| HS Code | 580823 |
| Grade Designation | Pocan B3215 |
| Polymer Base | PBT |
| Glass Fiber Content | 10% |
| Ul94 Flame Rating | HB |
As an accredited Lanxess Pocan® PBT+GF10% B3215 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Lanxess Pocan® PBT+GF10% B3215 is packaged in 25 kg moisture-barrier bags, supplied on pallets for industrial handling. |
| Container Loading (20′ FCL) | 20′ FCL dry container loaded with palletized 25 kg bags of Lanxess Pocan® PBT+GF10% B3215, shrink-wrapped and secured for ocean transport. |
| Shipping | Lanxess Pocan® PBT+GF10% B3215 is supplied as dry, glass-fiber-reinforced PBT pellets in moisture-barrier bags, boxes, or bulk containers. It is not classified as dangerous goods for transport (no UN number). Ship at ambient temperature, keep dry, and avoid direct sunlight, heat, and moisture exposure. |
| Storage | Store Lanxess Pocan® PBT+GF10% B3215 in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and incompatible materials. Keep original containers tightly closed to prevent moisture pickup and contamination. Protect from physical damage, use first-in/first-out stock rotation, avoid prolonged high humidity or elevated temperatures, and follow the safety data sheet and local regulations. |
| Shelf Life | The shelf life is typically 24 months when stored sealed, dry, at room temperature, and protected from moisture and sunlight. |
During injection molding of Pocan® B3215 into multi-pin automotive underhood connector housings and sensor bodies, the primary production conflict is not heat resistance alone but the interaction between glass-fiber orientation in thin-walled pin arrays and weld-line strength when gas counterpressure is not available. The grade contains 10% glass fiber by weight, which reduces mold-shrinkage anisotropy relative to unfilled PBT while retaining a high-flow skin layer that fills 0.8 mm walls around terminal pins. Hot-runner tools with naturally balanced manifolds are required because shear-induced fiber migration at the melt front changes local shrinkage and leads to terminal pin hole diameter ovality. Moisture control is non-negotiable: pellets should be dried in a desiccant dryer with a dew point at or below -30°C at 120°C for 4–6 h until residual moisture is below 0.02%; hopper residence time beyond 6 h at ambient humidity above 60% RH allows regain and hydrolytic chain scission during plastication. Barrel temperatures are normally set between 250°C and 270°C with the nozzle at 260–270°C, and the melt must not exceed 280°C; cumulative residence time above 270°C should remain under 10 min because terephthalate oligomers accumulate and lower notched impact. Mold temperature should be held at 80–100°C to promote crystallization and post-mold dimensional stability; higher values above 100°C extend cycle time without improving connector latch retention. Shrinkage determined according to ISO 294-4 is anisotropic, with flow-direction values typically below 1.0% and cross-flow values in the 1.0–1.5% range, so gate location must be validated by warpage simulation before tool steel is cut. In engine bay validation, connector bodies are exposed to thermal shock cycles from -40°C to 125°C, damp heat per IEC 60068-2-30, and oil immersion per ISO 175; a material is suitable only if it retains 70% of baseline tensile strength after the agreed exposure, a threshold set by the OEM reliability target rather than by the resin supplier.
