| HS Code | 155239 |
| Density | 1.30 g/cm³ |
| Meltvolumerate | 15 cm³/10 min (250 °C/2.16 kg) |
| Moldingshrinkage | 1.7 % parallel; 1.7 % normal |
| Tensilemodulus | 2600 MPa |
| Tensilestrength | 55 MPa |
| Elongationatbreak | 20 % |
| Charpynotchedimpactstrength23c | 4 kJ/m² |
| Charpyunnotchedimpactstrength23c | No break |
| Ballindentationhardness | 130 MPa |
| Heatdeflectiontemperaturea | 60 °C |
| Heatdeflectiontemperatureb | 150 °C |
| Vicatsofteningtemperatureb50 | 170 °C |
| Meltingtemperature | 225 °C |
| Waterabsorptionsaturation | 0.4 % |
| Volumeresistivity | 1E15 Ω·cm |
| Surfaceresistivity | 1E14 Ω |
| Dielectricstrength | 20 kV/mm |
| Comparativetrackingindex | 600 V |
| Flammabilityul94 | HB |
| Coefficientoflinearthermalexpansion | 1.2E-4 1/K |
As an accredited Lanxess Pocan® Food-Contact PBT B1501 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Lanxess Pocan® Food-Contact PBT B1501 is supplied in 25 kg moisture-proof bags, typically 40 bags per pallet (1,000 kg net). |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): palletized 25 kg bags of Lanxess Pocan® Food-Contact PBT B1501, loaded dry, ambient, evenly distributed, and secured. |
| Shipping | Lanxess Pocan® Food-Contact PBT B1501 is shipped as non-hazardous thermoplastic pellets in moisture-protected bags or octabins. Keep containers dry, closed, and away from heat or direct sunlight. No special transport classification is normally required; follow the SDS and local regulations. |
| Storage | Store Lanxess Pocan® Food-Contact PBT B1501 in a cool, dry, well-ventilated area, in original sealed containers. Protect from direct sunlight, heat, moisture, and contamination. Keep away from incompatible substances and follow the supplier’s SDS and local regulations. Avoid prolonged storage under humid conditions to preserve product quality. |
| Shelf Life | Store dry; shelf life is typically 12 months from delivery in unopened packaging at room temperature, per manufacturer recommendations. |
Competitive Lanxess Pocan® Food-Contact PBT B1501 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Lanxess Pocan B 1501 is an unreinforced polybutylene terephthalate (PBT) injection-molding resin supplied as a food-contact grade within the Pocan polyester range. The base polymer is identified under ISO 1043 as PBT, and the product is formulated without glass-fiber reinforcement or impact modification. The reported melt volume-flow rate of 22 cm³/10 min at 250 °C under 2.16 kg load (ISO 1133-1:2022) places the grade in the high-fluid segment for thin-wall and multi-cavity tooling. Density is 1.30 g/cm³ per ISO 1183-1, and the unreinforced composition provides more isotropic mold shrinkage than glass-fiber-filled PBT. The resin is intended for direct and indirect food-contact components in kitchen appliances, water-contact manifolds, coffee machine internals, conveyor guides, caps, sensor bodies, and repeated-use food-processing parts.
The application envelope covers short-cycle technical parts that require the inherent stiffness, low moisture absorption, and chemical resistance of PBT. Because the material is an ester-linked thermoplastic polyester, hydrolytic degradation during drying and melt processing is the primary operational risk. Food-contact certification does not remove that risk. In multi-cavity tooling with wall thickness below 1.0 mm, the high melt volume-flow rate reduces injection pressure and improves cavity filling, but rapid crystallization of PBT requires fast injection speed and a heated mold at 60 °C to 100 °C to avoid frozen-in stress and weak weld-line regions. Published migration data for this exact grade under fatty-food simulant D2 at 70 °C is limited; converter validation on the finished article remains mandatory before specification.
