Korea Engineering Plastics Kepex Pbt Pet Gf Md 3730gm5

Korea Engineering Plastics KEPEX® PBT+PET+GF+MD 3730GM5

    • Product Name: Korea Engineering Plastics KEPEX® PBT+PET+GF+MD 3730GM5
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 774208
    Density 1.60 g/cm³ (typical)
    Glass Fiber Mineral Content 30% (nominal)
    Tensile Strength 110 MPa (typical)
    Tensile Elongation At Break 2.0% (typical)
    Flexural Modulus 8,500 MPa (typical)
    Notched Izod Impact Strength 50 J/m (typical)
    Heat Deflection Temperature At 1 82 Mpa 200 °C (typical)
    Melting Point 225 °C (typical)
    Water Absorption At 23 C 24 H 0.06% (typical)
    Mold Shrinkage 0.3–0.6% (typical)
    Flammability Rating HB (UL 94)
    Dielectric Strength 20 kV/mm (typical)
    Volume Resistivity 1×10^16 Ω·cm (typical)

    As an accredited Korea Engineering Plastics KEPEX® PBT+PET+GF+MD 3730GM5 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg net moisture-resistant paper bags, palletized; optional 500 kg net jumbo bags.
    Container Loading (20′ FCL) 20′ FCL container loaded with Korea Engineering Plastics KEPEX® PBT+PET+GF+MD 3730GM5, palletized in 25 kg bags and secured for sea transport.
    Shipping KEPEX® PBT+PET+GF+MD 3730GM5 ships as moisture-sensitive thermoplastic pellets in sealed bags or octabins. Use dry, ventilated containers; protect from heat, humidity, contamination, and punctures. Keep packages closed and labeled per SDS and local transport regulations. No special hazardous classification is indicated under normal shipping conditions.
    Storage Store KEPEX® PBT+PET+GF+MD 3730GM5 in original, sealed packaging in a cool, dry, well-ventilated area, away from direct sunlight, heat sources, moisture, and incompatible substances. Keep containers closed to prevent moisture absorption and contamination. Use first-in, first-out rotation; if opened, reseal promptly and dry the resin before processing if required. Protect from physical damage.
    Shelf Life Shelf life is 12 months from manufacture when stored dry, cool, and in unopened original packaging.
    Free Quote

    Competitive Korea Engineering Plastics KEPEX® PBT+PET+GF+MD 3730GM5 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    The KEPEX® PBT+PET+GF+MD 3730GM5 compound from Korea Engineering Plastics is an injection-moulding grade based on a polybutylene terephthalate/polyethylene terephthalate matrix modified with glass fibre and a mineral filler. The suffix GF indicates glass fibre, MD indicates mineral filler, and the grade code 3730GM5 identifies the filler package and viscosity class within the supplier’s PBT/PET portfolio. Published lot-specific datasheets for this exact formulation are limited in open industrial literature; therefore, tensile, flexural, impact, and thermal values are treated as supplier-controlled parameters. This section defines the product class, processing boundaries, and comparative selection logic without assigning unverified scalar property values to 3730GM5.

    Within automotive under-bonnet qualification, the material class is considered for housings, brackets, connector bodies, sensor carriers, and structural retainers that require low moisture uptake, resistance to engine oil and fuel vapour, and stable dimensions during rapid thermal cycling. Component-level validation is normally conducted under OEM load profiles such as ISO 16750-4 or equivalent internal standards, rather than inferred solely from resin datasheets. In electrical connector and appliance applications, PBT/PET glass-mineral compounds are selected when flatness, low differential shrinkage, and good surface uniformity are controlling acceptance criteria.

    Because mould shrinkage, flammability class, and mechanical values depend on colour, part thickness, filler dispersion, and moulding parameters, no generic numeric comparison substitutes for a supplier-issued lot certificate. Where the datasheet is available, the property data should be read against the test designations listed later in this document; otherwise, no exact tensile modulus or Charpy value is asserted for 3730GM5.

    How does the combined glass–mineral filler system alter mould shrinkage anisotropy?

