Korea Engineering Plastics Kepex Pbt Unfilled 3700v

Korea Engineering Plastics KEPEX® PBT Unfilled 3700V

    • Product Name: Korea Engineering Plastics KEPEX® PBT Unfilled 3700V
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 700635
    Filler Content 0% (Unfilled)
    Density 1.35 g/cm³
    Melt Flow Rate 15 g/10 min
    Tensile Strength 50 MPa
    Elongation At Break 15%
    Flexural Modulus 2.5 GPa
    Flexural Strength 80 MPa
    Notched Izod Impact Strength 0.03 J/cm
    Heat Deflection Temperature At 1 82 Mpa 70 °C
    Heat Deflection Temperature At 0 45 Mpa 150 °C
    Melting Point 225 °C
    Water Absorption 0.08%
    Mold Shrinkage 1.5-2.0%
    Dielectric Strength 20 kV/mm
    Volume Resistivity 1.0E+16 Ω·cm
    Flame Rating UL94 V-0

    As an accredited Korea Engineering Plastics KEPEX® PBT Unfilled 3700V factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Korea Engineering Plastics KEPEX® PBT Unfilled 3700V is packaged in 25 kg moisture-proof bags, supplied palletized for industrial use.
    Container Loading (20′ FCL) KEPEX® PBT Unfilled 3700V, 25 kg bags palletized, loaded in 20′ FCL; approximate net weight 20–22 metric tons.
    Shipping Korea Engineering Plastics KEPEX® PBT Unfilled 3700V is shipped as non-hazardous thermoplastic resin pellets in moisture-barrier bags or boxes, palletized and stretch-wrapped. Transport in dry, cool conditions; avoid direct sunlight, heat, and moisture. No UN hazard class or special transport label is required.
    Storage Store KEPEX® PBT Unfilled 3700V in a cool, dry, well-ventilated area, away from direct sunlight, heat sources, and ignition. Keep containers tightly closed in original packaging to prevent moisture ingress and contamination. Avoid prolonged high temperature and humidity. Maintain clean handling practices and follow the supplier SDS and local storage regulations.
    Shelf Life KEPEX® PBT Unfilled 3700V has a shelf life of 12 months when stored dry, cool, and in original unopened packaging.
    Free Quote

    Competitive Korea Engineering Plastics KEPEX® PBT Unfilled 3700V prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Korea Engineering Plastics KEPEX® PBT Unfilled 3700V is an unfilled polybutylene terephthalate injection-moulding compound within the KEPEX PBT series. Publicly available grade-specific data for 3700V are limited; therefore, the values stated in this document are class-typical for unfilled PBT and are identified by test method. Lot-specific certificates, the supplier’s UL yellow card, and the manufacturer’s process recommendation sheet should be reviewed before tooling release or production qualification.

    The grade is used in thin-walled electrical, electronic, and precision mechanical components where fast crystallisation, low moisture absorption, and easy flow into long flow paths are required. Because PBT is a semi-crystalline polyester, hydrolysis control during processing is the primary technical boundary. Residual moisture must be held below 0.02 % by mass before plastication; otherwise molecular weight loss at melt temperature produces brittle mouldings and surface splay. A desiccant dryer with a dew point below -30 °C and a hopper residence time of 3–4 h at 120–130 °C is the standard class-typical preparation.

    What controls the processing window for KEPEX PBT Unfilled 3700V?

    The melt-temperature window for unfilled PBT is narrow because thermal degradation accelerates above 260 °C. Class-typical settings for a grade of this viscosity class are a barrel temperature profile from 240 °C to 260 °C at the nozzle, with melt temperature measured by an insertion probe in accordance with good injection-moulding practice. The mould temperature is generally held at 30–80 °C depending on surface finish requirements and crystallisation rate. At mould temperatures below 30 °C, thin-wall sections may freeze before full packing, producing underfilled ribs and high shrinkage variance. At mould temperatures above 80 °C, cycle time increases without a proportionate gain in mechanical properties.

