Korea Engineering Plastics Kepex Pbt Unfilled 3500sa

Korea Engineering Plastics KEPEX® PBT Unfilled 3500SA

    • Product Name: Korea Engineering Plastics KEPEX® PBT Unfilled 3500SA
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 188988
    Polymer Type Polybutylene terephthalate (PBT)
    Filler Content Unfilled
    Density 1.23 g/cm³
    Tensile Strength 50 MPa
    Tensile Elongation At Break 100%
    Flexural Modulus 1900 MPa
    Izod Notched Impact Strength 8 kJ/m²
    Heat Deflection Temperature At 0 45 Mpa 140 °C
    Heat Deflection Temperature At 1 8 Mpa 55 °C
    Vicat Softening Temperature 160 °C
    Melting Point 220 °C
    Mold Shrinkage 1.4%
    Water Absorption 0.08%
    Ul 94 Flammability Rating HB
    Dielectric Strength 20 kV/mm
    Volume Resistivity 1E16 Ω·cm

    As an accredited Korea Engineering Plastics KEPEX® PBT Unfilled 3500SA factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing KEPEX® PBT Unfilled 3500SA is packaged in 25 kg moisture-proof, polyethylene-lined paper bags, supplied palletized.
    Container Loading (20′ FCL) 20′ FCL container loaded with palletized 25 kg bags of KEPEX® PBT Unfilled 3500SA, shrink-wrapped and secured for ocean transport.
    Shipping **Shipping Description:** Korea Engineering Plastics KEPEX® PBT Unfilled 3500SA is a non-hazardous polybutylene terephthalate resin in solid pellet form. It is packed in moisture-proof bags within cartons or octabins on pallets. Keep dry, cool, and protected from direct sunlight, humidity, and high temperatures; comply with local transport regulations.
    Storage Store Korea Engineering Plastics KEPEX® PBT Unfilled 3500SA in its original sealed packaging in a cool, dry, well-ventilated area. Keep away from direct sunlight, heat, moisture, and contaminants. Maintain stable ambient conditions and good stock rotation; dry material before processing if moisture pickup is suspected.
    Shelf Life The shelf life of KEPEX® PBT Unfilled 3500SA is typically 24 months when stored unopened in a cool, dry place.
    Free Quote

    Competitive Korea Engineering Plastics KEPEX® PBT Unfilled 3500SA prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Korea Engineering Plastics KEPEX® PBT Unfilled 3500SA is an unfilled polybutylene terephthalate injection-moulding grade supplied as pellets for electrical, electronic, and automotive components. The designation identifies a medium-flow, general-purpose PBT with no glass-fibre or mineral reinforcement. Moulded density is 1.30–1.31 g/cm³ when measured to ISO 1183-1. Melt volume-flow rate at 250 °C and 2.16 kg is 20–30 cm³/10 min by ISO 1133-1:2022, placing the grade in the intermediate-flow range suitable for multicavity tools with filling paths below 0.8 mm. The material is not flame-retarded, and its UL 94 classification is HB at 1.6 mm. The following representative profile is based on unfilled PBT injection grades in this viscosity class; the manufacturer datasheet should be consulted for certified lot-specific values.

    Table 1. Representative property profile for KEPEX® PBT Unfilled 3500SA
    PropertyTest conditionTest methodValue
    DensityMoulded plaqueISO 1183-11.30–1.31 g/cm³
    Melt volume-flow rate250 °C, 2.16 kgISO 1133-1:202220–30 cm³/10 min
    Tensile stress at yield50 mm/minISO 527-255–60 MPa
    Tensile modulus1 mm/minISO 527-22500–2700 MPa
    Flexural strength2 mm/minISO 17880–90 MPa
    Flexural modulus2 mm/minISO 1782300–2600 MPa
    Charpy notched impact, 23 °CEdgewise, 1eAISO 179-1/1eA3–4 kJ/m²
    Melting temperatureSecond heating, 10 K/minISO 11357-3223–225 °C
    Heat deflection temperature1.8 MPa, flatwiseISO 75-2/A55–65 °C
    Mould shrinkage, plaque60 mm × 60 mm × 2 mm, parallelISO 294-41.4–1.8 %
    Water absorption24 h, 23 °CISO 620.08 %
    Dielectric strength2.0 mm plaqueIEC 60243-116–20 kV/mm
    Volume resistivity23 °C, 50% RHIEC 62631-3-11 × 1013 Ω·m
    Comparative tracking indexSolution AIEC 60112600 V

    What Changes When 3500SA Replaces GF15 PBT in Thin-Wall Connector Housings?

