Lanxess Pocan Pbt Gf30 E Cti B3235e

Lanxess Pocan® PBT+GF30%-E-CTI B3235E

    • Product Name: Lanxess Pocan® PBT+GF30%-E-CTI B3235E
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    Trusted Payment Partner
    Secure transactions supported by VTB Bank for reliable B2B procurement worldwide.
    Specifications
    HS Code 950172
    Polymer Type PBT
    Glass Fiber Content 30%
    Flame Retardancy Halogen-free flame retardant
    Volume Resistivity Ohm Cm 1E15
    Molding Shrinkage Percent 0.2-0.5
    Ul94 Rating V-0

    As an accredited Lanxess Pocan® PBT+GF30%-E-CTI B3235E factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg moisture-resistant paper bags on pallets, with 40 bags (1,000 kg) per pallet for safe handling and storage.
    Container Loading (20′ FCL) 20′ FCL container loaded with palletized, shrink-wrapped 25 kg bags of Lanxess Pocan® PBT+GF30%-E-CTI B3235E, securely stowed for export shipment.
    Shipping Shipping description: Lanxess Pocan® PBT+GF30%-E-CTI B3235E is a non-hazardous, glass-fiber-reinforced thermoplastic polyester compound. Not regulated for transport; no UN number, hazard class, or packing group. Ship in sealed original packaging, protected from moisture, heat, and sunlight, per SDS.
    Storage Store Lanxess Pocan® PBT+GF30%-E-CTI B3235E in a cool, dry, well-ventilated area away from direct sunlight, heat sources, and ignition. Keep in original sealed packaging to prevent moisture absorption and contamination. Avoid prolonged exposure to high humidity; dry material before processing if required. Do not store outdoors or near oxidizing agents. Maintain good housekeeping and follow local regulations.
    Shelf Life Typically 24 months when stored in original sealed packaging, dry, below 30°C, and protected from direct sunlight.
    Application of Lanxess Pocan® PBT+GF30%-E-CTI B3235E

    When 30 wt% glass fiber reinforced polybutylene terephthalate is specified for a high-voltage DC charging connector contact carrier, the governing design parameter is not short-term tensile strength but surface degradation behavior under combined electric stress, condensation, and conductive dust deposition. Lanxess Pocan® PBT+GF30%-E-CTI B3235E is positioned in the high tracking resistance range under IEC 60112, and in an EV charging inlet subjected to Pollution Degree 3 conditions this permits tighter creepage distances within the insulation coordination framework of IEC 60664-1:2020. A material assigned to Comparative Tracking Index group I supports reduced clearance and creepage dimensions compared with ordinary PBT grades, but only when the molded surfaces remain uncontaminated and the part geometry avoids sharp metallic inserts at the creepage boundary. Molding such contact carriers requires a hot runner manifold kept below 270 °C to avoid glass fiber clustering at the gate. The recommended pre-dry condition of 120 °C for 4–6 h brings pellet residual moisture below 0.02%, and this moisture limit is critical because processing above 0.02% produces hydrolytic chain scission that reduces tensile strength and surface track resistance simultaneously. In production tooling with 8 to 16 cavities, fill imbalance across a multicavity runner often produces short shots or fiber orientation gradients in the latch arms. Injection speed profiles with a short initial boost of 60–80 mm/s followed by a hold phase of 40–60 MPa hydraulic pressure reduce warpage at the mating face. The connector terminal retention force after thermal shock cycling from −40 °C to 125 °C is dominated by post-mold shrinkage and fiber orientation, not by the initial tensile modulus. Contact carriers in 800 V DC systems are frequently exposed to salt mist, ammonia-containing cleaning agents, and ozone. PBT is not intrinsically resistant to alkaline hydrolysis. The specification should exclude continuous exposure to aqueous solutions above pH 9 at temperatures above 60 °C. When a front-side seal is compressed, creep under continuous load at 90 °C must be evaluated according to ISO 899-1, because a 0.2 mm loss in sealing land height can open a moisture ingress path. Published data for B3235E in this specific configuration is limited; validation should include IEC 60512-11-4 contact retention after damp heat cycling and IEC 60068-2-30 humidity testing.

    What Changes When High Tracking Resistance Is Required in Molded Case Circuit Breaker Arc Barriers?

