Korea Engineering Plastics Kepex Pbt Pet Mx25 3725m7

Korea Engineering Plastics KEPEX® PBT+PET+MX25% 3725M7

    • Product Name: Korea Engineering Plastics KEPEX® PBT+PET+MX25% 3725M7
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 748332
    Density 1.50 g/cm³
    Water Absorption 0.08 %
    Tensile Strength 55 MPa
    Tensile Elongation At Break 3 %
    Flexural Modulus 4500 MPa
    Flexural Strength 90 MPa
    Notched Izod Impact Strength 4 kJ/m²
    Heat Deflection Temperature At 1 82 Mpa 150 °C
    Melting Point 220 °C
    Mold Shrinkage 0.5–0.8 %
    Flammability HB
    Dielectric Strength 20 kV/mm

    As an accredited Korea Engineering Plastics KEPEX® PBT+PET+MX25% 3725M7 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Korea Engineering Plastics KEPEX® PBT+PET+MX25% 3725M7 is supplied in 25 kg moisture-proof bags, palletized for industrial use.
    Container Loading (20′ FCL) 20’ FCL container loaded with Korea Engineering Plastics KEPEX® PBT+PET+MX25% 3725M7 in 25 kg bags, palletized and secured for shipment.
    Shipping KEPEX® PBT+PET+MX25% 3725M7 is shipped as non-hazardous polymer compound pellets, not regulated as dangerous goods. Use moisture-barrier bags, cartons, or FIBCs; keep dry, cool, and UV-protected. Include SDS with consignment and follow local transport/storage regulations. Avoid moisture absorption before processing; normal industrial handling is sufficient.
    Storage Store Korea Engineering Plastics KEPEX® PBT+PET+MX25% 3725M7 in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and strong oxidizers. Keep original containers sealed, clearly labeled, and protected from moisture, dust, and mechanical damage. Avoid excessive stacking and high humidity. Follow first-in, first-out stock rotation, and pre-dry before processing as recommended by the supplier.
    Shelf Life Typically 12 months from date of manufacture when stored unopened in a cool, dry place away from direct sunlight.
    Free Quote

    Competitive Korea Engineering Plastics KEPEX® PBT+PET+MX25% 3725M7 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Korea Engineering Plastics supplies KEPEX® PBT+PET+MX25% 3725M7 as a mineral-reinforced polybutylene terephthalate/polyethylene terephthalate injection-moulding compound. The grade designation PBT+PET+MX25% indicates a two-component polyester matrix compounded with a 25 wt% mineral filler fraction; 3725M7 is an internal control code for molecular weight, additive package, and colour. Published datasheet values for the exact 3725M7 configuration are limited in this reference set, so numerical ranges cited below are indicative values for 25 wt% mineral-filled PBT/PET alloys with equivalent filler mass fraction and must be confirmed against the supplier certificate of analysis. The material is used in automotive connector bodies, sensor housings, power-tool shells, appliance control enclosures, and electrical installation components where lower and more isotropic mould shrinkage than unfilled PBT/PET or glass-fibre reinforced PBT is required. In such parts, the mineral filler reduces ISO 294-4 mould shrinkage into a typical band of 0.006–0.011 mm/mm; the PET fraction raises the stable-use temperature and reduces surface gloss variation relative to PBT homopolymer at the same filler level.

    How Does 25% Mineral Reinforcement Alter Shrinkage, Impact, and Flow Profile?

    For a 25 wt% mineral-filled PBT/PET compound, the filler phase raises melt viscosity and reduces melt volume-flow rate relative to unfilled polyester. Melt volume-flow rate under ISO 1133-1 at 260 °C and 2.16 kg is commonly 8–18 cm³/10 min; finer particle size and higher aspect ratio lower the value toward the lower end of this range. The mineral particles act as heterogeneous nucleating sites, increasing crystallisation onset temperature during cooling and reducing cycle time in thick sections, but the effect is less pronounced than in talc-filled polypropylene because PBT already crystallises rapidly. Tensile modulus under ISO 527-2 or ASTM D638-14 typically falls between 4000 and 6500 MPa at 23 °C, compared with 2200–2800 MPa for unfilled PBT/PET. Notched Izod impact under ISO 180/A is generally 3–6 kJ/m²; the mineral filler reduces the ductile failure mode seen in unfilled polyester and must be considered for snap-fit geometries requiring deflection.

    Flow-simulation inputs should not use unfilled PBT/PET viscosity coefficients. Capillary rheometry according to ISO 11443 should be used to obtain Cross-WLF parameters, because shear heating at 10,000 s⁻¹ in thin-wall gates can increase melt temperature by 10–20 °C above the barrel front-zone setpoint. If the front zone is already at 260 °C, local melt temperature can approach the 270 °C degradation threshold without visible barrel alarm.

