| HS Code | 446686 |
| Manufacturer | Lanxess |
| Product Name | Pocan® B1600 |
| Polymer Type | Polybutylene terephthalate (PBT) |
| Grade Type | Extrusion grade |
| Density | 1.30 g/cm³ |
| Melt Volume Flow Rate | 16 cm³/10 min (190 °C, 2.16 kg) |
| Tensile Modulus | 2600 MPa |
| Tensile Strength | 55 MPa |
| Elongation At Break | 20% |
| Charpy Notched Impact Strength | 4 kJ/m² (23 °C) |
| Vicat Softening Temperature | 165 °C (B120) |
| Heat Deflection Temperature | 60 °C (A) / 150 °C (B) |
| Melting Temperature | 225 °C |
| Water Absorption | 0.4% |
| Molding Shrinkage | 1.5–2.0% |
| Processing Method | Extrusion |
As an accredited Lanxess Pocan® Extrusion-grade PBT B1600 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Lanxess Pocan® Extrusion-grade PBT B1600 is supplied in 25 kg moisture-proof, multi-layer bags, palletized for standard industrial transport. |
| Container Loading (20′ FCL) | 20′ FCL: Lanxess Pocan® B1600 extrusion-grade PBT in 25 kg bags on pallets, securely stowed with desiccant and moisture protection. |
| Shipping | Lanxess Pocan® Extrusion-grade PBT B1600 is typically shipped as dry thermoplastic pellets in moisture-proof 25 kg bags, big bags, or octabins. It is not classified as dangerous goods for transport. Ship at ambient temperature, avoiding moisture, direct sunlight, and excessive heat; follow local packaging and labeling regulations. |
| Storage | Store Lanxess Pocan® Extrusion-grade PBT B1600 in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep containers tightly closed to prevent moisture absorption and contamination. Avoid prolonged exposure to high humidity or elevated temperatures, and follow first-in, first-out stock rotation. Refer to the supplier’s SDS and datasheet for specific storage limits. |
| Shelf Life | Typically 24 months when stored dry at 15–25°C in unopened original packaging, protected from moisture. |
Competitive Lanxess Pocan® Extrusion-grade PBT B1600 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Lanxess Pocan® B1600 000000 is an unreinforced, medium-viscosity polybutylene terephthalate (PBT) extrusion grade supplied as natural, unfilled pellets. The 000000 suffix identifies an uncolored base polymer without flame-retardant additives. The grade is specified for profile, sheet, monofilament, and fiber-optic loose-tube buffer-tube extrusion rather than high-speed injection molding. According to manufacturer-published typical data, density is 1.30 g/cm³ under ISO 1183-1:2019 and melt volume-flow rate is 12 cm³/10 min under ISO 1133-1:2022 at 250 °C and 2.16 kg. These values place the material in the unfilled PBT envelope and distinguish it from injection-molding grades with significantly higher melt flow. Residual moisture after drying must be below 0.02 wt% under ISO 15512:2019 because PBT undergoes hydrolytic chain scission at melt temperature.
At 23 °C, the unreinforced grade shows a tensile modulus of 2500 MPa and tensile stress at yield of 55 MPa under ISO 527-2:2012. Charpy notched impact is 4.0 kJ/m² under ISO 179-1/1eA. Heat deflection temperature under ISO 75-2:2013 is approximately 150 °C at 0.45 MPa and 55 °C at 1.80 MPa. These values place B1600 below short-glass reinforced PBT compounds in modulus and creep resistance, but its absence of glass fiber eliminates glass-fiber orientation and reduces die-lip wear.
Low-viscosity injection-molding PBT grades with MVR above 25 cm³/10 min fill thin-wall connectors but produce unacceptable drawdown and poor diameter control in free-surface extrusion. High-viscosity PBT grades with MVR below 8 cm³/10 min generate higher extruder torque and may require melt temperatures above 260 °C for uniform output. B1600 sits between these classes at approximately 12 cm³/10 min. The practical consequence is that it can be processed on single-screw extruders without excessive melt pressure while retaining sufficient melt strength for tube and monofilament sizing. Relative to short-glass reinforced PBT compounds with tensile modulus above 5000 MPa, B1600 has lower stiffness and no fiber-related surface roughness, but it also has lower creep resistance. Relative to PBT/PET blends, B1600 crystallizes faster than PET and is less sensitive to quench-bath temperature, but the glass transition remains in the 45–60 °C range, which limits dimensional stability above that range unless the section is annealed.
Flame-retarded PBT compounds containing brominated or phosphinate systems shift UL 94 classification to V-0 but typically reduce comparative tracking index and increase melt density. B1600 does not carry those additives; its unfilled natural form is therefore different in both flow behavior and electrical tracking performance. The grade is also not optimized for thin-wall injection molding. Converting a low-viscosity injection-molding PBT to B1600 without adjusting barrel temperatures, screw speed, or die geometry commonly causes melt-pressure instability at the die.
In production-scale monofilament and fiber-optic buffer-tube lines, B1600 is normally predried in a desiccant dryer at 120 °C for 4–6 h. The dryer dew point should remain below -40 °C, and hopper residence time above 8 h at 120 °C should be avoided because extended heat exposure can shift melt viscosity and cause yellowing. Wet resin hydrolyzes in the barrel; the first indication is melt-pressure fluctuation followed by surface roughness, bubble formation, and loss of Charpy impact. A single-screw extruder with L/D between 25:1 and 30:1 and compression ratio between 2.5:1 and 3.5:1 is standard. Barrel setpoints from 230 °C in the feed zone to 245–250 °C in the metering zone, with adapter and die at 250–260 °C, are typical. Melt temperature measured at the die should remain below 270 °C, and residence time above 250 °C should not exceed 10 min. A gear pump between the extruder and die is often used to reduce pressure pulsation; its inlet pressure should be kept stable because PBT melt is shear-thinning and small speed changes can alter die flow. In fiber-optic loose-tube processes, inline vacuum sizing and low post-extrusion shrinkage are required; the tube is normally cooled in water at 30–60 °C and later annealed to reduce residual stress. PBT crystallization is fast enough to permit shorter cooling lengths compared with PET, but rapid cooling can produce a fine crystalline skin that affects bending behavior unless annealing is controlled.