    In low-voltage molded case circuit breakers built to IEC 60947-2, arc barriers and moving-contact supports are exposed to transient arcs, carbonized particles, and metallic vapor. A polymer with a 600 V Comparative Tracking Index under IEC 60112 retains dielectric integrity after surface contamination longer than a material in Material Group IIIa, and this allows narrower internal barrier walls without increasing surface flashover risk. For B3235E, glass fiber content of 30% raises stiffness and reduces creep under the compressive load of the mechanism spring, but fiber ends at the molded surface can reduce arc ignition resistance if gas entrapment occurs at the wall junction. Injection molding of arc barriers with wall thicknesses from 0.8 mm to 2.0 mm requires a mold temperature near 80–100 °C. Lower mold temperatures freeze the skin too quickly and orient fibers parallel to flow, producing anisotropic shrinkage that warps the barrier after ejection. In multi-cavity tools, the runner system should be naturally balanced. Measured cavity-to-cavity weight variation above 0.5% correlates with arc test failures at the thinnest wall section.

    The glow-wire flammability index and glow-wire ignition temperature are thickness-dependent and should be taken from the producer’s yellow card. Typical manufacturing validation includes IEC 60695-2-12 at the minimum wall thickness. Field failures observed on production lines occur when regrind is added above 30% because glass fiber length reduction in the recycled stream lowers impact strength and creates a wider fiber length distribution. This is critical because the arc barrier is not a static insulator; it is mechanically loaded by the toggle mechanism during the opening cycle. Creep testing under ISO 899-1 at 85 °C and 20 MPa flexural stress provides a better predictor of long-term dimensional stability than initial heat deflection temperature alone. Melt residence time above 280 °C causes chain scission in PBT and generates low-molecular-weight degradation products that migrate to the surface and reduce tracking resistance. Production equipment should use a screw with a low-compression ratio of 2.5:1 to 3.0:1 and a free-flow non-return valve to minimize shear heating. A barrel profile of 240 °C at the feed throat rising to 260 °C at the nozzle is typical for glass fiber filled PBT, but the actual profile must be tuned to the machine’s screw diameter and cycle time. The maximum melt residence time should not exceed 8 min, and purging with a glass-filled polypropylene or compatible PBT purge compound should be performed after any interruption longer than 20 min.

    Processing parameterRecommended windowMeasurement or equipment basis
    Pre-drying temperature120 °C for 4–6 hDew point below −30 °C; residual moisture below 0.02%
    Melt temperature range250–270 °CNozzle thermocouple, low-compression screw
    Mold temperature80–100 °CThermal oil or water mold-tempering unit
    Maximum melt residence timebelow 8 minBarrel residence at 260 °C
    Back pressure30–70 barHydraulic or electric screw drive
    Screw speed0.15–0.30 m/s circumferentialMedium-shear barrier screw
    Regrind additionup to 30%Closed-loop regrind with fiber length control

    A photovoltaic DC isolation assembly demands a different thermal profile from an EV charging connector. The polymer housing of a fuse holder or disconnect terminal block must withstand continuous current heating, UV exposure if not fully enclosed, and high surface pollution from desert or coastal environments. Pocan B3235E offers the required high tracking resistance for 1500 V DC strings under IEC 60947-3 and IEC 60664-1, but the designer must separate electrical clearance from physical creepage. Glass fiber reinforced PBT has a dielectric strength in the order of 20–30 kV/mm depending on specimen thickness under IEC 60243-1. For a terminal block with M6 screw terminals, the boss under the screw generates tensile stress at elevated temperatures. Brass threaded inserts are preferred because direct screw tapping into PBT GF30 can crack after repeated thermal cycles if the pilot hole diameter is below the insert manufacturer’s minimum. In production, the insert must be preheated to 80 °C to prevent cold surface tears. Ultrasonic insertion is not recommended because high-frequency vibration can cause glass fiber breakage at the boss wall. Relative tracking index stability is influenced by moisture absorption after molding. PBT reaches equilibrium moisture content around 0.2–0.4% at 23 °C and 50% RH under ISO 62, and this absorbed water can reduce dielectric performance if the part is not conditioned. In a combiner box located outdoors, internal temperature swings from −20 °C to 85 °C create condensation risk. Drainage slots and vertical orientation of creepage paths reduce conductive dust collection. Published data for this specific configuration is limited, so qualification should include IEC 62790 for PV junction boxes and IEC 60529 IP65 enclosure tests with the final assembly.

