Lanxess Pocan Pbt Gf30 E Cti Hr B3233hre

Lanxess Pocan® PBT+GF30%-E-CTI-HR B3233HRE

    • Product Name: Lanxess Pocan® PBT+GF30%-E-CTI-HR B3233HRE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    Trusted Payment Partner
    Secure transactions supported by VTB Bank for reliable B2B procurement worldwide.
    Specifications
    HS Code 490520
    Volume Resistivity Ohm Cm 1E15
    Molding Shrinkage Percent 0.3-0.8
    Flammability Ul94 HB

    As an accredited Lanxess Pocan® PBT+GF30%-E-CTI-HR B3233HRE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Lanxess Pocan® B3233HRE is supplied in 25 kg moisture-proof polyethylene bags, palletized for industrial shipment.
    Container Loading (20′ FCL) Lanxess Pocan® PBT+GF30%-E-CTI-HR B3233HRE loaded in 20′ FCL, 25 kg bags on pallets, securely stowed and restrained for transport.
    Shipping Lanxess Pocan® PBT+GF30%-E-CTI-HR B3233HRE is supplied as non-hazardous, glass-fiber-reinforced PBT granules. Ship in sealed moisture-barrier bags or containers, protected from heat, sunlight, and contamination. No UN hazard class applies; use standard freight. Store dry and avoid prolonged moisture exposure.
    Storage Store Lanxess Pocan® PBT+GF30%-E-CTI-HR B3233HRE in a cool, dry, well-ventilated area, protected from direct sunlight, heat, and moisture. Keep in original sealed packaging until use; avoid prolonged humidity exposure. Follow first-in/first-out stock rotation. If moisture uptake is suspected, pre-dry according to the manufacturer’s processing datasheet before molding.
    Shelf Life Typically 12 months when stored dry, in sealed containers, at temperatures not exceeding 30°C.
    Application of Lanxess Pocan® PBT+GF30%-E-CTI-HR B3233HRE

    Within 48 V and high-voltage automotive power distribution units, B3233HRE is injection molded into connector bodies, busbar retention frames, and phase separation walls. The 30 % by weight short-glass reinforcement raises flexural modulus measured according to ISO 178 and tensile properties verified on ISO 527-2/1A bars. Notched impact behavior is typically checked to ISO 179-1/1eA. The enhanced CTI package is screened by IEC 60112 on 3 mm plaques with test solution A. The hydrolysis-resistant modification is intended to reduce hot-wet chain scission when connectors operate near coolant lines or accumulate an aqueous salt film. In production, pellets are dried at 120 °C for 4 h in a desiccant dryer with a dew point no higher than -30 °C; residual moisture in the hopper feed should remain below 0.02 %. If drying is omitted or ambient relative humidity exceeds 60 %, the ester bonds of the PBT backbone undergo hydrolysis in the barrel. This produces a drop in melt viscosity, increased flash in the hot-runner valve-gate zone, and lower tensile strength in the molded wall. A process conflict arises in multi-cavity tools: mold temperatures below 80 °C yield a surface layer with reduced crystallinity and lower tracking resistance after damp heat, while mold temperatures above 110 °C can extend cycle time and increase flash on thin-wall edges. Published durability curves for B3233HRE under long-term 85 °C/85 % RH exposure with simultaneous DC bias are limited. Connector validation is therefore normally split into dry arc tracking by IEC 60112 and separate damp heat exposure by IEC 60068-2-78, followed by insulation resistance measurement.

    How Does Hot-Wet CTI Retention Influence VFD Busbar Spacing?

    Variable-frequency drive enclosures place busbar supports and gate-drive circuit insulators in close contact with switching devices that generate heat, condensation, and transient overvoltage. In such systems, insulation coordination is calculated under IEC 61800-5-1 or UL 840; the required creepage distance is directly influenced by the comparative tracking index of the insulating material. B3233HRE is processed in tools with cold slug wells and sequential valve gates to avoid weld lines at the busbar fixing bosses. Melt temperature at the nozzle is held at 250–260 °C; injection speed is set in the 80–120 mm/s range to fill glass-rich thin ribs without gas burns. The mold surface temperature is maintained at 90 °C using pressurized water lines, and the tool is designed with vent lands not exceeding 0.01 mm in depth to allow air evacuation while preventing flash. When the CTI of an insulator is insufficient, designers must increase creepage distance, which conflicts with the compact footprint of a drive power module. Because the E-CTI modification reduces the drop in tracking resistance after moisture absorption, less redesign margin is required. However, published correlation data between standard IEC 60112 coupons and long-term VFD busbar behavior under switching harmonics is limited. A conservative qualification includes thermal shock cycling at -40 °C to 125 °C for 500 cycles and damp heat per IEC 60068-2-30 before final CTI measurement.

