| HS Code | 720834 |
| Flame Retardancy Ul94 | V-0 |
| Molding Shrinkage Percent | 0.2-0.5 |
| Volume Resistivity Ohm Cm | 1E15 |
As an accredited Korea Engineering Plastics KEPEX® PBT+GF30%-FR 3330GVS factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | KEPEX® PBT+GF30%-FR 3330GVS is supplied in 25 kg polyethylene-lined bags, 40 bags per pallet (1,000 kg total). |
| Container Loading (20′ FCL) | Loaded in a 20′ FCL: palletized 25 kg bags of KEPEX® PBT+GF30%-FR 3330GVS, dry, ventilated, securely stowed, within container payload limit. |
| Shipping | Shipping description for Korea Engineering Plastics KEPEX® PBT+GF30%-FR 3330GVS: non-hazardous plastic molding compound; not regulated as dangerous goods for ADR, IMDG, or IATA. Transport as general cargo in sealed moisture-barrier bags/containers, kept cool, dry, ventilated, and protected from contamination, UV, and ignition sources. |
| Storage | Store KEPEX® PBT+GF30%-FR 3330GVS in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep in original sealed packaging to prevent moisture absorption and contamination. Avoid high humidity, static buildup, and incompatible chemicals. Maintain stable temperature, stack securely to prevent deformation, and follow local regulations and supplier guidance. Do not store outdoors. |
| Shelf Life | Typically, shelf life is 12 months when stored dry, cool, and in original unopened packaging, away from direct sunlight. |
Competitive Korea Engineering Plastics KEPEX® PBT+GF30%-FR 3330GVS prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Korea Engineering Plastics KEPEX® PBT+GF30%-FR 3330GVS is a flame-retarded, 30% glass-fibre-reinforced polybutylene terephthalate injection-moulding compound supplied in pellet form. The grade is intended for electrical, electronic, and electro-mechanical components in which dimensional stability, stiffness, heat deflection, and self-extinguishing behaviour are specified. Product-class data place density at 1.65–1.70 g/cm³ when measured under ISO 1183-1:2019, tensile strength at 120–135 MPa under ISO 527-2:2012, flexural modulus at 8,500–10,000 MPa under ISO 178:2019, notched Izod impact at 7–10 kJ/m² under ISO 180:2019, and heat deflection temperature at 195–210 °C at 1.8 MPa under ISO 75-2:2013. Melt volume-flow rate for glass-reinforced FR-PBT is typically 10–20 cm³/10 min at 250 °C and 2.16 kg according to ISO 1133-1:2022. Because published third-party data for the specific 3330GVS formulation are limited, exact mechanical values must be confirmed against the manufacturer’s certificate of analysis.
The principal differences are stiffness, heat deflection, elongation at break, density, and tracking resistance. Unfilled PBT exhibits tensile strength near 55–60 MPa, flexural modulus near 2,500 MPa, and HDT/A near 55 °C at 1.8 MPa. These values are below the product-class envelope of 3330GVS. Non-flame-retarded PBT reinforced with 30% glass fibre generally delivers tensile strength of 130–145 MPa and flexural modulus of 9,000–11,000 MPa, while retaining an HB classification under UL 94. The flame-retardant modification in 3330GVS typically lowers tensile strength by 5–15% relative to non-FR PBT-GF30, increases density by 0.10–0.15 g/cm³, and can reduce comparative tracking index from above 400 V to 200–250 V depending on the selected flame-retardant chemistry. Elongation at break for FR-PBT-GF30 is commonly 2–3%, compared with 3–4% for non-FR PBT-GF30 and 20–50% for unfilled PBT.
| Property | Unfilled PBT | PBT + 30% glass fibre, non-FR | 3330GVS class, FR | Standard method |
|---|---|---|---|---|
| Density | 1.31 g/cm³ | 1.53 g/cm³ | 1.65–1.70 g/cm³ | ISO 1183-1:2019 |
| Tensile strength | 55–60 MPa | 130–145 MPa | 120–135 MPa | ISO 527-2:2012 |
| Flexural modulus | 2,500 MPa | 9,000–11,000 MPa | 8,500–10,000 MPa | ISO 178:2019 |
| HDT/A at 1.8 MPa | 55 °C | 205–215 °C | 195–210 °C | ISO 75-2:2013 |
| Notched Izod impact, 23 °C | 4–6 kJ/m² | 8–12 kJ/m² | 7–10 kJ/m² | ISO 180:2019 |
| UL 94 rating | HB | HB | V-0 at 1.6 mm typical | UL 94 |
The matrix is assembled from published processing and property guides for PBT compounds; it is provided for comparison and not as a substitute for 3330GVS certificate values.
On a reciprocating-screw injection-moulding machine with a clamp force of 800–3,500 kN and a general-purpose screw of 18:1–22:1 L/D, 3330GVS must be dried before processing. Residual moisture should be reduced to 0.02 wt% maximum under ISO 15512:2019 using a desiccant dryer with a dew point below -30 °C at 120 °C for 4–6 h. At ambient relative humidity above 60%, open material should be consumed within 30 min or returned to the dryer. Barrel temperature settings are typically 240–260 °C at the nozzle, 235–255 °C in the front zone, 220–240 °C in the centre zone, and 60–80 °C in the feed throat. Mould temperature should be maintained at 70–90 °C; lower mould temperatures reduce crystallinity and increase post-mould shrinkage, while higher values can extend cycle time and cause ejection difficulty in deep ribs.