    Relay Bases, Contactor Supports and Creepage Management in IEC 60947-4-1 Apparatus

    Industrial relay bases and contactor coil formers are injection molded with complex pin rows. The high CTI of B3235E permits reduced spacing between adjacent terminal cavities at Pollution Degree 3. In contactor supports, the material must also endure mechanical shock from armature closure and localized heating from the coil. Glass fiber reinforcement at 30% raises heat deflection temperature under 1.8 MPa load, but the fiber orientation at the weld line behind a pin can reduce tensile strength by 40–50% compared with the bulk value. Mold flow simulation identifies the gate location that relocates the weld line away from the thinnest section. A production gate thickness of 0.6–1.0 mm is selected to balance packing and shear heating. Short shots in the terminal retention ribs are common when the tool is run below 80 °C mold temperature. Raising the mold temperature to 100 °C improves weld line strength and releases frozen-in stress but extends cooling time and may increase cycle time by 10–15%.

    Arc shields and relay bases often require glow-wire ignition temperature compliance under IEC 60695-2-13. The test is performed at the minimum wall thickness of the finished part, not at a standard test plaque. If the part contains metal inserts, heat is extracted from the polymer, but thermal expansion mismatch between brass and PBT creates microcracks after repeated overload cycles. Insert molding with a brass insert temperature of 100 °C and a preheated tool of 90 °C reduces immediate cracking. Long-term retention is assessed by thermal cycling between −40 °C and 125 °C for 100 cycles. Published data for this specific product in relay bases is limited, so internal validation is required before series production.

    During stall and running conditions in universal motors, brush holders see hot copper shunts, carbon dust, and mechanical vibration at frequencies from 50–200 Hz. PBT GF30 is selected because it combines a heat deflection temperature above 200 °C under 0.45 MPa with the stiffness needed to resist the brush spring force, which can exceed 10 N in high-current power tools. The high tracking resistance of B3235E is relevant when carbon brush dust is deposited on the molded surface and combined with moisture. The carbon layer can bridge the gap between live parts and create a tracking path. Under IEC 60112, a higher Comparative Tracking Index delays ignition of the surface, but it does not eliminate the need for adequate creepage distance. The molded brush holder develops an internal weld line where melt fronts meet around the core pin, and this weld line should be positioned in a low-stress region. Injection molding with a core pin heated to 110 °C and a fast injection speed above 80 mm/s increases weld line strength, but it may produce flash if the venting depth is too low. Tooling should use vacuum venting and parting line vents of 0.02–0.03 mm to prevent gas burn at the last filled corner.

    During armature stall conditions, the copper shunt can reach 200 °C. The polymer adjacent to the terminal rivet may undergo oxidative embrittlement over hundreds of cycles. Continuous use at 180 °C is outside the long-term service range for PBT. UL relative thermal index values for PBT GF30 FR grades commonly fall between 120 °C and 140 °C, but the exact value for B3235E must be confirmed from the yellow card. A brass rivet pressed into a boss creates hoop stress, and the boss outer diameter should be at least twice the rivet diameter to prevent stress cracking. Vibration testing under IEC 60068-2-6 should be performed on the complete tool assembly because natural frequencies above 500 Hz can excite glass-fiber-reinforced polymer parts and cause fatigue cracks at sharp corners.

    When Busbar Insulation Carriers Enter Thermal Cycling in IEC 61439-1 Assemblies

    UPS busbar insulation carriers are structural parts that support copper busbars and absorb magnetic forces during short-circuit conditions. In this application, the polymer is not simply an electrical insulator; it is a load-bearing component under continuous current heating. For Pocan B3235E, the combination of 30% glass fiber reinforcement and high CTI allows the use of compact busbar spacing, but the current rating is limited by the temperature rise limits in IEC 61439-1:2020. The material’s temperature index under electrical stress should be checked against the UL yellow card, while the mechanical index should be used for the support ribs. A typical design rule is to keep the polymer’s continuous use temperature below 130 °C; busbar temperature at the contact interface should not exceed that value after derating.