    When 3500SA replaces a 15% glass-fibre-reinforced PBT in a thin-wall connector housing, the unfilled grade lowers tensile modulus from approximately 4500–5500 MPa to 2500–2700 MPa and reduces flexural strength from the 120–150 MPa band to 80–90 MPa. Elongation at break increases to above 20% by ISO 527-2, and moulded-in weld-line strength is less sensitive to fibre orientation. Mould shrinkage increases from 0.4–0.7% to 1.4–1.8% by ISO 294-4, so cavity dimensions, core-pin retraction, and gate-seal time must be revalidated. In wall sections below 0.5 mm, 3500SA provides a longer flow path than lower-MFR unfilled PBT, but the absence of glass fibre reduces heat-deflection stability; HDT/A drops from approximately 190–200 °C for GF15 PBT to 55–65 °C for 3500SA. Applications with clips or snap-fits benefit from the unfilled grade’s lower notch sensitivity, whereas GF15 PBT remains preferred for structural brackets requiring creep resistance at 80–120 °C. Compared with impact-modified PBT/elastomer blends, 3500SA has higher tensile strength and lower notched Charpy impact, 3–4 kJ/m² compared with 20–40 kJ/m², making the unfilled grade unsuitable for high-velocity snap-fit assembly without generous radii. Against unfilled PBT grades with lower MFR in the 10–15 cm³/10 min range, 3500SA reduces fill-pressure requirements in long flow paths but may exhibit slightly lower Charpy impact because of molecular-weight differences. Published data for this specific configuration is limited, and direct substitution should be validated by spiral-flow moulding on the production tool.

    Desiccant drying with a dew point of ≤ -30 °C and inlet air temperature of 120 °C for 4 h is required before moulding. Residual moisture must be held below 0.02% by ISO 15512; at 0.03% moisture, melt-phase hydrolysis reduces molecular weight rapidly enough to shift MFR upward and lower impact strength. In plants where ambient relative humidity exceeds 60%, open hopper residence should be limited to 30 min unless dry-air blanketing is installed. Reciprocating-screw machines with clamp force from 600 to 1500 kN, screw L/D of 20:1 to 24:1, and compression ratio of 2.5:1 to 3.0:1 are typical for connector production. Barrel settings of 230–240 °C rear, 240–250 °C middle, 250–260 °C front, and 250–260 °C nozzle are applied. Mould temperature is maintained at 60–80 °C to balance crystallinity, surface gloss, and dimensional stability. Short-shot prevention in thin-wall tools relies on injection velocities of 150–300 mm/s and holding pressures in the 60–90 MPa hydraulic range, but gate dimensions below 0.6 mm may require higher values validated on the specific hot-runner tool. Back pressure should be set to 0.3–0.7 MPa hydraulic, and screw speed should remain in the 50–120 min⁻¹ range for the specified screw diameter, with no more than 30% regrind.

    When the Barrel Temperature Exceeds 265°C in Hot-Runner Tools

    When the barrel temperature exceeds 265 °C in a hot-runner tool, PBT degradation accelerates through chain scission of the tetramethylene ester repeat unit, releasing tetrahydrofuran, butadiene, and carboxyl end-groups. The degradation products reduce melt viscosity and produce silver streaking on moulded surfaces, while carboxylic acid species can accelerate further hydrolysis in regrind streams. Maximum total residence time should be limited to 8 min at 250 °C and 5 min at 260 °C; above 265 °C, the limit should not exceed 3 min. Hot-runner channels should be designed without unswept dead spots, and temperature controllers should be tuned to avoid overshoot above 270 °C during manifold start-up. If production is interrupted for more than 15 min, the barrel should be purged with a low-MFR PBT or a commercial purge compound, and the feed throat should be kept at 40–60 °C to prevent pellet bridging. Regrind from parts moulded above 270 °C should not be re-introduced into the virgin stream because hydrolytic chain scission is not reversible by drying.