    Compliance test matrix for humidity-exposed high-voltage insulation parts
    PropertyMethodConditionReported boundary
    Comparative tracking indexIEC 60112Solution A, 3 mm plaquesEnhanced CTI grade; verify supplier yellow card
    Damp heat enduranceIEC 60068-2-7885 °C/85 % RH, 1,000 hInsulation resistance and visual tracking after exposure
    Thermal shockISO 16750-4-40 °C to 125 °C, 500 cyclesNo crack at insert interface
    Tensile strength after hydrolysisISO 527-2Before and after damp heatRetention target set by application; published data limited
    CTI after salt mistIEC 60112 after IEC 60068-2-52Salt mist exposure, then tracking testSystem-specific

    Photovoltaic combiner boxes and microinverter housings introduce a parallel failure mode because dust and dew produce a conductive film across terminal strips. The hydrolysis-resistant formulation is relevant in roof installations where internal condensation occurs during night cooling. Component validation for such housings typically pairs IEC 60112 tracking resistance with IEC 60068-2-30 cyclic damp heat, because terminal creepage is calculated under IEC 60664-1 for pollution degree 2 or 3. The molding process uses a hot-runner manifold with individually heated nozzles; gate vestige above 0.1 mm can interfere with terminal insertion and is controlled by valve-gate shutoff. For a 2 mm nominal wall, typical mold shrinkage values for 30 % glass-fiber PBT are in the range of 0.4 %–0.8 % in the flow direction and 0.6 %–1.0 % transverse, measured according to ISO 294-4; this anisotropy requires different cavity allowances in long connector rails. The glass-fiber concentration does not eliminate hydrolytic attack if the polymer is exposed to hot water above 70 °C for extended periods. Published data for B3233HRE after 1,000 h in 85 °C/85 % RH with external UV exposure is limited. UV stabilizer content must be confirmed for unshielded enclosures, and a black or otherwise pigmented surface layer is specified to slow surface oxidation.

    Relay Contact Carrier Chemistry Under Patina and Salt Mist

    Relay bases, contact carriers, and arc barrier plates convert the CTI issue into a hot-wet surface chemistry problem because switching arcs generate metal oxides and nitrogen oxides that deposit on the insulator. In qualification, the material is exposed to IEC 60068-2-52 salt mist followed by IEC 60112 tracking evaluation to simulate industrial cabinet pollution. The B3233HRE grade is typically molded with insert pins that carry relay terminals; those inserts are preheated to 110–130 °C before loading into the mold to avoid an abrupt cold skin layer that can crack during first thermal cycle. The tool uses a central sprue or valve gate positioned to place the weld line away from the terminal socket root. Weld-line weakness in 30 % glass-fiber PBT is more severe than in unfilled PBT because fiber orientation parallel to the weld plane does not bridge the flow fronts. Mold temperature is held at 100 °C to produce adequate crystallinity at the surface. High holding pressure is maintained until the gate freezes; early pressure release creates sink marks around the thickest insert walls, and late pressure release can overpack the thin base. For circuit breaker internal housings, the grade must be checked against UL 746A PLC ratings and the final yellow card, because CTI after hot-wet aging rather than dry CTI controls creepage during arc-fault events. Published data for continuous exposure to switching arcs is limited; the polymer is not a substitute for ceramic or thermoset arc chambers where the arc is sustained.

    Small appliance motor end laminates and brush card supports represent a mass-production downstream where condensation and cleaning agents meet glass-fiber-rich surfaces. The injection molding process is often a two-cavity hot-runner setup running cycle times near 30 s; the material is pulled under vacuum from a closed conveying system to prevent moisture regain. Drying is repeated for regrind. Regrind addition above 20 wt% reduces average glass fiber length and can lower tensile strength by 10 %–15 % compared with virgin compound, as measured by ISO 527-2; the exact retention curve for B3233HRE should be generated on the production machine with ISO 1133-2 MVR before changing the feed blend. Motor commutator humidity tests place the brush card under condensation during locked-rotor or blocked-vent tests. IEC 60068-2-30 cyclic damp heat is used to look for tracking tracks between carbon brush deposits and steel terminal rivets. The hydrolysis-resistant grade reduces but does not eliminate the formation of conductive char when powdered copper and carbon are mixed with wet dust. Melt temperature at the nozzle is typically kept at 250–260 °C and screw speed low to limit shear heating. Published data for B3233HRE after repeated autoclave cycles is limited; the application boundary must be established by component-level testing.