    Manufacturing of these carriers often uses large injection molds with single-point gating. The glass fiber orientation in the long support ribs creates anisotropic shrinkage of 0.3–0.6% along the flow direction and 0.8–1.0% perpendicular to flow. Ribs with length-to-thickness ratios above 8:1 are prone to warpage if the mold cooling channels are not independently controlled. A conformal cooling channel located 8 mm from the cavity surface and held at 40–60 °C can reduce warpage in production, but it increases tooling cost. Assembly with busbars requires the polymer to accept M6 or M8 threaded inserts. Ultrasonic insertion should be avoided if the wall thickness is less than 1.5 mm. Instead, heat-staked or molded-in inserts are preferred. If the carrier is used in a UPS with forced convection cooling, condensed humidity can combine with copper dust to create conductive tracks. The high CTI rating of B3235E increases the time to tracking failure under IEC 60112, but the final assembly must still pass IEC 62477-1 insulation coordination verification at the rated working voltage.

    Property or certificationTest method or standardAcceptance criterion to verify
    Comparative tracking indexIEC 60112:2020CTI at least 600 V on 3 mm specimen
    Flame retardancyUL 94 yellow cardThickness-dependent V rating
    Electric strengthIEC 60243-1kV/mm on conditioned specimen
    Tensile modulus and stressISO 527-2Producer datasheet values
    Flexural strengthISO 178:2019Producer datasheet values
    Heat deflection temperatureISO 75-2:2013 method AfTypically above 200 °C at 1.8 MPa
    Moisture absorptionISO 62Saturation near 0.4%
    RegulatoryREACH Regulation (EC) No 1907/2006; RoHS Directive 2011/65/EUSupplier declaration

    Observe Moisture and pH Boundaries Before Moulding Appliance Control Housings

    For household appliance control housings in washing machines, dishwashers, and condensing tumble dryers, humid air at temperatures up to 70 °C and alkaline detergent residues create a demanding environment. The high tracking resistance of B3235E is advantageous for printed circuit board terminal blocks, but the polymer’s hydrolytic stability is conditional. Before drying, residual moisture in pellets below 0.02% is necessary for processing. After molding, the part may absorb water up to 0.4% at saturation under ISO 62, which slightly swells the polymer and reduces tensile strength. The design must avoid sharp internal corners below 0.25 mm radius because glass fiber reinforced PBT is notch-sensitive, and corner radii below 0.2 mm increase stress concentration factors. In appliance applications with hot alkaline cleaning, continuous contact with sodium hydroxide or sodium carbonate solutions at pH above 10 causes surface hydrolysis. If such contact is possible, the material is only suitable when the housing is sealed or the contact duration is short.

    The molding window for B3235E in thin-wall control housings is narrower than for unfilled PBT. The melt should be kept below 270 °C, and the hold pressure should be reduced after the gate freeze time, which is typically 2–3 s for a 1.0 mm wall. High hold pressure above 80 MPa can create warpage at the mating face of a control housing, preventing the seal from closing. In a hot runner mold, the manifold temperature should be isolated from the nozzle tip temperature. A thermal separation above 30 °C prevents stringing and premature solidification at the gate. Published data for B3235E in condensing appliance environments is limited. The relevant validation includes IEC 60335-1 clause 29 clearances and creepage distances, IEC 60335-2-7 for washing machines, and IEC 60335-2-23 for appliances for skin or hair care if a heated control housing is used.

    Free Quote

    Competitive Lanxess Pocan® PBT+GF30%-E-CTI B3235E prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    The polybutylene terephthalate compound marketed as Lanxess Pocan® PBT+GF30%-E-CTI B3235E is a 30% glass-fibre-reinforced polyester intended for injection-moulded electrical components in which surface tracking under contaminated or humid voltage stress is a design limit. The product designation combines the polymer matrix, reinforcement level, and an enhanced comparative tracking index specification; published datasheets list density according to ISO 1183 in the range 1.55–1.58 g/cm³ and a melt volume-flow rate measured under ISO 1133-1:2022 at 260 °C/2.16 kg of approximately 12–15 cm³/10 min. The nominal glass content of 30% by weight is controlled by ashing under ISO 3451-1; supplier certificates report glass content on each production lot. Principal application fields include terminal blocks, relay bases, miniature circuit-breaker housings, switch components, and electrical connectors where a comparative tracking index of ≥600 V under IEC 60112 permits more compact insulation coordination than is possible with conventional glass-filled PBT grades.