    Glass fibre reinforces the PBT/PET melt by preferential orientation along the flow direction, producing anisotropic shrinkage when the part is ejected and cooled. Mineral filler particles disrupt fibre alignment, reduce the coefficient of linear thermal expansion, and promote more uniform thermal contraction. For PBT/PET mouldings, the practical result is reduced warpage and lower flow-to-transverse shrinkage differential compared with glass-only PBT/PET compounds. Mould shrinkage should be measured on standard plaques in both flow and transverse directions according to ISO 294-4, and the acceptance window should be taken from the supplier datasheet and mould-filling simulation. Published numerical shrinkage data for this specific PBT+PET+GF+MD configuration are limited.

    When the material is processed in hot-runner tools, gate location and gate type dominate fibre orientation and mineral distribution. A central or diagonal pin gate on a flat cover can generate more warpage than a fan gate or a sequential valve-gated edge feed. Weld lines in glass-mineral PBT/PET are typically lower in strength than the surrounding matrix; they should not be placed through snap-fit retention features or structural bosses. If a long weld line is unavoidable, its strength should be evaluated on a weld-line plaque or prototype according to ISO 527-2 before production release.

    When predrying and melt-temperature control are treated as secondary parameters

    Residual moisture above 0.02% by mass in PBT/PET glass-mineral compounds can cause hydrolytic degradation during plastication. The resulting molecular-weight loss appears as reduced notched impact, live-edge delamination, splay, or short-shot instability. Drying in a closed-loop desiccant dryer at 120 °C for 4 h to 6 h is a class-typical starting point; the actual time must be extended when incoming pellet moisture exceeds supplier guidance. Dryer air dew point should remain below -30 °C, and residual moisture should be verified by ISO 15512 or a calibrated moisture analyser before processing. When plant relative humidity exceeds 60%, hopper loading should be closed-loop or protected by a dried-air sweep to prevent re-absorption.

    On production-scale reciprocating screw machines, wet material often presents as surface splay without a large shift in injection pressure. Shot-weight drift and unmelted PET domains may also occur because hydrolysis reduces melt viscosity and changes melt-temperature homogeneity. Batch-to-batch lot certificates should therefore record residual moisture, melt mass-flow rate, and dryer dew point before the material enters the press.

    Melt-temperature control, screw recovery, and tooling constraints

    Barrel profiles for PBT/PET glass-mineral injection-moulding grades of this class commonly range from 230 °C at the rear zone to 260 °C in the metering zone, with actual melt temperature maintained at 250 °C to 270 °C. Mid-barrel control within ±5 °C is required because PET and PBT melt and crystallise at different rates; a cold mid-zone produces screw slip and partially melted filler agglomerates, while an overheated transition zone accelerates thermal degradation. Melt temperature should not exceed 280 °C for extended residence, and total melt residence time should be kept below 10 min. On general-purpose screws with 20:1 to 24:1 L/D, back pressure should be set at 0.3 MPa to 0.7 MPa, with screw speed from 80 rpm to 150 rpm adjusted to limit fibre breakage. Mould temperature should be held between 60 °C and 110 °C depending on required gloss and dimensional stability; the higher region favours lower post-mould shrinkage but increases cycle time.

    Glass fibre and mineral filler increase abrasive wear on screw bodies, check rings, and barrels. For sustained production, bimetallic barrels, hardened screw tips, wear-resistant check rings, and hardened shut-off nozzles are appropriate. Shut-off nozzle seat wear should be monitored because mineral-filled melt leakage changes shot size and cushion position.

    In electrical connector production, the material should be processed with closed-loop barrel temperature control and dry-air mould protection because small changes in melt viscosity alter contact-pin position and flash formation. When thin ribs short-fill, raising mould temperature before increasing melt temperature is preferred because it preserves melt viscosity and avoids the degradation threshold.

    For ultrasonic or vibration welding, mineral filler can attenuate weld energy and alter joint strength. Weld parameters should be validated on moulded prototypes with production tooling because laboratory plaques do not reproduce part geometry, fibre orientation, or knit-line conditions.

    Evaluating differences from unfilled PBT/PET and glass-only PBT/PET grades

    The combined glass-mineral reinforcement shifts the property balance toward low-shrinkage anisotropy and improved flatness, with some loss of ductility compared with unfilled PBT/PET. Against glass-only PBT/PET, 3730GM5 is expected to reduce differential shrinkage and improve surface uniformity, but the exact tensile and impact response depends on the glass-to-mineral ratio and coupling package. Direct substitution into an existing mould should include a shrinkage study under ISO 294-4 and mechanical property comparison under ISO 527-2 and ISO 179-1. Melt flow length may also differ from glass-only grades because mineral particle aspect ratio and surface treatment influence viscosity and solidification rate.