    Connector housings in engine compartments and underhood fuse boxes are moulded from 3500SA where dielectric stability after thermal ageing is more important than structural modulus. Volume resistivity remains above 1 × 1013 Ω·m by IEC 62631-3-1 at 23 °C and 50% RH. Dielectric strength is 16–20 kV/mm on 2.0 mm plaques by IEC 60243-1, and dielectric constant at 1 MHz is 3.0–3.2 with a dissipation factor of 0.015–0.020 by IEC 60250. The unfilled PBT absorbs 0.08% water after 24 h by ISO 62, lower than polyamide 66, which limits moisture-induced drift in surface resistivity and comparative tracking index. Under damp heat cycling from 23 °C to 85 °C at 85% RH, surface resistivity may fall by two to three decades, but volume resistivity remains controlled by the bulk unfilled PBT matrix. End-product tests following IEC 60068-2-30 are therefore required for high-impedance circuits. Published data for 3500SA under partially wet and contaminated underhood exposure is limited and should be confirmed by end-product testing to IEC 60512-2-1 or the relevant connector qualification schedule.

    Chemical resistance of 3500SA follows the behaviour of unfilled PBT: strong resistance to aliphatic hydrocarbons, glycols, automotive fluids, and most dilute acids at temperatures below 60 °C; exposure to strong bases, hot chlorinated solvents, and boiling water above 80 °C causes surface attack and stress-crack formation. In transmission-fluid-soak testing at 120 °C, unfilled PBT typically retains tensile strength after 1000 h, but final retention depends on fluid composition and part wall thickness. The grade should not be specified for components in contact with amine-based additives or hot methoxypropanol-bearing cleaning fluids because ester linkage attack can occur before thermal ageing effects appear. Moulded parts with moulded-in stress should be annealed at 120 °C for 1 h to reduce solvent-craze sensitivity before assembly with aggressive lubricants.

    Dimensional stability in high-humidity testing is governed by moisture absorption and moulded-in orientation. A 2.0 mm plaque conditioned at 23 °C and 50% RH typically reaches dimensional equilibrium within 48 h, with longitudinal shrinkage of 1.4–1.8% and transverse shrinkage of 1.6–2.0% by ISO 294-4. Shrinkage anisotropy arises from flow-induced orientation and is reduced by higher mould temperatures in the 70–80 °C range. Post-moulding annealing at 120 °C for 1 h reduces warpage in thin-wall connectors but increases total shrinkage by an additional 0.1–0.3%. Fixture design during annealing should account for this change.

    Regulatory and Compliance Data Matrix

    Compliance status must be verified against the specific production batch, but the unfilled PBT grade is normally positioned for the following declarations. Korea Engineering Plastics should be contacted for current certification documents. The matrix below summarises applicable regulatory categories for the standard unfilled pellet form.

    Table 2. Regulatory and compliance matrix for KEPEX® PBT Unfilled 3500SA
    Regulation or standardClause or methodTypical status
    RoHS Directive 2011/65/EU, Annex II restricted substancesIEC 62321 seriesCompliant with 0.1% lead, mercury, hexavalent chromium, PBB, PBDE thresholds and 0.01% cadmium threshold
    REACH Regulation (EC) No 1907/2006Article 33, SVHC candidate listNo SVHC above 0.1% w/w declared for standard unfilled pellet
    UL 94 flammabilityUL 94, HBHB at 1.6 mm
    DesignationISO 1043-1PBT

    Operational boundaries for 3500SA are defined by hydrolysis sensitivity, shear heating in hot-runner tips, and the absence of inherent flame retardance. The grade should not be processed at melt temperatures above 270 °C, should not be moulded with moisture above 0.02%, and should not be specified for continuous exposure to strong alkaline solutions or steam above 80 °C. Regrind usage should be limited to 20–30 wt% for parts with mechanical load-bearing features, and the melt should be filtered through a screen pack of 600–800 µm if regrind is included. Tools with valve-gate hot runners require gate-temperature monitoring because local temperature overshoot above 280 °C generates carbonised deposits that disrupt gate sealing and create intermittent short shots.

    Top