The substitution of Pocan® B3215 in relay bases and coil formers is driven by the need to hold flatness across a two-part assembly while the coil itself generates local self-heating. Coil formers molded in 10% glass-fiber PBT exhibit lower creep under winding tension than unfilled PBT, but the improvement is direction-dependent; the wound bobbin is loaded radially by copper wire at 0.2–0.5 N per turn, which can be used to calculate creep strain after 1,000 h at 85°C. Mold shrinkage data from the datasheet should be checked against ISO 294-4, because the flow-direction shrinkage of glass-filled PBT is significantly lower than the transverse shrinkage, causing dome-shaped warpage in flat relay bases. The processing window should use a mold temperature at the upper end of the recommended 80–100°C range and a packing pressure of 60–80 MPa hydraulic equivalent for 5–8 s per mm of wall thickness to minimize post-ejection distortion. If the mold temperature is below 60°C, the frozen skin layer locks in flow-direction orientation and the base will warp after moisture conditioning or annealing. Because relay bases sit in panels with molded snap-fit latches, tensile creep after 24 h at 23°C and 50% relative humidity should be measured via ISO 899-1; this test is more relevant than short-time tensile modulus for latch relaxation. The material must also withstand copper-coil self-heating, so long-term heat aging per IEC 60216 at 120°C or 130°C is typically used to confirm that the coil former does not embrittle before the relay lifetime target. Published data for this specific configuration is limited, so oven aging of molded coil formers with windings in place is the responsibility of the relay manufacturer.
When a power tool housing is specified around Pocan® B3215, the engineering boundary should be set at room-temperature impact, because the 10% glass-fiber reinforcement raises stiffness but does not provide the ductile failure mode demanded by cold-temperature drop tests. Notched Charpy impact measured according to ISO 179-1/1eA falls in the low single-digit kJ/m² range at 23°C for standard glass-filled PBT grades; at -20°C the energy absorption is lower and fracture often initiates at surface glass-fiber ends. This limits the material to tool housings, gear case covers, and motor brush holder plates that are not subjected to direct impact from chuck keys, fall from scaffold height, or prying at battery interfaces. In production, the injection gate must be positioned away from the thinnest wall section adjacent to the motor ventilation slots; a tab gate entering a 2.0 mm nominal wall can create a visible glass-rich wake line that reduces unnotched impact by local fiber alignment. The mold surface should be polished to SPI A-2 or finer if appearance surfaces are required, because glass fibers at a 10% loading are less likely than 30% glass systems to produce severe fiber bloom but still create micro-roughness around the gate. For dimensional audit of power tool housings, shrinkage should be measured on plaques conforming to ISO 294-4 after 48 h conditioning at 23°C and 50% RH. The resulting values determine whether the motor-end and gear-case interfaces maintain sufficient clearance for bearing press-fit without flash or cracking after assembly.
Internal frames and dry-heat structural parts for domestic appliances are produced from Pocan® B3215 only when the service temperature remains below 130°C and the part is not in continuous contact with water above 60°C. The material is selected for coffee-machine internal brackets, air-outlet louvres, and toaster end panels where mold shrinkage must be low enough to hold snap-fit dimensions after annealing, but it is not the correct choice for pump housings running in hot detergent solution. In these applications the dominant specification is dimensional stability after thermal conditioning; a useful incoming inspection is to measure length change after 24 h at 120°C against ISO 294-4-derived reference dimensions, with a typical tolerance of ±0.05 mm across a 50 mm feature length. If the part is exposed to oil vapor or fruit acids, chemical compatibility can be screened by immersion according to ISO 175, but parts that sit in direct contact with food must be evaluated for overall migration under the relevant regional food-contact regulation before production release; PBT cannot be assumed compliant without extraction testing. Because these domestic parts are often produced in multi-cavity tools with 8–16 cavities, cavity pressure sensors are recommended to detect filling imbalance before the part warps, especially when ribs and bosses create flow restrictions that skew glass-fiber orientation. Mold temperatures below 80°C produce a resin-rich surface layer that improves gloss but delays crystallization and increases post-mold shrinkage, so the lower mold-temperature limit should be tested against downstream assembly rather than accepted from a generic processing table.
