulated to maintain higher tracking resistance while still achieving UL 94 V-0 at 0.75 mm. The CTI test applies 50 drops of 0.1% ammonium chloride solution between platinum electrodes spaced 4.0 mm apart and steps the test voltage in 25 V increments. A grade that withstands 600 V without tracking has a CTI of 600 V. This places the material in material group I under IEC 60664-1. For creepage calculation, group I permits shorter creepage distances than groups II, IIIa, or IIIb, which is the principal design difference from a 250 V CTI material. The exact expansion of the NF portion of the grade designation is supplier-internal; public technical documentation treats the CTI value and UL 94 classification as the relevant electrical acceptance criteria.
Representative published values for the grade are listed in the following table. Values are typical and should be confirmed against the current supplier datasheet and the relevant UL yellow card.
| Property | Test method | Value |
|---|---|---|
| Density | ISO 1183 | 1.68 g/cm³ |
| Tensile modulus | ISO 527-1/-2 | 11,000 MPa |
| Tensile stress at break | ISO 527-1/-2 | 130 MPa |
| Elongation at break | ISO 527-1/-2 | 2.5% |
| Charpy notched impact strength, 23°C | ISO 179/1eA | 8 kJ/m² |
| Heat deflection temperature, 1.8 MPa | ISO 75-1/-2 | 200°C |
| Comparative tracking index, solution A | IEC 60112 | 600 V |
| Flammability | UL 94 | V-0 at 0.75 mm |
| Volume resistivity | IEC 62631-3-1 | 1 × 1015 Ω·cm |
The CTI value is not a bulk property alone; it depends on surface composition, moulding morphology, and contamination. In multicavity injection tools, cavity-to-cavity variation in mould temperature and shear rate can alter the depth of the glass-fibre-poor or flame-retardant-rich skin. Published process-structure data for this specific grade is limited, but electrical testing of finished articles is normally required because the moulded surface is the functional insulator. A part moulded at low mould temperature may show lower CTI than the raw-material datasheet suggests if flame-retardant components migrate to the surface during cooling or if the surface is resin-rich. Mould release agents based on silicone or hydrocarbon wax can also alter surface wetting and change the CTI result. Release-agent use should be avoided in CTI-critical parts, or a non-silicone grade should be validated by IEC 60112 on production articles. A contamination layer as thin as 0.01 mm can change droplet spread area and concentrate current density at the electrode edges.
The intended application zone for BFN4230 is the set of electrical insulation parts that must survive pollution degree 2 or 3 conditions under IEC 60664-1. Connector bodies, terminal blocks, relay sockets, busbar insulators, photovoltaic junction-box housings, and power inverter interiors fall into this class. For a high-voltage DC busbar support, tracking initiates when conductive contamination forms a partially wet film between terminals; the surface path becomes a resistive heater and carbonises the resin. A material with CTI of 600 V withstands that failure at a higher voltage than a 250 V material, allowing the component to maintain the required creepage without increasing package size. The grade also provides UL 94 V-0 at 0.75 mm, making it suitable for accessible parts in applications governed by IEC 62368-1 and IEC 60335-1. Published application-specific test results are limited, so final qualification must include finished-part CTI testing at minimum wall thickness and at weld lines.
In photovoltaic junction boxes and electric-vehicle charging connectors, the material is processed in hot-runner multicavity tools. The filling pattern must orient glass fibres in relation to the voltage gradient if the designer wishes to avoid through-thickness conductivity paths created by fibre accumulation. A gate located at the centre of a rectangular connector body creates a radial flow field with transverse fibre alignment at the weld line; that weld line may exhibit lower CTI than the surrounding surface. Design validation therefore includes cross-sectional microscopy of the weld-line region and IEC 60112 testing with the electrolyte applied directly to the weld zone. If black colour is required, the pigment system must be CTI-neutral. Standard carbon-black concentrates can reduce tracking resistance and should be avoided unless validated on articles at the minimum wall thickness.
