Lanxess Pocan Pbt Gf15 E Cti Tough B3217e

Lanxess Pocan® PBT+GF15%-E-CTI-Tough B3217E

    • Product Name: Lanxess Pocan® PBT+GF15%-E-CTI-Tough B3217E
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    Trusted Payment Partner
    Secure transactions supported by VTB Bank for reliable B2B procurement worldwide.
    Specifications
    HS Code 288269
    Productdesignation Lanxess Pocan® PBT+GF15%-E-CTI-Tough B3217E
    Polymertype Polybutylene terephthalate (PBT)
    Reinforcement Glass fiber
    Glassfibercontent 15% by weight
    Density 1.41 g/cm³
    Tensilemodulus 5300 MPa
    Tensilestrength 95 MPa
    Elongationatbreak 3%
    Charpyimpactstrengthunnotched 23c 50 kJ/m²
    Charpyimpactstrengthnotched 23c 7 kJ/m²
    Hdt A 200 °C
    Hdt B 170 °C
    Vicatsofteningtemperature B 195 °C
    Meltingtemperature 225 °C
    Comparativetrackingindex 600 V
    Ul94flammability HB (1.5 mm)
    Waterabsorption 0.4%
    Moldingshrinkageparallel 0.4%
    Moldingshrinkagenormal 0.8%
    Processingmethod Injection molding

    As an accredited Lanxess Pocan® PBT+GF15%-E-CTI-Tough B3217E factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Lanxess Pocan® PBT+GF15%-E-CTI-Tough B3217E is supplied in 25 kg moisture-proof bags, palletized for safe industrial storage and handling.
    Container Loading (20′ FCL) 20′ FCL container loading of Lanxess Pocan® PBT+GF15%-E-CTI-Tough B3217E: palletized bags, dry stowage, secure, ventilated, no contamination.
    Shipping Lanxess Pocan® B3217E is supplied as moisture-protected, palletized bags or octabins of glass-fiber-reinforced PBT compound. Ship as non-hazardous goods in clean, covered transport; keep dry, avoid direct sunlight, heat, and humidity, and store sealed at moderate temperature.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep in original, tightly sealed packaging to prevent moisture absorption and contamination. Avoid prolonged exposure to high humidity and elevated temperatures. Follow local regulations and the manufacturer’s safety data sheet.
    Shelf Life Shelf life: typically 12 months in original unopened packaging, stored dry at 5–30°C, protected from moisture and direct sunlight.
    Application of Lanxess Pocan® PBT+GF15%-E-CTI-Tough B3217E

    AC electric vehicle charging connector bodies molded from Lanxess Pocan® PBT+GF15%-E-CTI-Tough B3217E require comparative tracking index stability under 250 V AC service voltage and exposure to condensation cycles. The relevant compliance framework includes IEC 62196-1 and IEC 62196-2 for vehicle couplers, IEC 60664-1 for insulation coordination, and IEC 60112 for tracking index classification; the selected pigmented lot should be qualified under the finished-device dielectric withstand sequence rather than on raw plaques alone. At the molding cell, the formulation addition ratio is controlled by limiting clean sprue and runner regrind to 15 wt% in 85 wt% virgin B3217E; regrind from hot-runner drops must be dried to 0.02 wt% moisture and blended gravimetrically at the machine throat. Downstream production employs a dehumidifying hopper dryer set to 120 °C for 4 h with a dew point of -30 °C, a hydraulic injection-molding machine with screw L/D 20:1, melt temperature 250–270 °C, mold surface temperature 80–100 °C, and sequential valve-gated hot runners to move weld lines away from creepage paths between live parts. Terminal component types include mode 2 and mode 3 AC charging plug housings, socket outlet bodies, and internal live-part support insulators. A processing limitation is that B3217E should not be assumed to carry a UL 94 V-0 listing unless the current datasheet explicitly states that classification; flame-retardant end-device requirements must be resolved before mold commissioning.

