Lanxess Pocan Pbt Gf30 Fr Nf Bf4235

Lanxess Pocan® PBT+GF30%-FR-NF BF4235

    • Product Name: Lanxess Pocan® PBT+GF30%-FR-NF BF4235
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    Trusted Payment Partner
    Secure transactions supported by VTB Bank for reliable B2B procurement worldwide.
    Specifications
    HS Code 756951
    Polymertype PBT (polybutylene terephthalate)
    Glassfibercontent 30%
    Flameretardantsystem Halogen-free flame retardant
    Halogenfree Yes
    Density approx. 1.54 g/cm³
    Tensilemodulus approx. 10000 MPa
    Tensilestressatbreak approx. 100 MPa
    Strainatbreak approx. 2.0%
    Charpynotchedimpactstrength23c approx. 8 kJ/m²
    Hdt A 1 8mpa approx. 200 °C
    Meltingtemperature approx. 225 °C
    Ul94flammabilityrating V-0
    Glowwireflammabilityindex approx. 960 °C
    Comparativetrackingindex approx. 600 V
    Moldingshrinkage approx. 0.3–0.6%
    Processingmethod Injection molding
    Melttemperaturerange approx. 250–270 °C
    Moldtemperaturerange approx. 80–100 °C

    As an accredited Lanxess Pocan® PBT+GF30%-FR-NF BF4235 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Lanxess Pocan® PBT+GF30%-FR-NF BF4235 is supplied in 25 kg moisture-proof bags, palletized for industrial storage and handling.
    Container Loading (20′ FCL) 20′ FCL container loading of Lanxess Pocan® PBT+GF30%-FR-NF BF4235, properly stowed, secured, and documented for export shipment.
    Shipping Lanxess Pocan® PBT+GF30%-FR-NF BF4235 is a non-hazardous, flame-retardant, 30% glass-fiber-reinforced PBT compound. It is not regulated for transport (no UN number, hazard class, or packing group) under DOT/IMDG/IATA/ADR. Ship in dry, closed bags or octabins at ambient temperature, protected from moisture and excessive heat.
    Storage Store Lanxess Pocan® PBT+GF30%-FR-NF BF4235 in a cool, dry, well-ventilated warehouse, protected from direct sunlight, heat, and moisture. Keep material in original, tightly closed containers and maintain stable ambient temperature. Avoid contact with strong oxidizing agents and ignition sources. Prevent dust generation and static buildup; use appropriate grounding and local exhaust ventilation. Observe good housekeeping and inventory rotation.
    Shelf Life Lanxess Pocan® PBT+GF30%-FR-NF BF4235 has a typical shelf life of 12 months when stored dry, cool, and in sealed packaging.
    Application of Lanxess Pocan® PBT+GF30%-FR-NF BF4235

    In AC charging infrastructure, connector bodies and contact carriers moulded from Pocan® BF4235 are evaluated against IEC 62196-1:2022, IEC 62196-2:2022 and UL 2251:2017; the associated system installation rules in IEC 61851-1:2017 determine overvoltage category and pollution degree. The compound is processed as a 30 wt% glass-fiber-reinforced PBT with a non-halogen flame-retardant package, and the moulded parts are required to hold UL 94 V-0 at 0.8 mm wall thickness without losing creepage resistance under pollution degree 3 and overvoltage category III conditions. Tracking resistance is checked by IEC 60112:2020, while glow-wire behaviour is assessed by IEC 60695-2-11:2021 at 850 °C or 960 °C depending on installation category and supervisory current limits. Because the connector system is subjected to cable strain, temperature cycling between -40 °C and 85 °C, and occasional short-term condensation, the dimensional contribution of the 30 wt% glass fibre and the low moisture absorption of PBT are used to control terminal position tolerances.

