| HS Code | 666582 |
| Density | 1.53 g/cm³ |
| Glass Fiber Content | 30% |
| Tensile Modulus | 10000 MPa |
| Tensile Strength | 135 MPa |
| Elongation At Break | 2.5% |
| Charpy Notched Impact Strength At 23 C | 9 kJ/m² |
| Hdt A At 1 8 Mpa | 205 °C |
| Hdt B At 0 45 Mpa | 220 °C |
| Melting Temperature | 225 °C |
| Molding Shrinkage Parallel | 0.3–0.5% |
| Water Absorption At 23 C 24 H | 0.1% |
| Volume Resistivity | 1E16 Ω·cm |
As an accredited Lanxess Pocan® PBT+GF30% B3235 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Supplied as pellets in 25 kg moisture-proof bags, 40 bags per pallet (1,000 kg net). |
| Container Loading (20′ FCL) | Lanxess Pocan® PBT+GF30% B3235 loaded in 20′ FCL dry container, palletized 25 kg bags, secured for export. |
| Shipping | Shipped as non-hazardous thermoplastic granules in sealed moisture-barrier 25 kg bags, palletized and stretch-wrapped. Use standard dry freight; protect from moisture, heat, and UV. No special dangerous-goods classification—follow the supplier SDS and keep packaging intact. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat sources, and moisture. Keep in original sealed packaging until use; reseal opened bags to prevent humidity pickup. Avoid contact with oxidizing agents and incompatible chemicals. Maintain moderate temperature, practice first-in/first-out, and protect from dust and physical damage. |
| Shelf Life | Typically 12 months from delivery when stored dry, at room temperature, in original sealed packaging; avoid moisture and direct sunlight. |
In automotive engine-compartment actuator manufacturing, a 30 wt% glass-fibre-reinforced PBT compound is specified where low moisture-absorption dimensional envelope and resistance to automotive operating fluids are design requirements. Lanxess Pocan® PBT+GF30% B3235 is processed neat at a fixed glass-fibre content of 30 wt%; downstream dilution with unreinforced PBT or post-industrial regranulate below 30 wt% glass content is not recommended because shrinkage anisotropy, weld-line strength and thermal expansion coefficients are calibrated to this filler level. The downstream production process is injection moulding on 800–1,500 kN horizontal injection units with L/D 20:1 three-zone screws, hardened check rings for glass-filled compounds, and open-nozzle or positive shut-off systems. Pre-drying at 120 °C for 4 h in a desiccant dryer to a residual moisture content below 0.02 wt% is mandatory; lot-to-lot moisture records above 0.05 wt% before melt processing generate visible surface silver streaks and a 15–25% reduction in weld-line tensile strength. Industry compliance for under-hood applications follows ISO 16750-5:2010 for chemical exposure, USCAR-2 Rev 8 for mechatronic housing validation, and ISO 527-1/-2 for tensile property verification. Production-scale outputs on such lines include throttle-body gear housings, EGR valve gear carriers, window-lift motor housings, seat-adjustment actuator housings and fuel-flap actuators. In thermal-cycling qualification from -40 °C to 125 °C, dimensional stability is governed by glass-fibre orientation and a mould temperature maintained at 80–100 °C; published data for this specific B3235 configuration under long-term glycol/water immersion is limited and should be verified against ISO 175 before release.
Regrind retention in glass-fibre-reinforced PBT power-tool gear housings is limited by fibre length attrition during repeated screw plasticating cycles, not solely by thermal degradation. In production-scale single-screw injection moulding with 25–35 mm barrier screws, initial fibre length distribution shifts from 250–350 µm to 180–220 µm after two regrind cycles; this shift reduces Charpy notched impact strength under ISO 179-1/1eA by 8–15%. The addition ratio of B3235 is therefore maintained at 100 wt% virgin material for structural gear housings, while regrind from sprues and runners is reintroduced at a maximum of 20 wt% in non-structural components. Processing uses melt temperatures of 260–280 °C, barrel residence times not exceeding 5 minutes, mould temperatures of 80 °C, and injection velocities of 150–300 mm/s. Compliance verification for power tools includes IEC 62841-1:2014 for mechanical safety, ISO 180/A for notched Izod impact, and UL 746B for relative thermal index documentation. Component families currently moulded from this material include angle-grinder gear covers, drill housing mid-shells, leaf-blower impeller shrouds and reciprocating-saw motor mounts; for double-insulated tool enclosures, B3235 is overmoulded with a thermoplastic elastomer grip layer, with the PBT substrate surface temperature above 100 °C during overmoulding to ensure interfacial adhesion. In production sites where relative humidity exceeds 60%, insufficient drying before melt processing leads to mould vent deposit and a 10–20% reduction in weld-line tensile strength, a failure documented on high-cavitation tooling.