    Why Does CTI Stability Matter in Miniature Circuit Breaker Arc Chambers at 230 V?

    The characteristic failure mode in miniature circuit breaker arc chambers is carbonized tracking across insulating walls after short-circuit interruption, which reduces creepage resistance and can lead to dielectric breakdown on subsequent operations. For this reason, the insulating polymer is selected against IEC 60112 tracking index verification and the finished device is evaluated under IEC 60898-1 temperature-rise and dielectric withstand tests. In this application, the formulation addition ratio is restricted to 15 wt% clean regrind from the same production campaign, with 0 wt% external mold release because silicone contamination on arc-chamber walls can affect arc-extinguishing behavior. Downstream production uses a two-plate mold with wall thickness between 1.2 mm and 2.0 mm, mold surface temperature 90–100 °C, and a profiled injection speed to avoid jetting at gate entry; hold pressure is maintained at 60–80 MPa until gate freeze. Terminal product types are miniature circuit breaker base housings, arc splitter retaining walls, and terminal shields for B- and D-curve devices rated up to 230/400 V. For reduced creepage distances under IEC 60664-1, the grade's tracking resistance is used only after mandatory dielectric tests on representative finished breakers; published data for this specific enclosure configuration is limited and requires tool-trial confirmation.

    In photovoltaic DC connector bodies and junction box terminal carriers, outdoor exposure introduces ultraviolet radiation, condensation, and surface pollution that accelerate tracking failure across insulator surfaces. The applicable compliance base includes IEC 62790 for junction boxes, IEC 62852 for photovoltaic connectors, IEC 60112 for comparative tracking index, and UL 746C for polymeric outdoor suitability. The formulation addition ratio for injection molding is 10 wt% maximum clean regrind; carbon black masterbatch for UV stabilization is held to ≤2 wt% because higher carbon black loadings can reduce the tracking index and must be re-verified after weathering. Downstream production involves insert molding of tin-plated copper busbars and diode lead frames inside a mold heated to 90–110 °C, using a screw with low-compression ratio 2.5:1 and injection speed controlled to prevent displacement of inserts; tooling is designed with pinch-off or tunnel gates at non-creepage locations, and weld lines are excluded from the shortest path between live conductors. Terminal product types include PV junction box terminal carriers, diode housing insulators, and DC connector body insulators for rooftop and utility-scale module strings. Published data for B3217E in certified outdoor PV connector bodies after 1,000 h damp-heat exposure is limited; qualification coupons should be molded from the production tool and tested for CTI retention.

    Contactor Arc Barriers and Relay Base Insulators at 400 V

    Contactors and relay bases rated at 400 V have live metal parts separated by molded polymer ribs that must resist surface tracking during coil interruption and contact bounce. The governing compliance documents are IEC 61810-1 for electromechanical elementary relays, IEC 60947-4-1 for contactors and motor starters, and IEC 60664-1 for creepage and clearance. At the molding machine, 20 wt% of clean runner regrind may be blended with 80 wt% virgin B3217E; 0 wt% silicone-based external mold release is specified because silicone migration onto contact surfaces can cause high contact resistance and coil failure. The production process employs a multi-cavity hot-runner mold with heated sprue bushing, mold surface temperature 90–100 °C, melt temperature 255–265 °C, and high injection speed to minimize glass-fiber orientation differences that cause warpage in long relay base cavities. Terminal product types include DIN rail relay bases, contactor arc barriers, and coil formers. The operational boundary is that B3217E is not a substitute for arc-quenching thermosets if the device design depends on high-temperature arc erosion resistance exceeding 250 °C continuous; short-term arc exposure must be validated on the actual contact gap geometry.