    Formulation boundary: BF4235 is moulded as 100 wt% virgin compound in current-carrying separation walls; sprues and runners may be reintroduced at no more than 10 wt% from the same production lot if the resulting dry-blend is conditioned in a desiccant hopper at 120 °C for 4 h to a residual moisture of ≤ 0.02 %. Dilution with unreinforced PBT or PA is not permitted in creepage-critical sections because flame performance and comparative tracking index are tested on the as-supplied 30 wt% glass-fibre grade. The injection-moulding process runs on machines with 80–150 t clamp force; melt temperature is maintained at 250–270 °C, tool surface temperature at 80–100 °C, and injection speed at 60–120 mm/s. Back pressure is held at 2–5 MPa, screw speed at 60–100 min⁻¹, and screw L/D ratio at 20:1. Residence time above 270 °C is kept below 8 min to limit non-halogen flame-retardant decomposition and PBT chain scission; if a hot-runner valve gate is used, manifold temperature is set 5–10 °C below the melt temperature. Typical terminal component outputs include Type 2 charge plugs, inlet sockets, connector bodies, contact carriers, wall-box internal mounting plates and charging station internal busbar supports.

    What Limits 960 °C Glow-Wire Compliance in Non-Halogen PBT-GF30 Circuit Breaker Housings?

    Miniature circuit breaker housings moulded from BF4235 are used where the assembly must satisfy IEC 60898-1:2019 and EN 60898-1:2019 for domestic and similar installations; for North American panel applications, the breaker is tested under UL 489. The key material input is the combination of UL 94 V-0 at 0.8 mm and tracking resistance verified by IEC 60112:2020. The non-halogen package reduces acid gas release compared with many halogenated flame-retardant systems, but the 30 wt% glass fibre can increase surface roughness and create micro-tracking paths if the mould surface becomes glass-rich. Formulation for arc chamber partitions and contact supports is 100 wt% virgin BF4235; regrind from the same production lot is restricted to ≤ 5 wt% and is not permitted in the arc ejection zone or across the moving contact slot. Injection moulding uses 80–120 t clamp force, melt temperature 255–265 °C, mould temperature 70–90 °C, and wall thickness controlled at 1.2–2.0 mm around the electromagnetic yoke and bimetallic strip. Hot-runner valve gates are preferred over cold sprue to reduce glass-fibre orientation mismatch at weld lines; if a cold runner is used, the runner diameter is sized to maintain shear rate below 10 000 s⁻¹ to avoid excessive fibre breakage and local reduction in tensile strength measured by ISO 527-2. Terminal products include miniature circuit breaker bases, covers, toggle carriers, arc runner supports, residual current device housings and busbar isolation plates.

    Glow-wire temperature capability is not an intrinsic fixed value; it is geometry-dependent. BF4235 sections below 0.8 mm may show cracking and drip after IEC 60695-2-11:2021 at 960 °C because the PBT matrix softens before the glass reinforcement can stabilise the char layer. In production-scale tests, the limiting factor has been sink marks around the screw terminal insert, where local wall thickness drops below 0.7 mm; for that reason, holding pressure is profiled to maintain compactness during cooling. Published data for arc-ignition resistance after short-circuit interruption at 6 kA breaking capacity is limited, so enclosure design must separate the plasma path from PBT surfaces by ceramic arc plates or metallic arc runner geometry.

    Photovoltaic Junction Boxes Demand Creepage Stability, Glass Orientation, and Thermal Index

    For crystalline silicon module junction boxes, BF4235 is selected for the base and diode carrier where the assembly is required to meet IEC 62790:2020 and EN 50548:2018, with insulation coordination determined by IEC 60664-1:2020. Creepage and clearance distances are generally designed for 1000 V DC or 1500 V DC system voltage, pollution degree 2 or 3, and overvoltage category II or III. The main process hazard is anisotropic shrinkage driven by glass-fibre orientation; long thin base plates exhibit 0.2–0.4 % linear shrinkage along the flow path and 0.5–0.9 % transverse to flow when moulded at 80 °C tool surface temperature. Sequential valve gating is used to fill long flow lengths without excessive internal stress, and melt temperature is held at 250–265 °C. Formulation ratio: live-part separation walls and diode sockets are moulded from 100 wt% virgin BF4235; non-live retention clips, lids and brackets may contain up to 10 wt% regrind from the same material. No additional impact modifier, FR masterbatch or glass fibre is added at the press, because the UL 94 V-0 classification and thermal aging profile are established only for the original formulation. If regrind exceeds 10 wt%, the enclosure is subjected to IEC 62790:2020 thermal cycling and humidity-freeze tests before release. Terminal product types include PV junction box base plates, diode carrier trays, lids, cable gland brackets and frame mounting supports.

