Korea Engineering Plastics Kepex Pbt Gf15 3315gfs

Korea Engineering Plastics KEPEX® PBT+GF15% 3315GFS

    • Product Name: Korea Engineering Plastics KEPEX® PBT+GF15% 3315GFS
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 435015
    Density 1.41 g/cm³
    Glassfibercontent 15%
    Tensilestrength 100 MPa
    Elongationatbreak 2.5%
    Flexuralmodulus 5500 MPa
    Notchedizodimpactstrength 5 kJ/m²
    Heatdeflectiontemperatureat1 82mpa 205 °C
    Meltingpoint 225 °C
    Waterabsorption24h 0.05%
    Moldshrinkage 0.3–0.6%
    Dielectricstrength 20 kV/mm
    Volumeresistivity 1×10^15 Ω·cm

    As an accredited Korea Engineering Plastics KEPEX® PBT+GF15% 3315GFS factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing KEPEX® PBT+GF15% 3315GFS is typically supplied in 25 kg moisture-barrier bags, 40 bags per pallet (1,000 kg).
    Container Loading (20′ FCL) A 20′ FCL container loaded with palletized 25 kg bags of KEPEX® PBT+GF15% 3315GFS, kept dry and secured for export.
    Shipping KEPEX® PBT+GF15% 3315GFS is a non-hazardous plastic resin compound and is not regulated for transport (no UN number, hazard class, or packing group under ADR/RID/IMDG/IATA). Ship in dry, sealed bags/containers, protected from moisture, heat, and sunlight; avoid dust and comply with local regulations.
    Storage Store KEPEX® PBT+GF15% 3315GFS in a cool, dry, well-ventilated area, away from direct sunlight, heat sources, moisture, and incompatible chemicals such as strong acids or oxidizers. Keep containers tightly closed and use original packaging. Avoid dust generation and contamination. Follow local regulations and the manufacturer’s safety data sheet for additional handling and storage requirements.
    Shelf Life Shelf life is approximately 24 months when stored dry, below 30°C, in original sealed packaging, protected from moisture and UV.
    Free Quote

    Competitive Korea Engineering Plastics KEPEX® PBT+GF15% 3315GFS prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Korea Engineering Plastics supplies KEPEX® PBT+GF15% 3315GFS as a 15 wt% glass-fibre-reinforced polybutylene terephthalate injection-moulding compound. The grade is positioned for dimensionally stable engineering parts requiring higher stiffness and heat resistance than unfilled PBT while retaining lower melt viscosity and reduced anisotropic shrinkage compared with PBT grades containing 20 wt% or 30 wt% glass fibre. The product code 3315GFS denotes the supplier-specific base-resin series and glass-fibre reinforcement; released lot-specific certificates control the final product specification.

    Because no single published datasheet replaces the supplier’s lot-specific quality documents, the following numerical ranges are representative values for commercial PBT compounds with a nominal 15 wt% glass-fibre loading. Final part design should be validated against the actual product specification issued by Korea Engineering Plastics for 3315GFS.

    The class-level mechanical and thermal profile is summarised in Table 1. Published data for this specific configuration is limited to supplier-controlled values, and the ranges below are drawn from general industrial data for PBT+GF15% grades.

    Property Test standard Unit Representative range
    Density ISO 1183-1 g/cm³ 1.41–1.43
    Tensile stress at break ISO 527-1/-2 MPa 90–110
    Tensile strain at break ISO 527-1/-2 % 2.0–4.0
    Flexural modulus ISO 178 MPa 5000–6000
    Charpy notched impact strength at 23 °C ISO 179-1/1eA kJ/m² 4–6
    Heat deflection temperature at 1.8 MPa ISO 75-2/A °C 190–200
    Melt volume-flow rate at 250 °C/2.16 kg ISO 1133 cm³/10 min 15–25
    Mould shrinkage, flow/transverse ISO 294-4 % 0.3–0.6 / 0.6–1.1

    What Processing Envelope Is Observed with 3315GFS During Injection Moulding?

    In a desiccant hopper-dryer operating at a dew point no higher than -30 °C, the granulate is dried at 120 °C for 3–4 h until residual moisture falls below 0.02 wt%. Moisture above this threshold hydrolyses the ester linkage during plastication, reducing molecular weight and causing measurable loss of tensile strength and impact resistance. Drying must be repeated if storage exceeds 4 h in an unheated hopper at ambient relative humidity above 60 %.

    Barrel temperature settings are typically maintained between 240 °C and 260 °C, with the rear zone near 230–240 °C, the centre zone near 240–250 °C, the front zone near 250–260 °C, and the nozzle near 245–255 °C. Melt temperatures above 270 °C accelerate thermal degradation and increase the formation of free formaldehyde and tetrahydrofuran. Tool temperature is held between 60 °C and 90 °C to obtain sufficient crystallinity without promoting post-mould warpage in glass-filled sections.