    When Double Insulation Requires Tracking Resistance Under Loaded Commutator Arcing

    Brush card carrier plates in double-insulated power tools are exposed to conductive carbon dust from commutator wear, which can form a tracking path if the polymer surface is insufficiently resistant under repetitive arcing. The applicable safety standard is EN 62841-1 for motor-operated hand-held and transportable tools, supplemented by IEC 60112 for tracking index and IEC 60695-2-11 glow-wire testing when required by the end-product housing evaluation. In this application, the formulation addition ratio is 10 wt% maximum clean regrind, with 0 wt% lubricant masterbatch because internal lubricants can exude and combine with carbon dust to accelerate surface leakage. Downstream production involves insert molding of brass brush holders and stamped terminal blades in a mold heated to 100 °C; injection velocity is set to fill 0.8–1.2 mm walls in less than 0.5 s to produce a resin-rich skin that encapsulates glass fibers and reduces wear-particle adhesion. Terminal product types include brush card carrier plates, trigger switch housings, and commutator end caps for angle grinders and drills. The material does not carry a flame-retardant classification sufficient for all exposed housing parts; if the finished tool requires a UL 94 V-0 or glow-wire ignition classification, the housing must be molded from a separate flame-retardant grade.

    When 48 V mild hybrid systems replace 12 V architectures in underhood electrical centers, connector insulators see higher sustained voltage, broader thermal cycling, and exposure to engine compartment fluids. Compliance is aligned to USCAR-2 for automotive electrical connector performance, ISO 16750-3 for environmental loads, and LV 214 for vehicle-specific connector validation; the material must be tested for tracking resistance under IEC 60112 after thermal shock. For OEM production, regrind addition is set to 0 wt% because material certificates require 100 wt% virgin B3217E. Downstream production uses high-cavitation molds with valve-gated hot runners, wall thickness between 0.6 mm and 1.0 mm, melt temperature 260–270 °C, mold surface temperature 90–100 °C, and gas counter pressure where weld lines cannot be avoided near terminal retention features. Terminal product types include 48 V battery management system connector housings, electric compressor connector bodies, and engine control unit connector shells. Published data for this specific compound in USCAR-2 sealed connector validation is limited; all connector-specific limits should be confirmed on production-tool samples before homologation.

    Free Quote

    Competitive Lanxess Pocan® PBT+GF15%-E-CTI-Tough B3217E prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Pocan® PBT+GF15%-E-CTI-Tough B3217E is an injection moulding compound based on a polybutylene terephthalate matrix with a nominal glass-fibre content of 15 wt.%. The E-CTI-Tough suffix identifies an impact-modified formulation with enhanced comparative tracking index performance relative to standard glass-reinforced PBT grades. The pelletised feedstock is used in electrical/electronic housings, connectors, sensor carriers, and thin-wall mouldings requiring dimensional stability, moderate stiffness, and resistance to surface tracking. Typical material properties are measured under ISO 1183-1 for density, ISO 1133-1:2022 for melt volume-flow rate, ISO 527-1/-2 for tensile modulus and strength, ISO 179-1/1eA for Charpy notched impact strength, and ISO 75-1/-2 for heat deflection temperature. Exact release values are lot-dependent and are provided only in the current manufacturer datasheet.

    The as-supplied resin is hygroscopic to a degree that requires controlled storage. When granules are exposed to ambient moisture above 60% relative humidity, surface water can exceed the recommended maximum within 4 hours. Sealed foil-lined bags should be opened only at the dryer station, and partially used material should be returned immediately to a desiccant hopper rather than left in open containers. Dried material held at machine hopper level should be blanketed with dry air at a dew point below −30 °C when ambient humidity is high.

    Why does moisture control dictate melt-processing outcomes for B3217E?

    In PBT matrices, melt-phase hydrolysis is the dominant processing risk. Residual moisture above 0.02% by weight, determined by ISO 15512, degrades ester linkages during plastication and produces irreversible loss of molecular weight. The resulting viscosity drop is not a flow improvement; it corresponds to chain scission and lower notched impact strength in the moulded part. Drying of glass-fibre-reinforced PBT compounds is therefore carried out in desiccant dryers at 120 °C for 4 to 6 hours, with a supply dew point of −30 °C or lower and a nominal airflow rate of 3.0 to 3.5 m³/h per kilogram of resin. Because glass fibres do not absorb the water but increase the surface area of the pellet, air channelling and hopper short-circuiting must be avoided.