Back pressure is set at 0.3–0.7 MPa, screw surface speed is held at 60–120 rpm, and hold pressure is typically 60–80% of peak injection pressure. A general-purpose screw with compression ratio of 2.0:1–2.5:1 and a wear-protected check ring is required because 30% glass fibre accelerates screw and barrel wear. Hot-runner manifold temperatures should not exceed 250 °C; dead spots in the manifold can retain stagnant melt and degrade the flame-retardant package. Production-scale troubleshooting of similar FR-PBT compounds has shown that black specks and inconsistent UL 94 ratings appear when melt residence time exceeds 5–6 min at melt temperatures above 250 °C. After an idle period, purging with 10–15 times barrel capacity is advisable before moulding test parts.
In multi-gated connector housings and relay bases with wall thickness of 0.5–0.8 mm, the melt front splits around core pins and produces weld lines where mechanical properties are lower than in the bulk. For 30% glass-fibre-reinforced PBT, thin sections orient glass fibres in the flow direction; the weld-line zone contains fibre-poor resin and exposed flame-retardant particles. Weld-line tensile strength is commonly 40–60% of the base material value, depending on melt temperature, mould temperature, and injection speed. Published data for 3330GVS in weld-line configurations is limited; injection-moulding trials with a pressure transducer at the melt front are required to determine local pressure at the weld-line position.
To reduce weld-line failure risk, the melt temperature should be held at 245–255 °C and the mould at 80–90 °C. Injection velocity should be increased to raise frictional heating, but shear heating above 1,000 s⁻¹ can fracture glass fibres and lower impact strength. A fill time of 0.5–1.5 s for thin-wall parts is typical for housing geometries. When hot-runner valve gates are used, sequential valve-gate control can move the weld line to a low-stress region; however, each valve-gate delay introduces a residence time increment that must remain below the 5 min total melt residence limit. Actual tooling validation should include short-shot analysis and weld-line tensile bars cut from moulded parts in accordance with ISO 527-2:2012 or ASTM D638-14.
For appliance and electrical distribution applications, the relevant test methods include IEC 60112:2020 for comparative tracking index, IEC 60695-2-11 for glow-wire flammability, and UL 94 for vertical burning classification. Flame-retarded PBT with 30% glass fibre typically records CTI values of 200–250 V; non-FR PBT-GF30 can exceed 400 V. CTI is strongly influenced by flame-retardant chemistry, glass sizing, and surface contamination; a value should not be transferred from another grade. Glow-wire ignition temperature is typically reported at 750–960 °C at thicknesses between 0.75 mm and 3.0 mm for FR-PBT grades, but grade-specific certification of 3330GVS is required.
| Property / compliance area | Reference method or regulation | Typical result / requirement for product class |
|---|---|---|
| Vertical burning classification | UL 94 | V-0 at 1.6 mm typical; thin-wall grading must be confirmed |
| Comparative tracking index | IEC 60112:2020 | 200–250 V |
| Glow-wire flammability | IEC 60695-2-11 | 750–960 °C depending on thickness |
| Restriction of hazardous substances | RoHS 2011/65/EU | Lead 0.1 wt%, cadmium 0.01 wt%, mercury 0.1 wt%, hexavalent chromium 0.1 wt%, PBB 0.1 wt%, PBDE 0.1 wt% |
| REACH SVHC | EC 1907/2006 | Supplier declaration required |
| Specimen preparation | ISO 294-1:2017 | Injection-moulded test specimens |
The product code does not identify the flame-retardant chemistry; therefore, the distinction between halogenated and halogen-free versions should not be inferred from the suffix unless the supplier datasheet explicitly states the chemistry. Halogenated FR-PBT grades typically require lower additive loading for V-0 but may show greater smoke density and corrosive gas release under fire conditions. Phosphorus-based or nitrogen-based synergists may alter CTI and thermal aging differently. If the end-use specification requires halogen-free composition under IEC 61249-2-21 or equivalent, a separate grade or written confirmation from Korea Engineering Plastics is required.
Water absorption at saturation is approximately 0.2–0.4 wt% at 23 °C for glass-reinforced PBT, which is lower than glass-reinforced polyamides but higher than unfilled PBT. This restricts use in hot-water contact applications; hydrolysis in the presence of water at continuous temperatures above 80 °C can reduce molecular weight over service life. Published data for this specific grade under hydrolytic aging is limited.
In relay bobbins, coil formers, and motor brush holders, 3330GVS is processed when the part must survive continuous operating temperatures near 120–140 °C and occasional contact with glowing or arcing electrical components. The glass-fibre reinforcement reduces creep and post-mould shrinkage; the flame-retardant package provides self-extinguishing after exposure to electrical arcs or glowing contacts. Processing on vertical insert moulding machines for brush holders requires the mould temperature to be held at 80 °C to minimise fibre-rich surfaces and to avoid premature solidification around metal inserts. Inserts should be preheated to 100–120 °C to reduce residual stress; otherwise cracking at the metal-polymer interface can occur within 500–1,000 h of thermal cycling. Published data for 3330GVS under insert-moulding conditions are limited, so thermal cycling tests should follow the end-use specification and the supplier’s processing guide.