    Long-term thermal ageing also changes with filler content. In air-oven ageing at 150 °C, mineral-filled PBT/PET may show slower loss of tensile strength than unfilled polyester because the filler reduces available matrix surface area and lowers residual stress in moulded parts. However, ISO 2578 thermal endurance classification should be performed on moulded specimens, not raw granules. At 80 °C, short-term tensile modulus values from ISO 527-2 are not appropriate for load-bearing design; ISO 899-2 creep modulus at 1000 h may fall below 50% of the short-term value depending on stress level and moisture condition.

    The table below summarises indicative published property ranges for comparable injection-mouldable polyester compound families under standard test conditions.

    Property Standard 25% mineral-filled PBT/PET Unfilled PBT/PET 30% glass-fibre PBT
    Tensile modulus ISO 527-2 4000–6500 MPa 2200–2800 MPa 8500–11000 MPa
    Tensile strength at yield ISO 527-2 55–75 MPa 50–60 MPa 110–140 MPa
    Notched Izod impact ISO 180/A 3–6 kJ/m² 4–7 kJ/m² 8–12 kJ/m²
    Heat deflection temperature ISO 75-2 at 1.8 MPa 95–135 °C 80–120 °C 195–210 °C
    Mould shrinkage ISO 294-4 0.006–0.011 mm/mm 0.015–0.025 mm/mm 0.002–0.006 mm/mm flow, 0.008–0.015 mm/mm transverse
    Density ISO 1183-1 1.40–1.55 g/cm³ 1.28–1.31 g/cm³ 1.52–1.60 g/cm³

    Specific datasheet values for KEPEX® PBT+PET+MX25% 3725M7 should be verified by moulded test plaques processed under the intended production parameters. The reduction in mould shrinkage relative to unfilled PBT/PET is approximately 30–60%, while tensile modulus increases by 50–120%. Elongation at break drops from 30–100% in unfilled polyester grades to 3–8% in the mineral-filled compound; this embrittlement is the principal trade-off when replacing an unfilled PBT or PBT/PET grade with 3725M7.

    Pre-drying of KEPEX® PBT+PET+MX25% 3725M7 prior to injection moulding follows the standard moisture boundary for PBT/PET alloys. Hydrolysis at melt temperatures above 240 °C becomes measurable when residual moisture exceeds 0.02 wt%; therefore, a desiccant dryer with a dew point of -40 °C or lower and a material bed temperature of 120–130 °C for 4–5 h is required. If the dryer cannot maintain a dew point below -30 °C, drying time should be extended to 6 h and the result verified by ISO 15512 moisture analysis. Over-drying above 140 °C should be avoided because PET-rich domains can undergo thermal-oxidative yellowing and molecular weight loss. Under warehouse conditions above 60% RH, open containers should be protected with sealed liners; surface moisture adsorption is rapid, and a 0.02 wt% residual moisture limit can be exceeded within 1–2 h in humid environments. On production lines, closed-loop hopper dryers and insulated feed throats are used to prevent re-absorption before the screw.

    Material Constitution and Grade Identification

    The designation PBT+PET+MX25% identifies a two-component polyester matrix compounded with a 25 wt% mineral additive package; the public grade description does not identify whether the mineral is talc, mica, wollastonite, or a mixed filler. In mineral-filled PBT/PET alloys, lamellar fillers such as talc and mica reduce shrinkage more isotropically, while acicular fillers such as wollastonite increase stiffness and heat distortion but can create anisotropic shrinkage. The PET component has a slower crystallisation rate than PBT and improves chemical stress-cracking resistance and surface gloss; however, it also raises the minimum mould temperature required to reach full crystallinity. The PBT phase contributes rapid crystallisation and good flow, which helps fill thin-wall sections despite the mineral filler. The 3725M7 suffix is a manufacturer-specific code for molecular weight, filler surface treatment, and stabilisation package; it is not an ISO 1043-2 descriptor and must not be used to infer exact filler chemistry.

    Production-scale dispersion of a 25 wt% mineral filler into PBT/PET is typically performed on a twin-screw extruder with an L/D ratio of 40:1 to 48:1. The mineral is side-fed through a mid-barrel port after the polyester pellets are melted; this prevents excessive screw torque and reduces mineral attrition. On a 65 mm twin-screw line at 350–500 kg/h, specific mechanical energy input commonly ranges from 0.15 to 0.25 kWh/kg. Die temperature is held below 260 °C to suppress PET degradation. If die temperature exceeds 270 °C, brown streaks and acrid degradation products can appear in the strand, and melt-flow drift may increase. Filler dispersion quality is assessed by ash content under ISO 3451-1 and by microscopy of cryogenic fracture surfaces; large agglomerates above 50 µm can initiate early failure in thin-wall sections.