    What electrical failure mechanism does the E-CTI designation address?

    Comparative tracking index describes the ability of an insulating solid surface to resist the formation of conductive carbonized tracks when a defined electrolyte solution is applied between electrodes under alternating voltage. The test method IEC 60112 uses platinum electrodes, a droplet of 0.1% ammonium chloride solution, an electrode spacing of 4 mm, a drop interval of 30 s, and a controlled voltage increase of 25 V per step; CTI is assigned as the highest voltage at which no tracking and no persistent flame occur over 50 drops. For PBT and other polyesters, local carbonization can occur because polymer degradation under dry-band arcing releases conductive carbon, especially when salts, dust, or condensation lower the surface resistance below the level at which the applied voltage can initiate a tracking path.

    Standard PBT+GF30 grades often exhibit CTI values between 250 V and 400 V under IEC 60112, which forces designers to increase creepage distances or select a higher-tracking material. The E-CTI modification in B3235E raises the published value to ≥600 V. The exact additive chemistry is proprietary, and published data for the specific stabilizer and filler package is limited; however, the practical outcome is a lower propensity for surface carbonization under electrical stress in polluted or condensing environments. This characteristic is relevant for insulation coordination governed by IEC 60664-1:2020: grades meeting ≥600 V CTI can be assigned to Material Group I, whereas ordinary PBT grades with lower CTI fall into Material Group III or worse, directly affecting required creepage and clearance distances.

    When 30% glass fiber reinforcement is retained in a PBT matrix

    In B3235E, the 30% chopped glass fibers are incorporated into the polybutylene terephthalate melt to raise tensile modulus, reduce creep under load, and lower unreinforced PBT shrinkage. The reinforcement also improves dimensional stability while maintaining the polyester matrix resistance to many hydrocarbon oils, alcohols, and cleaning agents. The following table summarises representative published property ranges from supplier technical literature; values are typical, not guaranteed, and should be confirmed lot-by-lot.

    PropertyTest standardPublished range or value
    DensityISO 11831.55–1.58 g/cm³
    Tensile modulusISO 527-1/-29,500–11,000 MPa
    Tensile stress at breakISO 527-1/-2120–140 MPa
    Nominal strain at breakISO 527-1/-22.0–3.0%
    Flexural modulusISO 1788,500–10,000 MPa
    Flexural strengthISO 178180–210 MPa
    Charpy notched impact strengthISO 179-1/1eA8–12 kJ/m²
    Charpy unnotched impact strengthISO 179-1/1eU45–60 kJ/m²
    Heat deflection temperature, 1.8 MPaISO 75-1/-2195–205 °C
    Comparative tracking indexIEC 60112≥600 V
    Melt volume-flow rate, 260 °C/2.16 kgISO 1133-1:202212–15 cm³/10 min

    Compared with unfilled PBT, the tensile modulus is raised from approximately 2,500–2,800 MPa to 9,500–11,000 MPa, while elongation at break decreases significantly. Compared with standard PBT+GF30 grades that do not carry the E-CTI suffix, the principal differentiator is not tensile strength or modulus but the tracking resistance described above. Lot-to-lot flow variation may be slightly higher because the stabilizer and additive package influences melt viscosity; published data for the exact rheological differences between B3235E and non-enhanced PBT+GF30 grades is limited. If B3235E is replaced on an existing tool with a standard PBT+GF30, the CTI margin may fall below the device approval limit even though the part fills and appears dimensionally identical. Conversely, substituting B3235E into a tool designed for standard PBT+GF30 may require adjusted fill speed or melt temperature because of possible flow differences. A mould-filling analysis using measured viscosity data is recommended before substitution.