    BF4235 should not be used as an uncovered outdoor lid in direct UV exposure unless a UV-stabilised top cover, co-moulded gasket or black cap protects the polymer surface; otherwise surface chalking and gloss loss occur. Published data for continuous 1500 V DC operation under combined salt-mist and thermal cycling is limited, so qualification is performed at application level.

    Application cellNormative matrixTest method designationProcessing boundary
    EV charging connector bodiesIEC 62196-1:2022, UL 2251:2017IEC 60695-2-11:2021, IEC 60112:2020Residual moisture ≤ 0.02 %; melt ≤ 270 °C
    Miniature circuit breaker housingsIEC 60898-1:2019, UL 489IEC 60695-2-11:2021, IEC 60112:2020Wall ≥ 0.8 mm; regrind ≤ 5 wt%
    Photovoltaic junction box basesIEC 62790:2020, EN 50548:2018IEC 60664-1:2020Live-wall virgin; regrind ≤ 10 wt%
    Automotive relay sockets and fuse boxesUSCAR-2:2020, ISO 16750-2:2012ISO 527-2Terminal-retention virgin; regrind ≤ 15 wt%
    Industrial terminal blocksIEC 60947-7-1:2018, UL 1059:2019IEC 60664-1:2020Screw torque 0.5–1.5 N·m; regrind ≤ 20 wt%
    Appliance power connectorsIEC 60335-1:2020, IEC 60320-1IEC 60695-2-11:2021, IEC 60695-10-2Current-carrying walls ≤ 10 wt% regrind; shell ≤ 25 wt%

    Under the bonnet of a vehicle, engine-compartment relay sockets and fuse boxes moulded from BF4235 are designed for USCAR-2:2020 class 2 and 3 mechanical and temperature requirements and for thermal load profiles in ISO 16750-2:2012. The material is specified because its 30 wt% glass reinforcement provides terminal retention forces above 60 N after thermal shock when the boss geometry is correct; the lower moisture uptake of PBT relative to PA66 reduces post-mould swelling in humid engine-bay air. Formulation boundary: current-carrying terminal retention walls are run at 100 wt% virgin BF4235; runners and sprues are reground up to 15 wt% for non-live fuse box walls if the regrind is dried separately to ≤ 0.02 % moisture and if a 100 μm melt filter screen is installed in the nozzle to remove glass-fibre agglomerates. Dilution with unfilled PBT is not used in terminal retention zones because insertion force and retention force may drift below USCAR-2:2020 limits. Production-scale moulding uses 100–180 t machines with 8–32 cavity tools, hot-runner manifold temperature 250–260 °C, mould surface 80–100 °C, and cycle time 20–35 s. Pre-drying is performed in a desiccant dryer with -35 °C dew point at 120 °C for 4 h. Terminal products include ISO/mini-ISO relay sockets, under-hood fuse box bases, engine control unit headers and battery sensor connectors.

    Operating exposure to hot engine oil, diesel and oxygenated fuel vapour can plasticise the PBT surface and reduce weld strength; seals, shields or continuous splash tests are required. Published data for long-term fuel vapour exposure at 120 °C on this specific FR grade is limited.