    Against a 30 wt% glass-fibre reinforced PBT grade, KEPEX® PBT+PET+MX25% 3725M7 occupies a position of lower anisotropic warpage and lower mould abrasion, but lower tensile strength and lower notched impact. Glass-fibre PBT typically exhibits tensile modulus of 8500–11000 MPa and notched Izod impact of 8–12 kJ/m²; mineral-filled PBT/PET does not reach the same impact performance. The critical difference appears in ISO 294-4 mould shrinkage: glass-fibre PBT can show 0.002–0.006 mm/mm parallel to flow and 0.008–0.015 mm/mm transverse, producing out-of-plane warpage in multi-gated flat parts; mineral-filled PBT/PET has more uniform shrinkage of 0.006–0.011 mm/mm. This difference is important for connector housings with long terminal cavities and for appliance control housings where flatness must be maintained over a 200–300 mm span without secondary straightening. Glass-fibre compounds also generate higher tool wear; the mineral-filled grade is less aggressive on gate lands and cavity edges, although not as low-wear as unfilled polyester.

    When Mold Temperature Drops Below 60°C in Thin-Wall Connector Geometries

    In thin-wall connector tools where core deflection limits packing pressure, mould temperatures below 60 °C reduce the crystallisation rate of the PBT/PET matrix. This condition can leave a shallow low-crystallinity skin in areas near the cavity wall, reducing heat deflection temperature and increasing post-mould dimensional movement. Under ISO 294-1 injection-moulding practice, the tool should be heated to 70–90 °C for sections below 1.5 mm. If the tool is run at 50–60 °C, the hold pressure required to keep shrinkage under 0.012 mm/mm increases, and the process window narrows. In a four-cavity connector tool with 0.8 mm wall stock, gate freeze time at 60 °C is typically 30–50% shorter than at 90 °C, causing backflow and cavity-to-cavity weight variation unless screw retraction is delayed.

    Injection-moulding barrel settings for mineral-filled PBT/PET should be profiled from 230 °C in the rear zone to 250–260 °C in the front zone and nozzle. Melt temperature should not exceed 270 °C; residence time at melt temperature should be limited to 5 min. Holding pressure is typically 50–80 MPa, back pressure 0.5–1.5 MPa, and screw speed 50–120 rpm. Hot-runner drops larger than 3 shot volumes can create dead zones where PET-rich material degrades and later releases as black specks. Nozzle drool at 260 °C is often thermal rather than back-pressure-related; reducing nozzle temperature by 5–10 °C before raising back pressure avoids unnecessary shear heating. Cavity pressure in thin-wall mineral-filled PBT/PET moulding can peak above 80 MPa near gate freeze; clamp force calculations should use a conservative cavity-pressure estimate of 50–80 MPa over the projected area.

    For engine-compartment connectors exposed to ethylene glycol/water at 105 °C and vibration, the shallow-shrinkage character of mineral-filled PBT/PET reduces terminal misalignment in multi-pin cavities. SAE/USCAR-2 class 3 thermal cycling and vibration schedules are commonly used to validate connector retention and contact normal force; the lower and more isotropic shrinkage of this grade supports cavity position over cycling. Water absorption under ISO 62 for mineral-filled PBT/PET is typically 0.2–0.6% at saturation, lower than many glass-fibre reinforced polyester grades because the mineral filler does not create capillary wicking along glass bundles. In electrical enclosures, comparative tracking index under IEC 60112 is design-dependent and may exceed 500 V when the formulation contains no conductive carbon black; UL 94 flame rating is not an intrinsic property and must be assessed on the final moulded part thickness. The material is not recommended for continuous immersion in hot water above 80 °C, strong aqueous ammonia, high-alkaline cleaning concentrates, or food-contact use unless a specific FDA 21 CFR compliance letter is supplied for the lot. EU market shipments require lot-specific RoHS 2011/65/EU confirmation by EN 62321-2 screening and REACH SVHC communication where any candidate substance exceeds 0.1 wt%. Regrind can be reincorporated up to 20 wt% in non-appearance parts if thoroughly dried and free of contamination; each heat cycle reduces molecular weight and notched impact, so the regrind fraction must be held constant to avoid lot-to-lot variation. Gas burn marks caused by residual mineral moisture or resin fines should be corrected by verifying dryer dew point and reducing screw speed when high-shear heating creates local melt temperatures above 270 °C.

    Top