In continuous water service, PBT+GF30 impeller parts are specified for dimensional stability and lower moisture uptake than polyamide, but hydrolytic chain scission remains the governing failure mechanism. In washing-machine drain pump impellers and dishwasher circulation pump rotors, B3235 is moulded neat at 100 wt% as-received; downstream addition of hydrolysis stabilizer masterbatch or blending with other PBT grades is not recommended because screw-level additive dispersion cannot be guaranteed without altering the 30 wt% glass-fibre distribution. The downstream process uses injection moulding with melt temperature controlled at 260–270 °C, mould temperature maintained at 90–100 °C, and back pressure of 5–10 bar to homogenize the glass fibre without excessive fibre breakage. High mould temperatures are required to maximize crystallinity and reduce free-volume fraction, which slows hydrolytic chain scission; increasing mould temperature from 60 °C to 100 °C measurably improves surface hardness and resistance to hot-water extraction. Compliance for pump components is assessed according to ISO 62 for water absorption, ISO 175 for chemical resistance, and IEC 60335-1 for appliance safety; potable-water or food-contact approvals are not automatically conferred and must be verified against NSF/ANSI 61 or EU 10/2011 where applicable. The moulded part envelope for this application covers dishwasher circulation pump impellers, washing-machine drain pump impellers, spa pump wet-end housings and small boiler condensate pump rotors. Published data for this specific B3235 grade under continuous immersion at water temperatures above 60 °C is limited; continuous operation above that threshold without hydrolysis-stabilized variants is not recommended because mechanical strength declines through random chain scission at a rate dependent on pH and dissolved oxygen.
Hydrolysis testing of PBT-GF30 under ISO 175 immersion protocols generally shows that tensile strength retention at 80 °C water is significantly lower than at 40 °C after the same exposure interval; this is driven by random ester bond scission, not by fibre-matrix debonding alone. Designers should therefore specify hydrostabilized PBT grades for long-term exposure above 60 °C, and for B3235 should request hydrothermal aging data from Lanxess rather than extrapolating from dry-heat aging. In mould flow, weld lines around impeller cores are a known failure site; their strength is governed by melt-front angle and fibre orientation at the converging flow front. Increasing mould temperature to 100 °C and slowing injection speed near the weld line to 60–80 mm/s improves weld-line strength by promoting molecular diffusion across the melt front, but this must be balanced against increased cycle time and cosmetic flow marks on visible areas.
Terminal block and relay-base moulding in high-volume electrical distribution equipment imposes a different requirement set: high comparative tracking resistance, low mould deposit, and precision for multi-pin brass insert moulding. In this scenario, B3235 is processed at 100 wt% as-received; any addition of colour masterbatch is limited to 2 wt% and should use a PBT-carrier masterbatch to avoid CTI suppression. The 30 wt% glass-fibre fill provides the flexural modulus above 8,000 MPa under ISO 178 needed for screw-torque retention in relay bases and terminal strips. Downstream production uses multi-cavity hot-runner injection moulding with valve gates; brass insert pins are preheated to 130–150 °C to reduce freeze-off and to minimize stress concentration at the pin-polymer interface. A higher mould temperature of 100 °C is used to obtain a crystalline surface layer that resists creep under terminal screw loads. Industry compliance is anchored to IEC 60664-1 for clearances and creepage distances, IEC 60112 for comparative tracking index, and UL 94 HB thickness verification where flame retardance is not required by end-use specifications. Parts representative of this application class are relay bases, DIN-rail terminal block housings, switch frames and contactor auxiliary contact housings. In 24/7 moulding operations, field data from high-cavitation tools show that lot-to-lot variance in glass-fibre length distribution below 200 µm can increase warp in long terminal strips by 0.12–0.20 mm over a 250 mm span, making incoming quality checks on fibre length distribution a practical control measure.