    If the Mold Temperature Drops Below 80 °C

    On charging inlet connectors and on-board charger insulation plates, the mold surface temperature is the single most decisive factor for post-molding performance. If the tool is run below 80 °C, the thin skin of the part cools before sufficient spherulite development occurs, reducing chemical resistance and increasing CTI loss after damp heat. Conversely, mold temperatures above 110 °C improve the crystalline surface layer but require longer holding time to prevent gate wrinkles. The charging inlet connector is produced with sequential valve gates that open from the pin socket area to the flange. The melt front velocity is held constant, not the injection speed, to avoid gas traps near the sealing ring. The material is dried at 120 °C for 4 h, with a dew-point monitor on the dryer outlet set to -40 °C or lower. When relative humidity in the plant exceeds 60 %, pellet conveying tubes should be purged with dry air and the open reservoir hopper should be avoided. For actual charging connectors, flame-retardant classification depends on wall thickness and color; the relevant UL 94 and UL 2251 ratings must be verified on the grade's yellow card before fixing final part dimensions. Electrical validation includes insulation resistance after simulated rain per IEC 62196-3 or SAE J3057 and thermal-shock cycling to check for microcracks at insert interfaces. Published data for B3233HRE under 1,000 V DC and condensing humidity for 1,000 h is limited; end-use tests must not assume CTI retention based only on dry as-molded data.

    In industrial flow-meter and sensor terminal blocks used in water treatment or outdoor natural gas metering, condensation and salt mist interact with permanent direct current bias across terminal banks. The material choice follows the same tracking index logic but includes additional exposure to cleaning chemicals such as hydrogen peroxide or sodium hypochlorite at low concentration. The glass-fiber-rich surface can wick moisture along exposed fibers if the molded skin is damaged by machining or insert staking. For this reason, inserts are placed by hot pressing rather than ultrasonic insertion when the wall is below 1 mm, because ultrasonic energy at the interface can create microcracks that later trap salt solution. The injection molding machine is configured with a decompression stroke of 3–5 mm to avoid drool at the hot nozzle; too much decompression pulls air into the melt cushion and causes splay. Back pressure is set at 5–10 bar hydraulic and screw speed at 40–60 min⁻¹ to keep melt temperature from rising above the 260 °C setpoint. Tracking index is measured after conditioning at 23 °C/50 % RH for 48 h according to IEC 60112. Published data for B3233HRE after continuous exposure to sodium hypochlorite solution is limited, so chemical compatibility testing per ISO 175 is required when terminal blocks are specified for sanitation systems.

    Free Quote

    Competitive Lanxess Pocan® PBT+GF30%-E-CTI-HR B3233HRE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    The product Lanxess Pocan® PBT+GF30%-E-CTI-HR B3233HRE is classified as a 30 wt% glass-fibre-reinforced polybutylene terephthalate injection-moulding compound with a hydrolysis-resistant stabilization system and a high comparative tracking index rating. The material is specified for moulded electrical housings, connector bodies, busbar supports, sensor enclosures, and power-distribution components in automotive and industrial systems where surface contamination, humidity, and sustained voltage stress can induce leakage current across insulation. The nominal glass-fibre content is 30 wt%; the E-CTI-HR suffix is a supplier-specific designation and the precise additive chemistry should be confirmed from the manufacturer’s published datasheet.

    For injection-moulded parts requiring simultaneous mechanical stiffness, dimensional stability, and dielectric function, the grade combines a tensile modulus of 9500 MPa under ISO 527-1/-2:2019 with a comparative tracking index of 600 V under IEC 60112:2020. The CTI value places the compound in material group I under IEC 60664-1, allowing reduced creepage distances in insulation coordination design when pollution degree and overvoltage category are fixed. This is a meaningful difference from many conventional 30 wt% glass-fibre PBT grades, where reported CTI values often fall in the 250–400 V range and therefore impose material group II or IIIa constraints.

    Electrical characterisation data for the moulded compound include a volume resistivity of 1×10¹⁵ Ω·m under IEC 62631-3-1:2016, surface resistivity of 1×10¹⁴ Ω under IEC 62631-3-2:2016, and electric strength of 32 kV/mm under IEC 60243-1:2013. These values are typical for natural, dry-as-moulded specimens and do not constitute guaranteed minima. The high CTI rating is measured with the standard electrolyte solution of 0.1% ammonium chloride in deionized water; the result is relevant only when the moulded surface is not covered with conductive carbon dust, metal swarf, or excessive mould release residue.