Residual moisture must be below 0.02 wt% before melt processing. The granulate is dried at 120°C for 2–4 h in a desiccant-bed dryer with a return-air dew point of -40°C or lower. In high-humidity production halls above 60% RH, open hopper residence should be kept below 30 min unless a dry-air hopper loader is installed. Barrel settings are typically 240–270°C from rear to nozzle, with a melt temperature of 260–280°C and mould temperature of 80–100°C. Mould temperatures below 60°C depress surface crystallinity and can produce a less dense amorphous skin with higher moisture absorption; this is a known risk for PBT grades in electrical service. Injection speed is set to produce a linear gate velocity of 100–300 mm/s for walls of 0.8–1.5 mm. Back pressure is held between 0.3–0.7 MPa and screw rotation speed below 0.4 m/s to minimise glass-fibre breakage. A screw compression ratio of 2.0–2.5:1 is typical; high-shear screws above 3.0:1 can shorten fibre length and lower weld-line strength.
Melt residence time at the upper end of the barrel profile should not exceed 5 min. Interruptions require seat pull or immediate purge with a low-viscosity PBT or dedicated purging compound. The flame-retardant system can decompose at hot spots in the check ring or hot-runner tip, leading to black specks and a drop in UL 94 classification. Hot-runner manifold temperatures should be held at the lower end of the melt-temperature range, and externally heated tips should not overshoot by more than 10°C. For multicavity tools, runner balance should be within ±5% of the mean fill weight; larger imbalance causes cavities to fill at substantially different shear rates and alters CTI across the production lot. Published capillary viscosity data for this specific grade is limited, but PBT-GF30 FR compounds generally show shear-thinning behaviour in thin-wall ranges, and pressure-dependent viscosity should be measured on the production mould when fill times fall below 0.5 s.
The material is not a guaranteed drop-in replacement for a halogenated PBT-GF30 FR in existing tools because shrinkage and crystallisation speed may differ. Tool trials should record cavity pressure at transfer and part dimensions under identical settings. If cavity pressure at transfer is lower than the incumbent material, packing intensity may be insufficient and moulded density lower, reducing CTI. Snap-fit arms should be designed with strain below the yield strain, using radii of at least 0.5 mm at the base and width-to-thickness ratios above 2:1 to reduce stress concentration. The low elongation at break makes sharp corners and abrupt wall-thickness transitions more likely to crack during ejection or subsequent terminal insertion.
Cross-contamination with acetal or polyamide is a known processing issue. PBT exposed to acetal at melt temperatures liberates formaldehyde and degrades rapidly. Polyamide contamination may react with the flame-retardant system and produce discoloration or changes in UL 94 performance. Hoppers, transfer lines, and granulate trays should be dedicated or cleaned between incompatible products. PBT ester linkages also hydrolyse at elevated temperature; the rate rises sharply above 80°C in saturated humidity. Outdoor enclosures should include drainage and seal design that prevents standing water in CTI-critical zones. Contact with hot concentrated alkalis, glycol-based coolants at elevated temperature, and strong mineral acids should be avoided.
Electrical-grade qualification is usually controlled by a matrix of supplier and independent laboratory results.
| Requirement | Standard / clause | Acceptance basis |
|---|---|---|
| Comparative tracking index | IEC 60112 | 600 V track-free with solution A |
| Flammability | UL 94 | V-0 at 0.75 mm |
| Insulation coordination material group | IEC 60664-1 | Group I for creepage-distance calculation |
| Polymeric material evaluation | UL 746B / UL 746C | Current yellow-card values for CTI, RTI, HWI, and HAI |
| RoHS recast | 2011/65/EU plus (EU) 2015/863 | Supplier declaration required; verify against shipped lot |
The material is not recommended for continuous hot-water immersion or steam service above 80°C unless validated on the finished part. Continuous service above its UL relative thermal index is not specified by the raw-material datasheet alone; published long-term thermal ageing data for this specific configuration is limited, so designers should obtain the current yellow-card RTI before specifying it for sustained exposure above 130°C. Regrind levels above 25 wt% should be qualified by repeating IEC 60112 and UL 94 on moulded articles because degraded polymer can accumulate in the surface layer and shift the tracking resistance. Batch acceptance should include melt volume-flow rate per ISO 1133-1:2022, ash content per ISO 3451-1 to confirm the 30% glass-fibre level, and a flammability check at the part wall thickness.