    DIN-Rail Terminal Block Screw Torque Retention and Fibre Orientation

    In industrial control cabinets, DIN-rail terminal blocks moulded from BF4235 are required to maintain screw torque after heat aging under IEC 60947-7-1:2018 and UL 1059:2019; insulation coordination is checked with IEC 60664-1:2020, and flame retardance is verified to UL 94 V-0 at 0.75 mm or 0.8 mm wall thickness. The main technical issue is that glass-fibre orientation in the screw boss determines torque retention; if the fibres align perpendicular to the screw axis, thread-forming torque is low initially but relaxation after thermal aging is high. Formula boundary: screw bosses and terminal clamping bodies are moulded from 100 wt% virgin BF4235; base housings and non-load-bearing partitions may use up to 20 wt% same-material regrind. At 20 wt% regrind, melt viscosity shifts slightly lower and injection pressure is raised by 5 MPa to maintain packing in the gate area. Processing: two-shot or insert moulding of brass/copper busbars is used for current-bar mounting; melt temperature 255–270 °C, mould temperature 70–90 °C, and screw torque at assembly 0.5–1.5 N·m. For thread-forming screw bosses without metal inserts, pilot holes are drilled to 0.75 × screw diameter, and boss wall thickness is kept above 2.0 mm to prevent radial cracking. Tool runners are balanced to keep weld lines away from the screw boss; cold runner shear and mould flow simulation are used to orient glass fibres parallel to the screw axis. Terminal product types include feed-through terminal blocks, fused disconnect blocks, knife-disconnect blocks, sensor terminal blocks, grounding blocks and multi-tier stacked terminal bodies. Prolonged clamping pressure above 25 MPa can lead to stress relaxation; contact with ammonia or amine-based cleaning agents is not recommended because surface microcracking can initiate at glass-rich weld lines.

    When Appliance Power Connector Regrind Ratios Exceed 20 wt% in Multi-Cavity Tools

    Where regrind ratios exceed 20 wt% in multi-cavity appliance power connector moulding, the downstream processor must separate the validation flow for flame-retardant current-carrying separators from that for non-live outer shells. Appliance inlet modules and cord connectors are required to meet IEC 60335-1:2020 and IEC 60320-1; glow-wire exposure is tested with IEC 60695-2-11:2021 at 750 °C or 850 °C depending on monitored/unattended use, and ball-pressure behaviour is tested with IEC 60695-10-2. BF4235 provides UL 94 V-0 at 0.8 mm when moulded from virgin material. If the regrind fraction is raised to 25 wt%, tensile strength measured by ISO 527-2 typically declines by 3–5 %, and notched Charpy impact by ISO 179-1/1eA may fall more sharply due to average fibre length reduction and hydrolytic chain scission. Current-carrying separation walls therefore stay at no more than 10 wt% regrind; outer shells may use up to 25 wt% regrind only after revalidation of glow-wire, ball-pressure and UL 94 V-0 on the exact final part thickness and colour. Injection moulding uses 8–24 cavity cold runner tools, melt temperature 250–265 °C, mould temperature 60–80 °C, and pre-drying at 120 °C for 4 h to ≤ 0.02 % residual moisture. Liquid colourant letdown should not exceed 2 wt% because the carrier can interfere with the non-halogen FR package; solid masterbatch at 1–2 wt% requires UL 94 requalification for the finished colour. Terminal product types include appliance inlet housings, cord connector bodies, coffee machine power modules, dryer control panels and dishwasher connector carriers. Published data for regrind ratios above 25 wt% in 1500 V class insulating parts is limited, so those applications are excluded from high-regrind use.

    Free Quote

    Competitive Lanxess Pocan® PBT+GF30%-FR-NF BF4235 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Lanxess Pocan® PBT+GF30%-FR-NF BF4235 is a 30 wt% glass-fibre-reinforced polybutylene terephthalate injection moulding compound with a halogen-free flame-retardant system. The grade is positioned for electrical connector bodies, relay bases, contact carriers, sensor housings and miniature circuit-breaker internals where a UL 94 V-0 classification at 0.75 mm must be retained with high stiffness and low moisture uptake. Because PBT contains ester linkages, hydrolytic degradation is the primary processing boundary. Desiccant drying at 120 °C for 4 h to 8 h to residual moisture below 0.02 wt% is required before melt processing; regrind exposed to ambient air above 50 % relative humidity should be re-dried for at least 3 h. Failure to maintain these limits produces surface splay, weld-line strength loss and mould deposit formation on tools with small vents.

    The “FR-NF” suffix separates the material from non-flame-retardant GF30 PBT and from brominated or chlorinated FR systems. In final component release, non-halogen status is not assumed from the suffix alone; the assembly is tested to IEC 61249-2-21 if a sub-900 ppm chlorine/bromine threshold is contractually binding. The UL yellow card records the tested colour, thickness and specimen geometry; a moulded part with thinner ribs or different pigmentation may require supplemental ignition testing.

    What Separates BF4235 from Reduced-Glass and Non-Retardant PBT Compounds?