From a production-scale equipment perspective, the resin is processed on injection molding machines using a three-zone screw with an L/D ratio of 20:1 to 24:1 and a compression ratio of 2.5:1 to 3.0:1. Small screw diameters below 25 mm can generate excessive shear heating at high screw speed; rotational speed should be adjusted so that melt temperature measured by an insertion pyrometer does not exceed 270 °C. On hydraulic equipment producing a 0.8 mm thin-wall lid, specific clamp force requirements in the range 0.6 t/cm² to 0.8 t/cm² of projected area are typical for unfilled PBT, although gate size, runner balance, and hold-pressure profile are the dominant factors in practice.
Incoming resin lots should be inspected for melt volume-flow rate according to ISO 1133-1:2022. A shift from the nominal 22 cm³/10 min toward 26 cm³/10 min may indicate hydrolytic or thermal degradation before molding. Moisture analysis by Karl Fischer titration at 160 °C is preferred over simple weight-loss methods because surface moisture on pellets can underreport the hydrolytic risk carried into the melt.
Food-contact conformity for Pocan B 1501 involves the entire formulated composition, not only the PBT polymer backbone. Under Regulation (EU) No 10/2011, all monomers and additives must be listed in Annex I, and overall migration must not exceed 10 mg/dm² when tested according to the EN 1186 series. The specific migration limit for 1,4-butanediol, a PBT monomer, is set at 5 mg/kg food. U.S. conformity is evaluated under 21 CFR 177.1660, which covers poly(tetramethylene terephthalate) resins for repeated food-contact use subject to the food types and temperature conditions stated in that section. Regulation (EC) No 2023/2006 imposes good manufacturing practice obligations on the converter, including traceability, documentation, and prevention of contamination from non-food-contact grades.
The food-contact designation separates B1501 from general-purpose unreinforced PBT compounds that may contain non-listed mold-release waxes, nucleating packages, recycled feedstocks, or high-carryover processing aids. Color masterbatch addition must also be revalidated because pigment carriers and dispersants can change overall migration. A food-contact pellet does not automatically produce a compliant finished part; the final dry blend and molded article are the regulated articles.
| Control | Standard or regulation | Requirement or limit |
|---|---|---|
| Overall migration | EU 10/2011 / EN 1186 | 10 mg/dm² |
| Specific migration of 1,4-butanediol | EU 10/2011 Annex I | 5 mg/kg food |
| Resin specification for PBT | U.S. FDA 21 CFR 177.1660 | Repeated-use food-contact conditions |
| Good manufacturing practice | EU 2023/2006 | Traceability and contamination prevention |
Migration of low-molecular-weight species from PBT is diffusion-controlled. At equal wall thickness, migration rises with service temperature and with food simulant aggressiveness. For aqueous simulants below 40 °C, unfilled PBT typically remains below the overall migration limit, but fatty simulants can extract lipophilic additives more aggressively. This is why the finished article must be tested under the food simulant assigned by Regulation (EU) No 10/2011 according to the intended food category: dry, acidic, aqueous, alcoholic, or fatty.
Before processing, Pocan B 1501 pellets must be dried to a moisture content below 0.02 wt%. A desiccant-type dehumidified air dryer with a dew point of −30 °C or lower is standard; circulating-air tray drying is inadequate because ambient humidity can leave sufficient moisture for hydrolytic chain scission. Pre-drying at 120 °C for 4 h is the usual starting condition for fresh bags. If hopper residence extends beyond 8 h at 120 °C, pellet discoloration can occur even when the drying air is dry. Hopper loading should therefore be matched to consumption rate.
During melt processing, barrel temperatures are typically set from 250 °C to 270 °C. The material should not be held above 270 °C for more than 10 min, because thermal degradation reduces molecular weight and notched impact even though melt fluidity may appear to improve. On hot-runner molds, valve-gated systems are preferred over open hot tips to prevent drool and to maintain packing pressure. Manifold dead spots must be minimized; a sharp 10 °C temperature reduction at the nozzle can create a cold slug and increase gate freeze-off risk in the cavity nearest the nozzle.