    PropertyTest methodB3233HRE typicalStandard PBT-GF30 published rangeUnreinforced PBT published range
    DensityISO 1183-1:20191.53 g/cm³1.52–1.56 g/cm³1.30–1.31 g/cm³
    Tensile modulusISO 527-1/-2:20199500 MPa9000–10000 MPa2500 MPa
    Tensile stress at breakISO 527-2:2019130 MPa120–135 MPa50–60 MPa
    Nominal strain at breakISO 527-2:20192.5%2.0–3.0%50–200%
    Charpy notched impact strength at 23 °CISO 179-1:201010 kJ/m²8–12 kJ/m²4–6 kJ/m²
    Heat deflection temperature HDT/A 1.8 MPaISO 75-1/-2:2013200 °C195–205 °C55–65 °C
    Comparative tracking indexIEC 60112:2020600 V250–400 V600 V
    Mould shrinkage parallelISO 294-4:20180.2%0.2–0.4%1.6–2.0%
    Mould shrinkage transverseISO 294-4:20180.9%0.8–1.0%1.6–2.0%

    Typical values are for natural injection-moulded specimens and do not represent guaranteed minima. Comparative values are drawn from published typical ranges for corresponding commercial PBT formulations; they should be confirmed against the specific grade datasheet because molecular weight, glass sizing, and stabilizer chemistry change the final properties.

    What Shifts the Processing Window When 30 wt% Glass Fibre and Hydrolysis Resistance Are Combined?

    The processing window is constrained by the interaction of heat, moisture, and residence time. In production-scale single-screw injection moulding, the melt temperature measured by nozzle pyrometry should be maintained between 250 °C and 270 °C. Above 270 °C, polybutylene terephthalate can undergo thermo-oxidative chain scission even when hydrolytically stabilized, producing free carboxylic acid end groups, reducing melt viscosity, and shifting the tracking index downward. The melt volume-flow rate under ISO 1133-1:2022 at 250 °C and 2.16 kg is 12 cm³/10 min. This moderate viscosity supports thin-wall filling, but the glass fibres generate higher shear heating than unfilled PBT; melt-temperature rise from shear can exceed 20 °C at high injection speeds, so actual nozzle settings must be adjusted to keep the material below 270 °C in the barrel.

    Because PBT crystallizes rapidly, the mould temperature controls the degree of crystallinity and final shrinkage. A mould temperature of 80–120 °C is recommended; the lower end supports faster cycles but produces a more amorphous skin and lower dimensional stability after annealing. The higher end improves crystallinity and reduces post-mould shrinkage but extends cycle time. In multi-cavity tools with hot-runner valve gates, cavity-to-cavity mass variation from glass-fibre orientation can exceed 0.5% when the runner is unbalanced. Sequential valve-gate control or rheological balancing is required to hold part mass within 0.3% across cavities for connectors with insertion-force and leakage requirements.

    Gate shear rate should be in the range 10,000–100,000 s⁻¹ for thin-walled connector bodies; below 5000 s⁻¹ the fibre-rich core may freeze prematurely and expose glass at the surface. In practice, injection speed is set to fill the cavity in 0.5–1.5 s for wall thicknesses of 1.0–2.0 mm; longer fill times produce premature freeze at the gate and excessive fibre orientation anisotropy. Because PBT is a fast-crystallizing polyester, the latitude for hesitation during filling is smaller than with slow-crystallizing engineering thermoplastics; flow-front hesitation creates weld lines and visible surface delamination.

    Drying, Screw Configuration, and Gate Freeze Limits in B3233HRE

    Predrying is mandatory at 120 °C for 4 h in a dehumidified-air dryer with a dew point no higher than -40 °C. Residual moisture before melt processing must be below 0.02 wt%; a higher level hydrolyzes the ester linkage in the melt before the part is filled. The effect is not always visible as splay; it can appear later as reduced tensile strength and lowered tracking resistance in the moulded part. Drying time must be extended if moisture-sensitive regrind is added or if the granulate has been exposed to humidity above 60% RH for more than a few hours.