    The defining structural variable is the 30 % glass mass fraction, which raises tensile modulus, lowers mould shrinkage and increases flow anisotropy relative to 10 %- and 20 %-glass FR PBT grades. In mouldings with long thin ribs, fibre orientation is frozen near the skin while the core remains less oriented; this shell-core morphology produces differential shrinkage and can bow a flat connector body if gate placement is asymmetric. Flow-direction shrinkage for this class typically falls between 0.3 % and 0.5 %, while transverse shrinkage may exceed 0.8 %. Tool cooling and gate location therefore influence final flatness more than melt temperature alone.

    The flame-retardant package changes both melt rheology and thermal stability. Compared with non-FR PBT GF30 of the same matrix molecular weight, BF4235 exhibits higher melt viscosity because FR solid particles raise the effective solid-volume fraction. Screw recovery at a fixed back pressure is longer, and the gate pressure required to fill a 0.5 mm wall can be 10 MPa to 25 MPa higher than a non-FR control under identical mould conditions. Barrel temperatures below 250 °C cause unmelted FR agglomerates, while temperatures above 290 °C degrade the phosphorus-nitrogen system and release acidic volatiles that attack hot-runner components. A melt-temperature band of 250 °C to 270 °C is therefore maintained in production.

    When Thin-Wall Connector Geometries Require Higher Flow and Better Tracking Resistance

    In connector strips with wall sections between 0.4 mm and 1.0 mm, filling is limited by frozen-layer formation rather than by heat capacity of the melt. Mould temperatures in the range 80 °C to 100 °C reduce the thickness of the solidified layer and allow glass fibres to move with the flow front without bridging. Hot-runner manifolds are balanced within ±2 °C, and valve-gate sequencing shifts weld lines away from contact retention features. The melt volume-flow rate at 260 °C/2.16 kg is typically reported in the 12 cm³/10 min to 18 cm³/10 min interval under ISO 1133-1:2022; this places BF4235 above low-flow extrusion grades and below hyperbranched high-flow moulding grades.

    Comparative tracking index is governed by the flame-retardant system and the presence of conductive carbon blacks rather than by the PBT matrix alone. For a PBT GF30 FR-HF compound of this class, IEC 60112 CTI values commonly fall between 250 V and 450 V, but the exact BF4235 certificate value must be used for creepage calculations to IEC 60664-1. Mould release agents and external lubricants can depress tracking resistance; the complete process-aid package therefore requires qualification, not only the base polymer.

    On a 40 mm twin-screw compounding line with an L/D ratio of 36:1, glass roving is fed downstream of the melt seal to limit fibre attrition. The flame-retardant powder is pre-blended with granular PBT before the main feed, and the FR hopper is kept under dry air to prevent caking. Vacuum venting below -0.08 MPa and melt filtration through 60 mesh breaker plates are standard because FR agglomerates that survive dispersion become nozzle-clogging gels in injection moulding. Production batches are tested for melt-pressure stability, ash residue and colour; batch-to-batch fibre-length variation is most visible in weld-line strength and is monitored by Charpy notched impact on end-gated specimens.

    Moisture verification is performed by Karl Fischer titration rather than hot-air balance because FR additives can release condensation water during heater-based methods and produce false-positive readings. During production stops, melt residence time above 270 °C is kept below 10 min; after a stoppage, barrels are purged with a non-FR PBT or an olefinic carrier to remove degraded high-viscosity residues.

    Injection moulding uses a general-purpose screw with a compression ratio between 2.0:1 and 2.5:1 and an L/D of at least 20:1. Clamp force is derived from a projected-area requirement of 0.4 kN/mm² to 0.6 kN/mm² for moderate flow, but thin-wall multicavity tools may require more. Holding pressure is maintained until gate freeze-off is confirmed by cavity-weight stability rather than fixed time, because glass and FR solids alter compressibility and solidification rate. Injection speed is set to avoid jetting; the flow front must advance as a continuous melt front, otherwise surface streaks occur at the intersection of glass-rich and resin-rich regions.