    Melt processing for 15 wt.% glass-filled PBT is typically performed with barrel settings between 250 °C and 270 °C. A profile from rear zone to nozzle in the order of 240–250 °C, 250–260 °C, 260–270 °C, and nozzle 255–265 °C avoids crystalline solidification while limiting thermal degradation. Mould temperature should be held at 80–100 °C to achieve the crystallinity needed for dimensional stability and chemical resistance. Residence time above 10 minutes at melt temperatures above 260 °C should be avoided. Screw geometry with an L/D of at least 18:1 and a low-compression, glass-fibre-compatible screw is preferred; high-compression screws can fracture fibre bundles and reduce reinforcement efficiency.

    Electrical evaluations of B3217E in connector and enclosure applications centre on comparative tracking index data under IEC 60112 and creepage distance requirements under IEC 60664-1. The E-CTI-Tough formulation is intended to move the compound into a higher material-group classification than standard glass-filled PBT, which often drops into material group IIIa or IIIb when CTI falls below 175 V or 100 V respectively. This classification shift can allow reduced creepage paths for a given pollution degree and working voltage. Published data for this specific configuration is limited, so the qualified CTI value must be taken from the supplier’s current datasheet and not inferred from standard PBT+GF15 grades. For parts exposed to condensation, conductive dust, or salt spray, end-product tracking tests should be performed on moulded parts with production gate locations and weld lines, because fibre orientation and mould release residues can alter surface tracking behaviour.

    Surface resistivity and volume resistivity for this family are often measured under IEC 62631-3-2 but are not reliable indicators of tracking resistance. A material with high volume resistivity can still form surface carbon tracks if thermal decomposition products accumulate. The CTI test under IEC 60112 applies a controlled electrolyte drop and records the voltage at which current persists; it is therefore a more direct qualification tool for creepage design.

    When 15% glass fibre replaces unfilled PBT in electrical enclosures

    The transition from unfilled PBT to a 15 wt.% glass-fibre-reinforced impact-modified PBT changes both mechanical and moulding response. Unfilled PBT typically exhibits tensile modulus between 2500 and 3000 MPa but may undergo post-moulding shrinkage of 1.8–2.2%. The reinforced grade increases modulus into the 3800–5000 MPa band and reduces isotropic mould shrinkage to approximately 0.4–0.8% under ISO 294-4. Elongation at break falls from unfilled values above 20% to a typical range of 3–8% in glass-reinforced toughened systems, meaning snap-fit features require generous radii and closer gate placement.

    Property / test method Unfilled PBT PBT+15% GF impact-modified (B3217E class) PBT+30% GF standard
    Density, ISO 1183-1 1.30–1.32 g/cm³ 1.35–1.42 g/cm³ 1.50–1.55 g/cm³
    Tensile modulus, ISO 527-1/-2 2500–3000 MPa 3800–5000 MPa 8500–10000 MPa
    Tensile strength, ISO 527-1/-2 50–60 MPa 70–90 MPa 110–130 MPa
    Elongation at break, ISO 527-1/-2 >20% 3–8% 2–3%
    Charpy notched impact, ISO 179-1/1eA 4–8 kJ/m² 5–10 kJ/m² 6–8 kJ/m²
    HDT/A, ISO 75-1/-2 60–70 °C 180–200 °C 205–215 °C

    The table summarises broad compound-family ranges from publicly available technical literature for unfilled PBT, 15 wt.% glass-reinforced impact-modified PBT, and 30 wt.% glass-reinforced PBT. It is not a certified lot-specific specification for B3217E.