When household appliance pump housings are exposed to alternating hot-water and cold-water cycles, the selection of a 30 wt% glass-fibre-reinforced PBT is driven by the need to maintain flatness for mechanical shaft seals and gasketed mating faces. In washing-machine drain pump front housings and dishwasher circulation system bases, B3235 is run neat; the fixed 30 wt% glass content is the formulation addition, as it balances shrinkage anisotropy against stiffness without exceeding the practical mouldability limit at thin wall sections of 1.2–2.0 mm. Processing is performed on injection moulding machines with clamp forces from 1,000–2,500 kN, screw L/D ratios of 20:1–23:1, and shot-size control at 40–60% of barrel capacity to avoid residence-time degradation. Mould filling is carried out with sequential valve gating at injection speeds of 100–250 mm/s; high-speed filling above 300 mm/s is avoided because it raises shear heating and can push local melt temperature beyond 300 °C, causing surface degradation and a 5–10% loss in impact strength. Compliance standards include ISO 75-2 for heat deflection temperature under 1.8 MPa, ISO 11357 for melting temperature verification, and IEC 60335-1 for end-product safety; dimensional stability is validated by ISO 294-4 shrinkage measurements on 60 mm × 60 mm × 2 mm plaques. Finished articles in this group are washing-machine drain pump bodies, dishwasher circulation pump front housings, heat-pump condensate trays and boiler flue condensate collectors. In cyclic thermal exposure from 5 °C to 90 °C at 2 cycles per hour, dimensional growth and warpage remain below 0.3% after 500 cycles when gate location and fibre orientation are controlled; published B3235-specific fatigue data under combined thermal and hydraulic load should be obtained before design freeze.
Solenoid valve coil bobbins and industrial sensor housings fabricated from B3235 are subject to stringent electrical insulation, chemical exposure and low-temperature impact requirements. The material is fed as a ready-to-mould compound at 100 wt% as-received with a 30 wt% glass-fibre content; nozzle-side addition of recycled flake is held to 10–15 wt% due to the higher risk of short shots in bobbins with wall sections below 0.8 mm. Downstream processing typically uses injection moulding with hot-runner tips of 0.8–1.2 mm gate diameters, cavity pressure sensors set to transfer at 600–900 bar, and holding pressure profiles of 40–60% of peak injection pressure for 3–6 seconds to minimise sink over thick sections around terminal pins. Compliance for industrial control applications is assessed under IEC 60079-7 for increased safety electrical equipment where applicable, IEC 60529 for ingress protection, ISO 175 for exposure to hydraulic oils and brake fluids, and ISO 180/A for low-temperature impact down to -40 °C. Representative moulded articles include solenoid coil bobbins, inductive proximity sensor housings, flow sensor bodies, pressure switch enclosures and railway signalling connector insulators. Experience from high-volume solenoid production indicates that failure to maintain resin moisture below 0.02 wt% before melt processing produces nozzle drool and dimensional variation in bobbin flange flatness of 0.05–0.10 mm, which directly affects coil winding tension.
Competitive Lanxess Pocan® PBT+GF30% B3235 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Lanxess Pocan® B3235 is a pelletised polybutylene terephthalate/polyethylene terephthalate compound reinforced with 30 wt% glass fibres. The grade is typically specified for injection-moulded and extruded components in which a straight PBT GF30 would show excessive differential shrinkage, surface replication defects, or post-mould dimensional drift. Glass content is controlled during compounding and verified by calcination according to ISO 1172. Lot certification normally reports melt volume-flow rate, tensile modulus, and notched Charpy impact determined under ISO 1133-1:2022, ISO 527-1/-2, and ISO 179-1/1eA respectively.
The material combines the fast crystallisation behaviour of PBT with the lower mould shrinkage anisotropy and improved surface appearance associated with PET. In practice, B3235 is positioned between lower-glass PBT+PET products and heavily reinforced PBT compounds. The 30 wt% filler fraction raises stiffness and reduces shrinkage, while the PET fraction modifies crystalline morphology and reduces visible glass-fibre orientation on textured surfaces when compared with straight PBT GF30.
In a straight PBT GF30, rapid crystallisation produces a pronounced shrinkage differential between the flow and transverse directions, often causing warpage in large flat parts. B3235 contains a PET fraction that alters nucleation and crystal growth, lowering that differential and improving surface replication in grained or textured tools. Tensile modulus remains in the same order as PBT GF30, typically 9500–10500 MPa under ISO 527-1/-2, but the blend generally requires a slightly higher melt temperature because of the PET phase. Density according to ISO 1183-1:2019 is normally 1.53–1.56 g/cm³. The material is not intended as a direct replacement for PBT GF30 where maximum crystallinity or highest chemical resistance to strong alkaline media is required without part-specific validation.
For PBT+PET glass-fibre compounds, moisture-induced hydrolytic chain scission accelerates above the polymer melting range. At melt temperatures above 270°C, residual moisture of 0.05 wt% can reduce tensile stress at break by 10–15% within a standard 30–60 s inventory residence time. B3235 must therefore be dried to 0.02 wt% or lower, verified by ISO 15512:2019. A desiccant dryer with a dew point of ≤ -30°C and an air temperature of 120°C for 4–6 h is the standard condition. When ambient relative humidity exceeds 60%, drying time is increased to 6–8 h, and hopper loading should be sealed or purged with dry air. Production trials on open-hopper moulding cells in high-humidity environments have shown tensile strength variation of 5–12% across otherwise identical moulded specimens, traceable to moisture variability rather than pellet lot differences.