    Residence time at melt temperature should not exceed 10 min. In production-scale operations, the shot size should use 40–70 % of the barrel capacity to limit residence time during interruptions. If a hot-runner system is used, thermally balanced nozzles with separate tip temperature control are preferable because unfilled PBT can drool or degrade in overheated dead spots. Screw design normally favours a low-compression, general-purpose screw with a length-to-diameter ratio of 20:1 to 24:1 and a non-return valve with clearances suitable for medium-viscosity engineering resins.

    Injection moulding of the unfilled grade on horizontal reciprocating-screw machines is performed with clamp force calculated from the projected area and melt-flow behaviour. A practical starting point for unfilled PBT is 3–5 kN/cm² of projected area, although gating, wall thickness, and flow length alter the required clamp pressure. Shrinkage is anisotropic and depends on mould temperature, holding pressure, and part geometry. Class-typical mould shrinkage values are 1.5–2.0 % in the flow direction and 1.5–2.0 % transverse when measured by ISO 294-4:2018. Because unfilled PBT has no fibre orientation to restrain shrinkage, the total post-mould shrinkage is often higher than that of glass-filled grades, but the difference between flow and transverse directions is smaller, which is advantageous for roundness and flatness.

    Dielectric and flame-retardancy characteristics in connector applications

    The suffix V in the 3700V designation is commonly associated with a flame-retardant package; however, the minimum thickness at which the grade meets a UL 94 V-0 classification is defined only in the material’s UL yellow card. If the supplier’s card lists a V-0 rating, it must be confirmed for the specific wall thickness used in the moulded part. Unfilled flame-retardant PBT of this class is used in connectors, relay housings, terminal blocks, and sensor enclosures because it provides electrical insulation with low high-voltage leakage risk.

    Typical unfilled PBT electrical properties are a volume resistivity in the range 1E14–1E16 Ω·cm when measured by IEC 62631-3-1, and dielectric strength of 20–25 kV/mm on a 1 mm specimen when tested by IEC 60243-1:2019. Comparative tracking index under IEC 60112:2020 is frequently reported at 600 V for unfilled PBT, which is adequate for many creepage-limited printed circuit board mounting applications. Where the part is exposed to conductive dust, humid environments, or process residues, the creepage and clearance distances required by the end-product safety standard should not be reduced solely because the base resin has a 600 V CTI.

    Flame-retardant packages in unfilled PBT may alter melt viscosity, mould release, and colour stability. Thermal ageing of flame-retardant grades can lead to additive migration or surface blooming at elevated continuous-use temperatures. Therefore, long-term exposure in sealed enclosures should be evaluated by accelerated ageing at the expected service temperature and humidity before part approval.

    Mechanical property selection for 3700V should begin with the table below. The data are reported for unfilled PBT using standardised specimen preparation and conditioning. Grade-specific values may differ from these class-typical entries, and the table is not a substitute for the manufacturer’s certificate of analysis.

    PropertyTest methodClass-typical value
    DensityISO 1183-1:20191.30–1.32 g/cm³
    Melt volume-flow rateISO 1133-1:2022, 250 °C/2.16 kg15–30 cm³/10 min
    Tensile stress at yieldISO 527-2:201255–60 MPa
    Tensile modulusISO 527-2:20122.4–2.6 GPa
    Flexural modulusISO 178:20192.3–2.6 GPa
    Charpy notched impact, 23 °CISO 179-1:2010/1eA3–5 kJ/m²
    Heat deflection temperature, 1.8 MPaISO 75-2:2013, method A55–65 °C
    Water absorption, 24 h immersion at 23 °CISO 620.2 %
    Volume resistivityIEC 62631-3-11E14–1E16 Ω·cm
    Dielectric strength, 1 mmIEC 60243-1:201920–25 kV/mm
    Comparative tracking indexIEC 60112:2020600 V
    Mould shrinkage, flow/transverseISO 294-4:20181.5–2.0 % / 1.5–2.0 %

    When glass-filled PBT is replaced by 3700V for dimensional stability or weld-line strength

    Replacement of a glass-filled PBT grade by KEPEX PBT Unfilled 3700V is justified when glass-fibre orientation causes warpage, anisotropic shrinkage, or unacceptable weld-line strength. Glass-filled PBT grades typically exhibit flexural moduli of 8–9 GPa, while unfilled PBT remains at 2.3–2.6 GPa under ISO 178:2019. The lower modulus of 3700V reduces load-bearing capability in snapping arms and structural ribs, so part geometry must be adjusted by increasing section modulus or rib depth. However, unfilled PBT has higher elongation at break than glass-filled PBT, typically above 20 % under ISO 527-2:2012, and it avoids the sharp weld-line strength losses caused by fibre depletion at converging flow fronts.