    Screw geometry with a length-to-diameter ratio of 20:1 to 24:1 and a compression ratio of 2.5:1 to 3.5:1 is used for homogeneous glass distribution. Back pressure is typically kept at 0.3–0.5 MPa; excessive back pressure raises melt temperature and reduces fibre length. Production-scale twin-screw compounding and injection moulding lines exhibit batch-to-batch variance in fibre-length distribution when regrind is reintroduced or when screw speed and residence time are not controlled. A short-shot study is required on multicavity tools because glass-fibre orientation produces cavity-to-cavity fill imbalance and anisotropic weld-line formation.

    Electrical-Connector Housing Applications Under Thermal Load

    For under-hood connector bodies, relay bases, sensor housings, bobbin carriers, and encapsulated power-distribution components, a 15 wt% glass-fibre PBT offers a balance of heat deflection, dimensional stability, and flow length. Connector housings moulded from 3315GFS require validation under the relevant electrical and fire-hazard standards: IEC 60695-2-11 glow-wire testing at the final wall thickness, IEC 60112 comparative tracking index, and IEC 62631-3-1 volume resistivity measurements. Because KEPEX 3315GFS is not inherently flame-retarded in the absence of a designated flame-retardant package, compliance with glow-wire ignition or flammability endpoints must be confirmed for each application.

    Low moisture absorption is a controlling variable in electrical applications. PBT absorbs less than 0.1 wt% water at 23 °C after 24 h under ISO 62, whereas comparable polyamide grades absorb one order of magnitude more. This difference reduces the shift in dielectric performance and dimensional change in humid service. At the same time, PBT is susceptible to hydrolytic degradation in hot aqueous environments above 60 °C, and contact with alkaline cleaners at elevated temperature should be avoided.

    In connector applications with snap-fit arms or thin latch features, weld-line strength is a critical risk. In glass-reinforced PBT, weld lines typically exhibit a strength reduction of roughly 40 % relative to the bulk value because fibres align parallel to the weld plane rather than across it. Gate placement must be configured so that weld lines are moved away from snap-fit roots, latch engagement surfaces, and pressure-loaded bosses. Where this is not possible, finite-element orientation models and short-shot verification on production tooling are required to establish maximum assembly strain.

    Dimensional control in PBT+GF15% is governed by anisotropic shrinkage. The mould shrinkage in flow direction is commonly 0.3–0.6 %, while the transverse value is 0.6–1.1 %. This anisotropy necessitates separate adjustment of cavity dimensions in the flow and transverse axes. For close-tolerance connector slots and terminal insertion features, steel-safe tool design and post-mould metrology using ISO 294-4 reference specimens are applied before final tool approval.

    When a 15% Glass-Fibre Grade Is Preferred Over 30% Filled PBT

    Compared with PBT+GF30%, the 15 wt% grade reduces melt viscosity, improves surface appearance, lowers density, and decreases the probability of fibre-rich surface defects near gates and ribs. The trade-off is lower flexural modulus and lower heat deflection temperature under load. A 30 wt% glass-fibre PBT typically raises flexural modulus to approximately 9000–10000 MPa, while the 15 wt% grade remains near 5500 MPa. Where a component requires maximum stiffness or reduced creep, a higher glass content is selected; where thin-wall fill, lower warpage, or better weld-line appearance controls the design, 3315GFS is preferred.

    Relative to PA66+GF15%, the PBT-based grade provides less moisture uptake and more stable mechanical and electrical properties across humid environments. Polyamide 66 with 15 wt% glass fibre exhibits greater toughness after moisture conditioning and higher short-term heat resistance, but its dimensions and stiffness vary more strongly with water content. In dry-as-moulded automotive connectors exposed to engine-bay humidity, PBT+GF15% reduces the shift in terminal retention force and latch stiffness. In applications requiring repeated hot-water or glycol exposure, polyamide or aliphatic-aromatic copolyester may still be required depending on the chemical environment.

    Unfilled PBT offers superior unnotched impact behaviour and isotropic shrinkage, but its flexural modulus is approximately 2500 MPa and its heat deflection temperature at 1.8 MPa is below 60 °C. The addition of 15 wt% glass fibre raises stiffness and heat resistance sufficiently for under-hood structural use while remaining easier to process than PBT+GF30%. This is the central positioning of KEPEX PBT+GF15% 3315GFS.

    Reground material should be limited to dry, uncontaminated sprues and runners. Reintroduction of high levels of glass-filled regrind reduces fibre length and notched impact strength; batch-to-batch variation can be observed on production lines if the regrind fraction exceeds 20 wt% without melt-flow compensation. When regrind is used, the dried blend should be checked for moisture before moulding because fibre-filled PBT absorbs water more rapidly than pelletised virgin material with lower surface area.

    Process capability studies on multicavity tools should include cavity-to-cavity fill imbalance, gate freeze time, and post-mould warpage as monitored variables. The stiffening effect of glass fibre can mask packing-related shrinkage variation during visual inspection, but residual stress levels can remain high enough to cause delayed cracking at metal inserts, ultrasonic welds, or press-fit terminals.

    Top