Terminal blocks and high-density connector strips require creepage distances and tracking resistance to be validated against the printed-circuit-board voltage system rather than against a generic resin datasheet. For Pocan® B3215, the tracking relevant parameter is the comparative tracking index determined according to IEC 60112; glass-fiber-reinforced PBT grades commonly fall in the 250–300 V range, but the specific published value for this exact grade, color, and wall thickness must be taken from the supplier test report because pigments and processing additives shift the result. The material’s low water absorption, evaluated by ISO 62 after 24 h immersion at 23°C, is generally below 0.5%, which helps maintain insulation resistance in humid tropical service, but creepage distances should still follow IEC 60664-1 pollution degree 2 limits rather than being reduced solely because of the polymer’s hydrophobic surface. In manufacturing, terminal-block walls with 0.6–0.8 mm thickness can be filled when the melt is held at 260–270°C and the mold at 80–100°C; the electrical weakness in such parts is almost always a knit line at the rear of the partition wall, where fiber separation reduces local tracking resistance. That knit line must be relocated by gate placement or eliminated by a short parallel flow at the end of the partition. Table 1 lists the core validation matrix used for electrical installation components, not as an exhaustive approval plan but as the minimum test set for global trading.
Table 1. Core electrical/electronic validation matrix for Pocan® B3215 applications. Consult the supplier yellow card and regional approval body for grade-specific values.
| Property / Requirement | Test Method / Standard | Application Relevance |
|---|---|---|
| Tensile modulus and stress at break | ISO 527-1/-2 | Terminal retention and snap-fit latch force |
| Flexural modulus | ISO 178 | Partition wall deflection under screw torque |
| Notched Charpy impact | ISO 179-1/1eA | Resistance to assembly cracking in thin webs |
| Heat deflection temperature | ISO 75-2/-1, 1.8 MPa | Short-term thermal load under rated current |
| Comparative tracking index | IEC 60112 | Creepage path toughness in polluted boards |
| Flammability | UL 94, IEC 60695-11-10 | Thickness-dependent classification; yellow card required |
| Damp heat aging | IEC 60068-2-30 | Insulation resistance after tropical cycling |
| Molding shrinkage | ISO 294-4 | Dimensional stability of pitch and contact apertures |
Solenoid valve bodies and water meter register plates can be injection molded from Pocan® B3215 for cold-water circuits below 40°C, but the application must not be extrapolated into continuous hot-water service because PBT undergoes hydrolytic chain scission at elevated water temperatures. The controlling test is ISO 62 water absorption kinetics combined with tensile strength retention after immersion; published data for this specific grade after 1,000 h in 60°C water is more informative than the 24 h immersion value. In solenoid valve bodies, the internal bore and valve seat area must be sealed against leakage under 1.0 MPa hydraulic test pressure, which requires a knit line to be kept out of the bore circumference; if a center gate or double side gate is not possible, the burst test must be repeated on production parts with variable melt temperature to confirm that hydrolysis-induced viscosity loss has not weakened the weld line. The material is resistant to mineral oil, aliphatic hydrocarbons, and many neutral salt solutions at room temperature, but hot alkaline cleaners above 50°C and glycol-based antifreeze at engine temperatures exceed the chemical compatibility boundary; these media should be tested using ISO 175 immersion before approval. Dimensional stability after moisture exposure can be checked by comparing ISO 294-4-prescribed shrinkage plaques after 48 h water immersion, because moisture absorption causes slight swelling that can bind a water meter register spindle if the clearance is below 0.05 mm. Molded parts must not be used in drinking-water contact without production-specific migration testing; the raw-material certification does not replace product-line approval.
Competitive Lanxess Pocan® PBT+GF10% B3215 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Lanxess Pocan® PBT+GF10% B3215 is a polybutylene terephthalate injection-molding grade containing a nominal 10% by mass loading of chopped glass fiber. The ISO 1043 designation is PBT-GF10. The product is supplied under the Pocan® trademark and is positioned for thin-walled technical components requiring higher stiffness than unfilled PBT but lower volumetric glass loading than 20% glass-fiber grades. In the dry-as-molded condition, the compound exhibits a density of approximately 1.36 g/cm³ when tested according to ISO 1183-1. During manufacture, the glass fiber is introduced downstream on a co-rotating twin-screw extruder with an L/D ratio of approximately 40:1 to limit excessive fiber attrition; excessive shear reduces fiber length and lowers notched impact strength and tensile modulus after molding. The unreinforced PBT matrix provides melt processability on conventional reciprocating-screw injection-molding machines, while the glass fiber content raises tensile modulus and reduces mold shrinkage relative to unfilled polyester. The base formulation is not a flame-retardant grade; typical flame performance is UL 94 HB at 1.6 mm thickness. The material is normally supplied as cylindrical pellets and must be protected from moisture absorption during open storage.