    Thermal ageing and hydrolysis resistance set the upper service boundary

    PBT ester hydrolysis restricts the grade in hot water and alkaline or acidic condensates. Immersion in water at 80 °C attacks the glass/matrix interface and reduces tensile strength over time; the material is therefore not selected for pressurised cooling-water pump housings or direct coolant contact unless validated by the end user. Dry-heat ageing is less aggressive, but oxidative embrittlement first appears at high orientation zones such as gate scars and weld lines. Long-term heat ageing must be carried out to the applicable UL 746B relative thermal index protocol or to the final device standard, not inferred from a short-term HDT/A value.

    Published multi-year ageing data for BF4235 in specific connector geometries is limited; designs requiring established long-term thermal indices should request UL 746B RTI data from the material supplier and validate on moulded parts.

    Standardised property bands guide initial design but do not replace lot data

    Indicative property bands for PBT GF30 halogen-free flame-retardant compounds of the BF4235 class
    PropertyTest methodTypical bandUnit
    DensityISO 1183-11.62–1.68g/cm³
    Tensile modulusISO 527-1/-210,500–12,500MPa
    Tensile stress at breakISO 527-1/-295–115MPa
    Flexural strengthISO 178150–180MPa
    Charpy notched impact strength, +23 °CISO 179-1/1eA6.5–9.5kJ/m²
    Heat deflection temperature, 1.8 MPaISO 75-1/-2195–210°C
    Melt volume-flow rate, 260 °C/2.16 kgISO 1133-1:202212–18cm³/10 min
    Flame retardanceIEC 60695-11-10V-0 at 0.75 mmclass

    These bands are not lot-to-lot guarantees; the supplier’s certificate of analysis and the UL yellow card remain authoritative. Fibre orientation, moisture state and specimen preparation influence mechanical values, and moulded-part values may be lower than datasheet values depending on weld lines and wall thickness.

    Regulatory and Compliance Data Matrix

    Compliance verification matrix for final component release
    RequirementStandard or clauseAssessment boundary
    Flammability classificationIEC 60695-11-10, UL 94V-0 certificate is limited to tested thickness and colour; the UL yellow card is not a finished-part approval.
    Halogen-free declarationIEC 61249-2-21Chlorine and bromine thresholds require polymer/FR package verification; not all “NF” grades automatically meet sub-900 ppm definitions.
    Tracking resistanceIEC 60112CTI depends on surface cleanliness, mould release and weathering; exact voltage class must be reported.
    RoHS restricted substancesDirective 2011/65/EU Annex IISupplier declaration covers the raw compound; final assembly excludes lead-bearing surface finishes and solders.
    Drying and storageISO 1110Open-container working depth, drying-air dew point and residence time must be validated for the specific dryer.

    Substituting PA66 GF30 FR with BF4235 in low-tension power connectors

    When PA66 GF30 FR is replaced by BF4235, the design benefits are lower moisture-conditioned dimensional change and stable dry-as-moulded mechanical values, while the sacrifice is low-temperature ductility and continuous heat resistance. PA66 absorbs roughly 1.5 % to 2.5 % water at saturation, swelling the part and reducing modulus; PBT absorbs below 0.2 % in normal ambient service, so contact alignment is maintained. Conversely, PA66 retains higher notched impact below 0 °C and often achieves higher weld-line strength in complex connector bodies. The substitution is justified only when humidity cycling and electrical creepage, not impact, are the dominant failure modes.

    Against a non-FR GF30 PBT, the flame-retardant variant carries higher melt viscosity, lower impact toughness and a narrower processing window because the FR particles act as stress concentrators. Against a 20 %-glass FR PBT, BF4235 increases stiffness and heat distortion but raises anisotropy and notch sensitivity. Against mineral-reinforced FR PBT, BF4235 offers higher flow and reduced visual mottling risk but more warpage; tooling with balanced gating and sequential valve gates is required.

    In miniature circuit-breaker internals, the material is specified for arc-guide plates and contact carriers where UL 94 V-0 at 0.75 mm, low absorption and resistance to thermal cycling around 100 °C are imposed by IEC 60898-1 or IEC 60947-2. Mould flow simulation should use measured pvT data for the grade, not generic PBT, because glass and FR solids change specific volume and cooling shrinkage.

    Top