    For parts with fine pitch, thin walls, or long flow lengths, unfilled PBT offers easier filling than glass-filled material because the absence of rigid fibres lowers melt viscosity and reduces abrasion in gates and runner bends. The trade-off is higher shrinkage and greater notch sensitivity. Sharp internal corners and insert edges should be radiused to avoid stress concentration because unfilled PBT has lower crack-propagation resistance than toughened or glass-filled grades. Thread-forming screws into boss holes are also more likely to produce microcracks unless the boss diameter is increased or the screw engagement is reduced.

    Moisture absorption and environmental resistance distinguish unfilled PBT from polyamide 66. Unfilled PBT absorbs only 0.2 % water after 24 h immersion at 23 °C by ISO 62, whereas PA66 typically absorbs 2.5 % at saturation. Consequently, electrical properties and dimensional stability of 3700V are less sensitive to humid environments than PA66. However, PBT is more susceptible to hydrolysis in hot water and steam than semi-aromatic polyamides at equivalent temperature. Continuous exposure to coolant mixtures above 85 °C may cause hydrolytic embrittlement, and the use of the unfilled grade in pressurised hot-water systems should be avoided unless long-term testing demonstrates sufficient life under the specific fluid composition and temperature cycle.

    Compared with polyoxymethylene, unfilled PBT generally provides a higher comparative tracking index and better resistance to acid-generated zinc chloride or calcium chloride road-salt deposits in underhood electrical housings. Polyoxymethylene is more susceptible to acidic hydrolysis and can emit formaldehyde when degraded, while PBT does not release formaldehyde under normal decomposition pathways. This difference is significant in enclosed passenger-compartment and underhood electrical connectors where low emission and low odour are required.

    Compliance status cannot be assumed without the supplier’s UL yellow card and REACH declaration

    Regulatory compliance of the 3700V grade depends on the exact pigment package, flame-retardant system, and processing aids supplied in the commercial product. The base polymer and additives must be assessed under the European Union RoHS Directive 2011/65/EU as amended by (EU) 2015/863. A REACH statement under Regulation (EC) No 1907/2006 should confirm whether the grade contains any substance of very high concern above the disclosure threshold. Electrical end-products must be evaluated according to the applicable insulation coordination standard, such as IEC 60664-1:2020, using the material’s CTI rating and creepage/clearance data.

    RequirementStandard / regulationVerification basis
    RoHS restricted substances2011/65/EU, (EU) 2015/863Supplier analytical declaration for specific colour and lot
    REACH SVHC statusRegulation (EC) No 1907/2006Supplier REACH compliance statement
    Flammability classificationUL 94UL yellow card minimum thickness for the specific grade
    Insulation coordinationIEC 60664-1:2020CTI from IEC 60112:2020 and creepage/clearance data
    Material condition after mouldingISO 291:2008Conditioning at 23 °C / 50 % RH before mechanical testing
    Drying and residual moistureManufacturer recommendation; ISO 15512:2019 for moisture methodResidual moisture below 0.02 % before processing

    Secondary operations for 3700V include ultrasonic welding, laser marking, and heat staking. Unfilled PBT welds best when weld joint geometry produces a uniform melt film without excessive glass-fibre shielding, which is absent in this grade. Laser marking performance is additive-dependent; dark-coloured flame-retardant grades may require contrasting pigment packages to achieve sufficient mark contrast at production line speed. Heat staking of pins or tabs requires controlled tip temperature below the degradation limit of 260 °C to prevent local carbonisation and loss of mechanical integrity at the stake head.

    Top