Isothermal crystallization half-times for PBT at 115 °C to 130 °C are commonly reported in the range 10 s to 30 s. This rapid crystallization is useful for short cycle times, but it narrows the processing window. When the cavity surface temperature falls below 60 °C, the melt can solidify before packing pressure compensates for volumetric shrinkage, leaving sink marks, post-mold dimensional movement, or residual stress. Mold-surface temperature should be verified by contact pyrometry because water-line set temperature does not equal actual cavity temperature.
| Property | Test standard | Unit | Typical value |
|---|---|---|---|
| Density | ISO 1183-1 | g/cm³ | 1.30 |
| Melt volume-flow rate | ISO 1133-1:2022 | cm³/10 min | 22 |
| Tensile modulus | ISO 527-1/-2 | MPa | 2500 |
| Tensile stress at yield | ISO 527-1/-2 | MPa | 55 |
| Flexural modulus | ISO 178 | MPa | 2400 |
| Charpy notched impact, 23 °C | ISO 179-1/1eA | kJ/m² | 3.0 |
| Heat deflection temperature, 1.8 MPa | ISO 75-1/-2 | °C | 60 |
| Vicat softening temperature, B120 | ISO 306 | °C | 180 |
| Mold shrinkage, flow/transverse | ISO 294-4 | % | 1.8 / 1.9 |
These are natural-grade reference values obtained from injection-molded specimens under standard test conditions. Colored or regrind-modified batches can shift modulus and flow by 5 % to 10 % relative to natural material. The values do not constitute a specification for every batch; incoming quality control should compare each lot against the processor’s approved reference.
Capillary rheometry at 250 °C shows shear-thinning behavior. At apparent shear rates of 100 s⁻¹ to 1,000 s⁻¹, viscosity declines substantially relative to low-shear values. This supports thin-wall filling but reduces melt strength in open-nozzle systems. In hot-runner manifolds with 8- or 16-cavity layouts, tip temperatures should be balanced within ±2 °C using independently controlled zones or valve-gate controllers. Thermal imbalance produces cavity-to-cavity variability in shrinkage, packing, and notched impact.
Compared with a 30 wt% glass-fiber reinforced PBT measured under the same ISO methods, Pocan B 1501 shows lower melt viscosity and lower tensile modulus. The reinforced grade can exhibit tensile modulus near 11,000 MPa and HDT/A near 200 °C, while the unreinforced grade remains near 2,500 MPa and 60 °C. Those differences are design-critical. A reinforced polyester should be selected for structural load-bearing supports, whereas B1501 is better suited to thin-walled flow-path components and parts where a sealing face must remain flat after ejection.
Because unfilled PBT shrinks nearly equally in flow and transverse directions, round parts and ribbed plates are less prone to warpage than glass-fiber-filled PBT, where fiber orientation can create differential shrinkage of 0.5 to 0.8 percentage points. Mold shrinkage measured on a 60 mm × 60 mm × 2 mm plaque per ISO 294-4 is 1.8 % in flow and 1.9 % in the transverse direction for B1501. This relative isotropy is an advantage in sealing faces, cylindrical housings, and components with circular ribs.
On cold-runner tools, the sprue diameter should not fall below 3.0 mm, because premature sprue freezing limits hold-pressure transmission. Short sprues, generous cold slug wells, and direct gates reduce short-shot rates. On hot-runner valve gates, gate freeze-off occurs when the valve-pin temperature is set too low; the typical symptom is short shots in the last cavity to fill and variable packing. These failure modes are common with rapid-crystallizing PBT and should be separated from moisture-related defects by checking dryer dew point and pellet moisture before altering tool temperature.
Regrind from sprues and runners can be reintroduced if the material is kept clean and dry. For food-contact articles, regrind from the same compliant grade is commonly limited to 20 wt% in Europe under good manufacturing practice. Each heat cycle reduces molecular weight and notched impact; higher regrind percentages require mechanical property verification per ISO 179-1/1eA at 23 °C and migration revalidation of the finished part.
Operational boundaries include limited resistance to hot hydrolysis. Continuous contact with water or steam above 60 °C accelerates hydrolytic degradation and reduces notched impact; hydrolytically stabilized PBT or another polyester is preferred for hot-water sterilization or aggressive dishwasher-heated cycles. The grade is also sensitive to strongly alkaline media and should be kept away from amine-containing processing aids that can attack the ester linkage. For colored articles, the carrier resin must carry the same food-contact status, and the processor should verify that masterbatch addition does not push overall migration above 10 mg/dm².