    For glass-fibre abrasion, a bimetallic barrel and hard-coated screw are recommended. A three-zone screw with L/D 20:1–25:1 and compression ratio 2.0:1–2.5:1 is typical; free-flow nonreturn valve geometry reduces fibre breakage. Screw speed should be set between 80 rpm and 150 rpm; back pressure between 3 MPa and 8 MPa improves melt homogeneity without excessive fibre length reduction. Injection pressure is commonly 60–100 MPa hydraulic and hold pressure 40–70 MPa, determined by gate seal studies. Gate freeze must be verified by part-weight measurements: premature hold release creates sink marks and voids in sections thicker than 2.5 mm, while excessive hold time causes mould stress and increases ejection force.

    Residence time of molten material in the barrel and hot runner should be kept below 10 min; longer residence at 270 °C causes progressive molecular weight loss. Hot-runner systems should avoid dead spots where material can stagnate; open-pipe nozzles and externally heated manifolds with a melt-to-nozzle temperature variation below 5 °C reduce the risk of degraded material reaching the cavity. If short shots or machine breakdowns force a shutdown, the barrel should be purged with fresh material before moulding resumes.

    Differential shrinkage of 0.7% between flow and transverse directions explains corner-to-corner warpage in flat enclosures. Gate placement at the centre of the long axis and mould temperature gradient control are used to reduce bow; post-mould annealing at 120 °C for 1–2 h can relieve moulded-in stress but may increase initial shrinkage. For parts with living hinges or snap-fit features, the low elongation at break of 2.5% makes the geometry more sensitive to corner radius, gate position, and fibre orientation than unfilled PBT.

    When the Grade Replaces Standard PBT-GF30 in Sealed High-Voltage Connector Bodies

    Substitution is typically evaluated when a standard 30 wt% glass-filled PBT meets mechanical requirements but fails to provide sufficient tracking resistance or hydrolytic stability. Under IEC 60112:2020, B3233HRE is specified at 600 V, whereas many standard glass-filled PBT grades are reported in the 250–400 V range. This moves the insulation coordination from material group II or IIIa to group I under IEC 60664-1, allowing smaller creepage distances for a given working voltage, pollution degree, and overvoltage category. The comparison is only valid when the final moulded surface is clean and not covered with conductive carbon dust, metal swarf, or mould release residues.

    In sealed connectors, moulded-in elastomer seals or ultrasonic welding can expose the polymer to hot water/glycol mixtures. Standard PBT-GF30 without hydrolysis stabilizers can lose more than 50% of initial tensile strength after 1000 h at 85 °C and 85% RH in published ageing studies; hydrolysis-stabilized PBT-GF30 grades are formulated to retain a higher fraction of initial strength. Published data for B3233HRE under specific OEM humidity/electrical bias profiles may be limited; component validation per LV214 or USCAR-2 is required before volume release.

    Compared with polyamide 66 grades reinforced with 30 wt% glass fibre, this polyester absorbs substantially less moisture. Published moisture uptake for PA66-GF30 at 50% RH can exceed 1.5% by weight, whereas PBT-GF30 under ISO 62:2008 typically exhibits approximately 0.2% moisture absorption. This gives the polyester compound more stable dielectric performance in humid enclosures, but it also means the material is less impact-tolerant in dry conditions than conditioned PA66-GF30 and must be dried strictly before processing.

    This grade is not a flame-retardant compound. If the application requires UL 94 V-0 at 0.8 mm or 1.5 mm, a halogenated or phosphorus-stabilized PBT-GF30 FR grade should be selected instead. For low-voltage signal connectors where impact is the dominant requirement, an unreinforced or low-glass PBT may provide higher elongation at break; the 2.5% nominal strain at break of B3233HRE is characteristic of rigid fibre-filled grades and limits snap-fit deflection.

    Chemical exposure limits the use of this grade to neutral or mildly acidic media. Prolonged contact with hot strong alkalis, concentrated mineral acids, and amine-containing corrosion inhibitors accelerates hydrolytic chain scission. Continuous immersion in hot water above 95 °C should be avoided unless component testing under ISO 175:2010 demonstrates acceptable property retention. Aqueous alkaline degreaser operations must be validated by mechanical testing after exposure; even short exposure at high pH can crack stressed glass-filled PBT when moulded-in metallic inserts create tensile stress concentrations.

    Regrind addition up to 20 wt% may be used if the granulate is dry, uncontaminated, and not thermally degraded. Higher regrind fractions reduce tracking resistance and impact strength because of cumulative fibre breakage and matrix molecular weight loss. Injection-moulded parts should have uniform wall sections and radiused corners; sharp transitions increase glass-fibre orientation gradients and create internal stress that lowers resistance to moisture-assisted cracking.

    Top