    The table indicates that 15 wt.% glass fibre occupies an intermediate position in stiffness and flow. The grade is specified instead of 30 wt.% glass-filled PBT when part designs require longer flow lengths, lower warpage, or reduced tool abrasion; it is specified instead of unfilled PBT when snap-fit creep, edge-load cracking, and uncontrolled post-moulding shrinkage are failure modes. However, fibre orientation at gates and weld lines creates anisotropy that must be accounted for in mould filling simulation. A fill pattern with a single gate and uniform wall thickness produces the least variation in tangential and radial tensile properties.

    Falling-dart impact and notched Charpy values are sensitive to mould temperature. At mould temperatures below 60 °C, the quenched amorphous skin thickens, reducing toughness. In contrast, mould temperatures above 100 °C can extend cycle time and cause ejection distortion in thin ribs. The optimised mould temperature window is 80–100 °C; for very thin walls, the lower half of this range is used with higher injection velocities to balance crystallinity and cycle time.

    Continuous-use temperature limits demand IEC 60216 thermal endurance data

    In PBT+GF15 systems, short-term heat deflection temperature under ISO 75-1/-2 is not a direct continuous-use rating. Typical HDT/A values for this compound family fall between 180 °C and 200 °C, but oxidative embrittlement at sustained temperature depends on the stabiliser package and part wall thickness. Thermal endurance should be evaluated using ISO 2578 or UL 746B relative thermal index methods. Most unfilled and 15 wt.% glass-filled PBT grades are assigned continuous-use ratings in the 130–140 °C range for electrical and mechanical retention, with lower limits in hot aqueous or alkaline environments. The E-CTI-Tough modification does not override this boundary; prolonged exposure above 140 °C may produce surface chalking, notch embrittlement, and CTI drift, particularly in sections below 1 mm.

    In hot aqueous or alkaline service, the PBT matrix is susceptible to hydrolytic attack even below the melt point. Ester linkages in the polymer backbone are cleaved by hot water; when the pH is above 9 or when the part is exposed to steam above 85 °C, tensile strength and elongation decline more rapidly than in dry-heat ageing. Chemical compatibility should therefore be verified using the actual fluid mixture under pressure and temperature cycling. Published data for this specific configuration is limited, so field validation is required for under-hood enclosures exposed to glycol/water blends above 85 °C.

    Water absorption at equilibrium in 23 °C water for 15 wt.% glass-filled PBT is commonly below 0.5% under ISO 62. This level is low relative to polyamide, but it is sufficient to plasticise the matrix and alter dielectric performance. Dimensional changes after moisture uptake are anisotropic because the glass fibres restrain shrinkage in the flow direction while transverse expansion is comparatively less restrained. Connectors designed for immersion should not use dry-as-moulded dimensions without post-conditioning or moisture-equilibrated measurement.

    Regulatory compliance for B3217E is application-specific. The base PBT polymer is generally assessed under REACH and RoHS; however, stabiliser, colorant, or processing-aid packages vary by order code and production site. The current product safety data sheet and supplier regulatory declaration should be requested before export, food-contact, or medical evaluations.

    On production-scale toggle-clamp injection moulding machines in the 80–120 tonne range, parts with wall-thickness variation from 0.8 to 2.5 mm typically require hold pressures between 60 and 90 MPa and screw back pressures below 5 MPa to limit glass attrition. Barrel residence time should not exceed 10 minutes at melt temperatures above 260 °C; prolonged residence produces discolouration and a drop in melt viscosity due to chain scission. Hot-runner temperature uniformity should be maintained within ±2 °C across nozzles because local overheating in multi-cavity tools creates asymmetric filling and post-moulding warpage. Mould release typically requires no external lubricant when draft angles are above 0.5° and polished cores are specified. When laser marking is required, contrast should be qualified at the lowest practical laser fluence because the high-CTI formulation may include mineral or additive packages that alter surface char behaviour.