Monofilament drafting conditions for PBT are process-specific. Published data for this specific configuration is limited, but general industrial practice uses a first-stage water quench at 30–60 °C, drawing at 60–80 °C with draw ratios between 3.5:1 and 5.0:1, and annealing under tension at 160–200 °C. These ranges are not a substitute for line-specific trials; the drawing window narrows if residual moisture exceeds 0.02 wt% or if melt temperature exceeds 270 °C. Die drool from crystalline deposits at the die lip can occur; maintaining a uniform die temperature and periodic purge-compound use reduces buildup.
Closed-loop edge trim and start-up waste can be reintroduced at up to 20 wt% if the trim is free of dust, oil, and moisture. Higher levels of recycled material are possible only after melt-flow-rate retention is checked; each pass through the extruder tends to raise MVR through thermal and hydrolytic chain scission. A 60/80/100 mesh breaker-screen pack ahead of the gear pump protects the die from carbonized gels. Pressure drop across the screen pack is tracked; a rise of more than 15 % from the clean-screen baseline generally indicates blocked screens or degraded melt. In buffer-tube extrusion, the screen pack also contributes to back-mixing and thermal homogeneity, but excessive pressure drop can shear-heat the melt above 270 °C.
Post-extrusion shrinkage is a critical processing parameter. Rapid quenching in water at 30–60 °C yields a fine spherulitic skin and low crystallinity, which can later shrink when the part is heated. To stabilize dimensions, PBT monofilament and tube are annealed under tension at 160–200 °C. Industrial hot-air shrinkage specifications at 150 °C often require below 2 %; achieving that target depends on draw ratio, line speed, and annealing residence time. Excessive annealing or draw ratios above 5:1 may reduce elongation at break and increase fibrillation in brush filaments.
Selection is driven by moisture absorption and hydrocarbon resistance. Polyamide 6 absorbs approximately 2.5–3.0 wt% moisture at 23 °C and 50 % relative humidity, whereas B1600 reaches about 0.2 wt% equilibrium under ISO 62:2008. In humid production environments, the lower moisture uptake reduces tension variation in monofilament and buffer-tube lines. The grade resists fuels, oils, aliphatic solvents, and many chlorinated solvents at room temperature. However, PBT is hydrolytically degradable in hot-water or steam exposure above 60 °C; it is not a direct replacement for polyamide in steam-sterilized components or continuous hot-water service. When compared with PET, B1600 crystallizes more rapidly, allowing higher line speeds or shorter quench baths, but its upper continuous-use temperature in air is lower than that of annealed PET. For outdoor use, carbon black or a UV stabilization package must be added because the natural grade has no UV stabilizer.
The following values are manufacturer-published typical values for natural grade, not guaranteed product specifications; lot-to-lot variation should be characterized using the relevant ISO method before process start.
| Property | Test method | Typical value |
|---|---|---|
| Density | ISO 1183-1 | 1.30 g/cm³ |
| Melt volume-flow rate | ISO 1133-1 | 12 cm³/10 min at 250 °C/2.16 kg |
| Melting temperature | ISO 11357-3 | 225 °C |
| Tensile modulus | ISO 527-2 | 2500 MPa |
| Tensile stress at yield | ISO 527-2 | 55 MPa |
| Tensile strain at yield | ISO 527-2 | 3.5 % |
| Flexural modulus | ISO 178 | 2400 MPa |
| Charpy notched impact | ISO 179-1/1eA | 4.0 kJ/m² at 23 °C |
| Heat deflection temperature | ISO 75-2 | 150 °C at 0.45 MPa; 55 °C at 1.80 MPa |
| Water absorption at equilibrium | ISO 62 | 0.2 wt% |
| Dielectric strength | IEC 60243-1 | 30 kV/mm |
| Comparative tracking index | IEC 60112 | 600 V |
| Flammability | UL 94 | HB at 1.5 mm |
Processing shrinkage and post-extrusion shrinkage are strongly affected by cooling rate, draw ratio, and annealing; no single value can be assigned without specifying line conditions. The unfilled nature preserves electrical tracking performance; the comparative tracking index of 600 V under IEC 60112 is higher than many flame-retarded PBT compounds, which often fall below 250 V. Volume resistivity for unfilled PBT is also high, but medium- and high-voltage cable dielectric use requires separate design verification.
Compliance documentation for B1600 000000 normally includes a declaration that the grade is compliant with RoHS Directive 2011/65/EU as amended by (EU) 2015/863, provided that final-article pigments and additives are also compliant. REACH registration and SVHC content are addressed in the safety data sheet. The UL 94 classification is HB at 1.5 mm; flame-retarded PBT compounds are separate grades and typically exhibit lower tracking resistance. For food-contact, medical, or potable-water applications, specific subgrades or additional validations are required. Avoid combining the material with unneutralized amine-based additives or highly alkaline concentrates because these can participate in ester-exchange or hydrolytic reactions under extended melt residence. At ambient relative humidity above 60 %, opened material should be dried before processing; even sealed bags can pick up moisture through diffusion over long storage. For continuous hot-water contact above 60 °C, hydrolysis-stabilized PBT or alternative polymers are normally required.