    For injection moulding on production lines with clamp force from 60 to 120 t, the compound is normally processed at melt temperatures of 250–270 °C, with 280 °C as an upper limit to avoid thermal degradation. Tool temperature should be held at 80–100 °C to promote crystallization, reduce post-mould shrinkage, and stabilize electrical performance. A desiccant dryer with dew point at or below −30 °C is required; pellets should be dried at 120 °C for 4 h to residual moisture below 0.02%. If ambient relative humidity exceeds 60%, hopper residence time should be limited or dry-air feeding maintained. Hydrolytic degradation in inadequately dried PBT produces lower melt viscosity, silver streaks on moulded parts, reduced weld-line strength, and measurable loss of tracking resistance. Screw recovery conditions should use a three-zone general-purpose screw with L/D between 20:1 and 25:1 and compression ratio in the range 2.5:1 to 3.0:1; back pressure of 30–70 bar and moderate screw speed reduce glass-fiber fracture while avoiding excessive residence time.

    Tooling for glass-filled PBT requires attention to abrasion. The 30% glass content accelerates gate and cavity wear compared with unfilled PBT; hardened tool steels, wear-resistant venting, and rounded runner bends are specified on high-volume moulds. Point gates below approximately 0.8 mm can restrict flow and increase fiber orientation at the gate, producing anisotropic shrinkage and weaker weld lines. Published data for the specific gating performance of B3235E is limited, so short-shot studies on the intended tool are advisable before production release. Shot weight should use 60–80% of barrel capacity to limit melt residence time; prolonged residence above 5 min at melt temperature above 270 °C can cause yellowing and reduce CTI.

    Connector, relay, and switch housing constraints

    In terminal blocks and relay housings, the E-CTI grade allows creepage distances to be selected using Material Group I under IEC 60664-1:2020, provided the final device passes the relevant overvoltage category and pollution-degree tests. For Pollution Degree 3 environments with conductive contamination or intermittent condensation, the higher tracking resistance reduces the probability of insulation failure across barriers between adjacent terminals. The compound is also specified in switch components and sensor housings where glass reinforcement supplies dimensional stability for press-fit pins and threaded inserts. The glass-fiber content reduces linear mould shrinkage; published values for similar PBT+GF30 grades are typically 0.2–0.5% in the flow direction and 0.6–0.9% transverse depending on gating. Inserts should be preheated or incorporated with generous radii because glass-filled PBT has lower elongation at break than unfilled PBT and can crack under high interference fit.

    Weld-line placement is a specific concern in connector and relay geometries. Glass-fiber orientation at converging melt fronts creates local anisotropy and can reduce CTI and strength at weld lines. For parts with multiple gates or large openings, mould-flow simulation should be used to position weld lines away from high-field regions, terminal retention features, or thin walls adjacent to metal inserts. Supplier documentation lists conformity with EU RoHS Directive 2011/65/EU including the 2015/863 phthalate amendments when the product is supplied in standard formulations. REACH SVHC declarations are lot-specific and must be requested from Lanxess. Electrical components using this compound are not themselves certified; end devices must satisfy the applicable product standard such as IEC 61984 for connectors or IEC 60669-1 for switches.

    RequirementStandard or directiveApplicability
    Comparative tracking indexIEC 60112≥600 V; Material Group I under IEC 60664-1:2020
    Restriction of hazardous substancesEU 2011/65/EU as amended by EU 2015/863Conformance declared in supplier literature
    REACH SVHC declarationEC 1907/2006Lot-specific declaration required
    Glass contentISO 3451-130% by weight nominal

    The material is susceptible to hydrolytic degradation in hot-water or steam service; continuous exposure above 60 °C in saturated conditions should be evaluated in the final part, not inferred from short-term datasheet values. Melt contamination with polyamide residues or amine-containing colorants should be avoided because ester-amide interchange can reduce molecular weight and shift crystallization. Regrind levels above 25% require requalification because repeated heat history can reduce CTI, impact strength, and surface appearance. The compound is not recommended for continuous contact with concentrated mineral acids, strong bases above pH 9, or hot ethylene glycol without validation. Flammability classification is colour- and thickness-dependent; if a UL 94 rating is required, the specific colour and minimum wall thickness must be confirmed against UL Yellow Card documentation. Published data for B3235E may vary by colour and lot. For outdoor electrical enclosures, UV resistance is limited in uncolored PBT grades; carbon-black or pigmented versions should be specified and tested under ISO 4892-2 exposure conditions if outdoor use is intended.

    Top