Relative to an unfilled medium-viscosity PBT reference, the B3215 formulation increases tensile modulus by approximately 1,800–2,000 MPa and lowers parallel mold shrinkage from roughly 1.8–2.0% to approximately 0.8–1.0%, as measured on a 60 mm × 60 mm × 2 mm plaque per ISO 294-4. The reduction in shrinkage anisotropy is particularly relevant for flat connector bodies and narrow wall sections where differential cooling creates post-mold warpage. Compared with a 20% glass-fiber PBT reference, B3215 retains a lower melt viscosity and lower density, reduces screw and barrel wear in filled systems, and produces a smoother surface finish with less fiber prominence at thin-walled surfaces. The trade-off is a lower tensile modulus, typically 4,400–4,600 MPa for B3215 versus approximately 6,500–7,000 MPa for the 20% glass-fiber grade, and a lower heat deflection temperature under load. Impact performance is less ductile than unfilled PBT; notched Charpy values at 23 °C are normally in the 4.0–5.5 kJ/m² range per ISO 179-1/1eA, whereas unfilled PBT can exceed 5.0 kJ/m² at the same thickness. This property positioning makes B3215 suitable when flow length and surface quality are limiting factors in tool design, but higher loading cannot be tolerated.
Processing on production-scale equipment requires closed-loop dehumidified-air drying at 120 °C for 4 h, with a residual moisture target below 0.02%. PBT hydrolysis at the melt stage is governed by time–temperature–moisture interactions; residual moisture above 0.03% produces melt viscosity loss, surface splay, and reduced tensile strength at the knit line. A desiccant-bed dryer with a dew point of −30 °C or lower is recommended for continuous operation at high humidity or when regrind fractions above 20% are added. Barrel temperature settings from rear to nozzle are typically 250 °C, 255 °C, 260 °C, and 265 °C; melt temperature measured by an air-shot pyrometer should remain below 280 °C. Mold temperature is controlled between 60 °C and 100 °C, with the higher portion of the range used for high-gloss surfaces and the lower portion for fast cycle times on thin-wall parts. Injection speed should be moderate to high, with a filled screw using a check ring; screw L/D ratios of 18:1 to 22:1 and compression ratios of 2.5:1 to 3.0:1 are standard. Holding pressure is adjusted until gate freeze is achieved, commonly 500–800 bar hydraulic pressure depending on part thickness. Total residence time should not exceed 10 min at melt temperature; longer residence can cause polyester chain scission and a measurable drop in notched impact strength. Batch-to-batch variation in melt volume-flow rate is monitored per ISO 1133-1:2022; a shift of more than 20% relative to the approved lot requires barrel temperature and injection velocity adjustment.
PBT is a semicrystalline polyester with good resistance to aliphatic hydrocarbons, automotive fuels, lubricating oils, greases, and many dilute acids at room temperature. However, the ester linkage is susceptible to hydrolysis in hot water and steam above 60 °C; continuous exposure to engine coolant at elevated temperature reduces molecular weight and impact strength unless the part is designed with a thick wall and low residual stress. Alcohols, ketones, esters, and chlorinated hydrocarbons can swell or attack PBT depending on concentration, temperature, and contact time. The B3215 grade should not be specified for continuous immersion in strong alkalis or concentrated oxidizing acids. Amine-containing processing aids or flame-retardant additives are generally incompatible with PBT because catalyzed ester cleavage can occur during compounding and molding. Parts that operate in humid underhood environments require post-mold conditioning or pre-drying at 120 °C if moisture uptake exceeds 0.05% before assembly. Published long-term aging data for B3215 in specific coolant-glycol mixtures is limited; qualification under end-use conditions is required when exposure exceeds 1,000 h at 85 °C.