    When moisture uptake is a controlling requirement, PBT/PET glass-mineral compounds can be compared with glass-filled PA66 grades under ISO 62; PBT/PET generally absorbs less moisture, which can reduce dimensional shift in humid electrical enclosures. The comparison is not absolute because PA66 has different elevated-temperature creep and fatigue behaviour. For optical or gloss-sensitive parts, mineral-filled PBT/PET usually has reduced fibre show relative to glass-only formulations, but gloss acceptance should be judged on moulded plaques, not pellets.

    Regulatory statements for RoHS 2011/65/EU, REACH Regulation EC 1907/2006, and flammability classification under UL 94 must be verified for the exact colour, wall thickness, and production plant. No universal compliance is claimed here. The UL Yellow Card, if issued for 3730GM5, is the only recognised reference for flammability marking.

    Chemical compatibility should be considered before specifying this grade. PBT/PET glass-mineral compounds generally resist dilute automotive fluids including engine oil, gasoline, diesel, alcohol mixtures, and greases at moderate temperature, but hot strong acids, alkaline cleaning concentrates, and some chlorinated solvents can initiate stress cracking at moulded-in strain points. Immersion testing should follow a defined chemical exposure procedure, such as ISO 22088 or an OEM specified method, using moulded tensile bars under controlled strain.

    For post-mould annealing, the final dimensions may shift as crystallinity increases. If annealing is required, it should be performed on a controlled batch using the supplier’s time–temperature profile and followed by a dimensional audit against ISO 294-4. Uncontrolled annealing can increase warpage even in low-shrinkage mineral-filled grades.

    For incoming inspection and first-article approval, the following test designations are relevant when a supplier datasheet is available:

    Property or parameter Test method / standard Lot-specific verification note
    Tensile strength and modulus ISO 527-1:2019, ISO 527-2:2012 Specimen prepared and conditioned according to ISO 291; compare with supplier datasheet
    Flexural strength and modulus ISO 178:2019 Test speed and support span to be recorded
    Charpy notched impact ISO 179-1:2010 Edgewise impact; notch radius Type A
    Heat deflection temperature ISO 75-1, ISO 75-2 Report at 1.8 MPa and 0.45 MPa; thickness-specific
    Mould shrinkage ISO 294-4:2018 Measure flow-direction and transverse-direction values
    Water absorption ISO 62:2008 Report conditioning temperature and time
    Melt mass-flow rate ISO 1133-1:2022 Use supplier-specified temperature and nominal load
    Flammability classification UL 94 Verify exact colour, minimum thickness, and grade code from the UL Yellow Card

    Directional property comparisons for material selection should be read as class-level generalisations, not acceptance criteria:

    Selection criterion Expected direction relative to unfilled PBT/PET Expected direction relative to glass-only PBT/PET Standard anchor
    Mould shrinkage anisotropy Lower Lower ISO 294-4:2018
    Tensile modulus Higher Similar to slightly lower depending on glass/mineral ratio ISO 527-2
    Notched impact Lower Similar to lower ISO 179-1
    Surface uniformity on moulded parts Reduced gloss variability possible depending on tool Improved fill pattern and reduced fibre show Tool trial and visual inspection
    Coefficient of thermal expansion Lower Similar to lower ISO 11359-2
    Weld-line strength Lower Similar to lower ISO 527-2 weld-line specimen

    When a mould is converted from a glass-only PBT/PET to 3730GM5, process revalidation should include a short-shot study, gate-seal time measurement, pressure-drop measurement, and post-mould shrinkage after 24 h conditioning at 23 °C and 50% relative humidity. Without these verification steps, differences in flatness, weld-line strength, and ejection behaviour between glass-only and glass-mineral PBT/PET grades cannot be attributed to the material change.

    Regrind should be controlled and kept free of polyamide contamination because PBT/PET and PA are not miscible; even small levels of PA regrind can create delamination and reduce impact strength. Regrind addition, if allowed by the supplier, should be kept at the lowest practical level for dimensional capability.

    Top