Across the ISO 527-1/-2 tensile protocol at 23°C, the glass network raises tensile modulus to approximately 10000 MPa and tensile stress at break to 125–135 MPa. Nominal strain at break is typically 2.0–2.5%. Flexural modulus under ISO 178:2019 is generally 8500–9500 MPa, with flexural strength above 180 MPa. Notched Charpy impact strength according to ISO 179-1/1eA is typically 7–9 kJ/m² at 23°C and may fall to 5–7 kJ/m² at -30°C. Heat deflection temperature under ISO 75-1/-2 method A is normally 180–200°C, and Vicat softening temperature under ISO 306 B50 is 185–210°C. Water absorption at saturation under ISO 62 is low, generally 0.2–0.3%, which supports dimensional stability in humid service compared with unreinforced PBT.
Flat plaques moulded from B3235 exhibit anisotropic shrinkage because glass fibres align predominantly parallel to flow. Typical values under ISO 294-4 are 0.2–0.5% in the flow direction and 0.6–1.0% transverse, depending on gate geometry, melt temperature, and mould temperature. Thick sections of 3–4 mm show less anisotropy than sections of 1–2 mm because the highly oriented shear layer occupies a smaller fraction of the cross-section. Gate location should be selected so that the longest part dimension coincides with the lower-shrinkage flow direction; otherwise edge warpage can exceed dimensional tolerances in flat parts. Differential shrinkage is lower than in straight PBT GF30 because the PET phase retards bulk crystallisation, but it is not eliminated and should be accounted for in tool compensation.
Injection moulding of B3235 should maintain melt temperature at 260–280°C at the nozzle and mould temperature at 80–100°C. Lower mould temperatures reduce PET crystallinity and increase post-mould shrinkage and dimensional drift. For a 50 mm screw, screw speed is normally 50–100 min⁻¹; speeds above 150 min⁻¹ can cause fibre attrition and reduce tensile modulus by 5–10%. Hydraulic back pressure in the 5–15 bar range improves melt homogeneity without starving the screw. Residence time at melt temperature should not exceed 8 min; holding the melt above 280°C for more than 10 min produces visible discoloration and a measurable loss in notched Charpy impact. Hot-runner systems with externally heated manifolds and valve gates of 1.5–2.5 mm diameter are preferred for multicavity moulds because freeze-off at cold runners is rapid.
In 30 wt% glass-reinforced PBT+PET, weld line tensile strength measured under ISO 527-1/-2 is typically 55–75% of the corresponding bulk value because the fibres do not cross the weld interface. Notched Charpy impact at a weld line may fall to 3–5 kJ/m². Multiple gate placement, flow-length balancing, and sequential valve gating are used to shift weld lines away from structural zones. If a weld line cannot be avoided, the part should be derated by a factor of 0.6 on ultimate tensile stress or validated by instrumented puncture impact testing under ISO 6603-2. The reduced weld line strength is not a compound defect but a flow-induced consequence of the glass-fibre orientation state.
Fibre content is controlled gravimetrically during compounding; release certificates report residual glass after ISO 1172 calcination. On production lines using co-rotating twin-screw extruders with L/D 40–48, glass roving is introduced downstream of the melting zone to limit fibre breakage. Screw speed is typically 250–400 min⁻¹, and specific mechanical energy is kept below 0.25 kWh/kg to preserve fibre length. Final pellet melt volume-flow rate under ISO 1133-1:2022 at 250°C and 2.16 kg is generally 8–15 cm³/10 min. Variation above 15% between lots generally indicates PET intrinsic-viscosity drift or glass feeding error, not normal process variation.
B3235 is used where PBT+PET GF30 meets the mechanical and thermal requirements but straight PBT GF30 fails on dimensional stability or surface finish. Typical applications include automotive latch housings, sensor brackets, pump bodies, exterior mirror mounts, and industrial enclosures requiring low warpage and high stiffness. Because the polyester matrix is susceptible to hydrolytic degradation in hot water above 60°C, prolonged service in aqueous glycol or engine coolant at elevated pressure is not recommended without part-specific testing. Chemical resistance to automotive oils and greases is generally acceptable at 23°C, but stressed parts should be evaluated under environmental stress-cracking conditions using ISO 22088-3. Flammability classification under UL 94 is typically HB at 0.75 mm; final wall thickness and colourants can change the rating. Electrical comparative tracking index values for this specific B3235 configuration are not uniformly published, and final parts should be tested under IEC 60112 where electrical safety compliance is required. The grade is normally supplied with REACH and RoHS recast conformity statements for electrical and electronic applications, but it is not automatically classifiable as food-contact material under FDA 21 CFR without grade-specific confirmation.