Electrical connector bodies, relay sockets, sensor housings, bobbins, and structural brackets are typical application fields. The combination of 10% glass reinforcement with PBT provides a balance between electrical insulating behavior, dimensional stability, and fast crystallization for short cycle times. In thin-walled connectors with 0.4–0.8 mm wall thickness, the grade fills long flow paths at moderate melt temperature, while the glass fiber content restricts post-mold warpage. Creep resistance under low load is improved relative to unfilled PBT when tested per ISO 899-1 at 23 °C, although long-term creep data for this specific formulation is limited in public literature. The base grade does not contain flame-retardant synergists; applications requiring glow-wire ignition resistance or V-0 classification at 0.75 mm require a flame-retarded Pocan® variant. Surface quality is acceptable for non-decorative technical surfaces; textured tools reduce visible fiber flow lines at gate regions.
| Property | Test standard | B3215 typical value | Unfilled PBT reference | 20% GF PBT reference |
|---|---|---|---|---|
| Glass fiber content | ISO 3451-1 | 10% | 0% | 20% |
| Density | ISO 1183-1 | 1.36 g/cm³ | 1.30 g/cm³ | 1.45 g/cm³ |
| Tensile modulus | ISO 527-1/-2 | 4,500 MPa | 2,600 MPa | 6,500 MPa |
| Tensile stress at break | ISO 527-1/-2 | 85–95 MPa | 50–60 MPa | 100–120 MPa |
| Nominal strain at break | ISO 527-1/-2 | 4.0–6.0% | >20% | 2.5–3.5% |
| Flexural modulus | ISO 178 | 4,300 MPa | 2,500 MPa | 6,000 MPa |
| Charpy notched impact strength, 23 °C | ISO 179-1/1eA | 4.0–5.5 kJ/m² | 5.0–7.0 kJ/m² | 6.0–8.0 kJ/m² |
| Heat deflection temperature, 1.8 MPa | ISO 75-1/-2 | 185–195 °C | 55–65 °C | 195–205 °C |
| Mold shrinkage, parallel | ISO 294-4 | 0.8–1.0% | 1.8–2.0% | 0.4–0.6% |
| Compliance area | Standard or regulation | Product condition |
|---|---|---|
| Material designation | ISO 1043-1 | PBT-GF10 |
| Recycling marking | ISO 11469 | PBT-GF10 |
| Flame rating | UL 94 | HB at 1.6 mm |
| EU RoHS | 2011/65/EU Annex II | Restricted substances below maximum concentration values based on supplier declaration |
| REACH SVHC | 1907/2006/EC Article 33 | No SVHC above 0.1% w/w in supplied article |
| Food-contact status | FDA 21 CFR 177.1660, EU 10/2011 | Not certified for food-contact use |
Tool design for B3215 must account for anisotropic shrinkage. Gates should be positioned away from flow obstacles; a land length of 0.5–1.0 mm and a gate diameter of 0.8–1.5 mm are typical for technical parts. The mold cavity should be tempered with sufficient cooling circuits to maintain a surface temperature of 80 °C on critical walls; variation above ±5 °C across the cavity increases part-to-part dimensional scatter. Ejector pins and slides require wear-resistant tool steel because glass fiber abrasion is higher than unfilled PBT, though lower than 20% glass-fiber compounds. Hydraulic clamp force for a projected part area of 100 cm² is typically 60–80 t at a cavity pressure of 600–800 bar. Start-up scrap should be minimized by running a dry-cycle mold heat-up and discarding the first 5–10 shots after material changeover. When regrind is reused at 20 wt%, consistent pellet size is required to avoid screw feeding variation.